• Title/Summary/Keyword: SiC particle size

Search Result 330, Processing Time 0.025 seconds

Fabrication of Reaction Sintered SiC Materials by Complex Slurry with Nano Size Particles (나노입자 혼합 복합슬러리를 이용한 반응소결 SiC 재료의 제조)

  • Lee Sang-Pill
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.29 no.3 s.234
    • /
    • pp.425-431
    • /
    • 2005
  • The efficiency of complex slurry preparation route for developing the high performance SiC matrix of $RS-SiC_{f}/SiC$ composites has been investigated. The green bodies for RS-SiC materials prior to the infiltration of molten silicon were prepared with various C/SiC complex slurries, which associated with both the sizes of starting SiC particles and the blending conditions of starting SiC and C particles. The characterization of Rs-SiC materials was examined by means of SEM, EDS and three point bending test. Based on the mechanical property-microstructure correlation, the process optimization is also discussed. The flexural strength of Rs-SiC materials greatly depended on the content of residual Si. The decrease of starting SiC particle size in the C/SiC complex slurry was effective for improving the flexural strength of RS-SiC materials.

R-Curve Behavior of Particulate Composites of ${Al_2}{O_3}$ Containing SiC and $ZrO_2$: II. Theoretical Analysis (SiC와 $ZrO_2$를 함유하는 ${Al_2}{O_3}$ 입자복합체의 균열저항거동: II. 이론적 분석)

  • 나상웅;이재형
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.4
    • /
    • pp.368-375
    • /
    • 2000
  • Fracture toughness of particulate composites of Al2O3/SiC, Al2O3/ZrO2 and Al2O3/ZrO2/SiC was analysed theoretically. According to the suggested particle bridging model for obtaining the R-curve height, the crack extension resistance for the long crack was linearly proportional to the residual calmping stress at the interface between the second phase and the matrix. It was also a function of the particle size and the content. It was confirmed that the rising R-curve behavior of Al2O3 containing 30 vol% SiC particles of 3${\mu}{\textrm}{m}$ was owing to the strong crack bridging by SiC particles. For Al2O3/ZrO2/SiC composites, the tensional stress from the 3${\mu}{\textrm}{m}$ SiC particles was large enough to activate the spontaneous transformation of the ZrO2. The crack extension resistance due to the particle bridging mechanism did not seem to be affected much by the coupled toughening, but its resultant toughness increase could be significantly smaller due to the dependency on the matrix toughness.

  • PDF

Effects of β-SiC Particle Seeds on Morphology and Size of High Purity β-SiC Powder Synthesized using Sol-Gel Process (β-SiC 분말 Seeds가 Sol-gel 공정으로 합성된 고순도 β-SiC 분말 형상 및 크기에 미치는 영향)

  • Kim, Gyu-Mi;Cho, Gyoung-Sun;Park, Sang-Whan
    • Journal of the Korean Ceramic Society
    • /
    • v.46 no.5
    • /
    • pp.528-533
    • /
    • 2009
  • High purity $\beta$-SiC powders were synthesized using sol-gel processing. TEOS and phenol resin were used as the starting material for the silicon source and carbon source, respectively. The process turned out to be capable of producing high purity SiC powder purity degree with 99.98 %. However, it was difficult to control the shape and size of $\beta$-SiC powders synthesized by sol-gel process. In this study, $\beta$-SiC powder with size of $1{\sim}5$ um an 30 nm were used as the seeds for $\beta$-SiC to control the $\beta$-SiC powder morphology. It was found that $\beta$-SiC powder seeds was effective to increase the powder average size of synthesized $\beta$-SiC using sol-gel process by acting as the preferred growing sites for $\beta$-SiC.

