Magnetocaloric Effect of LaPbMnO3 Alloy (LaPbMnO3 합금의 자기열량효과)

  • Min, Seong-Gi;Kim, Kyeong-Sup;Yu, Seong-Cho;Moon, Young-Mo
    • Journal of the Korean Magnetics Society
    • /
    • v.15 no.4
    • /
    • pp.236-240
    • /
    • 2005
  • The magnetocaloric effect and magnetization behaviors have been studied for $La_{1-x}Pb_{x}MnO_3$ (x=0.1, 0.2, 0.3) alloys. The Curie temperature increased from 195 K to 352 K with increasing Pb concentration. A large magnetic entropy change (${\Delta}S_M$), which is calculated from H vs M curves associated with the ferromagnetic-paramagnetic transitions, has been observed. The maximum ${\Delta}S_M$ of $La_{0.8}Pb_{0.2}MnO_3$ was 1.22 J/kg K at 294 K for an applied field of 1.5 T. Adiabatic temperature change (${\Delta}T_ad$) was measured directly by a special cryostat. The maximum ${\Delta}T_ad$ of $La_{0.7}Pb_{0.3}MnO_3$ was 1.00 K at 352 K for an applied field of 2 T.

Manufacturing of Hybrid Metal Matrix Composites used $Al_2O_3$ Short Fiber and $Al_2O_3$-TiC Composite Powder Synthesized by SHS Process (SHS법에 의해 제조된 $Al_2O_3$-TiC복합분말과 $Al_2O_3$단섬유를 강화재로 사용한 하이브리드 금속기 복합재료의 제조)

  • Kim, Dong-Hyeon;Maeng, Deok-Yeong;Lee, Jong-Hyeon;Won, Chang-Whan
    • Korean Journal of Materials Research
    • /
    • v.9 no.3
    • /
    • pp.315-321
    • /
    • 1999
  • Metal matrix composites have been extensively studied because of their excellent characteristics for structural application. $Al_2O_3$ and SiC have been used as a common reinforcement owing to their good mechanical properties. However the manufacturing cost of these ceramic reinforcement is expensive, so the use of the composites has been restricted to special purposes. In this study, we tested the application possibility as a reinforcement of $Al_2O_3$-TiC powder synthesized by SHS(Self-propagating High-temperature Synthesis) process to Al alloy matrix composite. Also, $Al_2O_3$ short fibers were added with the synthesized powders in order to apply to the Al matrix hybrid composites. Squeeze infiltration casting process was used to make the composite with 25vol% of reinforcement. Microstructure and crystal structure were examined by SEM, OM and XRD, also the mechanical properties were studied by the compressive test and wear test.

  • PDF

Transitions in Bronze Technology Observed in Bronze Artifacts Excavated from the Shilla Wang-Gyong (신라왕경 출토 청동유물에서 확인되는 청동기 제작기술의 변천)

  • Jeong, Young-Dong;Park, Jang-Shik
    • Korean Journal of Heritage: History & Science
    • /
    • v.37
    • /
    • pp.267-284
    • /
    • 2004
  • As an initial step to understand the transitions in Korean bronze technology the present study has examined metallurgical microstructures of 8 artifacts excavated from the Silla Wang-Gyong site in Kyongju. Important trends have been found in alloy compositions and also in manufacturing processes. In the design of alloys, the Sn content was apparently changing toward the peritectic point, 22 mass %, of the Cu-Sn phase diagram while the Pb addition was intentionally avoided. This trend in composition was found accompanied by the introduction, subsequent to casting, of such special thermo-mechanical treatments as quenching and forging in artifact manufacture. In addition, the Sn content in alloys containing a significant amount of As was relatively low and no evidence of forging was observed in them. The use of quenching and forging and the rejection of Pb and As from alloys are all necessary requirements if the brittle nature of high Sn alloys is to be overcome in bronze working. This paper will show that the Wang-Gyong era corresponds to that of innovations leading to the technical climax in Korean bronze tradition, which has been maintained up to the present.

THE BOND CHARACTERISTICS OF PORCELAIN FUSED BY TITANIUM SURFACE MODIFICATION (타이타늄의 표면개질에 따른 도재 결합 특성)

