The Transactions of the Korean Institute of Electrical Engineers C
/
v.51
no.12
/
pp.573-577
/
2002
We designed wideband HTS antennas which consists of two triangle -radiation patches using a $YBa_2Cu_3O_{7-X}$ (YBCO) superconducting thin film. The major limitation of high-Tc superconducting (HTS) microstrip antennas is the narrow bandwidth due to the high Q and thin substrate. Defining bandwidth as the frequency range over which standing wave ratio (SWR) 2:1 or less, HTS antenna bandwidths are typically 0.85 % to 1.1 %. Thus considerable effort has been focused on developing antennas for broadband operation. To calculate input impedance and design of the broadband HTS antennas a moment method technique was used. The HTS antenna fabricated in this work was designed for K-band, which is useful band for satellite to satellite communications. The bandwidth obtained was a significant 6.7 % and the other measured performance of our HTS antenna, including the bandwidth, radiation Pattern, efficiency, standing wave ratio (SWR) and return losses was reported.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2002.07a
/
pp.523-526
/
2002
We designed wideband HTS antennas which consists of two triangle-radiation patches using a YBa$_2$Cu$_3$O$\sub$7-x/ (YBCO) superconducting thin film. The major limitation of high-Tc superconducting (HTS) microstrip antennas is the narrow bandwidth due to the high Q and thin substrate. Defining bandwidth as the frequency range over which standing wave ratio (SWR) 2:1 or less, HTS antenna bandwidths are typically 0.85% to 1.1%. Thus considerable effort has been focused on developing antennas for broadband operation. To calculate input impedance and design of the broadband HTS antennas a moment method technique was used. The HTS antenna fabricated in this work was designed for K-band, which is useful band for satellite-to-satellite communications. The bandwidth obtained was a significant 6.7% and the other measured performance of our HTS antenna, including the bandwidth, radiation Pattern, efficiency, standing wave ratio (SWR) and return losses was reported.
Kwak Min Hwan;Kim Young Tae;Moon Seong Eon;Ryu Han Cheol;Lee Su Jae;Kang Kwang Yong
Progress in Superconductivity and Cryogenics
/
v.7
no.1
/
pp.13-16
/
2005
High temperature superconductor, $\YBa_2Cu_3O_{7-x}$ (YBCO) and ferroelectric, $\Ba_{0.1}Sr_{0.9}TiO_{3}$ (BST) multilayer thin films were deposited using on MgO(100) substrates pulsed laser deposition. The thin films exhibited only (001) peaks of YBCO and 1357 The HTS thin films demonstrated excellent zero resistance temperature of 92.5 K. We designed and fabricated HTS ferroelectric phase shifter using high frequency system simulator and standard photolithography method, respectively The HTS phase shifter shows a low insertion loss (2.97 dB) and large phase change ($\162^{circ}$) with 40 V do bias at 10 GHz. The HTS phase shifter shows 54 of figure of merit. These results can be applicable to phased anay antenna system for satellite communication services.
The fabrication of Y-Ba-Cu-O films and experimental factors affecting to characteristics of films are studied in detail. Superconducting thick films are fabricated by the screen printing method. The metal-citrate precursors are obtained simply by mixing of metal nitrate with citric acid. The particle size of heat treated powders is approximately 0.3-1${\mu}{\textrm}{m}$ and the thickness of film is estimated as 30-35${\mu}{\textrm}{m}$. According to the XRD analysis, the films sintered at 870-93$0^{\circ}C$ for 10min. -6hr with P(oxygen)=1atm has the unique orthorhombic crystal symmetry indicating the 123 phae. Tc, onset is determined around 92-87。K, but it shows semiconducting behavior probably due to the oxygen deficiency in the lattice, porosity and impurities in films. Extrapolated Tc, zero is estimated as 76-50。K. For films sintered at 90$0^{\circ}C$ for 1hr, superconducting properties are observed with the room temperature resistivity of 0.025$\Omega$.cm Tc, onset at 88。K and Tc, zero at 63。K.
Melt spun YB $a_2$C $u_3$A $g_{15}$ and YbB $a_2$C $u_3$A $g_{x}$(x=5, 16 and 53) precursor alloy ribbons were oxidized at 263~322$^{\circ}C$, and heat-treated at 872~89$0^{\circ}C$ under 1.0atm oxygen pressure. In addition, about ten ribbons were stacked and coupled by pressing, and then followed the same heat treatment. YB $a_2$C $u_3$$O_{7-{\delta}}$(1-2-3) or YbB $a_2$C $u_3$$O_{7-{\delta}}$(1-2-3) phase was formed in both the ribbons and the multilayered specimens. The formed 1-2-3 phases were not texturized in all the ribbons, but slightly texturized in the multilayered specimens. $J_{c}$ was not achieved in all the ribbons at 77K and zero magnetic field. Among the multilayered specimens, YB $a_2$C $u_3$A $g_{15}$ and YbB $a_2$C $u_3$A $g_{16}$ showed $J_{c}$ of 260 and 180A/$\textrm{cm}^2$, respectively. YB $a_2$C $u_3$A $g_{15}$ and YbB $a_2$C $u_3$A $g_{16}$ are considered to be the appropriate compositions in producing textured superconducting oxides with improved $J_{c}$ by pressing. Onset critical temperature ( $T_{on}$ ) of the multilayered YB $a_2$C $u_3$A $g_{15}$ was 92K while those of YbB $a_2$C $u_3$A $g_{x}$(x=5 , 16 and 53) were 88~90K. , 16 and 53) were 88~90K.
