A Study on the Bonding Process of Carbon Fiber-Thermoplastic Composite Using Induction Heating Technology (유도가열 기술을 이용한 탄소섬유-열가소성 복합재의 접합 공정에 관한 연구)

  • Kang, Chang-Soo;Yoo, Myeong-Han;Seo, Min-Kang;Choi, Bo-Kyung
    • Composites Research
    • /
    • v.34 no.6
    • /
    • pp.421-425
    • /
    • 2021
  • In this study, thermoplastic composites were manufactured using a thermoplastic resin (PEEK) with the same melting temperature and a highly heat-resistant carbon UD tapes with different carbon fibers (Type A, Type B). And the bonding characteristics and mechanical characteristics of each of the two produced thermoplastic composites by induction heating welding were examined. The bonding characteristics and mechanical characteristics of the thermoplastic composites were performed using C-Scan and B-Scan, which is a non-destructive inspection, and the single lap shear test, respectively. The temperature of the carbon composites surface was monitored using a thermal image camera.

Effect of Aluminum Treatment by Plasma on the Bonding Strength Between Aluminum and CFRP Composites (플라즈마를 적용한 알루미늄의 표면처리가 알루미늄/CFRP 복합재의 접합강도에 미치는 영향)

  • Lee, Gyeong-Yeop;Yang, Jun-Ho;Choe, Nak-Sam
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.25 no.12
    • /
    • pp.1981-1987
    • /
    • 2001
  • This paper documents the effect of surface treatment of aluminum on the bonding strength of aluminum/CFRP composites. The surface of aluminum panel was treated by DC plasma. The optimal treatment condition of the aluminum was determined by measuring the contact angle and T-peel strength as functions of mixture ratio of acetylene gas to nitrogen gas. The mixture ratios used were 1:9, 3:7, 5:5, 7:3, and 9:1 Lap shear tests and T-peel tests were performed using surface-treated alumiunm/CFRP composites and regular alumiunm/CFRP composites. The results showed that the contact angle was minimized and the T-peel strength was maximized iota the mixture ratio of 5:5. The results also showed that the shear strength of surface-treated alumiunm/CFRP composites was 34% greater than that of regular alumiunm/CFRP composites. The T-peel strength of surface-treated alumiunm/CFRP composites was also 5 times greater than that of regular alumiunm/CFRP composites.

Effect of Graphite/Epoxy (CERP) Surface Treatment on the Shear Strength of CERP/Metal Composites (탄소섬유/에폭시 복합재(CFRP)의 표면처리가 금속재/CFRP의 전단강도에 미치는 영향에 대한 연구)

  • 지창헌;양준호
    • Journal of the Korean institute of surface engineering
    • /
    • v.34 no.3
    • /
    • pp.225-230
    • /
    • 2001
  • In this study, the effect of surface treatment of CFRP (Carbon Fiber Reinforced Composites) on the shear strength of CFRP/metal composites was investigated. The surface of 14 plied unidirectional (0-dog ) CFRP was treated by an $Ar^{/}$ + ion beam under an oxygen environment. Shear strength tests were performed using SLS (Single Lap Shear) specimens based on the ASTM D906-94a procedure. The shear strength of the surface-treated CFRP/metal composites was compared with that of the untreated CFRP/metal composites. The results showed that the shear strength of surface-treated CFRP/metal composites was 36% greater than that of untreated CFRP/metal composites.

