• 제목/요약/키워드: SiC-C films

검색결과 2,101건 처리시간 0.034초

도포 열분해법을 이용한 Bi$_4$Ti$_3$O$_{12}$제조에 관한 연구 (Preparation of Bi$_4$Ti$_3$O$_{12}$ Films by Dipping-Pyrolysis Process)

  • 황규석;이형민;김병훈
    • 한국세라믹학회지
    • /
    • 제35권9호
    • /
    • pp.1002-1005
    • /
    • 1998
  • Bismuth titanate thin films were prepared on {{{{ { SrTiO}_{3 } }}(100) and Si(100) substrates by dipping-pyrolysis pro-cess using metal naphthenates as starting materials. crystallinity and in-phase alignment of the films were analyzed by X-ray diffraction $\theta$-2$\theta$ scans and $\beta$ scans (pole-figures) respectively. Highly c-axis-oriented {{{{ { { {Bi }_{4 }Ti }_{3 }O }_{12 } }} thin films with smooth surfaces were obtained after heat treatment at 75$0^{\circ}C$ on {{{{ { SrTiO}_{3 } }}(100) sub-strate while the films grown of Si(100) exhibited polycrstalline characteristics. C-axis oriented film show-ed an epitaxial relationship with the {{{{ { SrTiO}_{3 } }} substrate.

  • PDF

열교환 부품용 발열체 형성기술 (The Formation Technique of Thin Film Heaters for Heat Transfer Components)

  • 조남인;김민철
    • 반도체디스플레이기술학회지
    • /
    • 제2권4호
    • /
    • pp.31-35
    • /
    • 2003
  • We present a formation technique of thin film heater for heat transfer components. Thin film structures of Cr-Si have been prepared on top of alumina substrates by magnetron sputtering. More samples of Mo thin films were prepared on silicon oxide and silicon nitride substrates by electron beam evaporation technology. The electrical properties of the thin film structures were measured up to the temperature of $500^{\circ}C$. The thickness of the thin films was ranged to about 1 um, and a post annealing up to $900^{\circ}C$ was carried out to achieve more reliable film structures. In measurements of temperature coefficient of resistance (TCR), chrome-rich films show the metallic properties; whereas silicon-rich films do the semiconductor properties. Optimal composition between Cr and Si was obtained as 1 : 2, and there is 20% change or less of surface resistance from room temperature to $500^{\circ}C$. Scanning electron microscopy (SEM) and Auger electron spectroscopy (AES) were used for the material analysis of the thin films.

  • PDF

AlN 박막의 열처리에 따른 표면탄성파의 특성 (Effect of thermal annealing on surface acoustic wave properties of AlN films)

  • 황시홍;정귀상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 하계학술대회 논문집 Vol.9
    • /
    • pp.71-72
    • /
    • 2008
  • In this paper, the effect of thermal annealing on surface acoustic wave (SAW) properties of aluminum nitride (AlN) films were described. The films were fabricated on Si substrates by using Pulsed Reactive Magnetron Sputtering System. The SAW properties of $600^{\circ}C$-annealed AlN films were better than those of both $900^{\circ}C$-annealed AlN films and as-deposited ones. Their SAW velocities (Raleigh mode) and insertion losses were about 5212 m/s and 16.19 dB at $600^{\circ}C$ with the wavelength of $40{\mu}m$. The dependence of characteristics of AlN films on annealing conditions were also evaluated by using Fourier Transform-Infrared Spectroscopy (FT-IR) Spectrums and Atomic Force Microscopy (AFM).

  • PDF

3C-SiC 마이크로 히터의 제작과 그 특성 (Fabrication of 3C-SiC micro heaters and its characteristics)

  • 정귀상;정재민
    • 센서학회지
    • /
    • 제18권4호
    • /
    • pp.311-315
    • /
    • 2009
  • This paper describes the characteristics of a poly 3C-SiC micro heater which was fabricated on AlN(0.1 $\mu$m)/3C-SiC(1.0 $\mu$m) suspended membranes by surface micro-machining technology. The 3C-SiC and AlN thin films which have wide energy band gap and very low lattice mismatch were used sensors for high temperature and voltage environments. The 3C-SiC thin film was used as micro heaters and temperature sensor materials simultaneously. The implemented 3CSiC RTD(resistance of temperature detector) and the power consumption of micro heaters were measured and calculated. The TCR(thermal coefficient of the resistance) of 3C-SiC RTD is about -5200 ppm/$^{\circ}C$ within a temperature range from 25 $^{\circ}C$ to 50 $^{\circ}C$ and -1040 ppm/$^{\circ}C$ at 500 $^{\circ}C$. The micro heater generates the heat about 500 $^{\circ}C$ at 10.3 mW. Moreover, durability of 3C-SiC micro heaters in high voltages is better than Pt micro heaters. A thermal distribution measured and simulated by IR thermovision and COMSOL is uniform on the membrane surface.

