• 제목/요약/키워드: Shotcrete strength

검색결과 161건 처리시간 0.029초

Permanent Shotcrete Tunnel Lining 구축을 위한 고성능 숏크리트 개발( I : 고강도 숏크리트 개발을 위한 새로운 급결제 적용) (Development of High Performance Shotcrete for Permanent Shotcrete Tunnel Lining(I : Application of New Type Accelerator for High Strength Shotcrete))

  • 박해균;이명섭;김재권;안병제
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 봄 학술발표회 논문집
    • /
    • pp.1023-1030
    • /
    • 2002
  • From the early 1980s, the New Austrian Tunnelling Method (NATM) has been developed as a one of the standard tunneling method in Korea. Approximately 10 years ago, wet-mix shotcrete with sodium silicate accelerator (waterglass) was introduced and widely used to tunnel lining and underground support. However, this accelerator had some disadvantages due to the decrease of long-term strength compared to plain concrete (without accelerator) and low quality of the hardened shotcrete. In order to compensate for these disadvantages, recently developed alkali-free accelerator has been successfully demonstrated in numerous projects and applications as a new material to make tunnels more durable and safer. An experimental investigation was carried out in order to verify the strength behavior of wet-mix Steel Fiber Reinforced Shotcrete (SFRS) with alkali-free accelerator. Compressive strength, flexural strength and equivalent flexural strength were measured by testing specimens extracted from the shotcrete panels. From the results, wet-mix SFRS with alkali-free accelerator exhibited excellent strength improvement compared to the conventional shotcrete accelerator.

  • PDF

Permanent Shotcrete Tunnel Linings 구축을 위한 고성능 숏크리트 개발 II (II: 용수부에서의 조강시멘트 적용) (Development of High Performance Shotcrete for Permanent Shotcrete Tunnel Linings II(II: Application of high-early strength cement in sump water condition))

  • 박해균;이명섭;김재권;안병제
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.695-702
    • /
    • 2002
  • Shotcrete (or Sprayed concrete) has been used as an important support material in New Austrian Tunnelling Method (NATM). Since the mid of 1990, permanent shotcrete tunnel linings such as Single-shell, NMT (Norwegian Method of Tunnelling) has been constructed in many countries for reducing the construction time and lowing construction costs instead of conventional in-situ concrete linings. Among essential technologies for successful application of permanent shotcrcte linings, high performance shotcrete providing high strength, high durability, better pumpability has to be developed in advance as an integral component. This paper presents the Ideas and first experimental attempts to increase early strength and bond strength of wet-mixed Steel Fiber Reinforced Shotcrete(SFRS) in sump water condition. In order to increase early strength, a new approach using high-early strength cement with liquid alkali-free accelerator has been investigated From the results, wet-mix SFRS with high-early strength cement and alkali-free accelerator exhibited excellent early strength improvement compared to the ordinary portland content and good bond strength even under sump water condition.

  • PDF

화학적 침식에 의한 숏크리트의 압축강도 특성 (Uniaxial Compressive Strength Characteristic of Shotcrete Immersed in Chemical Solution)

  • 이규필;김동규;배규진;김홍삼
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2005년도 춘계 학술발표회 논문집
    • /
    • pp.1291-1298
    • /
    • 2005
  • Shotcrete for the support of tunnel can contact with groundwater. The hazardous components in the groundwater cause the corrosion of shotcrete. Also, the hazardous components may deteriorate the engineering properties of shotcrete, such as compressive strength, bond strength, and flexural strength. The more the effect of the hazardous components on the shotcrete may increase, the more the stability of tunnel structure may decrease. It was analyzed to find the hazardous components in the ground water. The uniaxial compressive strength test, XRD, SEM were conducted to evaluate the durability and corrosion of shotcrete. These tests were performed on shotcrete specimens at 2, 4, 8, and 16 weeks. The specimens were immersed in various chemical solutions including hazardous components after the specimens were made at the construction site.

