Evaluation of Setting Delay in Mortar Adding Superplasticizer Using Electrical Resistivity Measurement (전기비저항 측정법을 이용한 유동화 모르타르의 응결 지연 현상 평가)

  • Lee, Hanju;Yim, Hong Jae
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.22 no.6
    • /
    • pp.9-15
    • /
    • 2018
  • According to the development and use of self-consolidating concrete in field, interest in material properties of early-age concrete is rising. Setting time with hydration process of cement is one of significant indicator to evaluate the early-age material properties of concrete, various nondestructive methods including penetration resistance measurement have been proposed to estimate setting time. This study performed an experimental approach to evaluate setting time delay in mortar adding superplasticizer using electrical resistivity measurement. For this purpose, total nine types of mortar samples were prepared, and its electrical resistivity was monitoring during 24h after mixing. From the experimental result, rising time of electrical resistivity was used to evaluate setting delay of mortar, and penetration resistance was also measured for comparison. In addition, dynamic elastic modulus and compressive strength of 1day mortar were measured to investigate a possibility the use of electrical resistivity measurement for evaluation of early-age material properties.

Fluidity Performance Evaluation of Low Viscosity Typed Superplasticizer for Cement-Based Materials Incorporating Supplementary Cementitious Materials (혼화재료를 치환한 시멘트 계열 재료에 대한 저점도형 고성능 감수제의 유동 성능 평가)

  • Son, Bae-Geun;Lee, Hyang-Seon;Lee, You-Jeong;Han, Dong-Yeop
    • Journal of the Korea Institute of Building Construction
    • /
    • v.19 no.3
    • /
    • pp.219-228
    • /
    • 2019
  • The aim of the research is to provide a fundamental data of low viscosity typed superplasticizer (SP) on cement-based materials incorporating various supplementary cementitious materials (SCMs). As a relatively new product, low-viscosity typed SP has introduced for high performance concrete with high viscosity due to its high solid volume fraction with various SCMs. However, there are not enough research or reports on the performance of the low viscosity typed SP with cement-based materials incorporting SCMs. hence, in this research, for cement paste and mortar, fluidity and rheological properties were evaluated when the mixtures contained various SCMs such as fly ash, blast furnace slag, and silica fume. From the experiment conducted, it was checked that the low viscosity typed superplasticizer decreased the plastic viscosity of the mixture as well as the yield stress. From the results of this research, it is expected to contribute on introduction of new type SP for high performance concrete or high-viscous cementitious materials.

The influencing factors for the strength enhancement of composite materials made up of fine high-calcium fly ash

  • Olga M. Sharonova;Leonide A. Solovyov;Alexander G., Anshits
    • Advances in concrete construction
    • /
    • v.16 no.3
    • /
    • pp.169-176
    • /
    • 2023
  • The aim of the study was to establish the influence of particle size, chemical and phase composition of fine microspherical high-calcium fly ash (HCFA), as well as superplasticizer content on the strength of cementless composite materials based on 100% HCFA and mixtures of HCFA with Portland cement (PC). For the initial HCFA fractions, the particle size distribution, chemical and quantitative phase composition were determined. The compressive strength of cured composite materials obtained at W/B 0.4 and 0.25 was determined at a curing time of 3-300 days. For cementless materials, it was found that a change in the particle size d90 from 30 ㎛ (fraction 3) to 10 ㎛ (fraction 4) leads to an increase in compressive strength by more than 2 times. Compressive strength increases by at least another 2.2 times with the addition of Melflux 5581F superplasticizer (0.12%) and at W/B 0.25. The HCFA-PC blends were investigated in the range of 60-90% HCFA and the maximum compressive strength was found at 80% HCFA. On the basis of 80% HCFA-20% PC blend, the samples of ultra-high strength (108 and 150 MPa at 28 and 100 days of hardening) were obtained with the addition of 0.3% Melflux 5581F and 5% silica fume. The quantitative phase composition was determined for composite materials with a curing age of 28 days. It has been established that in a sample with ultra-high strength, a more complete transformation of the initial phases of both HCFA and PC occurs as compared to their transformation separately.