High-rate, Low-temperature Deposition of Multifunctional Nano-crystalline Silicon Nitride Films

  • Hwang, Jae-Dam;Lee, Kyoung-Min;Keum, Ki-Su;Lee, Youn-Jin;Hong, Wan-Shick
    • Journal of Information Display
    • /
    • 제11권3호
    • /
    • pp.109-112
    • /
    • 2010
  • The solid phase compositions and dielectric properties of silicon nitride ($SiN_x$) films prepared using the plasma enhanced chemical vapor deposition (PECVD) technique at a low temperature ($200^{\circ}C$) were studied. Controlling the source gas mixing ratio, R = $[N_2]/[SiH_4]$, and the plasma power successfully produced both silicon-rich and nitrogen-rich compositions in the final films. The composition parameter, X, varied from 0.83 to 1.62. Depending on the film composition, the dielectric properties of the $SiN_x$ films also varied substantially. Silicon-rich silicon nitride (SRSN) films were obtained at a low plasma power and a low R. The photoluminescence (PL) spectra of these films revealed the existence of nano-sized silicon particles even in the absence of a post-annealing process. Nitrogen-rich silicon nitride (NRSN) films were obtained at a high plasma power and a high R. These films showed a fairly high dielectric constant ($\kappa$ = 7.1) and a suppressed hysteresis window in their capacitance-voltage (C-V) characteristics.

초고온 MEMS용 단결정 3C-SiC의 Ohmic Contact 형성 (Ohmic contact formation of single crystalline 3C-SiC for high temperature MEMS applications)

  • 정귀상;정수용
    • 센서학회지
    • /
    • 제14권2호
    • /
    • pp.131-135
    • /
    • 2005
  • This paper describes the ohmic contact formation of single crystalline 3C-SiC thin films heteroepitaxially grown on Si(001) wafers. In this work, a TiW (Titanium-tungsten) film as a contact matieral was deposited by RF magnetron sputter and annealed with the vacuum and RTA (rapid thermal anneal) process respectively. Contact resistivities between the TiW film and the n-type 3C-SiC substrate were measured by the C-TLM (circular transmission line model) method. The contact phases and interface the TiW/3C-SiC were evaulated with XRD (X-ray diffraction), SEM (scanning electron microscope) and AES (Auger electron spectroscopy) depth-profiles, respectively. The TiW film annealed at $1000^{\circ}C$ for 45 sec with the RTA play am important role in formation of ohmic contact with the 3C-SiC substrate and the contact resistance is less than $4.62{\times}10^{-4}{\Omega}{\cdot}cm^{2}$. Moreover, the inter-diffusion at TiW/3C-SiC interface was not generated during before and after annealing, and kept stable state. Therefore, the ohmic contact formation technology of single crystalline 3C-SiC using the TiW film is very suitable for high temperature MEMS applications.

$TiO_2$ Thin Film Patterning on Modified Silicon Surfaces by MOCVD and Microcontact Printing Method

