• Title/Summary/Keyword: Solidification cracking

Search Result 67, Processing Time 0.026 seconds

A Study on Hot Cracking in Ni-Base Superalloy Welds (I) - Effect of Fe Contents on Solidification Cracking Susceptibility in Weld Metal - (Ni기 초내열합금 용접부의 고온균열에 관한 연구(I) - 용접금속의 응고균열 감수성에 미치는 Fe의 영향 -)

  • ;;Kazutoshi Nishimoto
    • Journal of Welding and Joining
    • /
    • v.19 no.6
    • /
    • pp.614-621
    • /
    • 2001
  • A study was carried out to determine the solidification cracking susceptibility of Ni-base superalloy as a function of Fe content in base metal. Three kinds of Ni-base superalloys with three different levels of Fe content were used. The solidification cracking susceptibility was evaluated by the Trans-Varestraint test at four different strain levels. Quantitative analysis of crack revealed that the solidification crack length and the temperature range in which hot cracking occurred in fusion zone (Brittle Temperature Range, BTR) decreased with a decrease in Fe content. Further, the thermo-calc data indicated that the solidification temperature range also decreased with decreasing Fe content. From these results, it was deduced that the improvement of the solidification cracking susceptibility with decreasing Fe content was attributed to the decrease of the solidification temperature range.

  • PDF

SOLIDIFICATION CRACKING SUSCEPTIBILITY OF

  • Yoon, Jong-Won
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.577-582
    • /
    • 2002
  • The solidification cracking susceptibilities of AI-Mg-Si alloy laser welds were assessed using the self-restraint tapered specimen crack test. The cracking susceptibility of 6061 and 6082 Al-Mg-Si alloy laser welds was substantially reduced when the filler wire containing high Si such as Al-12 wt.% Si (4047A) was used. The amount of eutectic was observed to affect the solidification cracking of Al-Mg-Si alloy laser welds. Abundant eutectic seems to heal the cracking and reduces the cracking susceptibility, while an initial increase in eutectic liquid leads to the increased cracking tendency.

  • PDF

A Study on the Cracking Behavior in the Welds of Ni-Cr-Fe and Ni-Fe-Cr-Mo Alloys Part I : Solidification Cracking in the Fusion Zone (Ni-Cr-Fe 및 Ni-Fe-Cr-Mo계 합금의 용접부 균열특성에 관한 연구 Part I : 용착금속의 응고균열)

  • 김희봉;이창희
    • Journal of Welding and Joining
    • /
    • v.15 no.4
    • /
    • pp.78-89
    • /
    • 1997
  • This study has evaluated the weld metal solidification cracking behavior of several Ni base superalloys (Incoloy 825, Inconel 718 and Inconel 600). Austenitic stainless steels(304, 310S) were also included for comparison. In addition, a possible mechanism of solidification cracking in the fusion zone was suggested based on the extensive microstructural examinations with SEM, EDAX, TEM, SADP and AEM. The solidification cracking resistance of Ni base superalloys was found to be far inferior to that of austenitic stainless steels. The solidification cracking of Incoloy 825 and Inconel 718 was believel to be closely related with the Laves-austenite (Ti rich in 825 and Nb rich in 718) and MC-austenite eutectic phases formed along the grain boundaries during solidification. Cracking in Inconel 600 was always found along the grain boundaries which were enriched with Ti and P. Further, solidifidcation cracking resistance was dependent not only upon the type of love melting phases but also on the amount of the phases along the solidification grain boundaries.

  • PDF

A Study of Metallurgical Phenomena in Austenitic Stainless Steel Fusion Welds (I) -Weldability of Commercial Austenitic Stainless Steels- (오스테나이트계 스테인리스강 용접부의 금속학적 현상에 관한 연구(I) - 시판 오스테나이트계 스테인리스강의 용접성 -)

  • 이종섭;김숙환
    • Journal of Welding and Joining
    • /
    • v.16 no.3
    • /
    • pp.111-120
    • /
    • 1998
  • To predict and evaluate metallurgical and mechanical behavior of th welds, it is essential to understand solidification behavior and microstructural evolution experienced in the welds, neither of which follows the equilibrium phase diagram because of rapid heating and cooling conditions. Metallurgical phenomena in austenitic stainless steel fusion welds, types 304, 309S, 316L, 321 and 304N, were investigated in this study. Autogenous GTA welding was performed on weld coupons, and primary solidification mode and phase distribution were investigated from the welds. Varestraint test was employed to evaluate solidification cracking susceptibilities of the alloys. GTA weld fusion zones in type 304, 321 and 304N stainless steels experienced primary ferrite solidification while those in type 309S primary austenite solidification. Type 316L exhibited a mixed type of primary ferrite and primary austenite solidification. The primary solidification mode strongly depended on $Cr_{eq}/Ni_{eq}$ ratio. In terms of solidification cracking susceptibility, type 309S that solidified as primary austenite exhibited high cracking susceptibility while the alloys experienced primary ferrite solidification showed low cracking susceptibility. The relative ranking in solidification cracking susceptibility was type 304=type 304N < type 321 < type 316L < type 309S.

