• Title/Summary/Keyword: SiC C3M

Search Result 1,713, Processing Time 0.034 seconds

Design on ultra low power consumption microhotplates based on 3C-SiC for high temperatures (고온용 저전력소비형 3C-SiC 마이크로 히터의 설계)

  • Jeong, Jae-Min;Chung, Gwiy-Sang
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.385-386
    • /
    • 2008
  • This paper reports the design of the ultra low power consumption microhotplates for high temperatures. The microhotplates consisting of a platinum-based heating element on AlN/poly 3C-SiC layers were designed. The microhotplate is a $600\times600{\mu}m^2$ square shaped membrane made of $1{\mu}m$ thick ploy 3C-SiC suspended by four legs. The microhotplate was compared with $Si_3N_4/SiO_2/Si_3N_4$(NON) structure microhotplate by COMSOL simulation system. Thermal uniformity, power consumption and thermal characterizations of microhotplates based on 3C-SiC thin film are better than microhotplates with NON structure.

  • PDF

Improvement of Oxidation Resistance and Erosion Resistance Properties of the C/C Composite with the Multilayer Coating (다층코팅을 이용한 C/C 복합재료의 내산화성 및 내마모성 증진)

  • 김옥희;이승윤;윤병일;박종욱
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.9
    • /
    • pp.1003-1008
    • /
    • 1995
  • CVD-Si3N4/CVD-SiC/pack-SiC/pyro-carbon/(3-D C/C composite) multilayer coating was performed to improve the oxdiation resistance and erosion resistance properteis of the 3-D carbon/carbon composite, and the plasma test was performed to measure the oxidation resistance and erosion resistance properties. The thicknesses of each film layer were about 10${\mu}{\textrm}{m}$ for pack-SiC, 5${\mu}{\textrm}{m}$ for CVD-SiC and 40${\mu}{\textrm}{m}$ for CVD-Si3N4. When the multilayer coated specimen was exposed to the plasma flame with temperature of 500$0^{\circ}C$ for 20 seconds, it showed the weight loss five times less than that of the only pyro-carbon coated specimen.

  • PDF

The characteristics of polycrystalline 3C-SiC microhotplates for high temperature M/NEMS (고온 M/NEMS용 3C-SiC 마이크로 히터 특성)

  • Jeong, Jae-Min;Chung, Gwiy-Sang
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.252-252
    • /
    • 2008
  • The microhotplates consisting of a Pt-ased heating element on AlN/poly 3C-SiC layers were fabricated. The microhotplate has a $600{\mu}m{\times}600{\mu}m$ square shaped membrane which made of $1{\mu}m$ thick ploycrystalline 3C-SiC suspended by four legs. 3C-SiC is known for excellent chemical durability, mechanical strength and sustaining of high temperature. The membrane is fabricated by surface micromachining using oxidized Si sacrificial layer. The Pt thin film is used for heating material and resist temperature sensor. The fabrication methodology allows intergration of an array of heating material and resist temperature detector. For reasons of a short response time and a high sensitivity a uniform temperature profile is desired. The dissipation of microhotplate was examined by a IR thermoviewer and the power consumption was measured. Measured and simulated results are compared and analyzed. Thermal characterization of the microhotplates shows that significant reduction in power consumption was achieved using suspended structure.

  • PDF

Characterization of 3C-SiC grown on Si(100) water (Si(100) 기판상에 성장된 3C-SiC의 특성)

