Preceramic Polymer Technology for High Temperature Ceramic Composite and its Application (초고온복합소재용 프리세라믹폴리머 합성 및 응용기술)

  • Lee, Yoonjoo;Kim, Younghee;Bae, Seong Gun;Lee, Hyeon Myoung;Cho, Kwang Youn;Kwon, Woo Teck;Kim, Soo Ryong;Riu, Doh Hyung;Shin, Dong Geun
    • Composites Research
    • /
    • v.30 no.2
    • /
    • pp.102-107
    • /
    • 2017
  • The preceramic polymer can realize a variety of complex ceramic structures that can not be obtained by conventional ceramic processes. Polycarbosilane, which is a typical preceramic polymer, can control the molecular structure, molecular weight and molecular weight distribution for preparing complex morphology and microstructure of SiC ceramics, including SiC fiber. In this paper, synthesis and molecular structure control technique of polycarbosilane is explained. The silicon carbide fiber prepared by melt spinning, stabilization and heat treatment, and ceramic fiber composites technology made by PIP process are also discussed. In addition, we introduce an example of the development of a complex silicon carbide material such as a silicon carbide hollow fiber having a nanoporous structure.

Nano-Structure Control of SiC Hollow Fiber Prepared from Polycarbosilane (폴리카보실란으로부터 제조된 탄화규소 중공사의 미세구조제어)

  • Shin, Dong-Geun;Kong, Eun-Bae;Cho, Kwang-Youn;Kwon, Woo-Tek;Kim, Younghee;Kim, Soo-Ryong;Hong, Jun-Sung;Riu, Doh-Hyung
    • Journal of the Korean Ceramic Society
    • /
    • v.50 no.4
    • /
    • pp.301-307
    • /
    • 2013
  • SiC hollow fiber was fabricated by curing, dissolution and sintering of Al-PCS fiber, which was melt spun the polyaluminocarbosilane. Al-PCS fiber was thermally oxidized and dissolved in toluene to remove the unoxidized area, the core of the cured fiber. The wall thickness ($t_{wall}$) of Al-PCS fiber was monotonically increased with an increasing oxidation curing time. The Al-PCS hollow fiber was heat-treated at the temperature between 1200 and $2000^{\circ}C$ to make a SiC hollow fibers having porous structure on the fiber wall. The pore size of the fiber wall was increased with the sintering temperature due to the decomposition of the amorphous $SiC_xO_y$ matrix and the growth of ${\beta}$-SiC in the matrix. At $1400^{\circ}C$, a nano porous wall with a high specific surface area was obtained. However, nano pores grew with the grain growth after the thermal decomposition of the amorphous matrix. This type of SiC hollow fibers are expected to be used as a substrate for a gas separation membrane.

Polycrystalline Ceramic Fibers by Extrusion

  • Sagesser, Peter;Wegmann, Markus;Gut, Beat;Berroth, Karl;,
    • The Korean Journal of Ceramics
    • /
    • v.4 no.4
    • /
    • pp.382-386
    • /
    • 1998
  • titanate and a silicon carbide/zirconium diboride particulate composite have each been blended with thermoplastic of aqueous binders and extruded. The green extrudates have diameters ranging between 50 and 150 ㎛ and polyethylene-base 150 ${\mu}m$ diameter fibers can be drawn down at elevated temperature to approximately 40 ${\mu}m$ diameter. Hollow fibers with 150${\mu}m$ outer and 90 ${\mu}m$ inner diameter can also be fabricated. Green fibers have been processed into chopped fiber felts for use as gas distributors/current collectors in an experimental solid oxide fuel cell (SOFC) and the first attempts at producing simple textile structures have been successful. The fibers, tubes and felts have been successfully debound and sintered and characterization of the sintered PSZ fibers, for example, has revealed a density in excess of 99% and tensile failure stresses up to 1.0 GPa for 78 ${\mu}m$ diameter fibers.