The Performance of Concrete Used High Strength Development Polycarboxylate Superplasticizer (고강도용 폴리카르본산계 고성능 감수제가 사용된 콘크리트의 성능)

  • Lee, Wan-Jo;Kang, Sung-Gu;Hwang, In-Dong;Lee, Jae-Yong;Park, Sung;Chug, Yun-Joong
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.3 s.274
    • /
    • pp.182-187
    • /
    • 2005
  • There are many kinds of polycarboxylate superplasticizer as a functional classification which are introduced to domestic; Water Reducer, Retention, Ultra High Strength Superplasicizer. These are showed different physical behaviors because of the difference in the chemical system and the manners after cement mixing. In the case of water reducer, when $1.2\% of cement weight used, water reducing which is over $30\% is observed, but it take with segregation and the reduction of slump flow shows over 30 cm after 45 min of concrete produce. In the case of retention, when the same quantity used, water reducing which is about $25\% is observed and slump flow which is up to 45 min shows under 15 cm. And in the case of ultra high strength, when $1.2\% of cement weight used, water reducing which is over $30\% is observed, and slump flow which is up to 45 min recorded fewer than 15 cm. Compressive strength of ultra high strength superplasticizer has take effect of early age strength, and in the condition of specific mixing, 18 h-compressive strength is insured for more than $60\;Kgf/cm^2$ and 24 h-compressive strength is insured for more than $80\;Kgf/cm^2$.

The Fluidity of High Flowing Concrete According to the Component Ratio of Superplasticizer (고성능감수제 구성비율에 따른 고유동콘크리트의 유동특성)

  • Kim Moo-Han;Kim Yong-Ro;Kim Jae-Hwan;Ho Jang-Jong;Lee Tae-Hee
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.2 s.80
    • /
    • pp.147-154
    • /
    • 2004
  • It is the aim of this study to propose the fundamental data for the establishment of the application and qualify standard of the mixed type superplasticizer after investigating and comparing the fluidity of high flowing concrete according to the component ratio of superplasticizer such as naphthalene sulfonated and melamine sulfonated. The results of this study were shown as the followings; 1) The fluidity and adsorption ratio of cement-paste were improved according to the increasing of naphthalene sulfonated component ratio, and apparent viscosity of cement-paste was improved according to the Increasing of melamine sulfonated component ratio. 2) In case of using the granulated blast-furnace slag, the fluidity of cement-paste was considerably good and the adsorption ratio was decreased and in case of using fly-ash, the apparent viscosity and adsorption ratio of cement-paste were improved. 3) The dispersive capacity performance of concrete can be improved by means of the increasing of naphthalene sulfonated component ratio. Also the viscosity and early strength can be improved by means of the increasing of melamine sulfonated component ratio.

Analysis of the Effect of Superplasticizer combined CASB on Ultra High Strength Mortar and Concrete Using Mineral Admixture (광물질 혼화재 사용 초고강도 모르타르 및 콘크리트에 CASB 화합 고성능감수제의 효과분석)

  • Han, Cheon-Goo;Yoo, Seung-Yeup
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.1
    • /
    • pp.72-79
    • /
    • 2011
  • This study is performed to analyze the effects of CASB by applying the superplasticizer combined CASB on the ultra high strength mortar and concrete that uses different mineral admixture depending on whether the silica fume was used and the results are summarized below. From the characteristics of Fresh mortar and concrete, the fluidity was lower in B2-CASB than B2-PC from the mixing of CASB and based on the viscosity of the mortar and concrete in the binary proportion but in the ternary proportion, B3-CASB showed a larger fluidity than B3-PC because of a reduction in the restriction level due to the effects of an improvement of particle size distribution. The compression strength was higher in ternary proportion than in binary proportion and higher in CASB than in PC from the characteristics of hardening mortar and concrete and this is analyzed as a result of increased minuteness from the calcium silicate hydrates produced from the pozzolan reaction of a mineral admixture, SF, and also the charging effects of capillary pore of CASB. Overall, when using the nanomaterial, CASB in combination with a superplasticizer, the fluidity and the strength aspects of the ternary proportion of ultra high strength mortar and concrete with silica fume may be improved to a higher quality.

  • PDF

Compressive, shear and torsional strength of beams made of self-compacting concrete

