• 제목/요약/키워드: Stress Parameters

검색결과 3,223건 처리시간 0.032초

Visual Analysis for Detection and Quantification of Pseudomonas cichorii Disease Severity in Tomato Plants

  • Rajendran, Dhinesh Kumar;Park, Eunsoo;Nagendran, Rajalingam;Hung, Nguyen Bao;Cho, Byoung-Kwan;Kim, Kyung-Hwan;Lee, Yong Hoon
    • The Plant Pathology Journal
    • /
    • 제32권4호
    • /
    • pp.300-310
    • /
    • 2016
  • Pathogen infection in plants induces complex responses ranging from gene expression to metabolic processes in infected plants. In spite of many studies on biotic stress-related changes in host plants, little is known about the metabolic and phenotypic responses of the host plants to Pseudomonas cichorii infection based on image-based analysis. To investigate alterations in tomato plants according to disease severity, we inoculated plants with different cell densities of P. cichorii using dipping and syringe infiltration methods. High-dose inocula (${\geq}10^6cfu/ml$) induced evident necrotic lesions within one day that corresponded to bacterial growth in the infected tissues. Among the chlorophyll fluorescence parameters analyzed, changes in quantum yield of PSII (${\Phi}PSII$) and non-photochemical quenching (NPQ) preceded the appearance of visible symptoms, but maximum quantum efficiency of PSII ($F_v/F_m$) was altered well after symptom development. Visible/near infrared and chlorophyll fluorescence hyperspectral images detected changes before symptom appearance at low-density inoculation. The results of this study indicate that the P. cichorii infection severity can be detected by chlorophyll fluorescence assay and hyperspectral images prior to the onset of visible symptoms, indicating the feasibility of early detection of diseases. However, to detect disease development by hyperspectral imaging, more detailed protocols and analyses are necessary. Taken together, change in chlorophyll fluorescence is a good parameter for early detection of P. cichorii infection in tomato plants. In addition, image-based visualization of infection severity before visual damage appearance will contribute to effective management of plant diseases.

절리면의 거칠기 특성이 정리암반의 거동에 미치는 영향에 대한 수치해석적 연구 (Numerical Evaluation of the Influence of Joint Roughness on the Deformation Behavior of Jointed Rock Masses)

  • 이연규
    • 터널과지하공간
    • /
    • 제11권3호
    • /
    • pp.225-236
    • /
    • 2001
  • 암반 절리면의 거칠기는 전단강도 및 변형거동에 가장 중요한 영향을 미치는 요소 중의 하나이다. 절리면은 전단변형이 발생하는 동안 손상을 받게 되고 이에 따라 거칠기각은 연속적으로 낮아진다. 절리면의 수직팽창성과 강도 경화 및 연화현상도 거칠기의 변화와 관련이 있는 것으로 이해되고 있다. 따라서 절리면의 거칠기의 변화를 효율적으로 반영시킬 수 있는 수치해석 모델의 개발이 중요하다. 이 연구에서는 탄소성이론을 바탕으로 거칠기 변화를 고려할 수 있는 탄소성 응력-변형 증분식을 유도하여 절리면 거질기 변화가 절리면 전단거동에 미치는 영향을 정량적으로 평가하는데 이용하였다. 유도된 탄소성 증분식을 검증하기 위하여 수치 주기전단시험을 실시하였다. 수치시험결과 개발된 탄소성 증분식은 거친 절리면의 주기전단시험에 나타나는 일반적인 현상들을 모사하는데 효과적임을 알 수 있었다.

  • PDF

재생골재 콘크리트의 강도 및 파괴특성 실험 (Characteristics of Strength and Fracture Toughness of Recycled Aggregate Concrete)

  • 김진철;양성철;조윤호;김남호
    • 한국도로학회논문집
    • /
    • 제6권1호
    • /
    • pp.37-45
    • /
    • 2004
  • 본 연구는 재생골재를 사용한 콘크리트의 강도 및 파괴특성을 고찰하므로써 콘크리트 포장체에 적용성 여부를 검토하기 위해 수행하였다. 재생콘크리트의 초기강도는 낮았으나 재령 증가에 따라 기준콘크리트와 거의 유사한 값을 나타내었으며. 탄성계수는 골재 강성 차이로 인하여 낮게 나타났다. 또한 고로슬래그 미분말을 혼합한 재생콘크리트의 강도개선효과를 확인할 수 있었다. TPFM에 의한 파괴에너지는 초기재령에서 재생콘크리트의 파괴특성이 우수한 것으로 나타났으나, 재령증가에 따라 기준콘크리트와 유사한 값으로 나타났다. 또한 P-CMOD 측정결과로부터 이론적으로 구한 탄성계수 및 인장강도와 실험으로 구한 탄성계수 및 쪼갬인장 강도사이의 상관성은 매우 높은 결과를 나타내어 시험방법의 신뢰성을 확인할 수 있었다.

