• 제목/요약/키워드: Superconducting phase

검색결과 424건 처리시간 0.021초

(BiPb)SrCaCuOx계에서 소결시간에 따른 조성과 초전도 성질의 변화 (Sintering Period Dependence of Composition and Superconducting Properties of (BiPb)SrCaCuOx System)

  • 박성;임호빈
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1988년도 추계학술대회 논문집
    • /
    • pp.98-101
    • /
    • 1988
  • The material system (Bi$\sub$0.7/Pb$\sub$0.3/)Sr$_1$Ca$_1$Cu$\sub$1.8/Ox forms, at 845$^{\circ}C$, two major phases having a high Tc(100K) and a low Tc(∼70K) both of which consists of platelets and a non-superconducting minor phase which has rod-like shape and isolated by the major phases. As the sintering period increases, the amount of high Tc phase increases accompanying the decrease in low Tc phase while the amount of the non-superconducting phase is sintering period independent, resulting in a superconductor with Tc of 100K. Changes in compositions of each phase also occur during sintering due to evaporation of bismuth and lead.

  • PDF

Bi-Pb-Sr-Ca-Cu-O 초전도상의 안정화에 미치는 소결시간의 영향 (The Effect of Sintering Time on the Stabilization of the Bi-Pb-Sr-Ca-Cu-O Superconducting Phase)

  • 형경우;박성호;이두원;한태종;최범식;김창은
    • 한국세라믹학회지
    • /
    • 제29권2호
    • /
    • pp.95-100
    • /
    • 1992
  • A high-Tc superconducting phase was obtained using long sintering time of 210 hours. From XRD and SEM analyses, it could be confirmed that the particles were plate phase, of which the structure is tetragonal system with lattice parameter a=b=5.44${\AA}$, C=37.18${\AA}$. Resistance and current density measurements were carried out using 4 probe method. The experimental data revealed that the stable high-Tc superconducting phase was easily formed by addition of Pb to Bi-system. Therefore, we could find the sintering condition to synthesis the system having the largest fraction of high Tc phase.

  • PDF

고온 초전도 한류기가 설치된 전력 시스템의 안정도 해석 (The Stability Analysis of Power System Installed Superconducting Fault Current Limiter)

  • 이승제;이찬주;고태국
    • 대한전기학회논문지:전기기기및에너지변환시스템부문B
    • /
    • 제48권5호
    • /
    • pp.227-232
    • /
    • 1999
  • The stability of Power system installed Hi-Tc Superconducting Fault Current Limiter(SFCL) is analyzed as a process of developing SFCL. For investigation, a simple mimic system(only one generator) is assumed and then the circuit with SFCL in that system is solved for transient performance. In case the SFCL is installed in the power system, it protected synchronization more effectively both in symmetrical 3-phase fault and single phase line to ground fault in that the machine remains in synchronism for the more time than of without superconducting fault current limiter. It shows that the superconducting fault current limiter not only limits fault current but also protest synchronism. So for design of this SFCL, its synchronism protection property must be considered.

  • PDF

이중퀜치를 이용한 삼상변압기형 한류기의 고장전류제한 동작 분석 (Analysis on Fault Current Limiting Operation of Three-Phase Transformer Type SFCL Using Double Quench)

  • 한태희;고석철;임성훈
    • 한국전기전자재료학회논문지
    • /
    • 제35권2호
    • /
    • pp.184-189
    • /
    • 2022
  • In this paper, the fault current limiting operations of three-phase transformer type superconducting fault current limiter (SFCL) using double quench, which consisted of E-I iron core with three legs wound by primary and secondary windings and two superconducting modules (SCMs), were analyzed according to three-phase ground fault types. To verify the effective operation of the three-phase transformer type SFCL using double quench, the test circuit for three-phase ground faults was constructed, and the fault current tests were carried out. Through analysis on the fault current test results, the different fault current limiting characteristics of three-phase transformer type SFCL using double quench from three-phase transformer type SFCL using three SCMs were discussed.

초음파 분무열분해에 의한 Bi-Pb-Sr-Ca-Cu-O의 미분체 제조 (Direct Preparation of fine Powders of Bi-Pb-Sr-Ca-Cu-O by Ultrasonic Spray Pyrolysis)

  • 주명희;박도순;김윤수
    • 한국세라믹학회지
    • /
    • 제28권5호
    • /
    • pp.353-358
    • /
    • 1991
  • Fine powders of the 2212 superconducting phase of bismuth system have been prepared directly from solution using ultrasonic spray pyrolysis. The fine superconducting powders produced by pyrolysis were characterized for the size, shape, and crystalline phase by SEM and XRD. The pyrolysis temperature, flow rate of the carrier gas, residence time of the droplets greatly influenced the size, shape, and crystalline phase. The optimum temperature and flow rate of the carrier gas for the preparation of fine powders of the 2212 superconduting phase were found to be 830$^{\circ}C$and 3ι/min, respectively.