  • PDF

시멘트광물계 숏크리트재의 강도특성과 친환경성 (The Strength and Environmental Friendly Characteristics of Cement Mineral Types Shotcrete)

  • 천병식;도종남;박덕흠;최희림;이해성
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2008년도 춘계 학술발표회 초청강연 및 논문집
    • /
    • pp.762-765
    • /
    • 2008
  • Shotcrete is NATM technique after tunnel excavation as major tunnel support for ground stability, curtail of execution period and reduction of execution expenses instead of general lining method. It is trend using constantly shotcrete lining. This high-strength shotcrete is require to use as constantly shotcrete lining. This brought out the solution of environmental pollution and harmfulness about human. Accordingly, in this study Specimens of strength measurement was made to develop shotcrete possible to develop in early materials with Cement Mineral Accelerator as NATM method construction. It's compared with existing shotcrete material, Unconfined Compression test, flexural strength test were experimented. The fish poison test was experimented to evaluate an influence of environment. On results of test, Unconfined Compressive Strength and flexural strength was equivalent with 28-day strength of existing material. On results of fish poison evaluation research subject material was founded environmentally friendly for existing shotcrete.

  • PDF

터널의 품질관리를 위한 숏크리트 초기강도의 현장강도 시험기술 (Field Testing Methods on Early Shotcrete Strength for Tunnel Quality Control)

  • 홍의준;장석부;이성우;김기림;문상조
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2007년도 춘계학술대회 논문집
    • /
    • pp.468-476
    • /
    • 2007
  • Generally, the strength of the field shotcrete is heavily dependent on the field mixing and spraying conditions so that it is different from the strength of the shotcrete mixed in laboratories. As a support member, the early strength of shotcrete unlike concrete as structural material is very important to the initial stabilization of the excavation face in tunnels. Therefore, the field methods to efficiently test the early strength of shotcrete have been highly required. This paper aimed to verify the pneumatic pin penetration test and the point load test for measuring the early strength of the field shotcrete. Through a series of uniaxial compression, pin penetration, and point load tests for the range of the early shotcrete strength, two equations to estimate reliably the uniaxial compressive strength by the pin penetration and the point load tests were derived. Field tests in working tunnel were carried out in order to estimate the economic efficiency. As a result, pin penetration method was proved to be the most effective method for testing the early strength of the field shotcrete.

  • PDF

숏크리트의 강도 특성과 분사압력에 대한 리바운드율 연구 (A Study on the Strength Characteristics and Rebound Ratio with Respect to Injection Pressure of Shotcrete)

  • 전준태;문인기;이양규
    • 대한토목학회논문집
    • /
    • 제39권1호
    • /
    • pp.115-122
    • /
    • 2019
  • 강섬유 습식Shotcrete는 굳지 않은 콘크리트를 노즐로부터 소정의 위치에 부착시키는 콘크리트를 시공함으로서 원지반 자체의 전단강도를 증가시켜 품질을 향상시키고 터널의 안정화를 도모한다. 강섬유 습식Shotcrete는 인장 저항능력을 증대시킴으로써 국부적인 균열의 생성 성장을 억제하는 콘크리트의 강도와 역학적 거동 특성을 개선 및 보강한다. 또한, 강섬유 습식Shotcrete는 불연속의 짧은 강섬유를 콘크리트 속에 균등하게 분산시켜 인장강도, 휨강도, 균열에 대한 저항성 등을 개선한 Shotcrete이다. 이 연구에서는 NATM 터널의 숏크리트에 대한 압축강도 시험과 휨강도 시험을 실시하고 숏크리트타설 압력을 900 RPM, 1,000 RPM, 1,100 RPM으로 변화시켜 리바운드 감소율을 측정하였다. 따라서 국내 NATM 터널공사에 적용할 수 있는 자료를 제시하였다.

형상을 개선한 강섬유보강 숏크리트의 강도특성 (The Strength Characteristic of Shotcrete Reinforced with Improved Shape Steel Fiber)

  • 김상환;박인준;김지태
    • 한국지반공학회논문집
    • /
    • 제27권12호
    • /
    • pp.127-136
    • /
    • 2011
  • 본 연구에서는 형상을 개선한 강섬유를 개발하였으며, 개발 강섬유로 보강된 숏크리트의 강도특성에 대해 알아보기 위하여 실내실험을 실시하였다. 본 연구에서 사용한 시료는 무보강 숏크리트, 기존 후크형 강섬유보강 숏크리트와 형상을 개선한 강섬유보강 숏크리트이며, 이들 시료를 이용해서 강도특성을 분석하기 위해 수행한 실험은 압축강도 및 휨인성시험이다. 실험결과를 통해 형상을 개선한 강섬유보강 숏크리트의 강도특성이 기존 강섬유보강 숏크리트에 비해 향상됨을 확인했다.