  • PDF

단순가력실험을 통한 콘크리트충전 강관기둥의 부착응력에 관한 연구 (An Experimental Study on the Bond Strengths for Concrete Filled Steel Tube Columns using a Push-Out Test)

  • 우해성;김진호;최성모
    • 한국강구조학회 논문집
    • /
    • 제14권4호
    • /
    • pp.481-487
    • /
    • 2002
  • 콘크리트충전 강관기둥의 외다이아프램 접합부형식에서, 철골보의 하중이 내부의 콘크리트로 전달되는 하중전달 메카니즘이 아직 명확하게 규명되지 않았다. 여기서 각 층에서 철골보의 전단력은 외부의 강관과 내부의 콘크리트 사이의 부착응력에 의해 전달된다고 본다. 따라서 본 연구는 콘크리트충전 강관기둥의 부착응력을 파악하기 위해, 콘크리트면에만 하중을 가하는 단순가력실험을 실시하였다. 콘크리트 종류, 강관의 형상/길이, 이음부의 유무/뒷댐재의 두께 등을 변수로 총 30개의 실험체를 제작하여 실험을 실시했으며, 각 변수에 따른 실험결과를 비교/분석하고자 했다.

고강도콘크리트충전 각형강관장주의 내력에 관한 실험적 연구 (An Experimental Study on Stength of Slender Square Tube Columns Filled with High Strength Concrete)

  • 서성연;정진안
    • 한국강구조학회 논문집
    • /
    • 제14권4호
    • /
    • pp.471-479
    • /
    • 2002
  • 본 논문에서는 고강도콘크리트충전 각형강관장주에 대한 실험결과와 탄소성해석결과를 비교분석했다. 실험체는 모두 고강도콘크리트 충전 각형강관장주로 18개를 제작하였으며, 편심비에 따라 중심 및 편심가력하였다. 본 연구의 주요 파라메타는 단면폭에 대한 유효좌굴 길이의 비($L_K$/D)= 4, 8, 12, 24, 30와 가력편심비(e)=0, k, 3k이다. 본 논문에서 고강도콘크리트 충전 각형강관장주의 내력에 관한 해석 및 실험을 통하여 다음과 같은 결과를 얻었다. $L_K$/D=12 이하의 고강도콘크리트충전 각형강관단주는 콘크리트 감소계수 $c{\gamma}u=0.85$를 고려한 전소성내역에 도달했으나, $L_K$/D=18 이상의 장주실험체는 콘크리트 감소계수를 고려한 전소성내력에 도달하지 않았다. 실험에 의한 고강도콘크리트충전 각형강관장주의 탄소성거동은 제안된 해석치의 종국내력$N_{ASSUMED}$과 비교적 양호한 접근을 보여주었다. 콘크리트 압축강도의 감소계수 $c{\gamma}u=0.85$를 고려하지 않은 CFT설계기준과 고강도 콘크리트를 충전한 각형강관기둥의 실험결과치는 비교적 잘 일치함을 알 수 있었다.

Neuroprotective Effect of Steamed and Fermented Codonopsis lanceolata

  • Weon, Jin Bae;Yun, Bo-Ra;Lee, Jiwoo;Eom, Min Rye;Ko, Hyun-Jeong;Lee, Hyeon Yong;Park, Dong-Sik;Chung, Hee-Chul;Chung, Jae Youn;Ma, Choong Je
    • Biomolecules & Therapeutics
    • /
    • 제22권3호
    • /
    • pp.246-253
    • /
    • 2014
  • Codonopsis lanceolata has been used as an herbal medicine for several lung inflammatory diseases, such as asthma, tonsillitis, and pharyngitis. Previously, we showed the neuroprotective effect of steamed and fermented C. lanceolata (SFC) in vitro and in vivo. In the current study, the treatment of HT22 cells with SFC decreased glutamate-induced cell death, suggesting that SFC protected HT22 cells from glutamate-induced cytotoxicity. Based on these, we sought to elucidate the mechanisms of the neuroprotective effect of SFC by measuring the oxidative stress parameters and the expression of Bax and caspase-3 in HT22 cells. SFC reduced contents of ROS, $Ca^{2+}$ and NO. Moreover, SFC restored contents of glutathione and glutathione reductase as well as inhibited Bax and caspase-3 activity in HT22 cells. These results indicate that steamed and fermented C. lanceolata (SFC) extract protected HT22 cells by anti-oxidative effect and inhibition of the expression of Bax and caspase-3.

니켈도금된 S45C강의 연속파형 Nd:YAG 레이저 겹치기용접 특성 (Characteristics of CW Nd:YAG Laser Lap Welds of Nickel Coated S45C Steel)

  • 유영태;신호준
    • Journal of Welding and Joining
    • /
    • 제25권3호
    • /
    • pp.18-27
    • /
    • 2007
  • Laser welding process is widely used in the industrial field due to its numerous advantages: a small heat affected zone(HAZ), deep penetration, high welding speed, ease of automation, single-pass thick section capability, enhanced design flexibility, and small distortion after welding. The objective of this research works is to investigate the influence of the process parameters, such as the welding fur metals with CW Nd:YAG lasers. The bead-on-plate and Lap welding experiments are carried out for several combinations of the experimental conditions. In order to quantitatively examine the characteristics of the welding quality of the cross section, tensile stress behavior and the hardness of the welded part are investigated in comparison of the Nickel coated and Nickel uncoated S45C steel. As a result of experiment, nickel coated S45C Steel showed more even weld zone than Nickel uncoated counterpart upon lap welding. Also, it showed relatively small amount of internal defects and spatter, and Nickel coated S45C showed better weldability than Nickel uncoated S45C steel. The optimum welding process upon lap welding of Nickel coated S45C steel is when each laser power is 1900W; focal positions is -1mm; welding speed is $0.9{\sim}1.0m/min$. The heat input was $4.178{\sim}4.36{\times}103J/cm^2$.