[$YBa_2Cu_3O_{7-x}$] thin films were deposited on various buffered-templates by a metal organic chemical vapor deposition(MOCVD). Three different templates of $CeO_2/YSZ/CeO_2/pure-Ni(CYC),\;CeO_2/YSZ/Y_2O_3/Ni-3at.%W(YYC)$ and $CeO_2/IBAD-YSZ$/stainless steel were used. The Ni and Ni-W alloy tapes were biaxially textured by cold rolling and annealing heat treatment. The dense YBCO films were grown on both the IBAD and YYC templates with no microcrack, while the YBCO films on the CYC templates were grown with the formation of microcracks and NiO. The YBCO film on the YYC template showed the higher $I_c$ than that on CYC template. Especially, the IBAD templates with a thin $CeO_2$(type I) and thick $CeO_2$(type II) top layer were used to compare the deposition nature of the YBCO on them. Comparing the current property of the YBCO films on IBAD templates, the YBCO film deposited on thick $CeO_2$ layer was better than the film on thin $CeO_2$ layer.
Chung Won Yang;Kweon Jung Ohk;Cho Eun Kyung;Kim Keyung Nam;Han, Sang Mok
Journal of the Korean Chemical Society
/
v.36
no.1
/
pp.16-23
/
1992
High $T_c$, superconductor $(Y_{1-x}Eu_x)Ba_2Cu_3O_{7-{\delta}}$ (x = 0.0, 0.2, 0.4, 0.6, 0.8, 1.0) were prepared and the physical properties were observed. XRD analysis showed that the structures of all the specimen were orthorhombic and the lattice parameters a, b and c increased with the increasing x value. Electrical resistivity and magnetization measurements revealed that pure high $T_c$, superconducting phases were formed at above 90 K. The critical temperatures increased with increasing the amount of Eu. From the measurement of magnetization and the size of the grains using SEM micrographs, volume diamagnetic susceptibilities for each specimen were calculated. These values decreased with the increasing x value. The composition of Ba in the lattice site decreased as the concentration of Eu increased, and this was confirmed by EPMA. It was found out that the volume diamagnetic susceptibility of each specimen was directly influenced by the composition of Ba in the lattice site.
We have fabricated good quality superconducting $YBa_2Cu_3O_{7-{\delta}}$ thin films on Hastelloy(Ni-Cr-Mo alloys) with $CeO_2$ buffer layers by in-situ pulsed laser deposition in a multi-target processing chamber. Using one of electrical properties of YBCO superconducting which the resistance approaches to zero dramatically on transition temperature, we have researched to make power transmission line, we have deposited YBCO thin film on flexible metallic substrate. However, it is difficult to make films on flexible metallic substrates due to both interdiffusion problem between metallic substrate and superconducting layer and non-crystallization of YBCO on amorphous substrate. From early research, two ways-using textured metallic substrate and buffer layer-were proposed to overcome theses difficulties. We have chosen $CeO_2$ as a buffer layer which has cubic structure of $5.41{\AA}$ lattice parameter and only 0.2% of lattice mismatch with $3.82{\AA}$ of a-axis lattice parameter of YBCO on (110) direction of $CeO_2$. In order to enhance the crystallization of YBCO films on metallic substrates we deposited $CeO_2$ buffer layers at varying temperature $700^{\circ}C$ to $800^{\circ}C$ and $O_2$ pressure. By X-ray diffraction, we found that each domination of (200) and (111) orientations were strongly relied upon the deposition temperature in $CeO_2$ layer and the change of the domination of orientation affects the crystallization of YBCO upper layer.
The Transactions of the Korean Institute of Electrical Engineers C
/
v.49
no.7
/
pp.375-381
/
2000
In this paper, we described the characterization of High-Tc Superconducting(HTS) microstrip antenna using non-radiating edge feeding technique and reported the microwave properties of HTS antennas with temperature. To do this, we prepared the $YBa_2Cu_3O_{7-x}$ superconducting thin film on MgO substrate using pulse-laser deposition techniques. The HTS microstrip antenna using non-radiating feeding technique was fabricated using chemical wet-etching. Then it was compared with identical antenna patterned with evaporated gold. The diverse measured results have been reported in terms of the input impedance, resonant frequency and return loss. In additional, at around the critical temperature, the effect of kinetic inductance which affect the resonant characteristic of the HTS microstrip antenna was reported.
The influence of water partial pressure in Metal-organic Deposition (MOD) method was investigated on the texture and the morphology of $YBa_2Cu_3O_{7-x}$ (YBCO) films grown on the buffered metal tapes. The water partial pressure was varied from 4.2% up to 10.0% with the other process variables, such as annealing temperature and oxygen partial pressure, kept constant. In this work, the fluorine-free Y & Cu precursor solution added with Sm was synthesized and coated by the continuous slot-die coating & calcination step. The next annealing step of the YBCO films was done by the reel-to-reel method with the gas flowed vertically down. From the x-ray diffraction analysis, the un-reacted phase like $BaF_2$ peak was found at the water partial pressure of 4.2%, but $BaF_2$ peak intensity is much reduced as the water partial pressure is increased. However, the higher water partial pressure of about 10% in this experiment leads to the poor crystallinity of YBCO films. The morphologies of the YBCO films were not different from each other when the water partial pressure was varied in this work. The maximum critical current density of 3.8MA/$cm^2$ was obtained at the water partial pressure of 6.2% with the annealing temperature of 780$^{\circ}C$ and oxygen partial pressure of 500ppm.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.