• 제목/요약/키워드: Surface films

검색결과 4,898건 처리시간 0.033초

Transparent Conductive Oxides for Display Applications

  • Szyszka, B.;Ruske, F.;Sittinger, V.;Pflug, A.;Werner, W.;Jacobs, C.;Kaiser, A.;Ulrich, S.
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2007년도 7th International Meeting on Information Display 제7권1호
    • /
    • pp.181-185
    • /
    • 2007
  • We report on our material and process research on ZnO:Al films and on our investigations on wet chemical etching using a variety of etching solutions. We achieve resistivity as low as $750{\mu}{\Omega}cm$ for ZnO:Al films with film thickness of 140 nm. Etching with phosphorous acid allows for accurate fine patterning of the ZnO:Al films on glass substrates.

  • PDF

TiN 코팅층 집합조직의 변화에 따른 마찰, 마멸과 내부식 특성 (The Characteristics of Frictional Behavior, Wear and Corrosion Resistance of Textured TiN Coated Layer)

  • 김희동;김인수;성동영;이민구
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 춘계학술대회논문집
    • /
    • pp.99-104
    • /
    • 2003
  • TiN coated films show a good mechanical properties, high thermal properties and wear, erosion and corrosion resistance and are widely used as a coating materials in tools, ornaments, parts and semiconductors. In spite of these good properties, the fracture of TiN coated films occur during use. The fracture of TiN thin films is related to their microstructure. Especially, the life of TiN coated layer is related to the texture of the TiN films. One researcher suggested that the corrosion and erosion resistance of the TiN thin films is related to a uniform and dense structure of films. In this study, we studied the relationships between textures and friction coefficient, erosion and corrosion in TiN coated films. The flatness of (115) texture surface of TiN thin films is flatter than that of (111) texture surface. The friction coefficient of (115) texture surface of TiN thin films is similar with that of (111) texture surface. The wear resistance of (115) texture surface of TiN thin films is better than that of (111) texture surface. The erosion and corrosion resistance of (115) texture surface of TiN thin films is better than that of (111) torture surface. As well as texture, the wear, erosion and corrosion of TiN thin films has to consider defects such as pinholes, cracks, surface roughness and open columnar structure. The life of TiN coated products is influenced by the properties of wear, erosion, and corrosion resistance of TiN thin films and is related to texture of TiN coated films, density of pinholes and cracks, density of structure, and surface flatness.

  • PDF

Surface Hardness Measurement of Anodic Oxide Films on AA2024 based an Ink-Impregnation Method

  • Moon, Sungmo;Rha, Jong-joo
    • 한국표면공학회지
    • /
    • 제53권2호
    • /
    • pp.80-86
    • /
    • 2020
  • This paper is concerned with type of imperfections present within the anodic oxide films on AA2024 and surface hardness of the anodic film measured after ink-impregnation. The anodic oxide films were formed for 25 min at 40 mA/㎠ and 15±0.5℃ and 300 rpm of magnet stirring rate in 20% sulfuric acid solution. The ink-impregnation allows clear observations of not only the imperfections within the anodic oxide films but also an indentation mark on the oxide film surface made by a pyramidal-diamond penetrator for the hardness measurement. There were observed four different regions in the anodic oxide films on AA2024 and the surface hardness of the anodic oxide films appeared to be crucially dependent on the type of defects, showing 60~100 Hv on the oxide surface region I with large size black defect, 100~140 Hv on the oxide surface region II with large size grey defect, 140~170 Hv on the oxide surface region III with mall size black and/or grey defects and 170~190 Hv on the oxide surface region IV without defects. The pyramidal indentation marks were observed to be distorted in the regions with a large size black and grey defects, while no distortion of the indentation mark was observed in the regions with small size defects and without visible defects.