  • PDF

Mechanical Properties of Cu and Ni Dissimilar Welds by High Welding Speed Using Single-Mode Fiber Laser (싱글모드 파이버 레이저를 이용한 Cu 와 Ni의 고속도 이종재료 용접부의 기계적 특성)

  • Lee, Su-Jin;Kim, Jong-Do
    • Journal of Welding and Joining
    • /
    • v.32 no.3
    • /
    • pp.81-88
    • /
    • 2014
  • As the industrial technology has been developed, a dissimilar welding has been received huge attention in various engineering fields. To understand the mechanical properties and possibility of applications of dissimilar metals joining, the laser welding of Cu and Ni dissimilar metals was studied in this paper. Cu and Ni have differences in materials properties, and Cu and Ni make no intermetallic compounds according to typical binary phase of Cu and Ni system. In this study, lap welds of Cu and Ni dissimilar metals using single-mode fiber laser with high welding speed were tried, and mechanical properties of the welds zone were evaluated using a Vickers hardness test and a tensile shear test. To recognize the relation between hardness and tensile shear load, weld fusion zone of interface weld area were observed. And it was confirmed that the ultra-high welding speed could make good weld beads and higher hardness parts had higher tensile shear load under the all conditions.

Fatigue Strength of Composite Joint Structures Reinforced by Jagged Shaped Stainless Steel Z-pins (요철 형상의 스테인레스강 Z-핀으로 보강된 복합재 접합 구조물의 피로강도)

  • Choi, Ik-Hyeon;Lim, Cheol-Ho
    • Journal of the Korean Society for Aeronautical & Space Sciences
    • /
    • v.41 no.12
    • /
    • pp.967-974
    • /
    • 2013
  • Recently the authors had proposed the z-pinning patch concept to simply manufacture z-pinned composite structures at industrial production site and manufactured composite single-lap shear joint specimens using the concept. Through static tensile test on the specimens they had obtained 54~68% improvement of the joint strength. As a sequential study of it, in this study, fatigue test has performed to measure an improvement of joint strength under cyclic loading. The z-pin's material is stainless steel and its surface was specially machined into zagged shapes and chemically corroded to increase the connection force with composite materials. Approximately 98~125% improvement of the joint strength under cyclic loading was obtained.

Numerical analysis of the combined aging and fillet effect of the adhesive on the mechanical behavior of a single lap joint of type Aluminum/Aluminum

  • Medjdoub, S.M.;Madani, K.;Rezgani, L.;Mallarino, S.;Touzain, S.;Campilho, R.D.S.G.
    • Structural Engineering and Mechanics
    • /
    • v.83 no.5
    • /
    • pp.693-707
    • /
    • 2022
  • Bonded joints have proven their performance against conventional joining processes such as welding, riveting and bolting. The single-lap joint is the most widely used to characterize adhesive joints in tensile-shear loadings. However, the high stress concentrations in the adhesive joint due to the non-linearity of the applied loads generate a bending moment in the joint, resulting in high stresses at the adhesive edges. Geometric optimization of the bonded joint to reduce this high stress concentration prompted various researchers to perform geometric modifications of the adhesive and adherends at their free edges. Modifying both edges of the adhesive (spew) and the adherends (bevel) has proven to be an effective solution to reduce stresses at both edges and improve stress transfer at the inner part of the adhesive layer. The majority of research aimed at improving the geometry of the plate and adhesive edges has not considered the effect of temperature and water absorption in evaluating the strength of the joint. The objective of this work is to analyze, by the finite element method, the stress distribution in an adhesive joint between two 2024-T3 aluminum plates. The effects of the adhesive fillet and adherend bevel on the bonded joint stresses were taken into account. On the other hand, degradation of the mechanical properties of the adhesive following its exposure to moisture and temperature was found. The results clearly showed that the modification of the edges of the adhesive and of the bonding agent have an important role in the durability of the bond. Although the modification of the adhesive and bonding edges significantly improves the joint strength, the simultaneous exposure of the joint to temperature and moisture generates high stress concentrations in the adhesive joint that, in most cases, can easily reach the failure point of the material even at low applied stresses.

Effects of Partial dampers on the Vibration Damping Behavior of a Single Lap Joint Beam (겹침이음부를 갖는 보의 진동감쇠거동에 미치는 부분층댐퍼의 효과)

  • 박정일;최낙삼
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 1999.04a
    • /
    • pp.57.1-60
    • /
    • 1999
  • This paper presents the effects of partial dampers on the lateral vibration of beams. Both shear and normal stresses in the viscoelastic layer were studied. Analytical results were compared with those obtained by a finite element method. Effects of the size of partial dampers on the system loss factors and resonant frequencies were discussed.

