Concrete is widely used in the construction industry; however, it has the disadvantage of deteriorating durability due to cracks occurring because of climate change and shrinkage. In addition, when cement is used as a binder, CO2 emitted during the manu-facturing process accounts for ~8% of global CO2 emissions. In this study, ecofriendly cementitious materials such as blast furnace slag powder and fly ash (FA) were used as cement substitutes in the production of mortar containing a chitosan-based polymer (CP), and their fluidity, compressive strength, and self-healing performance were examined. The 28-day compressive strength of the control sample was ~32.4 MPa (the lowest for all tested samples), while that of the sample containing 5% CP and 20% FA was ~49.6 MPa (the highest for all tested samples) and ~53.1% higher than that of the control sample. Even at a healing age of 56 days, the control sample exhibited the lowest healing performance, whereas the samples containing CP (5%, 10%) and 20% FA demonstrated excellent healing performance. After 28 days, the decrease in crack size for the control sample was minimal; however, for the sample containing only cement and CP, a significant decrease in crack size was observed even after 28 days. This study confirmed that the appropriate use of CP and cementitious materials improves not only compressive strength but also the selfhealing performance of mortar.
Proceedings of the Korean Institute of Building Construction Conference
/
2017.05a
/
pp.22-23
/
2017
The purpose of this study is to ascertain self-healing function on microcracks in bisphenol F-type epoxy-modified mortars using expansive admixtures. The specimens are prepared with various polymer-binder ratios of 0, 5, 10, 20%, expansive admixture contents of 0% and 10%, a sodium carbonate content of 0.25%, and subjected to exposure conditions of CR1, CR2, CR3 and CR4. The specimens are tested for self-healing effect, porosity and FE-SEM analysis. As a result, self-healing effects of bisphenol F-type EPMMs with expansive admixtures are visible in all of the outdoor exposure conditions. In particular, exposure conditions of CR3 and CR4 are most noticeable. And the porosity of EPMMs is reduced with an increase in the polymer-binder ratio, and is considerably smaller than that of unmodified mortar.
Proceedings of the Korean Institute of Building Construction Conference
/
2023.05a
/
pp.149-150
/
2023
Although concrete is a material widely used in the construction industry, it is very vulnerable to cracking and has a disadvantage in that durability deteriorates when cracks occur. When cracks occur, harmful factors are introduced through the micro-cracks of the structure, reducing durability. Therefore, in this study, as part of a study to alleviate the problems of maintenance and durability deterioration due to cracks in concrete structures, the mechanical properties of self-healing mortar according to the size of the capsule made of cement material were reviewed.
Journal of the Korean Recycled Construction Resources Institute
/
v.9
no.3
/
pp.359-366
/
2021
In this study, It was developed an monitoring cracks system based on image processing techniques in order to measure cracks, which are major damages in concrete, and to convert them into a database. The crack monitoring system consists of crack image captured equipment and a crack detection and analysis software. This system provides objective and quantitative data by replacing the conventional visual inspection. The crack detection algorithm w as verified through an indoor test using virtual cracks, and the amount of crack detection and crack width change was monitored by applying it to the self-healing repair mortar construction site. In the case of the crack width detected through image analysis, the maximum difference from the actual crack width was 0.0334mm. It was possible to detect microcracks of 0.1mm or less, and the effect of crack healing over time of the self-healing repair mortar was confirmed trough the field test.
Journal of the Korean Recycled Construction Resources Institute
/
v.9
no.3
/
pp.383-388
/
2021
In this study, constant head water permeability test was adopted to evaluate self-healing performance of mortars containing inorganic healing materials which consist of blast furnace slag, sodium sulfate and anhydrite. Clinker powder and sand replaced for a part of cement and fine aggregates. On constant head water permeability test for self-healing mortars, unit water flow rate of mortar specimens were measured according to crack width and healing period. As a result of evaluating the healing performance of self-healing mortar, it was confirmed that with the initial crack width of 0.3mm, the healing rate at healing period of 28 days increased by more than 30%p compared to plain mortar, greatly improving the healing performance. Furthermore, the coefficient(α) which was estimated from the relationship between crack width and unit water flow rate was used for calculating equivalent crack width. By analyzing the correlation of healing rate and equivalent crack width, the time and initial crack width attaining healing target crack width were predicted.
