A simple route for synthesis of SnO2 from copper alloy dross

  • Lee, Jung-Il;Lee, Bo Seul;Lee, Ji Young;Shin, Ji Young;Kim, Tae Wan;Ryu, Jeong Ho
    • 한국결정성장학회지
    • /
    • 제24권2호
    • /
    • pp.84-87
    • /
    • 2014
  • Separation/recovery of valuable metals such as zinc, nickel or tin from copper alloy dross has recently attracted from the viewpoints of environmental protection and resource recycling. In this study, preliminary investigation on separation of tin (Sn) from copper alloy dross using selective dissolution method was performed. The tin in the copper alloy dross did not dissolve in an aqueous nitric acid solution which could allow the concentration/separation of tin from the copper alloy dross. Precipitation of tin as $H_2SnO_3$ (meta stannic acid)occurred in the solution and transformed to tin dioxide ($SnO_2$) after drying process. The dried sample was heat-treated at low temperature and its crystal structure, surface morphology and chemical composition were investigated.

자은철광석으로부터 희토류광물 회수에 관한 연구 (A Study on the Recovery of Rare Earth Minerals from Ja-Eun Iron Ore.)

  • 전호석;김준수;문영배;이재장
    • 산업기술연구
    • /
    • 제21권A호
    • /
    • pp.257-261
    • /
    • 2001
  • The separation of rare earths minerals is very difficult because of their similar chemical properties. The rare earth minerals are used as the mixed rare earth minerals or the misch metal without separation to each element. However, the high purity rare earths are recently produced commercially to each element so they there are used as the materials for high tech. Based on the characterization results for the raw minerals, we have developed a combined process containing gravity seperation, magnetic seperation and flotation. The result obtained from this study is monazite concentration of TREO grade 69.11% and Recovery 56.02%.

  • PDF

수성2상계를 이용한 Cyclodextrin Glucanotransferase 분리 및 회수 (Separation and Recovery of Cyclodextrin Glucanotransferase Using Aqueous Two-Phase Systems)

  • 김진현;홍승서;이현수
    • KSBB Journal
    • /
    • 제15권6호
    • /
    • pp.556-559
    • /
    • 2000
  • Cyclodextrin Glucanotransferase(EC 2.4.1.19 : 1,4-${\alpha}$-glucano) transferase, cyclizing; CGTase) can be separated and recovered in an aqueous two-phase system composed of poly(ethylene glycol)(PEG)/dextran and PEG/salt. In an aqueous two-phase system consisting of PEG 35000 (5%) and dextran T2000 (7%), all cell and debris were collected at the interphase. CGTase partitioned to the denser dextran phase at an yield of 83.4%. On the other hand, in an aqueous two-phase system consisting of PEG 35000 (10%) and sodium phosphate (15%), CGTase partitioned to the denser salt phase at an yield of 95.5%. In order to recover CGTase using an aqueous two-phase system, the PEG/salt system proved to be more efficient than the PEG/dextran system in terms of yield and cost.

  • PDF

MIL-100(Fe)를 함유한 혼합기질막(mixed-matrix membranes, MMMs)의 제조 및 기체 투과 특성 연구 (Preparation and Characterization of Mixed-matrix Membranes Containing MIL-100(Fe) for Gas Separation)

  • 송혜림;남승은;황영규;장종산;이우황;박유인
    • 멤브레인
    • /
    • 제23권6호
    • /
    • pp.432-438
    • /
    • 2013
  • 본 연구에서는 metal organic frameworks (MOFs)의 한 종류인 MIL-100(Fe)을 이용하여 혼합기질막(mixed matrix membranes, MMMs)을 제조하였다. MIL-100(Fe)의 함량을 고분자 대비 0~30 wt%까지 변화시키면서 첨가된 MOF의 함량에 따른 기체의 투과 특성을 살펴보았다. $H_2$, $CO_2$, $O_2$, $N_2$, $CH_4$의 기체 투과도는 MIL-100(Fe) 첨가량이 증가함에 따라 투과도가 증가하는 경향을 보여주었으며, 상대적으로 큰 입자크기를 가진 $SF_6$의 투과도는 MIL-100(Fe)의 첨가량이 증가함에 따라 투과도가 감소하였다. 이상 선택도는 $N_2/SF_6$의 경우 폴리이미드막 대비 약 40% 증가하였으며, 이를 통해 $N_2/SF_6$ 분리에 적합한 분리막임을 확인할 수 있었다.

