• Title/Summary/Keyword: Specific wear amount

Search Result 25, Processing Time 0.02 seconds

Evaluation of Microscopic Wear Characteristics for CVD TiN Coatings with SEM Tribosystem (SEM Tribosystem에 의한 CVD TiN막의 미시적 마모 특성 평가)

  • 문봉호
    • Journal of the Korean institute of surface engineering
    • /
    • v.37 no.3
    • /
    • pp.137-145
    • /
    • 2004
  • This study surveys the microscopic wear of CVD TiN coatings in repeated sliding, using the SEM Tribosystem as in-situ system. According to the research, the depth of wear groove and the specific wear amount are changed by the transition of the microscopic wear mode. This investigation leads to the fact that the change of wear characteristics produces the transition of the wear mode. In this survey, four modes are observed for CVD TiN coatings with the thickness of 1.6$\mu\textrm{m}$: ploughing, powder formation, flake formation and coating delimitation. The microscopic wear properties is quantitatively evaluated in terms with the microscopic wear mode and the specific wear amount. These relationships prove that the observation of wear modes with a SEM Tribosystem is useful to evaluate wear properties.

An Experimental Study on the Specific Wear Amount of Base oil in Automotive Lubricant (자동차 윤활기유의 비마모량에 관한 실험적 연구)

  • Jeon, Chan-Yeal
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.10 no.3
    • /
    • pp.488-492
    • /
    • 2009
  • This paper have been analyzed specific wear characteristics of various base oils used in the automobile engine by experimental study. Specific wear amount has been calculated by the measured normal force and friction force under various speed operating conditions, such as, viscosities and temperatures. It have been verified that the specific wear characteristics relation of the base oil used in a engine oil is related to the various operating conditions.

Development of methodology for evaluating tribological properities of Ion-implanted steel (이온 주입한 강의 미시적 마모 튼성의 평가)

  • MOON, Bong-Ho;CHOI, Byung-Young
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.14 no.9
    • /
    • pp.146-154
    • /
    • 1997
  • Ion implantation has been used successfully as a surface treatment technology to improve the wear. fatigue and corrosion resistances of materials. A modified surface layer by ion implantation is very thin(under 1 m), but it has different mechanical properties from the substrate. It has also different wear characteristics. Since wear is a dynamic phenomenon on interacting surfaces with relative motion, an effective method for investigtating the wear of a thin layer is the observation of wear process in microscopic detail using in-situ system. The change of wear properties produces the transition of wear mode. To know the microscopic wear mechanism of this thin layer, it is very important to clarify its microscopic wear mode. In this paper, using the SEM and AFM Rribosystems as in-situ system, the microscopic wear of Ti ion-implanted 1C-3Cr steel, a material for roller in the cold working process, was investigated in repeated sliding. The depth of wear groove and the speciffc wear amount were changed with transition of microscopic wear mode. The depth of wear groove with friction cycles in AFM tribosystem and specific wear amount of Ti ion-implanted 1C-3Cr steel were less about 2-3 times than those of non-implanted 1C-3Cr steel. The microscopic wear mechansim of Ti ion-implanted 1C-3Cr steel was also clarified. The microscopic wear property was quantitatively evaluated in terms of microscopic wear mode and specific wear amount.

  • PDF

Fracture and Wear Characteristics of Al-Si alloy used for Compressor (컴프레서용 Al-Si 합금의 파괴 및 마모 특성)

  • 김재훈;김덕회
    • Tribology and Lubricants
    • /
    • v.15 no.2
    • /
    • pp.141-149
    • /
    • 1999
  • Fracture, fatigue and wear characteristics of Al-Si alloy used for compressor are experimentally studied. Plane strain fracture toughness test is carried out using three point bending specimen. Fatigue test is performed under constant loading condition and wear test is carried out as a function of sliding velocity and applied load. To obtain the crack propagation characteristics and wear mechanism of Al-Si alloy, fracture and worn surfaces are investigated using SEM. It is verified that fracture and fatigue strength of Al-Si alloy are improved by the fine microstructure of alloy. The wear behavior and specific wear amount of Al-Si alloy are not dependent on the microstructure but on a function of the silicon content. Anodizing on the surface of Al-Si alloy, surface hardness and wear characteristics are improved.

