Growth of Elongated Grains in $\alpha$'-Sialon Ceramics ($\alpha$'-Sialon 세라믹스에서의 주상형 입자성장)

  • 신익현
    • Journal of Powder Materials
    • /
    • v.6 no.3
    • /
    • pp.246-250
    • /
    • 1999
  • The effects of the ${\beta}-Si_3N_4$ starting particle size and $\alpha$/$\beta$ phase transformation during sintering process on the microstructure evolution of Yttrium $\alpha$-Sialon ceramics were investigated. As-received ${\beta}-Si_3N_4$ powder (mean particle size: 0.54$\mu$m) and classified ${\beta}-Si_3N_4$ powder(mean particle size: $0.26\mu{m}$) were used as starting powders. With decreasing the starting particle size, the growth of elongated grains was enhanced, which resulted in the whisker -like microstructure with elongated grains. These results were discussed in relation to the two-dimensional nucleation and growth theory. In the specimen heat treated at $1600^{\circ}C$ for 10h before sintering at $1950^{\circ}C$for 1h under 40atm(2-step sintering), the grain size was smaller than of the 1-step sintering at 195$0^{\circ}C$ for 1h. However, bimodal microstructure evolution were not not remarkable in both sample, which is ascribed to the $\alpha$-phase contents existing in ${\beta}-Si_3N_4$ starting powder.

  • PDF

Tribological Properties of Reaction-Bonded SiC/Graphite Composite According to Particle Size of Graphite (반응소결 SiC/Graphite 복합체에서 Graphite 입자의 크기에 따른 마찰마모특성)

  • Baik, Yong-Hyuck;Seo, Young-Hean;Choi, Woong;Lee, Jong-Ho
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.8
    • /
    • pp.854-860
    • /
    • 1997
  • The tribological property of ceramics is very important for use in seal rings, pump parts, thread guides and mechanical seal, etc. In the present study, which RBSC/graphite composites were manufactured by adding graphite powders with different particle sizes to mixtures of SiC powder, metallic silicon, carbon black and alumina, effects on the tribological property of each RBSC/graphite composite was investigated in accordance with the particle size of the added graphite powder. The water absorption, the bending strength and the resistance for the friction and wear were measured, and the crystalline phase and the microstructure were respectively examined by using XRD and SEM. In case that the particle size of the graphite powder was fine(2${\mu}{\textrm}{m}$), the formation of $\beta$-SiC was accelerated, thereby making the increase of the bending strength and the decrease of the water absorption, but no improvement for the tribological properties. Furthermore, in case that the particle size of the graphite powder was some large(88~149${\mu}{\textrm}{m}$), the formation of $\beta$-SiC was not accelerated, to thereby make the decrease of the bending strength and the increase of the water absorption, but the improvement for the tribological property of only the composite having the graphite powder of 20 vol%. In addition, in case that the particle size distribution of the graphite powder was large (under 53 ${\mu}{\textrm}{m}$), there was no improvement for every properties. However, the composites, which the graphite powder with the particle size of 53~88 ${\mu}{\textrm}{m}$ was added in 10~15 vol%, had the most increased resistance for the friction and wear which show the worn out amount of 0.4~0.6$\times$10-3 $\textrm{cm}^2$, and the value of the bending strength is 380~520 kg/$\textrm{cm}^2$.

  • PDF

The Effect of Casting Condition and Heat Treatment on the Mechanical Properties of AC4C Alloy Castings (AC4C 합금의 기계적 성질에 미치는 주조조건과 열처리의 영향에 관한 연구)

  • Kang, Hyo-Gyoung;Cheon, Byung-Wook;Choi, Chang-Ock
    • Journal of Korea Foundry Society
    • /
    • v.13 no.5
    • /
    • pp.450-461
    • /
    • 1993
  • AC4C alloy casts in the metallic mold, zircon sand mold, silica sand mold and shell mold with the pouring temperatures of 680, 710 and $740^{\circ}C$ have been investigated. The tensile strength, elongation and hardness of AC4C alloy castings have been influenced by the kind of molds used. The mechanical properties in zircon sand mold castings were greater than those in other sand mold castings, but were inferior to the properties in metallic mold castings. Eutectic Si particle size and DAS were increased in the order of metallic mold, ziron sand mold, silica sand mold and shell mold. Also, they were increased with the increase of pouring temperatures. DAS, eutectic Si particle size and grain size decreased with the increase of mechanical properties as the cooling rate increased. The eutectic Si particle size and DAS of AC4C alloy castings after T6 treatment were decreased in as-cast. The variation of eutectic Si particle size has been effected on the tensile strength, elongation and fractured surface.

