SLUMPING TENDENCY AND RHEOLOGICAL PROPERTY OF FLOWABLE COMPOSITES (Flowable 복합레진의 slumping 경향과 유변학적 성질)

  • Lee, In-Bog;Min, Sun-Hong;Kim, Sun-Young;Cho, Byung-Hoon;Back, Seung-Ho
    • Restorative Dentistry and Endodontics
    • /
    • v.34 no.2
    • /
    • pp.130-136
    • /
    • 2009
  • The aim of this study was to develop a method for measuring the slumping resistance of flowable resin composites and to evaluate the efficacy using rheological methodology. Five commercial flowable composites (Aelitefil flow:AF, Filtek flow:FF, DenFil flow:DF, Tetric flow:TF and Revolution:RV) were used. Same volume of composites in a syringe was extruded on a glass slide using a custom-made loading device. The resin composites were allowed to slump for 10 seconds at $25^{\circ}C$ and light cured. The aspect ratio (height/diameter) of cone or dome shaped specimen was measured for estimating the slumping tendency of composites. The complex viscosity of each composite was measured by a dynamic oscillatory shear test as a function of angular frequency using a rheometer. To compare the slumping tendency of composites, one way-ANOVA and Turkey's post hoc test was performed for the aspect ratio at 95% confidence level. Regression analysis was performed to investigate the relationship between the complex viscosity and the aspect ratio. The results were as follows. 1. Slumping tendency based on the aspect ratio varied among the five materials (AF

SLUMPING RESISTANCE AND VISCOELASTICITY OF RESIN COMPOSITE PASTES (치과용 복합레진의 중합 전 slumping resistance와 점탄성)

  • Suh, Hee-Yeon;Lee, In-Bog
    • Proceedings of the KACD Conference
    • /
    • 2008.05a
    • /
    • pp.235-245
    • /
    • 2008
  • The aim of this study was to develop a method for measuring the slumping resistance of resin composites and to relate it to the rheological characteristics. Five commercial hybrid composites (Z100. Z250. DenFil, Tetric Ceram. ClearFil) and a nanofill composite (Z350) were used to make disc-shaped specimens of 2 mm thickness. An aluminum mold with square shaped cutting surface was pressed onto the composite discs to make standardized imprints. The imprints were light-cured either immediately (non-slumped) or after waiting for 3 minutes at $25^{\circ}C$ (slumped). White stone replicas were made and then scanned for topography using a laser 3-D profilometer. Slumping resistance index (SRI) was defined as the ratio of the groove depth of the slumped specimen to that of the non-slumped specimen. The pre-cure viscoelasticity of each composite was evaluated by an oscillatory shear test and normal stress was measured by a squeeze test using a rheometer. Flow test was also performed using a flow tester. Correlation analysis was performed to investigate the relationship between the viscoelastic properties and the SRI. SRI varied between the six materials (Z100 < DenFil < Z250 < ClearFil < Tetric Ceram < Z350). The SRI was strongly correlated with the viscous (loss) shear modulus G' but not with the loss tangent. Also. slumping resistance was more closely related to the resistance to shear flow than to the normal stress. Slumping tendency could be quantified using the imprint method and SRI. The index may be applicable to evaluate the clinical handling characteristics of composites.

  • PDF

SLUMPING RESISTANCE AND VISCOELASTICITY OF RESIN COMPOSITE PASTES (치과용 복합레진의 중합 전 slumping resistance와 점탄성)

  • Suh, Hee-Yeon;Lee, In-Bog
    • Restorative Dentistry and Endodontics
    • /
    • v.33 no.3
    • /
    • pp.235-245
    • /
    • 2008
  • The aim of this study was to develop a method for measuring the slumping resistance of resin composites and to relate it to the rheological characteristics. Five commercial hybrid composites (Z100, Z250, DenFil, Tetric Ceram, ClearFil) and a nanofill composite (Z350) were used to make disc-shaped specimens of 2 mm thickness. An aluminum mold with square shaped cutting surface was pressed onto the composite discs to make standardized imprints. The imprints were light-cured either immediately (non-slumped) or after waiting for 3 minutes at $25{\circ}C$ (slumped). White stone replicas were made and then scanned for topography using a laser 3-D profilometer. Slumping resistance index (SRI) was defined as the ratio of the groove depth of the slumped specimen to that of the nonslumped specimen. The pre-cure viscoelasticity of each composite was evaluated by an oscillatory shear test and normal stress was measured by a squeeze test using a rheometer. Flow test was also performed using a flow tester. Correlation analysis was performed to investigate the relationship between the viscoelastic properties and the SRI. SRI varied between the six materials (Z100 < DenFil < Z250 < ClearFil < Tetric Ceram < Z350). The SRI was strongly correlated with the viscous (loss) shear modulus G' but not with the loss tangent. Also, slumping resistance was more closely related to the resistance to shear flow than to the normal stress. Slumping tendency could be quantified using the imprint method and SRI. The index may be applicable to evaluate the clinical handling characteristics of composites.