Characteristics of Hardness and Wear-Resistance of Plasma-Nitrided and Nitrocarburized Carbon Steels (플라즈마질화 및 침질탄화처리한 탄소강의 경도와 내마모특성)

  • Kim, M.K.;Jung, B.H.;Park, H.S.;Lee, B.C.;Shin, S.H.;Lee, J.S.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.12 no.2
    • /
    • pp.166-173
    • /
    • 1999
  • Commercial carbon steels containing 0.2~0.55 wt.----C were plasma-nitrided or plasma nitrocarburized at $550^{\circ}C$ for 21.6Ks using $H_2-N_2$ or $H_2-N_2$-CO mixed gas respectively. The characteristics of hardening and wear-resistance of each treatment were studied and compared. And also microstructure of nitrided layer and nitrides formed in compound layer near surface were studied. All plasma-nitrided steels investigated showed remarkable increase of surface hardness with the increase of carbon content. But nitrocarburized steels resulted in higher surface-hardness than plasma-nitrided steels, which means that nitrocarburized has higher surface-hardening effect. Plasma-nitrided steels showed hardness increase in through-thickness direction near surface. And also nitrocarburized steels showed similar hardness distribution in through-thickness direction to that of plasma-nitrided steel. However, nitrocarburized steels had higher cross-sectional maximum-hardness than plasma-nitrided steels as much as 100Hv. Wear test showed that the amount of specific wear was reduced by both plasma-nitriding and nitrocarburized, showing that the amount of specific wear was not related to the hardness. But non-treated specimen showed that the amount of specific wear was related to the hardness.

  • PDF

Development of Automatic Measuring Device for Cylinder Liner Wear Amount in Large Two Stroke Diesel Engine (대형 저속 디젤 엔진용 실린더 라이너 내면 마모량 자동 측정 장치 개발)

  • Kim, Jang-Kyu;Lee, Min-Cheol
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.32 no.6
    • /
    • pp.981-988
    • /
    • 2008
  • This paper describes a development of automatic measuring device for cylinder liner wear amount. An operator should regularly measure the wear amount of the cylinder liner to prevent the wear amount of the cylinder liner from exceeding the maximum limit specific to the engine type. In previous methods. an operator entered the inside of the cylinder liner on a ladder and measured the amount of wear using a inside micrometer. Such method is unpleasant in severe environments and full of hazards. In addition, in order to enter the cylinder, the piston head had to be detached. requiring much time and money. In order to solve these problems, a new measuring device that consists of two measuring units and a special install jig is developed. The measuring units are installed through the scavenging air port by the install jig and measures the wear amount during 1 revolution of crankshaft. so detaching of the cylinder head and entering inside the cylinder liner are not required.

Wear Behaviors of Ceramics TIN, TIC and TICN with Arc Ion Plating

  • Oh, Seong-Mo;Rhee, Bong-Goo;Jeong, Bong-Soo
    • Journal of Mechanical Science and Technology
    • /
    • v.17 no.12
    • /
    • pp.1904-1911
    • /
    • 2003
  • In order to determine the wear properties of AIP (Arc Ion Plating) deposition, wear process was evaluated by using a Falex test machine. Also, in order to determine the effects of coating material on the wear process, TiC, TiN, and TiCN coatings of thickness about 5 $\mu\textrm{m}$∼6 $\mu\textrm{m}$ coated by Arc ion plating deposition method were tested. The wear property was determined under a dry sliding condition as a function of the applied load, sliding distance, sliding velocity and temperature. The results show that when wear of the coating-layer occurred, specific wear amount increased with the wear rate. At initial state, the wear rate rapidly increased, but it gradually reduced as the velocity increased. Also, when raising the temperature, the wear rate increased in the order of TiCN, TiN and TiC due to the frictional heat.