Journal of the Korea institute for structural maintenance and inspection
/
v.25
no.2
/
pp.16-22
/
2021
In this paper, a solid capsule was prepared using a crystal growth type inorganic material capable of hydration reaction. The solid capsules were mixed at 3, 5, and 10% according to the composition ratio of 8:2, 7:3, 6:4 based on the cement mass, and the self-healing mortar was mixed, Durable healing properties were evaluated through the water permeability test. As a result of the water level permeability test, the effect of optimally improving the natural healing performance was shown by mixing the solid capsules prepared in a composition ratio of 7:3 of the solid capsules. In the case of a crack width of 0.3mm or less, it is estimated that more than 90% of the self-healing performance can be secured. As a result, it was judged that the self-healing performance of the solid capsule had an effect on the durable healing properties through the water permeability test, It is judged that there is a tendency to improve self-healing performance according to the mixing of solid capsules.
Jung-Il, Suh;Yoon-Suk, Choi;Byung-Sun, Park;Kwang-Myong, Lee
Journal of the Korean Recycled Construction Resources Institute
/
v.10
no.4
/
pp.561-568
/
2022
In this study, the mechanical properties and self-healing performance of cement mortar containing clinker binder, calcium sulfoaluminate(CSA), and sodium sulfate(Na2SO4) were evaluated. The mechanical properties of cement mortar were investigated by measuring compressive strength and flexural strength, and the healing performance was evaluated through hydrostatic water permeability test and gas diffusion test. In addition, the healing products precipitated in the cracks were visually observed through an optical microscope and a scanning electron microscope(SEM). As a result, the incorporation of the clinker binder-based inorganic additives improved the initial and 28-day strength by about 20 %. Depending on the healing performance evaluation method, there was a difference in the healing rate, and the healing rate showed a tendency to be underestimated. Nevertheless, CaCO3 was precipitated as the main healing product inside the 0.3 mm crack when the inorganic additives were mixed with cement mortar, improving the self-healing performance.
Journal of the Korean Recycled Construction Resources Institute
/
v.8
no.1
/
pp.120-128
/
2020
In this study, solid capsules using crystal growth-type inorganic materials that can be directly mixed with mortar were prepared. Thus, three levels of solid capsules were prepared. The prepared solid capsule was mixed with 3% of the cement mass, was evaluated quality and crack healing properties of the mortar. As a test results of the table flow and air content of the mortar mixed with the solid capsules showed that mix of the solid capsules was no effect on the table flow and air volume. As a test result of the crack healing properties of the mortar mixed with the solid capsule according to water flow test and crack closing test, the initial flow rate was decreased, it was confirmed that the reaction product occurred over time and the cracks were healed.
Self-healing (SH) technology of cracking is becoming a promising solution to improve the durability of cement based composites. However, little formula are available in the literature on determining the size and dosage of the self-healing capsules. Supposed that SH capsules will be broken and activated when they met cracks, a theoretical solution is developed to calculate the appropriate length of SH capsules based on Buffon's needle model. Afterwards, a method to calculate the dosage of capsules was proposed in terms of stereological theory. The reliability of the above mentioned theoretical methods was verified by computer simulation. An experiment of self-healing in mortar was performed as well, by which the theoretical models were verified.
Recently, the researches of self-healing concrete technology are being carried out actively due to the advent of importance for the maintenance of concrete structures. A water permeability test has been widely used for the evaluation of self-healing performance. However, it is difficult to compare tests results since there is no standard test method related to the self-healing. A standard method for measuring the crack width does not exist neither though the self-healing performance is significantly influenced by the initial crack width. In this study, the effect of water head and crack width on water flow was investigated using a constant water head permeability test equipment. The correlation equation between the initial crack width and water flow was suggested through the regression analysis of test data, and the predicted crack widths agree well with the real crack widths measured using microscopy.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.