• 제목/요약/키워드: Stress Intensity Limit

검색결과 71건 처리시간 0.019초

SMART제어봉구동장치의 압력용기에 대한 응력 및 열해석 (Stress and Thermal Analyses of Pressure Housing of SMART CEDM)

  • 조대희;유제용;김지호;김종인
    • 한국전산구조공학회:학술대회논문집
    • /
    • 한국전산구조공학회 2002년도 봄 학술발표회 논문집
    • /
    • pp.343-350
    • /
    • 2002
  • The structural stability of pressure housing of SMART CEDM forming pressure boundary must be evaluated. In this paper, the stress and thermal analyses of the upper pressure housing of CEDM are performed for design pressure, hydraulic test pressure and thermal loading. Finite element and boundary condition were generated from the model which is made by I-DEAS program and the stress and thermal analyses were performed by ANSYS Program. The upper Pressure housing was analysed using 2D axisymmetric model because it is symmetry about an axis. The stress values obtained by analysis were compared with the stress intensity limit of ASME and KEPIC MNB standard.

  • PDF

고강도 구상흑연주철의 피로한도에 미치는 2상 기지조직의 영향 (Effects of 2-Phase Matrix Structure on Fatigue Limit of High Strength Ductile Iron)

  • 김진학;지정근;김민건
    • 산업기술연구
    • /
    • 제19권
    • /
    • pp.75-79
    • /
    • 1999
  • Rotary bending fatigue tests were performed to investigate the effects of 2-phase matrix structure on fatigue limit with prepared specimens in high strength ductile irons. Two types of the specimens with different microstructures have been used. Series A has sorbite and series B has bainite. Fatigue limits of both specimens are improved comparing with as cast specimen. The fatigue limit is higher in series B than in series A. The reason why the fatigue limit of series A shows inferiority to that of series B is due to the transition of micro fatigue cracks to mesocrack occurs very rapidly, so increased stress intensity factor drives the fatigue crack growth. The higher fatigue limit of series B which has bainite is caused by the ${\gamma}$ layer contained in microstructure impede the rapid growth of micro fatigue crack to mesocrack and ${\alpha}$ layer around graphite has the higher capacity for the absorption of plastic deformation energy than sorbite.

  • PDF

ASME BPVC Section XI Appendix L의 결함허용평가에 따른 허용운전주기 민감도 분석 (Sensitivity Analysis for Allowable Operating Period Based on the Flaw Tolerance Evaluation of ASME BPVC Section XI Appendix L)

  • 오창식;조두호;정명조
    • 한국압력기기공학회 논문집
    • /
    • 제17권2호
    • /
    • pp.126-136
    • /
    • 2021
  • During operation of nuclear power plants, the fatigue assessment should be conducted repeatedly, considering changes of operating environments. For the case that cumulative usage factors (CUFs) may exceed the acceptance limit, flaw tolerance evaluation can be an alternative method to meet the regulatory requirements. In this respect, this paper analyzes the effects of the input variables for flaw tolerance evaluation based on ASME BPVC Section XI Appendix L. The reference analysis is performed for the example problem in NUREG/CR-6934. Then effects of the crack orientation, stress intensity factor solutions, thermal stress profiles, fatigue stress decomposition and fatigue crack growth curves are considered for the sensitivity analysis. The results show that the stress analysis considering the actual environment plays a crucial role in flaw tolerance evaluation.

원자로 용기의 압력-온도 한계곡선 Round Robin 해석 (Round Robin Analysis of Pressure-Temperature Limit Curve for Reactor Vessel)

  • 정명조;이진호;박윤원;최영환;김영진
    • 한국전산구조공학회논문집
    • /
    • 제16권2호
    • /
    • pp.153-163
    • /
    • 2003
  • 원자로 용기의 온도-압력 한계곡선을 위하여 국내공동비교연구를 수행하였다. 국내 원전의 데이터를 이용하여 국내 각 기관에서 온도-압력 한계곡선 작성에 사용하고 있는 방법 및 기법을 비교하기 위하여 round robin 해석을 제안하였고 주어진 문제에 대하여 각 기관이 문제를 해석한 후 결과를 제출하여 이들을 분석함으로써 온도-압력 한계곡선 작성에 대한 표준 해석 자료를 만들어 추후 평가에 이용할 수 있도록 하였다.

반복하중조건 하에서의 S45C 탄소강에 대한 미소피로균열 성장속도 해석의 수정 (A Modification in the Analysis of the Growth Rate of Short Fatigue Cracks in S45C Carbon Steel under Reversed Loading)

  • ;신용승
    • Journal of Welding and Joining
    • /
    • 제13권2호
    • /
    • pp.96-105
    • /
    • 1995
  • 본 연구에서는 종래의 미소피로균열 성장속도 해석방법에 대한 수정안을 제시하고 수정 후의 방 법에 의해서 계산한 값들과 S4SC 탄소강에 대한 Nisitani와 Goto의 실험결과를 비교하여 계산한 값과 실험데이터 사이에 양호한 일치가 있음을 보였다. 이미 제시된 피로균열성장속도 식에는 하한계수준과 피로한도를 연관시키는 재료상수와 탄소성 거동에 대한 수정 및 균열닫힘효과를 나타내는 방법이 포함되어 있다. 본 연구에서 행한 수정중의 하나는 기하학적인 상수대신에 퍼만(Forman)의 탄성응력 강도계수 범위식을 이용하는 것이고, 다른 하나는 균열이 성장함에 따라 편심형단면으로 되면서 모멘트에 기인해 발생되는 굽힘효과를 고려하는 것이다. 이 방 법을 수명예측에 사용하면 용접구조물은 물론 기계구조물의 보다 정확한 수명예측이 가능할 것 이다.