  • PDF

Bi계 세라믹에서 초전도체 특성에 미치는 도우핑 원소의 영향 (Effect of Doping Elements on Superconducting Characteristics in Bi-system Ceramics)

  • 양승호;박용필;김용주
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 하계학술대회 논문집
    • /
    • pp.198-203
    • /
    • 2000
  • This paper investigated the effects of doping elements on the Bi-Sr-Ca-Cu-O ceramics. The doping elements can be classified into four groups depending on their superconducting characteristics in the Bi-Sr-Ca-Cu-O structure. The first group of doping elements(Co, Fe, Ni and Zn) substitute into the copper site and can reduce the critical temperatures of the 2223 and 2212 phases. The second group of doping elements(Y and La) substitute into the Ca site and cause the disappearance of the 2223 phase and increase the critical temperatures in the 2212 phase. The third group of doping elements(P and K) have a tendency to decompose the superconducting phase and reduce the optimal sintering temperature. The fourth group of doping elements(B, Si, Sn and Ba) almost unaffected the superconductivity of the 2223 and 2212 phase.

  • PDF

유한 요소법에 의한 속응 여자 초전도 발전기의 과도 특성 해석 (Transient Characteristic Analysis of Quick Response Extraction Type Superconducting Generator by Finite Element Method)

  • 김정철;한성진
    • 한국초전도ㆍ저온공학회논문지
    • /
    • 제2권2호
    • /
    • pp.26-31
    • /
    • 2000
  • This paper deals with finite element analysis of 2GVA superconducting generator which has slitted electrothermal shield in d-axis (SES). Three phase fault is considered torque of the S.C.G. Using the result, generator parameters are calculated by F.E.M. The results are compared with superconducting generator having conventional electrothermal shield (CES). The result shows that quick response excitation could be applied to superconducting generator with slitted electrothermal shield.

  • PDF

Fault Current Limiting Characteristics of Separated and Integrated Three-Phase Flux-Lock Type SFCLs

  • Lim, Sung-Hun
    • Journal of Electrical Engineering and Technology
    • /
    • 제2권3호
    • /
    • pp.289-293
    • /
    • 2007
  • The fault current limiting characteristics of the separated and the integrated three-phase flux-lock type superconducting fault current limiters (SFCLs) were analyzed. The three-phase flux-lock type SFCL consisted of three flux-lock reactors and three $high-T_c$ superconducting (HTSC) elements. In the integrated three-phase flux-lock type SFCL, three flux-lock reactors are connected on the same iron core. On the other hand, three flux-lock reactors of the separated three-phase flux-lock type SFCL are connected on three separated iron cores. The integrated three-phase flux-lock type SFCL showed the different fault current limiting characteristics from the separated three-phase flux-lock type SFCL that the fault phase could affect the sound phase, which resulted in quench of the HTSC element in the sound phase. Through the computer simulation applying numerical analysis for its three-phase equivalent circuit, the fault current limiting characteristics of the separated and the integrated three-phase flux-lock type SFCLs according to the ground fault types were compared.

열분해법에 의한 전력기기용 초전도 합성 기술에 관한 연구 (A Study on the Fabrication of Superconductor Using Pyrolysis Methods for Electric power Machinery)

  • 이상헌;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.153-154
    • /
    • 2005
  • A high Tc superconducting with a nominal composition of $Bi_2Sr_2Ca_2Cu_3O_Y$ was prepared by the citarte method. The solid precursor produced by the dehydration of the gel at 120$^{\circ}C$ for 12h is not in the amorphous state as expected but in a crystalline state. X-ray diffraction peaks of nearly the same angular position as the peaks of high Tc phase were observed in the precursor. After pyrolysis at 400$^{\circ}C$ and calcination at 840$^{\circ}C$ for 4h, the (001)peak of the high Tc phase was cleary observed. Experimental results suggest that the intermediate phase formed before the formation of the superconducting phase may be the most important factro in determining whether it is easy to form the high Tc phase or not, because the nucleation barriers of the two superconducting phase may be altered by the variation of the crystal structures of those intermediate phase.

  • PDF