  • PDF

Solidification Cracking Susceptibility of Al-Mg-Si Alloy Laser Welds

  • Yoon, J.W.
    • International Journal of Korean Welding Society
    • /
    • v.2 no.2
    • /
    • pp.42-46
    • /
    • 2002
  • The solidification cracking susceptibilities of Al-Mg-Si alloy laser welds were assessed using the self-restraint tapered specimen crack test. The cracking susceptibility of 6061 and 6082 Al-Mg-Si alloy laser welds was substantially reduced when the filler wire containing high Si such as Al-12 wt.% Si (4047A) was used. The amount of eutectic was observed to affect the solidification cracking of Al-Mg-Si alloy laser welds. Abundant eutectic seems to heal the cracking and reduces the cracking susceptibility, while an initial increase in eutectic liquid leads to the increased cracking tendency.

  • PDF

The Effect of Primary Solidification Mode on Physical Properties of Austenitic Stainless Steels (오스테나이트계 스텐리스 강의 물성에 미치는 초정응고 형식의 영향)

  • 정호신
    • Journal of the Korean Society of Fisheries and Ocean Technology
    • /
    • v.26 no.4
    • /
    • pp.372-379
    • /
    • 1990
  • The effect of primary solidification phase on the solidification cracking sensitivity, corrosion resistance and toughness at cryogenic temperature was investigated for the austenitic stainless steel welds. The conclusions were summarized as follows; 1. Soldification crack sensitivity of austenitic stainless steel welds depends on the primary solidification mode. 2. Austenitic stainless steels were very susceptible to solidification cracking in case of solidification as primary ${\gamma}$ and immune when solidified as primary $\delta$. 3. When the ratio of Creq/Nieq is in the range of 1.46 to 1.55, the most resistance against solidification cracking was obtained. These results agreed well with the relationship between primary solidification mode, corrosion resistance and toughness at cryogenic temperature. 4. Optimum toughness, corrosion and solidification cracking resistance can be obtained when alloys having chemical compositions described above and solidifies as primary $\delta$ containing no ferrite at room temperature.

  • PDF

A Study of Weld Fusion Zone Phenomena in Austenitic Stainless Steels(2) - Effects of Nitrogen on Microstructural Evolution and Hot Cracking Susceptibility GTA Welds in STS 304 - (오스테나이트계 스테인리스강 용접부의 금속학적 현상에 관한 연구(2) - STS 304 용접부 조직특성 및 고온균열 감수성에 미치는 질소의 영향 -)

  • 이종섭;김숙환
    • Journal of Welding and Joining
    • /
    • v.18 no.1
    • /
    • pp.59-69
    • /
    • 2000
  • The purpose of the present study was to investigate weld metallurgical phenomena such as primary solidification mode, microstructural evolution and hot cracking susceptibility in nitrogen-bearing austenitic stainless steel GTA welds. Eight experimental heats varying nitrogen content from 0.007 to 0.23 wt.% were used in this study. Autogenous GTA welding was performed on weld coupons and the primary solidification mode and their microstructural characteristics were investigated from the fusion welds. Varestraint test was employed to evaluate the solidification cracking susceptibility of the heats and TCL(Total Crack Length) was used as cracking susceptibility index. The solidification mode shifted from primary ferrite to primary austenite with an increase in nitrogen content. Retained delta ferrite exhibited a variety of morphology as nitrogen content varied. The weld fusion zone exhibited duplex structure(austenite+ferrite) at nitrogen contents less than 0.10 wt.% but fully austenitic structure at nitrogen contents more than 0.20 wt.%. The weld fusion zone in alloys with about 0.15 wt.% nitrogen experienced primary austenite + primary ferrite solidification (mode AF) and contained delta ferrite less than 1% at room temperature. Regarding to solidification cracking susceptibility, the welds with fully austenitic structure exhibited high cracking susceptibility while those with duplex structure low susceptibility. The cracking susceptibility increased slowly with an increase in nitrogen content up to 0.20 wt.% but sharply as nitrogen content exceeded 0.20 wt.%, which was attributed to solidification mode shift fro primary ferrite to primary austenite single phase solidification.

