Sintering Effects on Fe/Mo Ordering and Magnetoresistance in Double Perovskite Sr2FeMoO6

  • Kim, J;Park, B.J;Lee, B.W
    • Journal of Magnetics
    • /
    • v.9 no.1
    • /
    • pp.9-12
    • /
    • 2004
  • We have investigated sintering effects on Fe/Mo ordering and magnetoresistance (MR) in double perovskite-reflection lines due to $Sr_2FeMoO_6$ (SFMO). Polycrystalline samples have been prepared by the conventional solid-state reaction by sintering in a stream of 5% $H_2/Ar$ gas. All samples are single phase and exhibit a series of superstructurecation ordering at Fe and Mo sites. As sintering temperature increases from 900 to $1300^{\circ}C$, the degree of Fe/Mo ordering increases from 82 to 92%, magnetization (15 K, 7 kOe) increases from 1.6 to 2.7 ${\mu}_B/f.u.,$ and Curie temperature increases at a rate of 4.3 K/% with the increase of Fe/Mo ordering ratio. The magnitude of MR measured at 5 K is 19% for sample prepared at $1000^{\circ}C$ with magnetic fields of 7 kOe. The observed MR is proportional to the square of magnetization indicating that the MR feature in SFMO is explained by the spin-polarized tunneling at grain boundaries.

A Study on the Grain Growth and PLZT Ceramics Fabrication by Freeze Drying Method. (동결건조법에 의한 PLZT 세라믹 제조 및 결정립 성자에 관한 연구.)

  • Lee, Sung-Gap;Ryu, Ki-Won;Lee, Young-Hie
    • Proceedings of the KIEE Conference
    • /
    • 1987.11a
    • /
    • pp.492-495
    • /
    • 1987
  • In this study, PLZT ceramics were fabricated by freeze-drying and normal sintering method. The compositional rate of specimen was selected 9/65/35 (La/Zr/Ti) which have good optical and dielectric properties, sintering time was varied 1, 10, 30, 40, 50, 55, 60 and 65 hr at $1250^{\circ}C$. After sintering, the optical and dielectric properties were investigated with the grain size. As the result of the experiment, freeze-dried powder appeared particle size less than 1 um. The relative dielectric constant was increased linearly with the sintering time, specimen which sintered for 65 hr had the highest value, 5780. Grain was grown with increasing time, in the case of specimen sintered for 60 hr, the grain size was 8.4 um. Transmittance was increased with the grain size. In the case of 8.4 um grain size, the transmittance was 56 %. Curie temperature was decreased linearly by the surface-layer effect of space-charge, in the case of grain size which were 1.8 um and 8.4 um, appeared at $100^{\circ}C$ and $80^{\circ}C$, respectively.

  • PDF

Optimization of selective laser sintering process parameter for Fe-Ni-Cr coating fabrication (Fe-Ni-Cr 코팅층 형성을 위한 SLS 공정변수의 최적화)

  • Joo, B.D.;Jang, J.H.;Yim, H.S.;Son, Y.M.;Moon, Y.H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2009.05a
    • /
    • pp.278-281
    • /
    • 2009
  • Selective laser sintering(SLS), a kind of rapid prototyping technology, can provide a process to form many types of coatings. Coated layers by selective laser melting are highly influenced by substrate, powder and laser parameters such as laser power, scan rate, fill spacing and layer thickness. Therefore an attempt to fabricate Fe-Ni-Cr coating on AISI H13 tool steel has been performed by selective laser sintering. In this study, Fe-Ni-Cr coating was produced by experimental facilities consisting of a 200W fiber laser which can be focused to 0.08mm and atmospheric chamber which can control atmospheric pressure with Ar. With power increase or energy density decrease, line width was decreased and line surface quality was improved with energy density increase. Surface quality of coating layer was improved with fill spacing optimization or layer thickness decrease.

