Continuous Nanocomposite Coatings on a Phosphor for the Enhancement of the Long-term Stability

  • Kim, Jong-Woung;Song, Jung-Oh;Kim, Chang-Keun
    • 한국고분자학회:학술대회논문집
    • /
    • 한국고분자학회 2006년도 IUPAC International Symposium on Advanced Polymers for Emerging Technologies
    • /
    • pp.233-233
    • /
    • 2006
  • [ $Y_{2}O_{2}S:Eu$ ], a red phosphor, coated with silica nanoparticles or nanocomposites composed of silica nanoparticles and polymeric materials such as PMMA and PVP was prepared via sol-gel process. Samples were prepared from four different methods coded P1, P2, P3, and P4. P1 includes a conventional sol-gel process and a dip-coating method while P2 has the same procedure with P1 except that nanocomposites containing both silica nanoparticles and polymer prepared by sol-gel process were used as coating materials. In P3 method, phosphors were dispersed in a solution containing silica precursor, i.e., TEOS and then polymerization was performed to coat onto the phosphors surface while P4 followed the same procedure with P3 except that a solution containing both TEOS and organic monomer were used in preparing coating materials. Among various coating methods examined in this study, uniform coating of phosphor could be achieved by using method P4, i.e., phosphor surface coating in a solution containing hydrophobic monomer and TEOS. Furthermore, $Y_{2}O_{2}S:Eu$ red phosphor coated with nanocomposite composed of PMMA matrix and silica nanoparticles exhibited enhanced PL intensity and long-term stability.

  • PDF

Electrical Properties of Sol-Gel Derived Ferroelectric Bi3.35Sm0.65Ti3O12 Thin Films

  • Kang, Dong-Kyun;Cho, Tae-Jin;Kim, Byong-Ho
    • 한국세라믹학회지
    • /
    • 제42권3호
    • /
    • pp.150-154
    • /
    • 2005
  • Ferroelectric $Bi_{3.35}Sm_{0.65}Ti_{3}O_{12}(BSmT)$ thin films were synthesized by sol-gel process. In this experiments, $Bi(TMHD)_{3},\;Sm_{5}(O^{i}Pr)_{13},\;Ti(O^{i}Pr)_4$ were used as precursors, which were dissolved in 2-methoxyethanol. The BSmT thin films were deposited on the Pt/TiO/SiO/Si substrates by spin-coating. Thereafter, the thin films with the thickness of 240 nm were annealed from 600 to $720^{\circ}C$ in oxygen atmosphere for 1 h, and post-annealed in oxygen atmosphere for 1 h after deposition of Pt electrode to enhance the electrical properties. To investigate the effects of Sm-substitution in the BTO thin films, the BTO and BSmT thin films were prepared, respectively. The remanent polarization and coercive voltage of the BSmT thin films annealed at $720^{\circ}C$ were $19.48{\mu}C/cm^2$ and 3.40 V, respectively.

알콕사이드로부터 $Al_2O_3-TiO_2$계 복합분체의 합성(I) 1. Sol-Gel법에 의한 $Al_2TiO_5$ 분말합성과 첨가제의 영향 (Preparation of $Al_2O_3-TiO_2$ Composite Powder from Alkoxides (I) 1. Preparation of $Al_2TiO_5$ by the SOl-gel Method and the effects of Additives)

  • 정종열;이형민;이홍림
    • 한국세라믹학회지
    • /
    • 제33권10호
    • /
    • pp.1138-1146
    • /
    • 1996
  • Al2TiO5 powder was prepared by the sol-gel processing from th metal alkoxides ; aluminium sec-butoxide (Al(OC4H9)3 and tetraethyl orthotitanate (Ti(OC2H5)4) The particles of Al2TiO5 produced from alkoxides were measured to be below $1.5mutextrm{m}$ and mre than 90% weere below 1 ${\mu}{\textrm}{m}$ however those from commercial alumina and titania were over 0.5-7${\mu}{\textrm}{m}$ and only 60% were below 1${\mu}{\textrm}{m}$ and 90% were below 2.5${\mu}{\textrm}{m}$ Therefore Al2TiO5 powder produced from alkoxides had the narrower distributionin size than that produced from the commercial alumina and titania powders. The addition of mullite or Al2O3 powder to the prepared aluminum titanate inhibited the grain growth and this resulted in decreased and increase in density.

