• Title/Summary/Keyword: Shear fracture

Search Result 884, Processing Time 0.028 seconds

Beam-Type Bend Specimen for Interlaminar Fracture Toughness of Laminated Composite under Mixed-Mode Defmrmations (보 형태의 굽힘시편을 이용한 적층복합재료의 혼합모우드 층간파괴인성 평가)

  • 윤성호;홍창선
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.13 no.5
    • /
    • pp.911-920
    • /
    • 1989
  • It this study, beam-type bend specimen is used to evaluate the interlaminar fracture toughness of laminated composite under mixed-mode deformations. The specimen is loaded under three-point bending and hence produced mixed-mode deformations in the vicinity of the crack tip according to the variation of the thickness ratio on delamination plane. Total energy release rate is obtained by elementary beam theory considering the effect of shear deformation. The partitioning of total value into mode-I and mode-II components is also performed. The mixed-mode interlaminar fracture toughness is evaluated by experiments on specimens with several thickness ratios of delamination plane. As the part of delamination plane is thicker, the effect of shear deformation on total energy release rate is increased. Beam-type bend specimen men may be applied to obtain informations on the mixed-mode interlaminar fracture behavior of laminated composites.

High Strain-rate Deformation Behavior of NiAl/Ni Micro-laminated Composites (NiAl/Ni 미세적층복합재료의 고속변형거동)

  • Kim Hee-Yeoun;Kim Jin-Young;Jeong Dong-Seok;Enoki Manabu;Hong Soon-Hyung
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2004.04a
    • /
    • pp.237-240
    • /
    • 2004
  • High strain-rate deformation behavior of NiAl/Ni micro-laminated composites was characterized by split hopkins on pressure bar(SHPB). When the strain rate increased, the compressive stress of micro-laminated composites were increased a little. When the intermetallic volume fraction increased, the compressive stress of micro-laminated composites increased linearly irrespective of strain rate. Absorbed energy during the quasi-static and SHPB tests was calculated from the integrated area of stress-strain curve. Absorbed energy of micro-laminated composites deviated from the linearity in terms of the intermetallic volume fraction but merged to the value of intermetallic as the strain rate increased. This was due to high tendency of intermetallic layer for the localization of shear deformation at high strain rate. Microstructure showing adibatic shear band(ASB) confirmed that the shear strain calculated from the misalignment angle of each layer increased and ASB width decreased when the intermetallic volume fraction. Simulation test impacted by tungsten heavy alloy cylinder resulted that the absorbed energies multiplied by damaged volume of micro-laminated composites were decreased as the intermetallic volume fraction increased. Fracture mode were changed from delamination to single fracture when the intermetallic volume fraction and this results were good matched with previous results[l] obtained from the fracture tests.

  • PDF

Fracture Mode Analysis with ISB Bonding Process Parameter for 3D Packaging (3차원 적층 패키지를 위한 ISB 본딩 공정의 파라미터에 따른 파괴모드 분석에 관한 연구)

  • Lee, Young-Kang;Lee, Jae-Hak;Song, Jun-Yeob;Kim, Hyoung-Joon
    • Journal of Welding and Joining
    • /
    • v.31 no.6
    • /
    • pp.77-83
    • /
    • 2013
  • 3D packaging technology using TSV (Through Silicon Via)has been studied in the recent years to achieve higher performance, lower power consumption and smaller package size because electrical line is shorter electrical resistivity than any other packaging technology. To stack TSV chips vertically, reliable and robust bonding technology is required because mechanical stress and thermal stress cause fracture during the bonding process. Cu pillar/solder ${\mu}$-bump bonding process is usually to interconnect TSV chips vertically although it has weak shape to mechanical stress and thermal stress. In this study, we suggest Insert-Bump (ISB) bonding process newly to stack TSV chips. Through experiments, we tried to find optimal bonding conditions such as bonding temperature and bonding pressure. After ISB bonding, we observed microstructure of bump joint by SEM and then evaluated properties of bump joint by die shear test.