  • PDF

Mechanical Properties of 2024/(Al2O3.SiC)p Composite Reinforced with Al2O3.SiC Particle Prepared by SHS Process (자전연소법으로 제조한 Al2O3.SiC 입자로 보강된2024/(Al2O3.SiC)p 복합재료의 기계적특성)

  • 맹덕영
    • Journal of Powder Materials
    • /
    • v.7 no.1
    • /
    • pp.35-41
    • /
    • 2000
  • Al2O3$.$SiC particle was prepared was prepared by the self-propagting high temperature sYthesis(SHS) process from a mixture of SiO2, Al and C powders, The fabricated Al2O3$.$SiC particle was applied to 2024Al/(Al2O3$.$SiC)pcomposite as a reinforcement. Aluminum matix composites were fabricares by the powder extrusion method using the synthesized Al2O3$.$SiC particle and commercial 2024Al powder. Theoptimum preparation conditions for Al2O3$.$SiC partticle by SHS process were described. The influence of the Al2O3$.$SiC voiume fraction on the mechanical was composite was also discussed. Despite adiabatic temperature was about 2367K, SHs reaction was completed not by itself, but by using pre-heating. Mean particle size of final particle synthesized was 0.73 ${\mu}$m and most of the particle was smaller than 2${\mu}$m. Elastic modulus and tensile strength of the composite increased with increase the volume fraction of reinforcement but, tensile strength depreciated at 30 vol% of reinforcement.

  • PDF

Effect of SiC Particles Size on the Densification of $Al_2O_3-SiC$ Composite During Pressureless Sintering ($Al_2O_3-SiC$ 복합재료의 상압소결시 치밀화에 미치는 SiC 원료분말의 크기영향)

  • 채기웅
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.11
    • /
    • pp.1261-1265
    • /
    • 1999
  • Effect of SiC particle size of the densification of Al2O3-SiC composite during pressureless sintering was investigated. Two types of SiC powders having average particle size of 0.15${\mu}{\textrm}{m}$ and 3${\mu}{\textrm}{m}$ were used. Densification rate of the specimen containing 0.15${\mu}{\textrm}{m}$ SiC particles was slower than that of the specimen containg 3${\mu}{\textrm}{m}$ SiC particles. Although the relative density of the specimen containing 0.15${\mu}{\textrm}{m}$ SiC particles was below 90% of theoretical density after sintering at 155$0^{\circ}C$ the complete closure of open pores occurred. Therefore full densification could be obtained by subsequent HIP. On the other hand in the specimen containing 3${\mu}{\textrm}{m}$ SiC particles the complete closed pore was observed at 95% of theoretical density. Such a fast pore closure in the specimen containing 0.15${\mu}{\textrm}{m}$ SiC particles is likely to occur as a result of dense reaction layer formation on the specimen surface which is attributed to the high reactivity of small size particles with sintering atmosphere.

  • PDF

High Strength $Si_3N_4/SiC$ Structural Ceramics (고강도 $Si_3N_4/SiC$ 구조세라믹스에 관한 연구)

  • 김병수;김인술;장윤식;박홍채;오기동
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.12
    • /
    • pp.999-1006
    • /
    • 1993
  • Si3N4(p)-SiC(p) composites were prepared by gas pressure sintering at 190$0^{\circ}C$ for 1 hour. $\alpha$-SiC with average particle size of 0.48${\mu}{\textrm}{m}$ were dispersed from zero to 50vol% in $\alpha$-Si3N4 with average particle size of 0.5${\mu}{\textrm}{m}$. Y2O3-Al2O3 system was used as sintering aids. When 10vol% of SiC was added to Si3N4, optimum mechanical properties were observed; relative density of 98.8%, flextural strength of 930MPa, fracture toughness of 5.9MPa.m1/2 and hardness value of 1429kg/$\textrm{mm}^2$. Grain growth of $\beta$-Si3N4 was inhibited as the amount of added SiC was increased. SiC particles were found inside the $\beta$-Si3N4 intragrains in case of 10, 20 and 30vol%SiC added composites.

