  • STS 304 steel is used as pressure vessel material, and although it exhibits excellent mechanical characteristics at a low temperature, it is heavier than other materials. To address this issue, a method using cold-stretching techniques for STS 304 can be applied. In this study, a cold-stretching part and welded joint specimen were directly obtained from a cold-stretching pressure vessel manufactured according to ASME code. Fatigue crack propagation tests were carried out at room temperature and $-170^{\circ}C$ using the compliance method for stress ratios of 0.1 and 0.5. The results indicate that crack growth rate of the welded joint is higher than that of the cold-stretching part within the same stress intensity factor range. The outcome of this work is expected to serve as a basis for the development of a cold-stretched STS 304 pressure vessel.

Influences of Environmental Gradients on the Patterns of Vegetation Structure and Tree Age Distribution in the East Side of Cascade Range, Washington, USA (워싱턴주(州) 케스케이드산맥(山脈) 동(東)쪽 산림(山林)에서 환경구배(環境勾配)가 식생구조(植生構造)와 연령분포(年齡分布)에 미치는 영향(影響))

  • Woo, Su Young;Lee, Kyung Joon;Lee, Sang Don
    • Journal of Korean Society of Forest Science
    • /
    • v.85 no.1
    • /
    • pp.107-119
    • /
    • 1996
  • To understand vegetation changes along environmental gradients in the natural forests in the east side of the Cascade Range in Washington state, USA, line transects were used to sample six different forest environments in the Wenatchee National Forest in the north-facing and south-facing sites at 975, 1280 and 1700m elevation. Data were analyzed using ordination by detranded correspondence analysis. Pseudotsuga menziesii was found as one of the dominant species on all the six sites regardless of elevation or aspect, while Pinus ponderosa was dominant on south slopes only. Abies grandis and A. lasiocarpa were dominant species on north slopes at elevations of 1280 and 1700m, respectively. Moisture, as it related to aspect, was identified as one of the most important environmental gradients for explaining the variation of vegetation types. On north-facing slopes, compared to south-facing slopes, where moisture was not as limiting and canopies could grow denser, probably, elevation or competitive interaction was more important. Species diversity tended to decrease with increasing environmental severity, with south slopes having less diversity than north slopes due to extended water stress and harsher temperature extremes on south slopes. The age structure on north-facing and south-facing slopes was different. Light intensity, moisture and climate were different between these two slopes. Large scale disturbances(e.g., big fire or insects) were major causes in changing age structure. Younger trees showed a closer relationship between size and age than adult trees. DBH values of shade intolerant species in south-facing slope were bigger than those of north-facing slope, which suggested that aspect of stands be the most important factor for age and size.

  • PDF

The Propagation Behaviour of the Fatigue Crack in the Compact Tension Specimens of the Welded Structural Steels (On according to the difference of the welding direction, the input heat level, the strength of weld material and so on) (용접(鎔接)이음한 구조강(構造鋼)의 소인장시험편(小引張試驗片)에서의 피로구열진전거동(疲勞龜裂進展擧動) (용접방향(鎔接方向), 입열량(入熱量), 용접재료(鎔接材料)의 강도(强度) 등이 다를 때))

  • Chang, Dong Il;Chung, Yeong Wha
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.4 no.2
    • /
    • pp.133-142
    • /
    • 1984
  • With the weld-joined compact tension specimens compared with each other, that is, transverse and lengthwise about the crack propagation direction, high and low in the input heat level, same as and lower than the base metal in the strength of weld material, the fatigue test were performed. With these data, the log-log curves between the fatigue crack propagation rate ${\frac{da}{dN}}$ and the transition range of the stress intensity factor ${\Delta}K$ ahead the crack tip were drawed. These curves were compared and estimated among each compared specimens, among each zones, that is, the base metal, the heat-affected metal and the weld-mixed metal, and between this study and the past studies. Basically, Little difference in the slope of the $da/dN-{\Delta}K$ relation was showed in all the welded directions, all the input heat levels and all the zones. But, First, to comparison with in the past studies about the base metals, it was showed that da/dN started in the much later rate, increased faster and stoped in the little faster rate. Second, it was showed that, near the time the crack's going from the heat-affected zone to the weld-mixed metal da/dN decreased a little for a while. Third, in the lengthwise weld compared with the transverse weld, in the high input heat weld compared with the low input heat weld in the case used the weld material of the same strength as the base metal, in the opposite case in the case used the one of the lower strength than the base metal, in the case used the weld material of the same strength as compared with the lower strength than the base metal beside the high input heat and the lengthwise weld, it was showed that the crack occured earlier in lower ${\Delta}K$ and later da/dN, the curves went with the same slope. Forth, in the lengthwise weld compared with the transverse weld in the low input heat weld, in the low input heat weld compared with the high input heat weld, it was showed that da/dN went with the lower level.