  • PDF

A study on the grain growth and PLZT ceramics fabrication by freeze drying method (동결건조법에 의한 PLZT 세라믹제조 및 결정립 성정에 관한 연구)

  • 이성갑;류기원;배선기;이영희
    • Electrical & Electronic Materials
    • /
    • v.1 no.1
    • /
    • pp.35-43
    • /
    • 1988
  • In this study, PLZT ceramics were fabricated by the freeze-drying and normal sintering method. The composition rate of the specimen was selected 9/65/35(La/Zr/Ti) which had good optical and dielectric properties, sintering time was varied 1, 10, 30, 50, 55, 60 and 65(hr) at 1250(.deg.C). After sintering, the optical and dielectric properties were investigated with the grain size. As the result of the experiment, the particle size of the powder prepared by freeze-drying method was less than 1(um). The relative dielectric constant was increased linearly with the sintering time and specimen sintered for 65(hr) had the highest value, 5780. Grain was grown with increasing time, in the case of specimen sintered for 60(hr), the grain size was 8.4(um). Transmittance was increased with the grain size. In the case of 8.4(um) grain size, the transmittance was 56(%). Curie temperature was decreased linearly by the surface-layer effect of space-charge. In the case of grain size, 1.8(um), 8.4(um), curie temperatures were appeared at 100(.deg.C) and 80(.deg.C), respectively.

  • PDF

Behaviors of Grain Growth in Carbide Added TiC Matrix Cermets (탄화물첨가 TiC기지 서멧의 입성장 거동)

  • Shin, Soon-GI;Lee, Jun-Hee;Lee, Hwa-Sang
    • Korean Journal of Materials Research
    • /
    • v.12 no.10
    • /
    • pp.825-830
    • /
    • 2002
  • The growth rate of solid grains in TiC-XC-2vol% and TiC-XC-30vo1% Ni cermets, where X=Zr, W or Mo, was fitted to an equation of the form $d^3$-$do^3$=Kt. The grain growth behavior during liquid phase sintering at 1673K decreased markedly with addition of $Mo_2$C or WC and increased with addition of ZrC. The contiguity ratio was greater in the alloys with smaller growth rate constant and decreased with increasing Ni content in the $TiC-Mo_2$C-Ni cermet. The grain growth mechanism could be explained by the effect of contiguous grain boundaries in restricting the overall grain growth.

Effects of the Colloid/Interface Variables on Densification and Pore Elimination of Zirconia (콜로이드/계면변수가 Zirconia의 치밀화와 기공제거에 미치는 영향)

  • 장현명;한규호;이기강;정한남
    • Journal of the Korean Ceramic Society
    • /
    • v.27 no.2
    • /
    • pp.169-178
    • /
    • 1990
  • The sintering characteristics of ZrO2 were analyzed in terms of pore microstructure and kinetics of pore elimination. The pore structue of the ZrO2 sample prepared from colloid suspension was characterized by three distinct types of pores ; intradomain, interdomain, and intergglomerate pores. Sintering data at 1600$^{\circ}C$ showed that pores larger than a certain critical size(∼3$\mu\textrm{m}$) were difficult to remove, and this was analyzed in terms of the interagglomerate pore formed from the suspension under the condition of low kinetic stability, that is, the stability ratio smaller than its critical value. A theoretical equation for densification rate was derived and was applied to the densification rate of the ZrO2 polycrystalline body containging both the matrix(the 1st-generation) pores and the interagglomerate (the 2nd-generation) pores under the condition of slow grain growth.

  • PDF

A Study on Dielectric Properties of PCW-PNN-PZT ceramics (PCW-PNN-PZT계 세라믹의 유전 특성에 관한 연구)

  • Shin, Hye-Gyeong;Lee, Sung-Ho;Jung, Bo-Ram;Bae, Seon-Gi
    • Proceedings of the KIEE Conference
    • /
    • 2005.11a
    • /
    • pp.51-53
    • /
    • 2005
  • This study was to measure the minuteness structure, dielectric properties of 0.03PCW-0.07PNN-0.9PZT ceramics according to sintering temperature manufacture the specimens with a general method. The results of this study were gotten such as follows. The crystal structure of ceramic changed the rombohedral structure into teteragonal structure according to rising sintering temperature in XRD. Dielectric constant at $20^{\circ}C$ showed its maximum value 510.599 in specimens sintered at $1100^{\circ}C$ and dielectric loss showed its minimum value 7.43% in specimens sintered at $1100^{\circ}C$. The variation rate of dielectric constant according to the change of frequency showed its minimum value 0.029/kHz at $1100^{\circ}C$. The variation rate of dielectric constant according to the change of temperature showed its minimum value $1.40/^{\circ}C$ at $1500^{\circ}C$.

