• 제목/요약/키워드: Short-term creep rupture

검색결과 13건 처리시간 0.129초

Creep strain modeling for alloy 690 SG tube material based on modified theta projection method

  • Moon, Seongin;Kim, Jong-Min;Kwon, Joon-Yeop;Lee, Bong-Sang;Choi, Kwon-Jae;Kim, Min-Chul
    • Nuclear Engineering and Technology
    • /
    • 제54권5호
    • /
    • pp.1570-1578
    • /
    • 2022
  • During a severe accident, steam generator (SG) tubes undergo rapid changes in the pressure and temperature. Therefore, an appropriate creep model to predict a short term creep damage is essential. In this paper, a novel creep model for Alloy 690 SG tube material was proposed. It is based on the theta (θ) projection method that can represent all three stages of the creep process. The original θ projection method poses a limitation owing to its inability to represent experimental creep curves for SG tube materials for a large strain rate in the tertiary creep region. Therefore, a new modified θ projection method is proposed; subsequently, a master curve for Alloy 690 SG material is also proposed to optimize the creep model parameters, θi (i = 1-5). To adapt the implicit creep scheme to the finite element code, a partial derivative of incremental creep with respect to the stress is necessary. Accordingly, creep model parameters with a strictly linear relationship with the stress and temperature were proposed. The effectiveness of the model was validated using a commercial finite element analysis software. The creep model can be applied to evaluate the creep rupture behavior of SG tubes in nuclear power plants.

Type 316LN 스테인리스강의 크리프 수명예측과 오차분석 (Creep Life Prediction and Error Analysis for Type 316LN Stainless Steel)

  • 이원;윤송남;김우곤;류우석
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.109-110
    • /
    • 2006
  • Various parametric methods, Larson-Miller (L-M), Orr-Sherby-Dorn (O-S-D), Manson-Haferd (M-H) parameters, and minimum commitment method (MCM), were used to predict longer rupture time from short-term creep data. A number of the creep data were collected through literature surveys and experimental data produced in KAERI for predicting the creep type of type 316LN SS. Polynomial equations for predicting the creep life were obtained by the time-temperature parameters (TTP) and the MCM. standard error (SE) and standard error or mean (SEM) values were compared for the each method with temperatures. The TTP methods were good in the creep-life prediction, but the MCM was much superior to the TTP ones at $700^{\circ}C\;and\;750^{\circ}C$. The MCM was found to be lower in the SE values compared to the TTP methods

  • PDF

초초임계 석탄발전 보일러 튜브(SA213 TP347H) 용접부 안정화 열처리 효과 (Effect on the Stabilizing Heat Treatment to Weld Joint for the USC Coal Boiler Tubes(SA213 TP347H))

  • 안종석;박진근;이길재;윤재연
    • Journal of Welding and Joining
    • /
    • 제33권4호
    • /
    • pp.30-36
    • /
    • 2015
  • Austenite stainless steel(SA213-TP347H) has widely been used for the superheater & reheater tube in USC(ultra-supercritica) coal boiler because of its high creep rupture strength and anti-oxidation. But recently, the short-term failures have happened frequently in heat affected zone for only 4,000~15,000hours of service. Many investigations have been conducted to understand the failure mechanism. The root cause of failure was comfirmed to "strain induce participation hardening crack" or "reheat cracking". This mechanism often occurred due to weld residual stress and precipitation of the Cr, Nb carbides in the stabilized stainless steel such as TP347H. This paper presents an analysis of failure tube and effect of the sample tubes that conducting stabilizing heat treatment in site after 11,380hours & 16,961hours of service. Visual inspection was performed. In addition, microscopic characteristics was identified by O.M, SEM, and hardness test was carried out to find out the heat treatment effects. Failures seem to happen because of being not conducted stabilizing heat treatment in site. And another cause is inadequate weld parameter such as pass, ampere, voltage, inter-pass temperature. Thus, this paper has the purpose to describe that how to prevent similar failures in those weld-joints.