This paper presents the ultrasonic characteristics of weldment and detectability of defects of weldment in Austenitic Stainless Steel Type 304 that is composed of mostly coolant piping system in nuclear power plants. The results of this experient show as follows: 1. When the ultrasonic beam detects the defects on the side of base metal and on the opposite side of weldment, the indications which was detected on the screen show different amplitude and different metal path each. 2. The ultrasonically estimated notch depth is generally oversized than actual notch depth. 3. It is easy for the false indication to show up on the screen because of columnar structure of weldment in austenitic stainless steel. 4. The higher frequencies of transducer have more difficulties to detect the defects of the opposite side of weldment because of ultrasonic attenuation in weldment and the longitudinal transmitter-receiver transducer is the most effective in detecting the opposite side defects of weldment.
In this paper the influence of postweld heat treatment on mechanical properties of SMAW and FCAW stainless steel weldments was examined and the obtained results are as follows ; (1) The amount of $\delta$-ferrite formed by SMAW and FCAW process decreased with increasing holding temperature and time in post weld heat treatment(PWHT), and it was found that the reduced ferrite was transformed into sigma phase after $800^{circ}C{\times}50hr$ PWHT. This sigma phase, even though it was very small, resulted in brittleness of dissimilar weldment between carbon steel and stainless steel in bending test, however in similar weldment between stainless steel and stainless steel was not occured. (2) The chemical composition of sigma phase was measured to 28-30%Cr, 7-9%Mo, 4-6Ni in 316L weldment, and also 35-37%Cr, 0.9-1.0Mo, 6-8%Ni in 309L weldment by EDS analysis.
The stress corrosion cracking(SCC) and hydrogen embrittlement cracking(HEC) characteristics of a weathering steel weldment were investigated in aerated acid-chloride solution. The electrochemical properties of weldment were investigated by polarization test and galvanic corrosion test. Weathering steel did not show passive behavior in the acid-chloride solution. Galvanic corrosion between the weld metal and the base metal was not observed because the base metal was anodic to the weld metal. The slow-strain-rate tests(SSRT0 were conducted at a constant strain rate o 7.87×{TEX}$10^{-7}${/TEX}/s at corrosion potential, and at potentiostatically controlled anodic and cathodic potentials. The weldment of weathering steel was susceptible to both anodic dissolution SCC and hydrogen evolution HEC.
In order to evaluate the proper fracture strength of microstructures in a steel weldment, smaller size loading ball than used for a conventional small punch(CSP) testing is required due to regional limitation on constitutive structures. In this study, the minimized loading ball(${\varphi}1.5mm$) and bore diameter of lower die(${\varphi}3mm$) were designed for an advanced small punch(ASP) test. The results obtained from the ASP test were compared with those from a CSP testing for a X20CrMoV121 steel weldment. It was found that the ASP test clearly showed the microstructural dependance on fracture strength and ductile-brittle transition behavior of the weldment. In the ASP test, especially, the cracks tend to initiate for various directions within hemispherical indentation region of an objective structure in SP test. This indicates that the evaluation of more proper fracture strength for F.L+CGHAZ, FGHAZ and ICHAZ can be performed by means of the ASP test in a steel weldment.
T/P92 steels are created for using USC boiler tube and header in next generation power plant. SP-Creep test and tensile creep test are performed to characterize creep for local structures of T/P92 steel weldment. The results are shown that P92 steel weldment is clearly superior than that of X20CrMoV121 steel weldment, which is widely used in supercritical power Plant. while fine gram HAZ is most weakest in X20 steel weldment, coarse grain HAZ is most weakest in P92.
In order to evaluate the proper fracture strength of microstructures in a steel weldment, smaller size loading ball than used for a conventional small punch(CSP) testing is required due to regional limitation on constitutive structures. In this study, the minimized loading ball(φ 1.5mm) and bore diameter of lower die(φ 3mm) were designed for an advanced small punch(ASP) test. The results obtained from the ASP test were compared with those from a CSP testing for a X20CrMoV121 steel weldment. It was found that the ASP test clearly showed the microstructural dependance on fracture strength and ductile-brittle transition behavior of the weldment. In the ASP test, especially, the cracks tend to initiate for various directions within hemispherical indentation region of an objective structure in SP test. This indicates that the evaluation of more proper fracture strength for F.L+CGHAZ, FGHAZ and ICHAZ can be performed by means of the ASP test in a steel weldment.
Journal of Advanced Marine Engineering and Technology
/
제12권1호
/
pp.47-54
/
1988
TMCP steel manufactured by controlled rolling followed by accelerated cooling process is known to have extra-ordinary mechanical properties such as tensile strength and toughness. However, there is much uncertainty about the fatigue fracture characteristics of this steel. In this paper, the fatigue fracture behaviour of the TMCP steel in base metal and weldment were inspected through the Dynamic Implant test method. Those results were quantitavely compared with those of the ordinary normalized steel of same strength level. Moreover, the effect of the diffusible hydrogen included in the welded part on the fatigue fracture behaviour were made clear. As the experimental results, the fatigue fracture characteristics of the TMCP steel in case of base metal proved out to be superior to that of the normalized steel. However, the TMCP steel weldment including the diffusible hydrogen appeared to have inferior fatigue characteristics compared with the same conditioned normalized steel weldment.
The research trend in the corrosion behaviour of stainless steel weldment has been reviewed. The welding technology plays an important role in the fabrication of structure such as chemical plant, power plant, because welding can influence various factors in the performance of plant and equipment. This has led to an increasing attention towards the corrosion behaviour of weldment which has been one of the major issues for both welding and corrosion research engineers. The aim of this paper is to give a short survey of the recent technical trends of welding and corrosion including the electrochemical corrosion, stress corrosion cracking, and corrosion fatigue in connection with the welding materials, welding process, and welding fabrication. This study covers the corrosion behaviour of stainless steel weldment collected from the COMPENDEX DB analysis of published papers, research subject and research institutes.
Cold rolled and high strength steel were used for vehicle bodys to satisfy environmental regulation and improve fuel ratio. This paper presented a method far determining the fatigue life of cold rolled steel sheet EZNCEN and high strength steel sheet HS40R spot weldment used in vehicles. We can estimate the fatigue life of the spot weldments from the MSC/FATIGUE using the finite element method. The maximum load is found in the nugget part of both surfaces. The cold rolled steel and the high strength steel showed the maximum stress 746MPa and 730MPa in the effective nugget part when the weld current was 8KA and 7KA, respectively. Also the some weld current of the cold rolled steel and high strength steel is applied, the fatigue life of high strength steel is obtained about four times longer than the cold rolled steel.
The influence of welding heat input variation(600-900J/cm) and heat-treatment condition after welding on tensile strength of butt welded joint in $175Kg/mm^2$ strength level Maraging steel(Co-free and Co-containing) sheets was investigated on the basis of hardness distribution, microstructure of weld metal and fracture surface. The obtained main results are as follows; 1. The strength of weldment (UTS, NTS), joint efficiency showed a little decreasing tendency with the increase in welding heat input, and the elongation showed a little increasing tendency with the increase in the width of weld metal. It was considered because of the plastic constraint of the high strength base metal. 2. The strength of weldment was better in the solution treatment and aging than the aging only after welding due to the disappearance of almost denverite in weld metal. 3. The hardness distribution in weldment after welding and heat-treatment was almost similar to both Co containing and Co free Maraging steel with change in welding heat input. 4. The fracture was occurred at weld metal, and the fracture surface showed a relatively shallow dimples in both Co containing and Co free Maraging steel.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.