Effect of the Amount of Free Silicon on the Tribological Properties of Si-SiC (Free Silicon 함량에 따른 Si-SiC 복합재료의 마찰 마모 특성)

  • 김인섭;이병하
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.5
    • /
    • pp.520-528
    • /
    • 1994
  • An investigation was carried out to understand the effect of the amount of free silicon on the tribological properties of Si-SiC. The specimens of dense Si-SiC composites with various amount of free silicon were fabricated in the temperature of 175$0^{\circ}C$ after molding under various pressure. Wear properties were measured by ball-on-plate wear tester under the constant weight of 4 Kgf at constant sliding speed of 500 mm/sec in water. As the result, the Rockwell hardness and fracture strength of Si-SiC composites remained nearly constant up to 16.62 vol% of free silicon in the Si-SiC microstructure. The Si-SiC composites containing the free silicon of 16.62 vol% was considered to be prominent in the tribological properties, which had the friction coefficient of 0.08 and the specific wear rate of 2.4$\times$10-8$\textrm{mm}^2$Kgf-1. The analysis of the wear surface indicated the complicated processes occuring on the surface such as fine polishing, abrasion, microfracture.

  • PDF

Wear Characteristics of Cylinder-Liner Materials for Diesel Engine at Elevated Temperature (디젤엔진용 실린더 라이너 소재의 고온 마모특성)

  • Kim, Jin-Yeol;Kim, Jae-Hoon;Oh, Kwang-Keun;Lee, Seung-Hak;Chang, Joon-Yong
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.39 no.11
    • /
    • pp.1131-1136
    • /
    • 2015
  • In a diesel engine, the wear of the cylinder liner occurs because of the continuous reciprocating motion of the piston ring. This wear reduces the performance of the diesel engine and shortens its service life. This study evaluated the wear characteristics of GT metal and a conventional metal used for cylinder liners using a ship's diesel engine. Wear tests were performed at temperatures of $25^{\circ}C$, $175^{\circ}C$, and $325^{\circ}C$, and under loads of 10 N, 30 N, and 50 N. The amount of wear, specific wear rate, and friction coefficient were evaluated for each condition. To analyze the wear mechanism, observations were made on an SEM. In the case of both metals, abrasive and adhesion wear occurred on the wear surfaces at room temperature, and corrosion wear was observed at high temperatures. The amount of wear and the specific wear rate of the GT metal were lower than those of the conventional metal at all temperatures, and hence it can be concluded that the wear characteristics of the GT metal are much better.

High temperature Friction and Wear of Friction Material; The Effect of the Relative Amount of Graphite and Zirconium Silicate (ZrSiO$_4$) (흑연과 지르콘의 상대적 함량에 따른 마찰재의 고온 마찰 및 마모특성)

  • Kim, Seong-Jin;Jang, Ho
    • Tribology and Lubricants
    • /
    • v.16 no.5
    • /
    • pp.365-372
    • /
    • 2000
  • Tribological behavior of novolac resin-based friction materials with three different relative amounts of graphite and zirconium silicate was investigated by using a pad-on-disk type friction tester. The goal of this paper is to examine the effects of the relative amount of a lubricant and an abrasive in the automotive friction material on friction and wear characteristics at elevated temperature. Friction and wear of friction materials were affected by the existence of transfer film(3$\^$rd/ body layer) at friction interface and the composition of friction material, especially lubricant amount. The friction material with higher content of graphite indicated homogenized and durable transfer film, and resulted in stable friction coefficient regardless of the increase in friction heat. The experimental result also showed that the higher concentration of ZrSiO$_4$ in friction material aggravated friction stability and wear resistance due to the higher friction heat generated at fiction interface during high temperature friction test.