  • Na, Kyung-Il;Chung, Yun-Sik;Ryu, Ji-Goo;Chung, Gwiy-Sang
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11b
    • /
    • pp.533-536
    • /
    • 2001
  • Single crystal cubic silicon carbide(3C-SiC) thin film were deposited on Si(100) substrate up to a thickness of $4.3{\mu}m$ by APCVD(atmospheric pressure chemical vapor deposition) method using hexamethyildisilane(HMDS) at $1350^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like. The growth rate of the 3C-SiC films was $4.3{\mu}m/hr$. The 3C-SiC epitaxical layers on Si(100) were characterized by XRD(X-ray diffraction), raman scattering and RHEED(reflection high-energy electron diffraction), respectively. The 3C-SiC distinct phonons of TO(transverse optical) near $796cm^{-1}$ and LO(longitudinal optical) near $974{\pm}1cm^{-1}$ were recorded by raman scattering measurement. The deposition films were identified as the single crystal 3C-SiC phase by XRD spectra($2{\theta}=41.5^{\circ}$). Also, with increase of films thickness, RHEED patterns gradually changed from a spot pattern to a streak pattern.

  • PDF

Crystal Characteristics of 3C-SiC Thin-films Grown on 2 inch Si(100) wafer (2 inch Si(100)기판위에 성장된 3C-SiC 박막의 결정특성)

  • Chung, Su-Young;Chung, Yun-Sik;Ryu, Ji-Goo;Chung, Gwiy-Sang;Shigehiro, Nishino
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.11a
    • /
    • pp.452-455
    • /
    • 2002
  • Single crystal 3C-SiC(cubic silicon carbide) thin-films were deposited on Si(100) substrate up to a thickness of $4.3{\mu}m$ by APCVD method using HMDS(hexamethyildisilane) at $1350^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like crystal surface. The growth rate of the 3C-SiC films was $4.3{\mu}m/hr$. The 3C-SiC epitaxical films grown on Si(100) were characterized by XRD, AFM, RHEED, XPS and raman scattering, respectively. The 3C-SiC distinct phonons of TO(transverse optical) near $796cm^{-1}$ and LO(longitudinal optical) near $974{\pm}1cm^{-1}$ were recorded by raman scattering measurement. The heteroepitaxially grown films were identified as the single crystal 3C-SiC phase by XRD spectra$(2{\theta}=41.5^{\circ})$.

  • PDF

Characterization of 3C-SiC grown on Si(100) wafer (Si(100) 기판상에 성장된 3C-SiC의 특성)

  • 나경일;정연식;류지구;정귀상
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.533-536
    • /
    • 2001
  • Single crystal cubic silicon carbide(3C-SiC) thin film were deposited on Si(100) substrate up to a thickness of 4.3 $\mu\textrm{m}$ by APCVD(atmospheric pressure chemical vapor deposition) method using hexamethyildisilane(HMDS) at 1350$^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like. The growth rate of the 3C-SiC films was 4.3 $\mu\textrm{m}$/hr. The 3C-SiC epitaxical layers on Si(100) were characterized by XRD(X-ray diffraction), raman scattering and RHEED(reflection high-energy electron diffraction), respectively The 3C-SiC distinct phonons of TO(transverse optical) near 796 cm$\^$-1/ and LO(longitudinal optical) near 974${\pm}$1 cm$\^$-1/ were recorded by raman scattering measurement. The deposition films were identified as the single crystal 3C-SiC phase by XRD spectra(2$\theta$=41.5$^{\circ}$). Also, with increase of films thickness, RHEED patterns gradually changed from a spot pattern to a streak pattern

  • PDF

Crystal Characteristics of 3C-SiC Grown on Si(100) Wafers (Si(100)기판상에 성장된 3C-SiC의 결정 특성)

  • Chung, Yun-Sik;Ryu, Ji-Goo;Seon, Joo-Heon;Chung, Soo-Yong;Chung, Gwiy-Sang
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.05a
    • /
    • pp.30-34
    • /
    • 2002
  • Single crystal 3C-SiC(cubic silicon carbide) thin-films were deposited on Si(100) wafers up to a thickness of 4.3 ${\mu}m$ by APCVD method using HMDS(hexamethyldisilane) at $1350^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like crystal surface. The growth rate of the 3C-SiC films was 4.3 ${\mu}m$/hr. The 3C-SiC epitaxial films grown on Si(100) were characterized by XRD, AFM, RHEED, XPS and raman scattering, respectively. The 3C-SiC distinct phonons of TO(transverse optical) near 796 $cm^{-1}$ and LO(longitudinal optical) near $974{\pm}1cm^{-1}$ were recorded by raman scattering measurement. The heteroepitaxially grown films were identified as the single crystal 3C-SiC phase by XRD spectra($2{\theta}=41.5^{\circ}$).