LaNi5를 이용한 혼합기체로부터 수소의 선택적 분리 (Selective Separation of Hydrogen from Gas Mixture using LaNi5)

  • 선양국;남기석;이화영
    • 한국수소및신에너지학회논문집
    • /
    • 제1권1호
    • /
    • pp.15-23
    • /
    • 1989
  • The selective separation of hydrogen from gas mixture containing hydrogen was experimentally studied using $LaNi_5$. The capacity and the rate of hydrogen separation, the purity of recovered hydrogen and the optimum condition of the regeneration of deactivated $LaNi_5$ were investigated. The separation rate and the recovery ratio of hydrogen were slowly decreased with the increase of the number of hydrogen absorption cycle. It was found that this result comes from the deactivation of $LaNi_5$ partly because of the blocking of hydrocarbon compounds in the $LaNi_5$ lattice and partly because of the poisoning of $LaNi_5$ surface by carbon monoxide contained in the gas mixture. The optimum condition for the regeneration of deactivated $LaNi_5$ was obtained by heating in a vacuum to about 637 K. The recovery ratio of hydrogen at the optimum condition was observed to be about 80%. The rates of hydrogen separation were measured in the ${\alpha}$-phase and two phase regions. The rate equations could be expressed as follows ; ${\alpha}$ - phase : $$-\frac{dP{_{H_2}}}{dt}=9.836{\times}10^{-3}(P{_{H_2}}_{-P_{eq}})$$ two phase region : $$-\frac{dP_{H{_2}}}{dt}=1.6909{\times}10^2\exp(-17560/RT)(P{_{H_2}}_{-P_{eq}})$$.

  • PDF

청정석탄(淸淨石炭) 이용(利用)을 위한 정전선별(靜電選別) 기술개발(技術開發) (Development of New Techniques of Electrostatic Separation for Using of Clean Coal)

  • 백상호;전호석;한오형
    • 자원리싸이클링
    • /
    • 제14권5호
    • /
    • pp.54-61
    • /
    • 2005
  • 국내 경제성장과 더불어 발전소 에너지원으로 이용되고 있는 석탄은 매년 증가하여 2006년에는 전체 에너지 구성의 30%인 16,000MW에 이를 것으로 예측되고 있다. 이러한 석탄은 다른 화석연료에 비해 매장량이 풍부하고 경제성은 높지만, 사용이 불편하고 석탄회, 아황산가스 등 많은 공해물질을 배출하고 있다. 따라서 본 연구에서는 마찰하전형정전선별법을 이용하여 석탄과 회분구성 광물의 선별기술을 확립, 청정석탄을 생산하고자 한다. 본 연구에서는 bench-scale의 마찰하전형정전선별 장치를 제작하였으며, 선별에 영향을 미치는 인자들을 선정하고 분리실험을 수행하여 최적조건을 확립하였다. 연구결과 최적조건에서 석탄 회수율과 회분 및 유황분 제거율이 각각 68.10%. 31.23% 그리고 28.33%인 정제석탄을 얻을 수 있었다.

막 분리와 흡착 과정을 통한 해수로부터의 주요 광물 회수: 리뷰 (Recovery of Valuable Minerals from Sea Water by Membrane Separation and Adsorption Process: A Review)