The Correlation between Fatigue Fracture Crack Surface Friction and Crack Closure Effect in Crack Growth under Mixed-mode loading (혼합모드 하중 하에서의 균열성장 중 피로파단면 마찰과 균열닫힘효과의 상호관계)

  • Seo, Ki-Jeong;Song, Sam-Hong;Lee, Jeong-Moo
    • Proceedings of the KSME Conference
    • /
    • 2004.11a
    • /
    • pp.214-219
    • /
    • 2004
  • Crack tip behavior of single mode loading condition(mode I)depend on tensile loading component but one of mixed mode loading condition(mode I+II) have influenced on shear loading component like the practical structure. Because crack closure is caused by shear loading component under mixed-mode loading a research on the behavior in the stage of crack initiation and propagation require to be evaluate about crack closure effect by fatigue crack surface friction. For that reasion we examined the behavior at the crack tip by direct measuring method. Measured behavior at the crack tip was analyzed through vector crack tip displacement. As a result, crack propafation equation was corrected by considering with crack closure effect. In addition we compared fatigue fracture crack surface and crack closure level.

  • PDF

Simulation on Spot Welding Behavior of Car Body Sheet (자동차용 판재의 점 용접시 용접거동 Simulation)

  • 이재갑;강춘식
    • Journal of Welding and Joining
    • /
    • v.12 no.2
    • /
    • pp.76-86
    • /
    • 1994
  • Spot welding behavior of galvanized steel has been studied using both numerical and experimental techniques. The model that used to calculate temperature distribution within weldment is two-dimensional axis-symmetric finite difference method, and nugget sizes of specimen welded in condition of welding current and time has been estimated by experiment Results have shown that nugget sizes are increased in proportion to welding current and time, but the growth rate of nugget is decreased. Shear-tensile strength tests have shown interface fracture when welding current is 7, 9KA, welding time is 8-14cycle and 11KA, 8-10cycle respectively, but above 7, 9KA fracture shows button type. In button fracture, shear-tensile strengths have been proportional to nugget sizes.

  • PDF

Enhanced plasticity in a bulk amorphous matrix composite

  • Lee, Jae-Chul;Kim, Yu-Chan;Ahn, Jae-Pyoung;Kim, Hyoung-Seop
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2003.10a
    • /
    • pp.54-54
    • /
    • 2003
  • We have developed a Cu-based bulk amorphous composite reinforced with a micron-sized crystalline phase, the (Cu60Zr30Ti10)95Ta5 amorphous matrix composite. The composite demonstrates the ultimate strength of 2332 MPa with a dramatically enhanced fracture strain of 15.3 %. Macroscopic observation of the fractured (Cu60Zr30Ti10)95Ta5 amorphous matrix composite showed the development of multiple shear bands along with numerous branching and deflection of shear bands. Microscopic observation on the amorphous matrix of the composite showed that cracks propagate through the residual amorphous matrix located between nanocrystallites, which had formed during deformation. Simulations based on finite element method were conducted to understand the formation mechanisms of multiple shear bands, the initiation site of shear bands, and interaction of shear bands with crystalline particles. Other microscopic fracture mechanism responsible for the enhanced plasticity was discussed.

  • PDF

Mechanical Reliability Evaluation of Sn-37Pb Solder/Cu and Sn-37Pb Solder/ENIG Joints Using a High Speed Lap-shear Test (고속 전단시험법을 이용한 Sn-37Pb/Cu 와 Sn-37Pb/ENIG 솔더 접합의 기계적신뢰성 평가)

  • Jeon, Seong-Jae;Hyun, Seung-Min;Lee, Hoo-Jeong;Lee, Hak-Joo
    • Proceedings of the KSME Conference
    • /
    • 2008.11a
    • /
    • pp.250-255
    • /
    • 2008
  • This study utilized a high speed lap-shear test to evaluate the mechanical behavior of Sn-37Pb/Cu and Sn-37Pb/Electroless Nickel immersion Gold under bump metallization solder joints under high speed loading and hence the drop reliability. The samples were aged for 120 h at different temperatures ($120^{\circ}C,\;150^{\circ}C,\;170^{\circ}C$) and afterward tested at different displacement rates (0.01 mm/s to 500 mm/s) to examine the effects of aging on the drop life reliability. The combination of the stress-strain graphs captured from the shear tests and identifying a fracture mode dominant in the samples for different strain rates leads us to conclude that the drop reliability of solder joints degrades as the aging temperature increases, possibly due to the role of the IMC layer. This study successfully demonstrates that the analysis based on a high speed lap-shear test could be critically used to evaluate the drop reliability of solder joints.