  • PDF

Microwave Sol-Gel Derived NaGd(MoO4)2:Ho3+/Yb3+ Phosphors and Their Upconversion Photoluminescence Properties

  • Lim, Chang Sung
    • Transactions on Electrical and Electronic Materials
    • /
    • 제18권6호
    • /
    • pp.364-369
    • /
    • 2017
  • Double molybdate $NaGd_{1-x}(MoO_4)_2:Ho^{3+}/Yb^{3+}$ phosphors with proper doping concentrations of $Ho^{3+}$ and $Yb^{3+}$ ($x=Ho^{3+}+Yb^{3+}$, $Ho^{3+}=0$ and 0.05, and $Yb^{3+}=0$, 0.35, 0.40, 0.45, and 0.50) were successfully synthesized using the microwave sol-gel method. Well-crystallized particles formed after heat-treatment at $800^{\circ}C$ for 16 h showed fine and homogeneous morphologies with particle sizes of $1{\sim}3{\mu}m$. The spectroscopic properties were examined using photoluminescence emission and Raman spectroscopy. Under excitation at 980 nm, the upconversion doped samples exhibited strong yellow emissions, from the combination of strong emission bands at 545 nm and 655 nm in the green and red spectral regions, respectively. The strong 545 nm emission band in the green region corresponded to the $^5S_2/^5F_4{\rightarrow}^5I_8$ transition in the $Ho^{3+}$ ions, while the strong 655 nm band in the red region appeared because of the $^5F_5{\rightarrow}^5I_8$ transition in the $Ho^{3+}$ ions. The pump power dependence and the Commission Internationale de L'Eclairage chromaticity of the upconversion emission intensity were evaluated in detail.

Microwave Sol-Gel Derived NaLa(MoO4)2 Yellow Phosphors Doped with Ho3+/Yb3+ and Upconversion Photoluminescence

  • Lim, Chang Sung
    • 한국재료학회지
    • /
    • 제26권1호
    • /
    • pp.29-34
    • /
    • 2016
  • $NaLa_{1-x}{(MoO_4)}_2$:$Ho^{3+}/Yb^{3+}$ phosphors with the correct doping concentrations of $Ho^{3+}$ and $Yb^{3+}$ ($x=Ho^{3+}+Yb^{3+}$, $Ho^{3+}=0.05$ and $Yb^{3+}=0.35$, 0.40, 0.45 and 0.50) were successfully synthesized by the microwave-modified sol-gel method. Well-crystallized particles formed after heat-treatment at $900^{\circ}C$ for 16 h showed a fine and homogeneous morphology with particle sizes of $3-5{\mu}m$. The optical properties were examined using photoluminescence emission and Raman spectroscopy. Under excitation at 980 nm, the UC intensities of the doped samples exhibited strong yellow emissions based on the combination of strong emission bands at 545-nm and 655-nm emission bands in green and red spectral regions, respectively. The strong 545-nm emission band in the green region corresponds to the $^5S_2/^5F_4{\rightarrow}^5I_8$ transition in $Ho^{3+}$ ions, while the strong emission 655-nm band in the red region appears due to the $^5F_5{\rightarrow}^5I_8$ transition in $Ho^{3+}$ ions. Pump power dependence and Commission Internationale de L'Eclairage chromaticity of the upconversion emission intensity were evaluated in detail.

졸-겔 공정에 의한 유기변성 하이브리드 세라믹 물질의 미세 마찰마모 특성 (Micro Friction and Wear Characteristics of Organically Modified Hybrid Ceramic Materials Synthesized by A Sol-Gel Process)

  • 한흥구;공호성;윤의성;양승호
    • Tribology and Lubricants
    • /
    • 제18권5호
    • /
    • pp.324-332
    • /
    • 2002
  • In order to enhance the thermal stability of binder materials of bonded type solid lubricants, several metal-alkoxide based sol-gel materials such as methyltrimethoxysilane(MTMOS), titaniumisopropoxide$(Ti(Opr^i)_4),$ zirconiumisopropoxide $(Zr(Opr^i)_4)$ and aluminumbutoxide$(Al(Obu^t)_4)$ were chemically modified by epoxy-, acrylic- and fluoro-silane compounds, respectively. Friction and wear characteristics of these hybrid ceramic materials were tested with a micro tribo-tester, and evaluated with respect to both heat-curing temperature and the time. Test results generally showed that hybrid ceramic materials modified by epoxy-silane compounds had a low friction compared to others. And the higher het-curing temperature and the longer heat treatment time resulted in the higher friction and the lower wear. IR spectroscopic analyses revealed that these results were caused mainly by the increased metal oxide content in hybrid ceramics when the heat-curing temperature was over $320^{\circ}C.$