  • 강병창;이종현;정덕영;이순보;부진효
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2000년도 제18회 학술발표회 논문개요집
    • /
    • pp.77-77
    • /
    • 2000
  • Titanium oxide (TiO2) thin films have valuable properties such as a high refractive index, excellent transmittance in the visible and near-IR frequency, and high chemical stability. Therefore it is extensively used in anti-reflection coating, sensor, and photocatalysis as electrical and optical applications. Specially, TiO2 have a high dielectric constant of 180 along the c axis and 90 along the a axis, so it is highlighted in fabricating dielectric capacitors in micro electronic devices. A variety of methods have been used to produce patterned self-assembled monolayers (SAMs), including microcontact printing ($\mu$CP), UV-photolithotgraphy, e-beam lithography, scanned-probe based micro-machining, and atom-lithography. Above all, thin film fabrication on $\mu$CP modified surface is a potentially low-cost, high-throughput method, because it does not require expensive photolithographic equipment, and it produce micrometer scale patterns in thin film materials. The patterned SAMs were used as thin resists, to transfer patterns onto thin films either by chemical etching or by selective deposition. In this study, we deposited TiO2 thin films on Si (1000 substrateds using titanium (IV) isopropoxide ([Ti(O(C3H7)4)] ; TIP as a single molecular precursor at deposition temperature in the range of 300-$700^{\circ}C$ without any carrier and bubbler gas. Crack-free, highly oriented TiO2 polycrystalline thin films with anatase phase and stoichimetric ratio of Ti and O were successfully deposited on Si(100) at temperature as low as 50$0^{\circ}C$. XRD and TED data showed that below 50$0^{\circ}C$, the TiO2 thin films were dominantly grown on Si(100) surfaces in the [211] direction, whereas with increasing the deposition temperature to $700^{\circ}C$, the main films growth direction was changed to be [200]. Two distinct growth behaviors were observed from the Arhenius plots. In addition to deposition of THe TiO2 thin films on Si(100) substrates, patterning of TiO2 thin films was also performed at grown temperature in the range of 300-50$0^{\circ}C$ by MOCVD onto the Si(100) substrates of which surface was modified by organic thin film template. The organic thin film of SAm is obtained by the $\mu$CP method. Alpha-step profile and optical microscope images showed that the boundaries between SAMs areas and selectively deposited TiO2 thin film areas are very definite and sharp. Capacitance - Voltage measurements made on TiO2 films gave a dielectric constant of 29, suggesting a possibility of electronic material applications.

  • PDF

초고온 MEMS용 다결정 3C-SiC의 Ohmic Contact 형성 (Ohmic contact formation of polycrystalline 3C-SiC for high-temperature MEMS applications)

  • 온창민;정귀상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.406-407
    • /
    • 2006
  • This paper describes the ohmic contact formation between a TiW film as a contact material deposied by RF magnetron sputter and polycrystalline 3C-SiC films deposied on thermally grown Si wafers. The specific contact resistance (${\rho}_c$) of the TiW contact was measured by using the C-TLM. The contact phase and interfacial reaction between TiW and 3C-SiC at high-temperature were also analyzed by XRD and SEM. All of the samples didn't show cracks of the TiW film and any interfacial reaction after annealing. Especially, when the sample was annealed at $800^{\circ}$ for 30min., the lowest contact resistivity of $2.90{\times}10^{-5}{\Omega}cm^2$ was obtained due to the improved interfacial adhesion.

  • PDF

RTA처리한 PZT 박막의 강유전 특성 (Ferroelectric Properties of PZT thin Films by Rapid Thermal Annealing)

  • 정규원;박영;주필연;조익현;임동건;이준신;송준태
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제49권4호
    • /
    • pp.232-238
    • /
    • 2000
  • PZT thin films(3500 ) have been prepared onto $Pt/Ti/SiO_2/Si$ substrates with a RF magnetron sputtering system using PB1.05(Zr0.52,Ti0.48)O3 ceramic target. We used two-step annealing techniques. As the RTA times and temperatures were increased, crystallization of PZT thin films were enhanced. The ferroelectric characteristics of PZT capacitors fabricated at $700^{\circ}C$ for 60 seconds were like these remanent polarization were $12.1 \muC/cm^2$, coercive field were 110 kV/cm, leakage current density were $4.1\times10-7 A/cm^2,\; \varepsilonr=442,$ and remanent polarization were decreased by 22% after 1010 cycles, respectively.

  • PDF

$(Sr_{1-x}Ca_x)TiO_3$세라믹 박막의 미세구조 및 특성 (Microstructure and Properties of $(Sr_{1-x}Ca_x)TiO_3$Ceramic Thin film)

  • 김진사;이준웅
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제50권10호
    • /
    • pp.504-508
    • /
    • 2001
  • The$(Sr_{1-x}Ca_x)TiO_3$(SCT) thin films are deposited on Pt-coated electrode $(Pt-TiN /SiO_2Si)$ using RF sputtering method at various deposition temperature. The crystallinity of thin films was increased with increased of deposition temperature n the temperature range of 200~500 $[^{\circ}C]$. The capacitance changes almost linearly in temperature ranges of -80~+90$[^{\circ}C]$. All SCT thin films used in the study the phenomena of dielectric relaxation with the increase of frequency, and the relaxation frequency is observed above 200[kHz]. V-I characteristics of SCT thin films show the increasing leakage current with the increases of deposition temperature.

  • PDF