고체추진제의 파괴인성에 대한 온도 및 두께의 영향 (Effect of Temperature and Thickness on Fracture Toughness of Solid Propellant)

  • 서보휘;김재훈
    • 대한기계학회논문집A
    • /
    • 제37권11호
    • /
    • pp.1355-1360
    • /
    • 2013
  • 균열이 발생된 고체추진제는 연소면적 증가에 따른 과연소 현상으로 인해 로켓의 손상 또는 파괴까지 일어날 수 있기 때문에 파괴인성을 평가하는 것은 매우 중요하다. 이 재료에 파괴인성에 미치는 온도 및 두께의 영향을 확인하기 위하여, 시험 온도는 $-60^{\circ}C$에서 $60^{\circ}C$ 범위, 시편의 두께는 4, 12.5, 24.5 mm 의 3 종류로 변화하여 Center cracked tension(CCT) 시편을 이용하여 파괴인성을 평가하였다. 본 시험 결과로부터 파괴인성은 온도 증가와 함께 감소하는 경향을 보이고 두께 변화에 대한 파괴인성은 $-60^{\circ}C$를 제외한 다른 온도조건에서 두께 12.5 mm 일 때 가장 크게 나타나고 있다. 고체추진제의 파괴인성은 $-60^{\circ}C$부근에서 유리전이거동에 의한 변화하는 것을 알 수 있다.

Nonlinear response of the pile group foundation for lateral loads using pushover analysis

  • Zhang, Yongliang;Chen, Xingchong;Zhang, Xiyin;Ding, Mingbo;Wang, Yi;Liu, Zhengnan
    • Earthquakes and Structures
    • /
    • 제19권4호
    • /
    • pp.273-286
    • /
    • 2020
  • The pile group foundation is widely used for gravity pier of high-speed railway bridges in China. If a moderate or strong earthquake occurs, the pile-surrounding soil will exhibit obvious nonlinearity and significant pile group effect. In this study, an improved pushover analysis model for the pile group foundation with consideration of pile group effect is presented and validated by the quasi-static test. The improved model uses simplified springs to simulate the soil lateral resistance, side friction and tip resistance. PM (axial load-bending moment) plastic hinge model is introduced to simulate the impact of the axial force changing of pile group on their elastic-plastic characteristics. The pile group effect is considered in stress-stain relations of the lateral soil resistance with a reduction factor. The influence factors on nonlinear characteristics and plastic hinge distribution of the pile group foundation are discussed, including the pier height, longitudinal reinforcement ratio and stirrup ratio of the pile, and soil mechanical parameters. Furthermore, the displacement ductility factor, resistance increase factor and yielding stiffness ratio are provided to evaluate the seismic performance of soil-pile system. A case study for the pile group foundation of a railway simply supported beam bridge with a 32 m-span is conducted by numerical analysis. It is shown that the ultimate lateral force of pile group is not determined by the yielding force of the single one in these piles. Therefore, the pile group effect is essential for the seismic performance evaluation of the railway bridge with pile group foundation.

동결융해 및 부착재료 변화에 따른 GFRP-구조물 경계면의 최대 부착강도 및 유효부착길이 평가 (Investigation of Maximum Strength and Effective Bonding Length at the Interface Between Structure and GFRP Material Under Freeze-thaw Cycles and Applied Different Bonding Materials)

  • 최현규;정우영;안미경
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제15권2호
    • /
    • pp.107-115
    • /
    • 2011
  • 본 연구는 부착재료의 변화 및 동결융해에 따른 FRP-콘크리트구조물 경계면의 거동을 조사하였다. 실험 시 고려된 연구변수로는 부착경계면의 부착강도, 경계면 유효부착길이 등을 조사하였다. 경계면 부착재료에 따른 거동변화 실험체의 경우 FRP-구조물 부착경계면에 사용되는 에폭시의 종류를 각각 3가지로 분류하며 FRP-콘크리트간 다양한 부착길이를 고려하여 시편을 제작하였으며 동결융해에 따른 경계면 거동조사의 경우 0 cycle에서 300cycle까지 계속적으로 증가되는 주기에 대하여 실험체들을 제작, 장기거동 부착실험을 수행하였다. 본 실험결과, 적용 부착재료의 종류에 따라 최대 유효부착길이는 5~7% 차이가 있었으며 동결융해 주기증가에 따른 최대부착하중 및 유효부착길이의 경우 초기에 나타난 급격한 거동변화 이후 상대적으로 불규칙한 변화를 장기적으로 나타내었다.