졸-겔 공정에 의해 제조된 ITO (Indium-Tin-Oxide) 박막의 표면처리 (Surface Treatment of ITO (Indium-Tin-Oxide) thin Films Prepared by Sol-Gel Process)

  • 정승용;윤영훈;연석주
    • 한국세라믹학회지
    • /
    • 제44권6호
    • /
    • pp.313-318
    • /
    • 2007
  • ITO (Indium-tin oxide) thin films have been prepared by a sol-gel spinning coating method and fired and annealed in the temperature range of $450-600^{\circ}C$. The XRD patterns of the films indicated the main peak of (222) plane and showed higher crystallinity with increasing an annealing temperature. The surface of the ITO thin films were treated with 0.1 N HCl 20% solution at room temperature. The effects of surface treatment on electrical properties and surface morphologies of the ITO films were investigated with the results of sheet resistance and FE-SEM, AFM images. The samples, subsequently treated with acidic solution for 40 sec showed the sheet resistance of $0.982\;k{\Omega}/square$. The surface treatment using acidic solution diminished the RMS (root mean square) value and the residual carbon content of the ITO films. It seemed that the acid-cleaning of the ITO thin films lead to the decrease of surface roughness and sheet resistance.

Anodic Oxide Films Formed on AZ31 Magnesium Alloy by Plasma Electrolytic Oxidation Method in Electrolytes Containing Various NaF Concentrations

  • Moon, Sungmo;Kwon, Duyoung
    • 한국표면공학회지
    • /
    • 제49권3호
    • /
    • pp.225-230
    • /
    • 2016
  • The present work was conducted to investigate the effects of NaF concentration in phosphate and silicate-containing alkaline electrolyte on the morphology, thickness, surface roughness and hardness of anodic oxide films formed on AZ31 Mg alloy by plasma electrolytic oxidation (PEO) method. The PEO films showed flat surface morphology with pores in the absence of NaF in the electrolyte, but nodular features appeared on the PEO film surface prepared in NaF-containing electrolyte. Numerous pores ranging from 1 to $20{\mu}m$ in size were observed in the PEO films and the size of pores decreased with increasing NaF concentration in the electrolyte. Surface roughness and thickness of PEO films showed increases with increasing NaF concentration. Hardness of the PEO films also increased with increasing NaF concentration. It was noticed that hardness of inner part of the PEO films is lower than that of outer part of them, irrespective of the concentration of NaF. The low hardness of PEO films was explained by the presence of a number of small size pores less than $2{\mu}m$ near the PEO film/substrate interface.

고체윤활용 $MoS_2$Bonded Film의 마찰마모 특성에 관한 실험적 고찰 (Experimental Studies on Friction and Wear of the Solid Lubricating $MoS_2$ Bonded Films)

  • 공호성;윤의성;한홍구;권오관
    • Tribology and Lubricants
    • /
    • 제12권1호
    • /
    • pp.15-21
    • /
    • 1996
  • Friction and wear properties of MoS$_2$ bonded films were studied using the Falex testing machine, and their properties were evaluated in terms of the life and the load carrying capacity of the films. MoS$_2$ bonded films were formulated from the mixtures of MoS$_2$ solid particles and epoxyphenol resin, and they were applied onto AISI 4130 steel surface by dipping method to form lubricating bonded films. The results of the life and the load carrying capacity of the films showed that films were mainly affected by the surface temperature arisen from the frictional heat at the contact surface. To obtain enhanced tribological properties of the films, various combinations of solid lubricants and additives with a basic polymer resin were attempted and evaluated. The effects of surface pretreatment, such as sand blast or Zn-phosphating, were also investigated.