Effect of Starting SiC Particle Size on Nitridation and Strength of Silicon Nitride-Bonded Silicon Carbide Ceramics (출발 SiC 입자 크기가 Si3N4-Bonded SiC 세라믹스의 질화율과 강도에 미치는 영향)

  • Choi, Young-Hoon;Kim, Young-Wook;Woo, Sang-Kuk;Han, In-Sub
    • Journal of the Korean Ceramic Society
    • /
    • v.47 no.2
    • /
    • pp.157-162
    • /
    • 2010
  • Effect of starting SiC particle size on nitridation rate and flexural strength of $Si_3N_4$-bonded-SiC (SNBSC) ceramics was investigated by using SiC particles of different size (${\sim}200\;{\mu}m$, ${\sim}100\;{\mu}m$ and ${\sim}45\;{\mu}m$). The specimen prepared from smaller SiC particles resulted in higher nitridation rate after nitridation at $1450^{\circ}C$, owing to the lower packing density in green body. The flexural strength showed maxima after 1-h nitridation for all specimens and then decreased with prolonged nitridation because of local densification-induced pore coarsening. The specimen prepared from smaller SiC particles showed better flexural strength because of smaller pore size and partly higher nitridation rate in the specimen. A maximal flexural strength of 29 MPa was obtained in the specimen with a density of $2.04\;g{\cdot}cm^3$, which was prepared from $45\;{\mu}m$-SiC particles.

Microstructure and Properties of Ni-SiC Composite Coating Layers Formed using Nano-sized SiC Particles (SiC 나노입자를 이용하여 형성한 Ni-SiC 복합도금막의 미세구조 및 특성)

  • Lee, Hong-Kee;Son, Seong-Ho;Lee, Ho-Young;Jeon, Jun-Mi
    • Journal of the Korean institute of surface engineering
    • /
    • v.40 no.2
    • /
    • pp.63-69
    • /
    • 2007
  • Ni-SiC composite coating layers were formed using two kinds of SiC nano-particles by DC electrodeposition in a nickel sulfamate bath containing SiC particles. The effect of stirring rate and SiC particle type on the microstructure and properties of Ni-SiC composite coating layers were investigated. Results revealed that the trend of deposition rate is closely related to the codeposition of SiC and the deposition rate. or nickel, and the codeposition behavior of SiC can be explained by using hydrodynamic effect due to stirring. The average roughness and friction coefficient are closely related to the codeposition of SiC and SiC particle size. It was found that the Victors microhardness of the composite coating layers increased with increasing codeposition of SiC. The composite coating layers containing smaller SiC particle showed higher hardness. This can be explained by using the strengthening mechanism resulting from dispersion hardening. Anti-wear property of the composite coating layers formed using 130 nm-sized SiC nano-particles has been improved by 2,300% compared with pure electroplated-nickel layer.

Microstructure of Squeeze Cast AC4A $Al/Al_2O_3+SiC_p$ Hybrid Metal Matrix Composite (용탕단조한 AC4A $Al/Al_2O_3+SiC_p$ 하이브리드 금속복합재료의 미세조직과 기계적 성질)

  • Kim, Min-Soo;Cho, Kyung-Mox;Park, Ik-Min
    • Journal of Korea Foundry Society
    • /
    • v.14 no.3
    • /
    • pp.258-266
    • /
    • 1994
  • AC4A $Al/Al_2O_3+SiC_p$ hybrid composites were fabricated by the squeeze infiltration technique. Effect of applied pressure, volume fraction of reinforcement($Al_2O_3$ and SiC) and SiC particle size($4.5{\mu}m$, $6.5{\mu}m$ and $9.3{\mu}m$) on the solidification microstructure of the hybrid composites were examined. Mechanical properties were estimated preliminarly by fractographic observation, hardness measurement and wear test. Results show that the microstructure of the hybrid composites were quite satisfactory, namely revealing relatively uniform distribution of reinforcements and refined matrix. Some aggregation of SiC particle caused by particle pushing was observed especially in the hybrid composites containg in fine particle($4.5{\mu}m$). Refined matrix was attributed to applied pressure and increased nucleation sites with addition of reinforcements. Fractured facet also revealed finer for the hybrid composites possibly due to refined matrix. Hardness and wear resistance increased with volume fraction of reinforcements. For hybrid composites with $9.3{\mu}m$ SiC, hardness was somewhat lower and wear resistance higher than other composites.