  • Mazloom, Moosa;Saffari, Amirali;Mehrvand, Morteza
    • Computers and Concrete
    • /
    • v.15 no.6
    • /
    • pp.935-950
    • /
    • 2015
  • The aim of this study is to provide experimental data regarding the compressive, shear and torsional strength of self-compacting concrete (SCC) used in rectangular beams, and then comparing the results with the equations presented by the CSA A23.3-04 and ACI 318-11. In fact, the gathered information in this field is quite useful for calibrating the computer models of other researchers. The other goal of this study was to investigate the effects of silica fume and superplasticizer dosages on the mechanical properties of SCC. In this research, SCC is made based on 16 different type mixing layout. Also two normal concrete (NC) or vibrating concrete are constructed to compare the results of SCC and NC. This work concentrated on concrete mixes having water/binder ratios of 0.45 and 0.35, which contained constant total binder contents of $400kg/m^3$ and $500kg/m^3$, respectively. The percentages of silica fume that replaced cement were 0% and 10%. The superplasticizer dosages utilized in the mixtures were 0.4%, 0.8%, 1.2% and 1.6% of the weight of cement. Beam dimensions used in this test were $30{\times}30{\times}120cm^3$. The results of this research indicated that shear and torsional strength of SCC beams to be used in computer models can be calculated utilizing the equations presented in CSA A23.3-04 and ACI 318-11.

A Fundamental Study on the Estimation of Construction Cost of High Fluidity Concrete Applying Flowing Concrete Method (유동화공법에 의해 제조한 고유동 콘크리트의 원가분석에 관한 기초적 연구)

  • 한민철;손성운;오선교;김성수;한천구
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2002.11a
    • /
    • pp.99-102
    • /
    • 2002
  • This paper discusses the estimation of construction cost of high fluidity concrete using segregation reducing type superplasicizer with 350kgf/cm2 of design strength and 60$\pm$5cm of slump flow in order to verify the cost down effect of high fluidity concrete compared with that of plain concrete with 350kgf/cm2 of design strength and 18cm of slump and with 210kgf/cm2 of design strength and 15cm of slump. According to research, under same strength levels, although material cost of high fluidity concrete is somewhat higher than that of plain concrete due to segregation reducing type superplasticizer, labor cost and equipment cost of high fluidity concrete is cheaper than that of plain concrete. However, based on the strength differences, high fluidity concrete shows lower material cost, labor cost and equipment cost than that of plain concrete due to decreasing in size of member and re-bar caused by high strength development of concrete.

  • PDF

Cost effective optimal mix proportioning of high strength self compacting concrete using response surface methodology

  • Khan, Asaduzzaman;Do, Jeongyun;Kim, Dookie
    • Computers and Concrete
    • /
    • v.17 no.5
    • /
    • pp.629-638
    • /
    • 2016
  • Optimization of the concrete mixture design is a process of search for a mixture for which the sum of the cost of the ingredients is the lowest, yet satisfying the required performance of concrete. In this study, a statistical model was carried out to model a cost effective optimal mix proportioning of high strength self-compacting concrete (HSSCC) using the Response Surface Methodology (RSM). The effect of five key mixture parameters such as water-binder ratio, cement content, fine aggregate percentage, fly ash content and superplasticizer content on the properties and performance of HSSCC like compressive strength, passing ability, segregation resistance and manufacturing cost were investigated. To demonstrate the responses of model in quadratic manner Central Composite Design (CCD) was chosen. The statistical model showed the adjusted correlation coefficient R2adj values were 92.55%, 93.49%, 92.33%, and 100% for each performance which establish the adequacy of the model. The optimum combination was determined to be $439.4kg/m^3$ cement content, 35.5% W/B ratio, 50.0% fine aggregate, $49.85kg/m^3$ fly ash, and $7.76kg/m^3$ superplasticizer within the interest region using desirability function. Finally, it is concluded that multiobjective optimization method based on desirability function of the proposed response model offers an efficient approach regarding the HSSCC mixture optimization.

Improvement of the Early Age Strength of Low Cement Concrete Using High Volume Mineral Admixture

  • Park, Jong-Ho;Kim, Yong-Ro;Song, Young-Chan;Song, Dong Yub;Kim, Gyu-Yong
    • Journal of the Korea Institute of Building Construction
    • /
    • v.12 no.6
    • /
    • pp.566-574
    • /
    • 2012
  • To address the problem of global warming, consumption of cement, the main material of concrete, should be decreased. Unfortunately, when industrial by-products are used in large quantities as admixture, the early age strength of concrete will be decreased, reducing its viability for use in concrete structures. Therefore, in this study, the application of an ionization accelerator and alkaline activator as addition agent of superplasticizer were investigated to secure a similar early age strength to that of normal concrete, thus increasing the viability of low cement concrete. Through the investigation, it was found that specimens that used a combination of Alkaline-activator (Na2Sio3) and ionization accelerator (Amine) had the highest early and long-age compressive strength. From this, we can determine an appropriate range of application of superplasticizer to improve early-age compressive strength of low cement concrete.