• 제목/요약/키워드: Sintering characteristics

검색결과 911건 처리시간 0.046초

Characteristics of Pre-alloyed Powders for Diamond Tools

  • Luo, Xi-Yu;Ma, Hong-Qiu;Kuang, Xing;Huang, Man;Tang, Ming-Qiang
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1144-1145
    • /
    • 2006
  • In this paper, the fundamental attributes, phase composition of three pre-alloyed powders for diamond tools by water atomization were investigated. The density, hardness, bend strength and bending modulus of their hot pressing samples were examined. The results showed that the three pre-alloyed powders have excellent low temperature sintering characteristics. The physical and mechanical properties of the samples were found to be nearly the same as those of fine cobalt powders.

  • PDF

ZPCCL계 바리스터의 충격전류 스트레스에 대한 노화 특성 (Degradation Characteristics Against Impulse Current Stress of ZPCCL-Based Varistors)

  • 박종아;유대훈;남춘우;서형권
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.315-317
    • /
    • 2005
  • The microstructure, electrical, and degradation characteristics against impulse current of ZPCCL-based varistors were investigated with various sintering temperature in the range of $1240\sim1300^{\circ}C$. The densification of varistors was improved, but the nonlinearity was deteriorated with increase of sintering temperature. The varistors sintered at $1250^{\circ}C$ and $1260^{\circ}C$ exhibited high stability against surge stress. On the whole, the variation of characteristics of varistor for surge stress was increased in order of varistor voltage$\rightarrow$nonlinear exponent$\rightarrow$dissipation factor$\rightarrow$leakage current.

  • PDF

Binder가 PZT계 세라믹스의 소결특성에 미치는 영향 (Effect of Binder on the Sintering Characteristics of PZT Ceramics)

  • 정우환;김정주;조상희
    • 한국세라믹학회지
    • /
    • 제25권4호
    • /
    • pp.385-389
    • /
    • 1988
  • Effects of binder addition on the porosity, pore size and grain size of PZT ceramics were investigated. The binders were used PVA, PEG and MC, they were added separately and simultaneously. After sintering for 90 min 125$0^{\circ}C$, the porosity and the pore size were determined by using an image processing method. Simultaneous addition of two different binders resulted in the highest sintered density and the large pore size.

  • PDF

Aluminium Titanate Sintering Study Aimed at Rational Design of Microstructure for Optimal Thermal Shock Characteristics

  • Alecu, Ioan D.;Stead, Rodney J.
    • The Korean Journal of Ceramics
    • /
    • 제5권1호
    • /
    • pp.78-81
    • /
    • 1999
  • Aluminium titanate is highly anisotropic in thermal expansion. As a result, thermal stresses build up in the material and intergranular cracks can develop. Both the outstanding thermal shock resistance and the low mechanical strength of aluminium titanate ceramics are a result of intergranular microcracking. The authors have previously identified a possibility of remarkably increasing fracture toughness of aluminium titanate without excessive penalty on strength. The paper shows that sintered density and porosity measurements can be used for optimizing the sintering and microstructure of aluminium titanate for an ideal balance between toughness and strength and, hence, the best thermal shock resistance.

  • PDF

Al2O3 첨가에 따른 potashborosilicate glass ceramic 기판의 특성변화에 관한연구 (Properties of Potashborosilicate Glass-ceramic Substrate by adding Al2O3)

  • 김용철
    • 마이크로전자및패키징학회지
    • /
    • 제5권2호
    • /
    • pp.53-58
    • /
    • 1998
  • Sintering and dielectric characteristics of substrates were estimated by mixing rate of alumina and potashborosilicate glass(PBSG) powders. PBSG powders were used 7761(corning code)and alumina powders were used in extra pure rate(99.9%) and had 0.1 ${\mu}$m mean size. After ball milling with organic additives green sheets which were casted by doctor blade machine were sintered at 800$^{\circ}C$ for 1∼3hrs. Microstructure, linear shrinkage and dielectric constant of substrates were surveyed in order to fabricate low-dielectric and low tem-perature sintering substrate.

Manufacture of Permalloy Soft Magnets by Powder Injection Molding

  • W.Y. Jeung;Park, J.W.
    • Journal of Magnetics
    • /
    • 제6권1호
    • /
    • pp.13-18
    • /
    • 2001
  • Permalloy soft magnets have been produced by the powder injection molding process. Rheological characteristics of mixtures, debinding conditions, and the magnetic properties of permalloy after sintering have been investigated. A permalloy soft magnet with a permeability of 14200 could be obtained by preparing a mixture with a powder loading of 65.4 vol % and a PP/PEG binder systems solvent extraction, thermal debinding, and subsequent sintering at 1350$\^{C}$ in hydrogen. The permalloy soft magnet sintered in hydrogen had 95% of theoretical density and a magnetic induction of 13.2 kG in an applied magnetic field of 50 Oe.

공침법에 의한 PZT의 분체제조 및 소결특성 (Powder Preparation and Sintering Properties of PZT-Ceramics by Coprecipitation)

  • 안영필;김복희;이병우
    • 한국세라믹학회지
    • /
    • 제25권1호
    • /
    • pp.54-58
    • /
    • 1988
  • In order to depress PbO vaporization during calcination and improve sinterability in low temperature, a method for preparing homogeous Lead-Zirconate-Titanate (PZT) powder from aqueous salt solution by precipitation is described. In this method, single phae PZT fine powders are formed at above 500$^{\circ}C$. PZT-ceramics using these powders have high sinterability, and good sintering characteristics relatively low temp. (-high apparent density, low porosity, low water adsorption etc.)

  • PDF

Manufacturing of the Permalloy Soft Magnet by Powder Injection Molding Process

  • W. Y. Jeung;Park, J. W.
    • 한국자기학회:학술대회 개요집
    • /
    • 한국자기학회 2000년도 International Symposium on Magnetics The 2000 Fall Conference
    • /
    • pp.217-227
    • /
    • 2000
  • The permalloy soft magnet was produced by powder injection molding process. Rheological characteristics of mixtures, debinding conditions and the magnetic properties of permalloy after sintering ware investigated. The permalloy soft magnet with a permeability of 14200 could be obtained by preparing a mixture with a powder loading of 65.4 vol.% and PP/PEG binder system, solvent extraction, thermal debinding and subsequent sintering at 1350 $^{\circ}C$ in hydrogen. The permalloy soft magnet sintered in hydrogen showed a 95 % of theoretical density and a magnetic induction of 13.2 kG at the applied magnetic field of 50 Oe

  • PDF