출발 SiC 입자 크기가 Si3N4-Bonded SiC 세라믹스의 질화율과 강도에 미치는 영향 (Effect of Starting SiC Particle Size on Nitridation and Strength of Silicon Nitride-Bonded Silicon Carbide Ceramics)

  • 최영훈;김영욱;우상국;한인섭
    • 한국세라믹학회지
    • /
    • 제47권2호
    • /
    • pp.157-162
    • /
    • 2010
  • Effect of starting SiC particle size on nitridation rate and flexural strength of $Si_3N_4$-bonded-SiC (SNBSC) ceramics was investigated by using SiC particles of different size (${\sim}200\;{\mu}m$, ${\sim}100\;{\mu}m$ and ${\sim}45\;{\mu}m$). The specimen prepared from smaller SiC particles resulted in higher nitridation rate after nitridation at $1450^{\circ}C$, owing to the lower packing density in green body. The flexural strength showed maxima after 1-h nitridation for all specimens and then decreased with prolonged nitridation because of local densification-induced pore coarsening. The specimen prepared from smaller SiC particles showed better flexural strength because of smaller pore size and partly higher nitridation rate in the specimen. A maximal flexural strength of 29 MPa was obtained in the specimen with a density of $2.04\;g{\cdot}cm^3$, which was prepared from $45\;{\mu}m$-SiC particles.

소결조건의 변화에 따른 질화규소계 탄화규소질 탈황분사 슬러리 노즐의 제조 및 특성 (Fabrication and Characteristics of Silicon Nitride Bonded Silicon Carbide-based Slurry Nozzle for Desulfurization with Variation of Sintering Conditions)

  • 우상국;한인섭;서두원;이기성;홍기석;배강;임광현
    • 한국에너지공학회:학술대회논문집
    • /
    • 한국에너지공학회 2002년도 추계 학술발표회 논문집
    • /
    • pp.201-207
    • /
    • 2002
  • 배가스 탈황 공정은 흡수제의 형태에 따라 습식과 건식, 반응생성물로부터 흡수제의 회수여부에 따라 재생법과 비재생법으로 분류할 수 있으며, 현재 전 세계적으로 상용화되고 있는 처리공정은 비재생 습식 석회석-석고 공정이 채택되어 전체 설치용량의 80% 이상을 점유하고 있다.(중략)

  • PDF

실험적 방법에 의한 파인세라믹스의 연삭성에 관한 연구 (A study on the Grindability of Fine Ceramics by Experimental Method)

  • 김성겸
    • 반도체디스플레이기술학회지
    • /
    • 제10권3호
    • /
    • pp.35-42
    • /
    • 2011
  • This paper describes the characteristics of high speed grinding and the influence of wheel surface speed V and a grindability of the grinding materials. The various fine ceramics pieces was ground by metal and vitrified bonded diamond wheel. The surface roughness of fine ceramics(Zirconia($ZrO_2$), Silicon Carbide(SiC), Silicon Nitride($Si_3N_4$), Alumina($Al_2O_3$)) decreases from $0.05{\mu}m(R_{max})$ to $0.025{\mu}m(R_{max})$ when the wheel speed at grinding point increases the wheel speed. Relation between the temperature at grinding point and surface roughness was linear. Abrasive jet machining(AJM), a specialized from of shot blasting, is considered one of the most helpful micro machining methods for hard and brittle materials such as glasses and ceramics by constant pressure grinding.