SPUTTERING법에 의해 성장시킨 PZT박막의 표면 분석 (Surface Analysis of PZT Film Prepared by Sputting Method)

  • 김영관;박주상;추정우;손병청;이전국
    • 한국진공학회지
    • /
    • 제5권2호
    • /
    • pp.107-112
    • /
    • 1996
  • Thin films of $Pb(Zr_xTi_{1-x})O_3$)PZT) were grown on $Pt/SiO_2/Si(100)$ at various temperatures by RF magnetron sputtering method. Surface morphology of these films were studied by using Atomic Force Microscopy(AFM). These films were also analyzed by using Atomic Force Microscopy(AFM). These films were also analyzed by using X-ray photoemission spectroscopy(XPS) for determining their chemical composition and their depth profile. It was found that the films grown at the substrated temperature of $300^{\circ}C$ have much more smooth surface characteristics in comparison to those films grown at room temperature, which may be explained in terms of surface mobility of ad-atoms such as Pb. It was also found that Pb enrichment in the near surface region enhanced for the films grown at higher substate temperature.

  • PDF

Cemented Carbide기판의 레이저 표면 개질이 다이아몬드 박막의 접합력에 미치는 영향 (Effect of Laser Surface Modification of Cemented Carbide Substrates on the Adhesion of Diamond Films)

  • 이동구
    • 열처리공학회지
    • /
    • 제13권3호
    • /
    • pp.170-176
    • /
    • 2000
  • A novel method for improving the adhesion of diamond films on cemented carbide tool inserts has been investigated. This method is based on the formation of a compositionally graded interface by developing a microrough surface structure using a pulsed laser process. Residual stresses of diamond films deposited on laser modified cemented carbides were measured as a function of substrate roughness using micro-Raman spectroscopy. The surface morphology and roughness of diamond films and cemented carbides were also investigated at different laser modification conditions. It was found that the increasing interface roughness reduced the average residual stress of diamond films, resulting in improved adhesion of diamond films on cemented carbides.

  • PDF

Adhesion of Human Osteoblasts Cell on CrN Thin Film Deposited by Cathodic Arc Plasma Deposition

  • Pham, Vuong-Hung;Kim, Sun-Kyu
    • 한국표면공학회지
    • /
    • 제42권5호
    • /
    • pp.203-207
    • /
    • 2009
  • Interaction between human osteoblast (hFOB 1.19) and CrN films was conducted in vitro. CrN films were produced by cathodic arc plasma deposition. The surface was characterized by atomic force microscopy (AFM). CrN films, glass substrates and TiN films were cultured with human osteoblasts for 48 and 72 hours. Actin stress fiber patterns and cell adhesion of osteoblasts were found less organized and weak on CrN films compared to those on the glass substrates and the TiN films. Human osteoblasts also showed less proliferation and less distributed microtubule on CrN films compared to those on glass substrates and TiN films. Focal contact adhesion was not observed in the cells cultured on CrN films, whereas focal contact adhesion was observed well in the cells cultured on glass substrates and TiN films. As a result, the CrN film is a potential candidate as a surface coating to be used for implantable devices which requires minimal cellular adhesion.

표면 플라즈몬 공명을 이용한 유전체 박막의 광학 상수 결정과 형상 측정 (Determination of Optical Constants and Observation of Patterns of Dielectric Thin Films Using Surface Plasmon Resonance)

  • 황보창권;김성화;이규진
    • 한국광학회지
    • /
    • 제3권4호
    • /
    • pp.205-216
    • /
    • 1992
  • 공명각과 비공명각에서 각각 표면 플라즈몬의 전기장 분포를 계산하고 두 경우를 비교하였다. 표면 플라즈몬 공명의 응용으로서 (1) 은박막 위에 덧증착한 얇은 ZnS 박막의 광학 상수를 두께가 증가함에 따라 측정하였고, (2) 발산하는 입사파를 이용하여 은박막 위에 덧증착한 두께가 서로 다른 SiO 박막에 의한 4개의 표면 플라즈몬 공명을 한 화면에서 관측하였으며 (3) 평행광을 이용하여 은박막 위에 덧증착한 격자 모양의 SiO박막과 문자 "가" 모양의 SiO 박막의 형상을 측정하였다.

  • PDF