  • PDF

Effect of SiC whisker addition on microstructure and mechanical properties of silicon carbide (탄화규소 휘스커 첨가가 탄화규소의 미세구조와 기계적 특성에 미치는 영향)

  • Young-Wook Kim;Kyeong-Sik Cho;Heon-Jin Choi
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.7 no.3
    • /
    • pp.473-480
    • /
    • 1997
  • $\beta-SiC$powder with or without the addition of 1-3 wt% of $\beta-SiC$ whiskers (seeds) was hot-pressed at $1850^{\circ}C$ for 1 h using $Al_2O_3$ and $Y_2O_3$ as sintering aids. The hot-pressed materials were subsequently annealed at $1950^{\circ}C$ to enhance grain growth. The introduction of $\beta-SiC$ whiskers into $\beta-SiC$ does not affect the microstructure as well as mechanical properties significantly because the whiskers are not viable in the presence of liquid phase during hot-pressing. The strengths and fracture toughnesses of the hot-pressed and subsequently 5 h-annealed materials with 1 wt% $\beta-SiC$ whiskers and without $\beta-SiC$ whiskers were 465 MPa and 5.8 MPaㆍ$m^{1/2}$, and 451 MPa and 5.5 MPaㆍ$m^{1/2}$, respectively.

  • PDF

Crystal Growth of 3C-SiC Using HMDS Gas Source (HMDS 가스원을 이용한 3C-SiC의 결정성장)

  • Sun, Ju-Hun;Chung, Yun-Sik;Chung, Gwiy-Sang;Nishino, Shigehiro
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.07b
    • /
    • pp.735-738
    • /
    • 2002
  • Single crystal 3C-SiC(cubic silicon carbide) thin-films were deposited on Si(100) substrate up to a thickness of $4.3{\mu}m$ by APCVD method using HMDS(hexamethyildisilane) at $1350^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like crystal surface. The growth rate of the 3C-SiC films was $4.3{\mu}m/hr$. The 3C-SiC epitaxical films grown on Si(100) were characterized by XRD, AFM, RHEED, XPS and raman scattering, respectively. The 3C-SiC distinct phonons of TO(transverse optical) near $796cm^{-1}$ and LO(longitudinal optical) near $974{\pm}1cm^{-1}$ were recorded by raman scattering measurement. The heteroepitaxially grown films were identified as the single crystal 3C-SiC phase by XRD spectra$(2{\theta}=41.5^{\circ})$.

  • PDF

A Steel Ball Impact Damage Behavior of RS-SiC Ceramic Materials (RS-SiC 세라믹 재료의 강구 입자충격 손상 거동)

  • Oh, Sang-Yeob
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.34 no.8
    • /
    • pp.1015-1021
    • /
    • 2010
  • In this study, the effect of the C/SiC composition ratio on the impact damage of a reaction sintered SiC (RS-SiC) plates was evaluated. An impact test was conducted by using an air gun. The impacter used was a steel ball with a diameter of 2 mm, and the impact velocities were 113, 122, and 180 m/s. The RS-SiC plates were $20\times20\times3$ mm with different C/SiC composition ratios. The ring crack diameters damaged by a steel ball were determined using SEM images. It was observed that the maximum diameter increased with increasing impact velocity, and it rapidly changed with increasing C/SiC composition ratio because of the effect of residual Si and the variation flexural strength. Cone cracks were formed in the case of C/SiC composition ratios of 0.4~0.5, this indicated that the impact damage changed from a ring crack to a cone crack in this critical range of C/SiC composition ratios. The C/SiC composition ratio of 0.3 was determined to be the optimal ratio for the RS-SiC manufacturing process.