  • 전성수;라즈쿠마 파텔
    • 멤브레인
    • /
    • 제32권1호
    • /
    • pp.13-22
    • /
    • 2022
  • 세계적인 에너지 수요의 증가는 통제할 수 없는 환경 오염을 야기하고 있다. 화석 연료에 대한 수요와 그로 인한 탄소 배출이 지구 온난화와 기후 변화로 이어진 것이다. 핵에너지는 청정 에너지를 생산하는 대체 자원이지만 핵연료 채굴은 유해한 화학물질과 관련이 있다. 반면에 막 분리 과정을 통해 바닷물에서 중요 광물을 채굴하는 것은 효율적이며 친환경적이다. 분리와 흡착을 통해 해수로부터 주요 광물을 채굴하는 것은 또 다른 효율적인 과정이다. 희토류 원소에서 악티늄족을 회수하는 것은 매우 어렵고 고비용의 과정이다. 압력 기반 막 분리 과정은 친환경적일 뿐만 아니라 경제적으로 실현가능한 과정이기도 하다. 본 리뷰에서 다루는 막 공정에는 폴리에테르 설폰, 폴리아미드, 폴리이미드, 폴리아미독신 및 하이브리드 막이 있다. 또한 흡착 공정의 경우, 주로 아미독심 종류의 흡착제가 논의될 것이다.

혼합가스에서 수소분리를 위한 애용량 PSA공정 (Large-Scale PSA Process for Hydrogen Separation from Gas Mixture)

  • 최대기;김은철;강석현;노경호
    • 한국수소및신에너지학회논문집
    • /
    • 제17권1호
    • /
    • pp.8-20
    • /
    • 2006
  • For large scale separation hydrogen from different mixing ratio(60/40 and 80/20 vol.%) of hydrogen and methane $1Nm^3/hr$ and $4Nm^3/hr$ 2bed-6step pressure swing adsorption(PSA) process was used, respectively. The effects of the feed gas pressure, adsorption time, the feed flow rate and the P/F(purge to feed) ratio on the process performance were evaluated. In the $1Nm^3/hr$ PSA results, 11 atm adsorption pressure and 0.10 P/F ratio might be optimal values to obtain more than 75 % recovery and 99 % purity hydrogen in these processing. The optimum feed flowrate was 22 LPM and 17 LPM in the ratio 60/40 and 80/20, respectively. In the $4Nm^3/hr$ PSA results, 10 atm adsorption pressure might be simulated values to obtain more than 80 % recovery and 99 % purity hydrogen in these processing.

국내(國內) 흑색(黑色) 점판암으로부터 우라늄 및 바나듐 회수(回收)의 연구개발(硏究開發) (Research and Development for the Recovery of Uranium and Vanadium from Korean Black Shale Ore)

  • 김준수
    • 자원리싸이클링
    • /
    • 제22권1호
    • /
    • pp.3-10
    • /
    • 2013
  • 본 발표는 국내 흑색 점판암으로부터 우라늄 및 바나듐 회수의 일반적인 현황 및 연구개발에 관한 내용이다. 우라늄 화합물(yellow cake)의 세계적인 수급 및 향후 전망뿐만 아니라, 국내 우라늄광의 매장량, 품위 및 특성에 대해 설명하였다. 그리고 국내 우라늄광의 기술개발에 관한 기 연구 실적 및 수행중인 연구과제의 개략적인 내용에 대해 기술하였다. 또한, 우라늄 및 바나듐 성분이 함유된 국내 흑색 점판암을 대상으로 하여 침출, 분리정제 및 회수에 관한 기술을 하였다.

폐 젤리충진 통신케이블로부터 고순도 구리회수를 위한 대형화 방안 연구 (A Study on the Scale-up of Highly Effective Copper Metal Recovery from Waste Jelly-filled Communication Cables)

  • 조성수;이수영;서민혜;엄성현
    • 공업화학
    • /
    • 제25권2호
    • /
    • pp.157-160
    • /
    • 2014
  • 폐 젤리충진 통신케이블로부터 고순도 구리회수를 위하여 실리콘계 및 톨루엔계 합성 열매유와 폐식용유를 사용하여 적용성을 평가하였다. 실리콘계 오일의 경우 모든 조건에서 분리효율이 낮은 반면, 톨루엔계 오일 및 폐식용유의 경우 처리온도 및 시간을 조절함에 따라 높은 분리효율을 얻을 수 있었다. 폐식용유를 사용하는 50 kg급 밀폐형 대용량 설비를 이용하여 $300^{\circ}C$에서 60 min 이상 처리할 경우 99.2% 이상의 고순도 구리와이어를 100% 회수할 수 있었다.