Sol-gel Synthesis and Properties of Phosphate Ceramics

  • Lee, Burtrand I.;Cao, Zhicheng;Samuels, Willam D.;Exarhos, Gregory J.
    • The Korean Journal of Ceramics
    • /
    • 제6권4호
    • /
    • pp.390-395
    • /
    • 2000
  • Silicon, titanium, zirconium phosphates were synthesized by starting with appropriate chemical precursors in a solution. The synthetic procedure, chemical and physical structures were examined by FT-IR, liquid and solid state NMR, TGA, SEM, XRD, etc. The phosphates were examined for thermal and electrical properties. Advantages of the synthesis technique and the data on unique structures and thermal properties are reported.

  • PDF

The Concentration-Dependent Distribution of Tris(4,7'-diphenyl-1,10'-phenanthroline) Ruthenium (II) within Sol-Gel-Derived Thin Films

  • Lee, Joo-Woon;Cho, Eun-Jeong
    • Bulletin of the Korean Chemical Society
    • /
    • 제32권8호
    • /
    • pp.2765-2770
    • /
    • 2011
  • Organic dye-doped glasses, viz., ruthenium (II) tris(4,7'-diphenyl-1,10'-phenanthroline) $[Ru(dpp)_3]^{2+}$ incorporated into thin silica xerogel films produced by the sol-gel method, were prepared and their $O_2$ quenching properties investigated as a function of the $[Ru(dpp)_3]^{2+}$ concentration (3-400 ${\mu}M$) within the xerogel. The ratio of the luminescence from the $[Ru(dpp)_3]^{2+}$-doped films in the presence of $N_2$ and $O_2$ ($I_{N2}/I_{O2}$) was used to describe the film sensitivity to $O_2$ quenching. ($I_{N2}/I_{O2}$ changed three-fold over the $[Ru(dpp)_3]^{2+}$ concentration range. Time-resolved intensity decay studies showed that there are two discrete $[Ru(dpp)_3]^{2+}$ populations within the xerogels (${\tau}_1$ ~ 300 ns; ${\tau}_2$ ~ 3000 ns) whose relative fraction changes as the $[Ru(dpp)_3]^{2+}$ concentration changes. The increased $O_2$ sensitivity that is observed at the higher $[Ru(dpp)_3]^{2+}$ concentrations is a manifestation of a greater fraction of the 3000 ns $[Ru(dpp)_3]^{2+}$ species (more susceptible to $O_2$ quenching). A model is presented to describe the observed response characteristics resulting from $[Ru(dpp)_3]^{2+}$ distribution within the xerogel.

P-I-N 역구조 페로브스카이트 태양전지 응용을 위한 Nickel oxide 홀전달층의 열처리 온도 연구 (Annealing Temperature of Nickel Oxide Hole Transport Layer for p-i-n Inverted Perovskite Solar Cells)

  • 김기성;김미정;김효정;양정엽
    • Current Photovoltaic Research
    • /
    • 제11권4호
    • /
    • pp.103-107
    • /
    • 2023
  • A Nickel oxide (NiOx) thin films were prepared via sol-gel process on a transparent conductive oxide glass substrate. The NiOx thin films were spin-coated in ambient air and subsequently annealed for 30 minutes at temperatures ranging from 150℃ to 450℃. The structural and optical characteristics of the NiOx thin films annealed at various temperatures were measured using X-ray diffraction, field emission scanning electron microscopy, and ultraviolet-visible spectroscopy. After optimizing the NiOx coating conditions, perovskite solar cells were fabricated with p-i-n inverted structure, and its photovoltaic performance was evaluated. NiOx thin films annealed at 350℃ exhibited the most favorable characteristics as a hole transport layer, resulting in the highest power conversion efficiency of 17.88 % when fabricating inverted perovskite solar cells using this film.