  • PDF

Assessing interfacial fracture in orthotropic materials: Implementing the RIS concept with considering the T-stress term under mixed-mode I/II

  • Zahra Khaji;Mahdi Fakoor
    • Steel and Composite Structures
    • /
    • 제50권2호
    • /
    • pp.237-247
    • /
    • 2024
  • Research on interfacial crack formation in orthotropic bi-materials has experienced a notable increase in recent years, driven by growing concerns about structural integrity and reliability. The existence of a crack at the interface of bi-materials has a substantial impact on mechanical strength and can ultimately lead to fracture. The primary objective of this article is to introduce a comprehensive analytical model and establish stress relationships for investigating interfacial crack between two non-identical orthotropic materials with desired crack-fiber angles. In this paper, we present the application of the Interfacial Maximum Tangential Stress (IMTS) criterion, in combination with the Reinforcement Isotropic Solid (RIS) model, to investigate the behavior of interfacial cracks in orthotropic bi-materials under mixed-mode I/II loading conditions. We analytically characterize the stress state at the interfacial crack tip using both Stress Intensity Factors (SIFs) and the T-stress term. Orthotropic materials, due to their anisotropic nature, can exhibit complex crack tip stress fields, making it challenging to predict crack initiation behavior. The secondary objective of this study is to employ the IMTS criterion to predict the crack initiation angle and explore the notable impact of the T-stress term on fracture behavior. Furthermore, we validate the effectiveness of our approach in evaluating Fracture Limit Curves (FLCs) for interfacial cracks in orthotropic bi-materials by comparing our FLCs with relevant experimental data from existing literature.

작은 표면균열의 성장특성에 의한 수명예측 (A Fatigue Life Prediction by Growth Characteristics of a Small Surface Crack)

  • 서창민;임창순;강용구
    • 한국해양공학회지
    • /
    • 제3권2호
    • /
    • pp.617-617
    • /
    • 1989
  • This paper deals with a fatigue life prediction of a surface crack based on the experimentally obtained relationship between surface crack length ratio $a/a_{f}$ and cycle ratio $N/N_{f}$ using micro computer. Firstly $a/a_{f}$-$N/N_{f}$ curves obtained from experimental tests, were assumed as three curves UC(the upper limit curve), LC(the lower limit curve) and MC(the middle curve), and these were utilized to predict the fatigue life. Comparing the calculated values which represent the characteristics of crack growth behaviors from the three assumed curves with the experimental ones, it has been found that in the stable crack growth region, they coincide reasonably well each other. And the differences between the fatigue lives obtained from the assumed curves and the experimental fatigue life did not exceed 20%. Using the characteristics of $a/a_{f}$-$N/N_{f}$ curves, it is possible to predict the da/dN-Kmax curves and the S-$N_{f}$ curves.

작은 표면균열의 성장특성에 의한 수명예측 (A Fatigue Life Prediction by Growth Characteristics of a Small Surface Crack)

  • 서창민;임창순;강용구
    • 한국해양공학회지
    • /
    • 제3권2호
    • /
    • pp.108-117
    • /
    • 1989
  • This paper deals with a fatigue life prediction of a surface crack based on the experimentally obtained relationship between surface crack length ratio $a/a_{f}$ and cycle ratio $N/N_{f}$ using micro computer. Firstly $a/a_{f}$-$N/N_{f}$ curves obtained from experimental tests, were assumed as three curves UC(the upper limit curve), LC(the lower limit curve) and MC(the middle curve), and these were utilized to predict the fatigue life. Comparing the calculated values which represent the characteristics of crack growth behaviors from the three assumed curves with the experimental ones, it has been found that in the stable crack growth region, they coincide reasonably well each other. And the differences between the fatigue lives obtained from the assumed curves and the experimental fatigue life did not exceed 20%. Using the characteristics of $a/a_{f}$-$N/N_{f}$ curves, it is possible to predict the da/dN-Kmax curves and the S-$N_{f}$ curves.

  • PDF

복합조직강의 미시조직변화가 피로파괴전파에 미치는 영향 (The Effects of the Microstructural Change of Dual Phase Steel on Fatigue Fracture Propagation)

  • 오세욱;김웅집
    • 한국해양공학회지
    • /
    • 제5권2호
    • /
    • pp.58-66
    • /
    • 1991
  • Not only difference of fatigue crack growth and propagation behavior resulted from the grain size, the hardness ratio and volume fraction in M.E.F. dual phase steel composed of martensite in hard phase and ferrite in soft phase, but also the effects of the plastic constraint were investigated by fracture mechanics and microstructural method. The main results obtained are as follows: 1) The fatigue endurance of M.E.F. steel increases with decreasing the grain size, increasing the ratio of hardness and volume fraction. 2) The initiation of slip and crack occures faster as the stress level goes higher. These phenomena result from the plastic constraint effect of the second phase. 3) The crack propagation rate in the constant stress level is faster as the grain size gets larger, the ratio of hardness lower and volume fraction smaller.

  • PDF