  • PDF

Effect of Primary Si size and Residual Stress on the Wear Properties of B.390 Al Alloys (B.390 알루미늄 합금의 마모특성에 미치는 초정Si 입자크기와 잔류응력의 영향)

  • Kim, Heon-Joo;Kim, Sung-Jae
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.19 no.1
    • /
    • pp.20-29
    • /
    • 2006
  • Wear behaviour of B.390 aluminum alloy with different particle sizes of primary Si against a SM45C counterface was studied as a function of wear load and sliding velocity, using pin-on-disk apparatus under dry condition. The wear rate of specimen with fine primary Si particles showed increased wear resistance at high wear load, on the other side wear resistance of coarse primary Si particle size was improved at low wear load. As the compressive residual stress in the matrix increased remarkably by liquid nitrogen(LN) treatment, wear resistance of the LN treated specimen was more excellent than that of T6 treated specimen.

Variation of Cone Crack Shape in Ceramic Materials According to Spherical Impact Velocity (입자충격속도에 따른 세라믹재료의 콘크랙 형상 변화)

  • O, Sang-Yeop;Sin, Hyeong-Seop;Seo, Chang-Min
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.26 no.2
    • /
    • pp.380-386
    • /
    • 2002
  • Damage behaviors induced in silicon carbide by an impact of particle having different material and size were investigated. Especially, the influence of the impact velocity of particle on the cone crack shape developed was mainly discussed. The damage induced by spherical impact was different depending on the material and size of particles. Ring cracks on the surface of specimen were multiplied by increasing the impact velocity of particle. The steel particle impact produced larger ring cracks than that of SiC particle. In the case of high velocity impact of SiC particle, radial cracks were produced due to the inelastic deformation at the impact site. In the case of the larger particle impact, the damage morphology developed was similar to the case of smaller particle one, but a percussion cone was farmed from the back surface of specimen when the impact velocity exceeded a critical value. The zenithal angle of cone cracks developed into SiC material decreased monotonically with increasing of the particle impact velocity. The size and material of particle influenced more or less on the extent of cone crack shape. An empirical equation, $\theta$= $\theta$$\sub$st/, v$\sub$p/(90-$\theta$$\sub$st/)/500 R$\^$0.3/($\rho$$_1$/$\rho$$_2$)$\^$$\frac{1}{2}$/, was obtained as a function of impact velocity of the particle, based on the quasi-static zenithal angle of cone crack. It is expected that the empirical equation will be helpful to the computational simulation of residual strength in ceramic components damaged by the particle impact.

Preparation and Characterization of Zn2SiO4:Mn2+ Green Phosphor with Solid State Reaction (고상법에 의한 Zn2SiO4:Mn2+녹색 형광체의 제조와 특성에 관한 연구)

  • Yoo, Hyeon-Hee;Nersisyan, Hayk;Won, Hyung-Il;Won, Chang-Whan
    • Korean Journal of Materials Research
    • /
    • v.21 no.6
    • /
    • pp.352-356
    • /
    • 2011
  • [ $Zn_{2(1-x)}Mn_xSiO_4$ ]$0.07{\leq}x{\leq}0.15$) green phosphor was prepared by solid state reaction. The first heating was at $900^{\circ}C-1250^{\circ}C$ in air for 3 hours and the second heating was at $900^{\circ}C$ in $N_2/H_2$(95%/5%) for 2 hours. The size effect of $SiO_2$ in forming $Zn_2SiO_4$ was investigated. The temperature for obtaining single phase $Zn_2SiO_4$ was lowered from $1100^{\circ}C$ to $1000^{\circ}C$ by decreasing the $SiO_2$ particle size from micro size to submicro size. The effect of the activators for the Photoluminescence (PL) intensity of $Zn_2SiO_4:Mn^{2+}$ was also investigated. The PL intensity properties of the phosphors were investigated under vacuum ultraviolet excitation (147 nm). The emission spectrum peak was between 520 nm and 530 nm, which was involved in green emission area. $MnCl_2{\cdot}4H_2O$, the activator source, was more effective in providing high emission intensity than $MnCO_3$. The optimum conditions for the best optical properties of $Zn_2SiO_4:Mn^{2+}$ were at x = 0.11 and $1100^{\circ}C$. In these conditions, the phosphor particle shape was well dispersed spherical and its size was 200 nm.