  • PDF

The magnetic properties of ferrite for chip-induotor about 2GMz (2GHz 대역 Chip-Inductor용 자성재료의 자기적 특성)

  • 정승우;김태원;최우성
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.205-208
    • /
    • 1999
  • We have studied properties(crystal structure, density, absorption, contraction, initial permeability, and permeability) of Ba$\sub$0.2/Me$\sub$0.31/Fe$\sub$0.49/(Me:Ni$\sub$1-x/, Cu$\sub$x/ x=0~1) ferrites with various Me site, because of development of magnetic materials for inductor. As a results of the density, absorption rate, and shrinkage rate, the sintering temperature of Ba$\sub$0.2/ Me$\sub$0.31/ FEesub 0.49/(Me:Ni$\sub$1-x/ x=0.25, 0.75) had got over 1100$^{\circ}C$ for 3 hours. According to SEM images, the configurations of grain were hexagonal, Increasing the sintering temperature, initial Permeability increased. The complex permeabilities as a function of for several MHz showed constants.

  • PDF

Abnormal Grain Growth Behavior of $BaTiO_3$ Ceramics with Addition of Seed Grains (Seed 입자 첨가에 따른 $BaTiO_3$ 요업체의 비정상 입성장거동)

  • 이태헌;김정주;김남경;조상희
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.5
    • /
    • pp.587-593
    • /
    • 1995
  • Abnomal grain growth behavior of BaTiO3 ceramics was investigated with addition of seed grains. It was foudn that the nucleation rate of abnormal grain was constant and growth of abnormal grain was linearly increased with sitnering time, regardless of amount of seed grains. These facts were also confirmed by fitting of the volume fraction of abnormal grain vs. sintering time using Avrami type equation (n=4). It was suggested that seed grains did not change the nucleation rate or growth mechanism of abnormal grain but increase the number of abnormal grains at initial stage of sintering and then it led to fine microstructure of BaTiO3 ceramics.

  • PDF

Microstructure Development of Spark Plasma Sintered Silicon Carbide with Al-B-C (Al-B-C 첨가 탄화규소의 스파크 플라즈마 소결에 의한 미세구조 발달)

  • Cho, Kyeong-Sik;Lee, Kwang-Soon;Lee, Hyun-Kwuon;Lee, Sang-Jin;Choi, Heon-Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.8 s.279
    • /
    • pp.567-574
    • /
    • 2005
  • Densification of SiC powder with additives of total amount of2, 4, 8 $wt\%$ Al-B-C was carried out by Spark Plasma Sintering (SPS). The unique features of the process are the possibilities of a very fast heating rate and a short holding time to obtain fully dense materials. The heating rate and applied pressure were kept at $100^{\circ}C/min$ and 40 MPa, while the sintering temperature and holding time varied from 1700 - $1800^{\circ}C$ for 10 - 40 min, respectively. The SPS-sintered specimens with different amount of Al-B-C at $1800^{\circ}C$ reached near-theoretical density. The $3C{\rightarrow}6H,\;15R{\rightarrow}4H$ phase transformation of SiC was enhanced by increasing the additive amount. The microstructure of SiC sintered up to $1750^{\circ}C$ consisted of fine equiaxed grains. In contrast, the growth of large elongated grains in small matrix grains was shown in sintered bodies at $1800^{\circ}C$, and the plate-like grains interlocking microstructure had been developed by increasing the holding time at $1800^{\circ}C$. The grain growth rate decreases with increasing amount of Al-B-C in SiC starting powder, however, the both of volume fraction and aspect ratio of large grains in sintered body increased.