  • PDF

The effect of particle size on tool wear of SiCp-reinforced metal matrix composite

  • Sahin, Y.;Sur, G.
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2002.10b
    • /
    • pp.237-239
    • /
    • 2002
  • The effect of particle sizes of the metal matrix composites containing 10 wt.%SiCp was investigated with using various tools. The results showed that tool life decreased considerably with increasing particle size and cutting speed. The wear resistance of TiC-coated tools was considerably higher than that of the other tools. It was observed that abrasive wear was the main responsible mechanism for wear of the tool thermal cracks were at high speed while a built-edge formation was also evident at lower speed.

  • PDF

Variation of Cone Crack Shape and Impact Damage According to Impact Velocity in Ceramic Materials (세라믹에서 충격속도에 따른 충격손상 및 콘크랙 형상의 변화)

  • Oh, Sang-Yeob;Shin, Hyung-Seop;Suh, Chang-Min
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.383-388
    • /
    • 2001
  • Effects of particle property variation of cone crack shape according to impact velocity in silicon carbide materials were investigated. The damage induced by spherical impact having different material and size was different according to materials. The size of ring cracks induced on the surface of specimen increased with increase of impact velocity within elastic contact conditions. The impact of steel particle produced larger ring cracks than that of SiC particle. In case of high impact velocity, the impact of SiC particle produced radial cracks by the elastic-plastic deformation at impact regions. Also percussion cone was formed from the back surface of specimen when particle size become large and its impact velocity exceeded a critical value. Increasing impact velocity, zenithal angle of cone cracks in SiC material was linearly decreasing not effect of impact particle size. An empirical equation, $\theta=\theta_{st}-\upsilon_p(180-\theta_{st})(\rho_p/\rho_s)^{1/2}/415$, was obtained from the test data as a function of quasi-static zenithal angle of cone crack($\theta_{st}$), the density of impact particle(${\rho}_p$) and specimen(${\rho}_s$). Applying this equation to the another materials, the variation of zenithal angle of cone crack could be predicted from the particle impact velocity.

  • PDF

Effect of SiC Particle Size on Hot Workability of AA2024/$SiC_P$ Composites (AA2024/$SiC_P$ 복합재료의 열간 가공성에 미치는 강화상 크기의 영향)

  • 고병철;홍흥기;유연철
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1997.03a
    • /
    • pp.81-84
    • /
    • 1997
  • The hot deformation behavior of SiCp/AA2024 composites reinforced with different sizes of SiCp reinforcements (1, 8, 15, 36, and 44${\mu}{\textrm}{m}$) was investigated by hot torsion tests. The hot restoration of the composites depending on the SiCp reinforcements particle size was studied from the effective stress - strain curves. Dynamic recrystallization (DRX) was occurred in the SiCp/AA2024 composites during the hot deformation at 320 - 43$0^{\circ}C$ under a strain rate of 1.0/sec. Also, the critical strain for DRX decreased with decreasing the reinforcement size of SiCp from 44 to 8${\mu}{\textrm}{m}$. The composite reinforced with SiCp of 8${\mu}{\textrm}{m}$ showed the highest flow stress (265 MPa) and the work hardening rate at 32$0^{\circ}C$ under a strain rate of 1.0/sec.

  • PDF

Fabrication and Characteristics of SiCp/AC8A Composites by Pressureless Metal Infiltration Process (무가압함침법에 의한 SiCp/AC8A 복합재료의 제조 및 특성)

  • 김재동;고성위
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2000.04a
    • /
    • pp.139-142
    • /
    • 2000
  • The SiCp/AC8A composites were fabricated by the pressureless metal infiltration process successfully. The effect of additional Mg, which were mixed with SiC particles to promote interfacial wetting between the reinforcement and matrix alloy, and particle size on the mechanical properties was investigated. By increasing the additional Mg content the hardness of SiCp/AC8A composites was increased due to the hard reaction products, but the bending strength was decreased by the excess reaction of Mg and high porosity level when the additional Mg content is over 7%. The Hardness and bending strength was increased by decreasing the size of SiC particle.

  • PDF