  • PDF

Seismic behavior of thin cold-formed steel plate shear walls with different perforation patterns

  • Monsef Ahmadi, H.;Sheidaii, M.R.;Tariverdilo, S.;Formisano, A.;De Matteis, G.
    • Earthquakes and Structures
    • /
    • v.20 no.4
    • /
    • pp.377-388
    • /
    • 2021
  • Thin perforated Steel Plate Shear Walls (SPSWs) are among the most common types of seismic energy dissipation systems to protect the main boundary components of SPSWs from fatal fractures in the high-risk zones. In this paper, the cyclic behavior of the different circular hole patterns under cyclic loading is reported. Based on the experimental results, it can be concluded that a change in the perforation pattern of the circular holes leads to a change in the locations of the fracture tendency over the web plate, especially at the plate-frame interactions. Accordingly, the cyclic responses of the tested specimens were simulated by finite element method using the ABAQUS package. Likewise, perforated shear panels with a new perforation pattern obtained by implementing Topology Optimization (TO) were proposed. It was found that the ultimate shear strength of the specimen with the proposed TO perforation pattern was higher than that of the other specimens. In addition, theoretical equations using the Plate-Frame Interaction (PFI) method were used to predict the shear strength and initial stiffness of the considered specimens. The theoretical results showed that the proposed reduced coefficients relationships cannot accurately predict the shear strength and initial stiffness of the considered perforated shear panels. Therefore, the reduced coefficients should be adopted in the theoretical equations based on the obtained experimental and numerical results. Finally, with the results of this study, the shear strength and initial stiffness of these types of perforated shear panels can be predicted by PFI method.

An Experimental Study on Block Shear Fracture of Base Metal in Ferritic Stainless Steel Welded Connection (페라이트계 스테인리스강 용접접합부의 모재 블록전단파단에 관한 실험적 연구)

  • Kim, Tae Soo
    • Journal of Korean Society of Steel Construction
    • /
    • v.28 no.5
    • /
    • pp.303-312
    • /
    • 2016
  • Many researches on the application of stainless steels as structural steels have been performed thanks to their material properties such as superior ductility and corrosion resistance. Ferritic stainless steels(STS430) with little or no nickel have been used increasingly in building structure because it is inexpensive compared to austenitic stainless steels(STS304) with nickel, but provide performances similar to the austenitic stainless steel. This paper deals with block shear fracture behavior of base metal in stainless steel welded connection. Although the block shear fracture behavior for welded connection due to stress triaxiality is different from that of bolted connection, the block shear strength of welded connection in current design specifications has been predicted based on that of bolted connection. The main parameters are weld length and welding process(Arc and TIG welds). The ultimate strengths of TIG welded specimens were higher than those of arc welded specimens and current design predictions by AISC, EC3 etc. were compared with test strengths.

Shear Bond Strength and Failure Mode between Sinfony Indirect Composite Resin and Non Precious Metal (Sinfony 간접복합수지와 비귀금속합금간의 전단결합강도와 파절양상)

  • Min, Byung-Rok;Chung, In-Sung
    • Journal of Technologic Dentistry
    • /
    • v.30 no.2
    • /
    • pp.79-86
    • /
    • 2008
  • The purpose of this study was to investigate the effect retention element formed by metal surface treatment method on the bond strength of indirect composite resin and metal. The metal specimens were cast from Ni-Cr alloy($Rexillium^{(R)}$ III). They were divided into 5 groups by applied retention element: $50{\mu}m$ aluminium oxide sandblasting group, $250{\mu}m$ aluminium oxide sandblasting group, 0.2mm retention crystal group, 10% $H_{2}SO_{4}$ solution etching group, $110{\mu}m$ $Rocatec^{TM}$ Plus system group. Total 50 metal specimens were veneered with Sinfony indirect composite resin system. Specimens were tested for shear bond strength on an Instron universal testing machine and fracture mode of fractured specimens were analyzed by SEM and EDS. 1. 0.2 mm retention crystals were most effective in improving the resin-metal shear bond strength (p<0.05). 2. Sandblasting by $250{\mu}m$ aluminium oxide were more effective than sandblasting by $50{\mu}m$ aluminium oxide in improving the resin-metal shear bond strength(p<0.05). 3. Fracture mode of resin-metal fractured surface were cohesive failure mode in 0.2mm retention crystal, mixed failure mode in sandblasted specimens, etched specimens and the specimens sandblasted with $110{\mu}m$ $Rocatec^{TM}$ Plus system.