  • PDF

Microstructural behavior on weld fusion zone of Al-Ti and Ti-Al dissimilar lap welding using single-mode fiber laser

  • Lee, Su-Jin;Kawahito, Yousuke;Kim, Jong-Do;Katayama, Seiji
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.37 no.7
    • /
    • pp.711-717
    • /
    • 2013
  • Titanium (Ti) metal and its alloys are desirable materials for ship hulls and other structures because of their high strength, light weight and corrosion-resistance. And light weight and corrosion-resistant aluminum (Al) is the ideal metal for shipbuilding. The joining of Ti and Al dissimilar metals is one of the effective measures to reduce weight of the structures or to save rare metals. Ti and Al have great differences in materials properties, and intermetallic compounds such as Ti3Al, TiAl, TiAl3 are easily formed at the contacting surface between Ti and Al. Thus, welding or joining of Ti and Al is considered to be extremely difficult. However, it was clarified that ultra-high speed welding could suppress the formation of intermetallic compounds in the previous study. Results of tensile shear strength increases with an increase in the welding speed, and therefore extremely high welding speed (50m/min in this study) is good to dissimilar weldability for Ti and Al. In this study, therefore, full penetration dissimilar lap welding of Ti (upper) - Al (lower) and Al (upper) - Ti (lower) with single-mode fiber laser was tried at ultra-high welding speed, and the microstructure of the interface zones in the dissimilar Al and Ti weld beads was investigated.

Microstructural behavior on weld fusion zone of Al-Ti and Ti-Al dissimilar lap welding using single-mode fiber laser

  • Lee, Su-Jin;Katayama, Seiji;Kim, Jong-Do
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.38 no.2
    • /
    • pp.133-139
    • /
    • 2014
  • Titanium (Ti) metal and its alloys are desirable materials for ship hulls and other ocean structures because of their high strength, corrosion-resistance and light weight properties. And light weight and corrosion-resistant aluminum (Al) is the ideal metal for shipbuilding. The joining of Ti and Al dissimilar metals is one of the effective methode to reduce weight of the structures. Ti and Al have great differences in materials properties, and intermetallic compounds such as $Ti_3Al$, TiAl, $TiAl_3$ are easily formed at the contacting surface between Ti and Al. Thus, dissimilar welding and joining of Ti and Al are considered to be very difficult. However, it was clarified that ultra-high speed welding could suppress the formation of intermetallic compounds in the previous study. Results of tensile shear strength increases with an increase in the welding speed, and therefore extremely high welding speed (50 m/min) is good to dissimilar weldability for Ti and Al. In this study, therefore, full penetration dissimilar lap welding of Ti (upper) - Al (lower) and Al (upper) - Ti (lower) with single-mode fiber laser was tried at ultra-high welding speed, and the microstructure of the interface zones in the dissimilar Al and Ti weld beads was investigated.

EFFECT OF SURFACE ROUGHNESS ON ADHESIVE STRENGTH OF HEAT-RESISTANT ADHESIVE RTV88

  • Cho, Tae-Min;Choo, Yeon-Seok;Lee, Min-Jung;Oh, Hyeon-Cheol;Lee, Byung-Chai;Park, Tae-Hak;Shin, Young-Sug
    • Proceedings of the KSME Conference
    • /
    • 2008.11a
    • /
    • pp.115-120
    • /
    • 2008
  • In this study, effects of surface roughness on adhesive strength of heat-resistant adhesive RTV88 were examined. Sandblast was used to generate rough surfaces on aluminum adherends, and then tensile-shear tests of Al/RTV88 single lap joints were performed. The shear strength was shown to be affected by the surface roughness. Effective area, peel failure area, and cohesive failure area were introduced to explain the effects of surface roughness on the adhesive strength. An empirical relation for the failure force was proposed based on these parameters and verified by the test results.