  • PDF

Solidification Cracking Behavior in Austenitic Stainless Steel Laser Welds (Part 1) - Evaluation of Solidification Cracking Susceptibility by Laser Beam Welding Varestraint Test - (오스테나이트계 스테인리스강 레이저 용접부의 응고균열 거동 (Part 1) - 레이저 용접용 Varestraint 시험 시스템을 이용한 응고균열 민감도 평가 -)

  • Chun, Eun-Joon;Lee, Su-Jin;Suh, Jeong;Kang, Namhyun;Saida, Kazuyoshi
    • Journal of Welding and Joining
    • /
    • v.34 no.5
    • /
    • pp.54-60
    • /
    • 2016
  • In order to quantitatively evaluate the solidification cracking susceptibility in laser welds of three types of austenitic stainless steels (type 310: A mode, type 316-A: AF mode, type 316-B: FA mode solidifications), the laser beam welding (LBW) transverse-Varestraint tests consisted of multi-mode fiber laser, welding robot and hydraulic pressure system were performed. As the welding speed increased from 1.67 to 40.0 mm/s, the solidification brittle temperature range (BTR) of laser welds for type 316 stainless steels enlarged (316-A: from 37 to 46 K, 316-B: from 14 to 40 K), while the BTR for type 310 stainless steel reduced from 146 to 120 K. In other words, it founds that solidification cracking susceptibility could not be simply mitigated through application of LBW process, and the BTR variation behavior is quite different upon solidification mode of austenitic stainless steels.

Effect of Scrap Addition Ratio on Tensile and Solidification Cracking Properties of AC4A Aluminum Casting Alloy (AC4A 알루미늄 합금의 인장 및 응고균열 특성에 미치는 스크랩 첨가 비율의 영향)

  • Oh, Seung-Hwan;Kim, Heon-Joo
    • Journal of Korea Foundry Society
    • /
    • v.40 no.3
    • /
    • pp.85-96
    • /
    • 2020
  • The effect of an aluminum scrap addition ratio on the tensile and solidification cracking properties of the AC4A aluminum alloy in the as-cast state and heat-treated state were investigated in this study. Generally, the expected problem of using scrap in aluminum casting is an increase of hydrogen and Fe element inside the aluminum melt. Another issue is an oxide film which has a weak interface with the molten aluminum and acts as potent nucleation sites for internal porosity and crack initiation. Solidification cracking is one of the critical defects that must be resolved to produce high quality castings. A conventional evaluation method for solidification cracking is a relative and qualitative analysis method which does not provide quantitative data on the thermal stress in the solidification process. Therefore, a newly designed solidification cracking test apparatus was used in this study, and the device can provide quantitative data. As a result, after conducting experiments with different scrap addition ratios (0%, 20%, 35%, 50%), the tensile strengths and elongations in the as-cast state were 214, 187.7, 182.1 and 170.4MPa and 4.6%, 3.4%, 3.1% and 2.3%, respectively. In the case of the T6 heat-treated state, the tensile strengths and elongations were 314.9, 294.6, 293.1 and 271.1MPa and 5.4%, 4.6%, 3.8% and 3.1%, respectively. The strength of the solidification cracking was 3.1, 2.4, 2.2and 1.6MPa as the scrap addition ratio increases.

Solidification Crackin in Root Pass for One-side Welding of 590MPa Class Steel for Pressure Vessels by FCAW (FCAW에 의한 590MPa급 고장력압력용기강의 초층편면용접부에서 발생하는 고온균열)

  • 김우열;한일욱;유덕상;방한서;안용식;박화순
    • Journal of Welding and Joining
    • /
    • v.17 no.5
    • /
    • pp.47-54
    • /
    • 1999
  • It is well known that solidification cracking often occurs in welds of root pass for one-side welding under the conditions of high welding currents and speeds. In this study, the solidification in 590MPa class steel for pressure vessels SPPV490 was investigated by using flux-cored arc welding(FCAW) with 4 types of welding wires and welding conditions of 200∼280A and 2.8∼ 4.2mm/sec. In order to compared the result of cracking in SPPV490, 0.2%C steel for welded structure of SWS400 and 0.45%C steel for machine structural SM45C were also used as base metals. As the results, all the cracks formed in some welding conditions were observed near the center of weld bead. The solidification cracks were generally initiated near the upper surface of bead and propagated toward the inner part. The solidification cracking generally increased with welding current and welding speed in the same base metal and welding material. In cracking susceptibility, SPPV490 showed higher cracking susceptibility than SWS400 in all welding conditions and welding materials. It was considered that cracking susceptibility could not be evaluated with the hardness of weld metals. The cracking ratio increased with decreasing of a/b(a and b; the width of the upper surface and the back surface of the bead) as shape factor of bead. The cracking tendency with shape factor of bead was extended under the condition of higher welding currents.

  • PDF