  • Choi, Taek-Huw;Park, Sang-Won;Vang, Mong-Sook;Yang, Hong-So;Park, Ha-Ok;Lim, Hyun-Pil;Oh, Gye-Jeong;Kim, Hyun-Seung;Lee, Kwang-Min;Lee, Kyung-Ku
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.2
    • /
    • pp.169-181
    • /
    • 2007
  • Statement of problem: Titanium is well known as a proper metal for the dental restorations, because it has an excellent biocompatibility, resistance to corrosion, and mechanical property. However, adhesion between titanium and dental porcelains is related to the diffusion of oxygen to the reaction layers formed on cast-titanium surfaces during porcelain firing and those oxidized layers make the adhesion difficult to be formed. Many studies using mechanical, chemical and physical methods to enhance the titanium-ceramic adhesion have been actively performed. Purpose: This study meant to comparatively analyse the adhesion characteristics depending on different titanium surface coatings after coating the casts and wrought titanium surfaces with Au and TiN. Material and method: In this study, the titanium specimens (CP-Ti, Grade 2, Kobe still Co. Japan) were categorized into cast and wrought titanium. The wrought titanium was cast by using the MgO-based investment(Selevest CB, Selec). The cast and wrought titanium were treated with Au coating($ParaOne^{(R)}$., Gold Ion Sputter, Model PS-1200) and TiN coating(ATEC system, Korea) and the ultra low fusing dental porcelain was fused and fired onto the samples. Biaxial flection test was done on the fired samples and the porcelain was separated. The adhesion characteristics of porcelain and titanium after firing and the specimen surfaces before and after the porcelain fracture test were observed with SEM. The atomic percent of Si on all sample surfaces was comparatively analysed by EDS. In addition, the constituents of specimen surface layers after the porcelain fracture and the formed compound were evaluated by X-ray diffraction diagnosis. Result: The results of this study were obtained as follows : 1. The surface characteristics of cast and wrought titanium after surface treatment(Au, TiN, $Al_2O_3$ sandblasting) were similar and each cast and wrought titanium showed similar bonding characteristics. 2. Before and after the biaxial flection test, the highest atomic weight change of Si component was found in $Al_2O_3$ sandblasted wrought titanium(28.6at.% $\rightarrow$ 8.3at.%). On the other hand, the least change was seen in Au-Pd-In alloy(24.5at.% $\rightarrow$ 9.1at.%). 3. Much amount of Si components was uniformly distributed in Au and TiN coated titanium, but less amount of Si's was unevenly dispersed on Al2O3 sandblasting surfaces. 4. In X-ray diffraction diagnosis after porcelain debonding, we could see $Au_2Ti$ compound and TiN coating layers on Au and TiN coated surfaces and $TiO_2$, typical oxide of titanium, on all titanium surfaces. 5. Debonding of porcelain on cast and wrought titanium surface after the biaxial flection is considered as a result of adhesion deterioration between coating layers and titanium surfaces. We found that there are both adhesive failure and cohesive failure at the same time. Conclusion: These results showed that the titanium-ceramic adhesion could be improved by coating cast and wrought titanium surfaces with Au and TiN when making porcelain fused to metal crowns. In order to use porcelain fused to titanium clinically, it is considered that coating technique to enhance the bonding strength between coating kKlayers and titanium surfaces should be developed first.

Influence of taper on the screw-in effect of nickel-titanium rotary files in simulated resin root canal (모형 레진근관에서 니켈-티타늄 전동 파일의 경사도가 screw-in effect에 미치는 영향)

  • Sung, Hye-Jin;Ha, Jung-Hong;Kim, Sung-Kyo
    • Restorative Dentistry and Endodontics
    • /
    • v.35 no.5
    • /
    • pp.380-386
    • /
    • 2010
  • Objectives: The introduction of nickel-titanium alloy endodontic instruments has greatly simplified shaping the root canal systems. However, these new instruments have several unexpected disadvantages. One of these is tendency to screw into the canal. In this study, the influence of taper on the screw-in effect of the Ni-Ti rotary instrument were evaluated. Materials and Methods: A total of 20 simulated root canals with an S-shaped curvature in clear resin blocks were divided into two groups. ProFile .02, .04, .06 (Dentsply-Maillefer) and GT rotary files .08, .10, .12 (Dentsply) were used in Profile group, and K3 .04, .06, .08, .10, and .12 (SybronEndo, Glendora) were used in K3 group. Files were used with a single pecking motion at a constant speed of 300 rpm. A special device was made to measure the force of screw-in effect. A dynamometer of the device recorded the screwin force during simulated canal preparation and the recorded data was stored in computer with designed software. The data were subjected to one-way ANOVA and Tukey's multiple range test for post-hoc test. p value of less than 0.05 was regarded significant. Results: The more tapered instruments generated more screw-in forces in Profile group (p < 0.05). In K3 group, 0.08, 0.10. and 0.12 tapered instruments showed more screw-in force than 0.04 tapered one, and 0.08 and 0.12 tapered instruments showed more screw-in force than 0.06 tapered one (p < 0.05). Conclusions: The more tapered instruments seems to produce more screw-in force. To avoid this screw-in force during instrumentation, more attention may be needed when using more tapered instruments.