대단면 암반터널의 안정성에 미치는 숏크리트 부착강도의 영향에 관한 연구 (A Study on Effect of Shotcrete Adhesive Strength on Large Section Rock Tunnel Stability)

  • 장석부;홍의준;문상조
    • 한국터널지하공간학회 논문집
    • /
    • 제7권4호
    • /
    • pp.305-311
    • /
    • 2005
  • 암반에 건설되는 대단면 터널에서 숏크리트의 부착강도는 암반탈락 방지와 발파진동에 의한 숏크리트 탈락방지에 매우 중요하다. 그럼에도 불구하고 숏크리트 부착강도는 압축강도에 비하여 설계 및 시공단계에서 중요한 요소로 고려되지 않았다. 따라서 본 연구의 목적은 숏크리트 부착강도가 대단면 암반 터널의 안정성에 미치는 영향을 분석하는 것이다. 먼저, Holmgren의 punch-loaded 시험조건을 모사한 수치해석 모델을 이용하여 다양한 부착강도에 대한 매개변수연구를 수행하였다. 그 결과, 숏크리트의 최대지지력은 숏크리트층과 블록간의 부착 강도와 선형 비례관계를 보임을 확인하였다. 또한, 숏크리트층과 굴착면에 부착강도를 고려하는 경우와 기존의 완전부착 조건에 대한 개별요소해석을 수행하여 숏크리트 부착강도의 영향을 검토하였다.

  • PDF

분말형 폴리머 혼화제를 적용한 고강도.고차수성 레디믹스트 숏크리트의 물리적 성능 평가 (Evaluation of Physical Performance of High-Strength.High Waterproof Ready-mixed Shotcrete using Powdered Polymer Dispersion)

  • 마상준;최희섭;이흥수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2008년도 추계 학술발표회 제20권2호
    • /
    • pp.337-340
    • /
    • 2008
  • As the Ready-mixed Shotcrete using Powdered Polymer Dispersion, Shotcrete Matrix as totally shotcrete gel that a part of second binder in Shotcrete materials is dense. Also, Ready-mixed Shotcrete is showed the decreasing Rebound and rising Durability. Therefore, it is possible that Ready-mixed Shotcrete for High-Strength and High-Waterproof can apply to the Powdered Polymer Dispersion.

  • PDF

지하 대공간 숏크리트 품질관리를 위한 현장강도 시험기술에 관한 연구 (A Study on Field Testing Methods for the Shotcrete Quality Control of Large Underground Spaces)

  • 장석부;이성우;홍의준;문상조
    • 터널과지하공간
    • /
    • 제16권5호
    • /
    • pp.405-412
    • /
    • 2006
  • 지하대공간 건설에 있어서 숏크리트는 가장 중요한 지보재임은 주지의 사실이다. 숏크리트의 강도는 현장 배합 및 타설 조건에 따라 실험실 조건의 숏크리트와는 큰 차이를 보이는 것이 일반적이다. 구조부재인 일반 콘크리트와 달리 숏크리트의 초기강도는 지하공간의 초기 안정화에 매우 중요하다. 그러나, 숏크리트 초기강도의 측정은 적절한 현장강도시험방법의 부재로 인하여 잘 관리되지 않은 실정이다. 따라서, 현장에서 숏크리트 초기강도를 효과적으로 측정할 수 있는 방법이 요구되고 있는 실정이다. 본 논문에서는 핀관입시험법 및 점하중강도시험법의 현장 숏크리트 초기강도 측정에 대한 적합성을 검토하였다. 이를 위해 다양한 양생강도에 따른 일축압축시험, 핀관입시험, 점하중시험을 수행하여 일축압축강도에 대한 신뢰성 높은 핀관입깊이와 점하중 지수의 상관관계식을 도출하였다.