The Transactions of the Korean Institute of Electrical Engineers P
/
v.66
no.4
/
pp.263-266
/
2017
In this study, the characteristics of anti-pollution coatings on glass substrates through annealing treatment were investigated. To investigate the change of properties by coating method and number of annealing treatment, after the anti-pollution coating was performed on the surface of glass substrate in three ways, the annealing treatment was performed by setting three kinds of annealing treatment conditions. The annealing treatment method is a torch using gas, which is advantage in that it can be installed directly on the site in an easy way compared with a annealing treatment process which is generally difficult. The anti-pollution properties, contact angle, transmittance, hardness, and adhesion of films on glass substrate were measured under 9 conditions of combination of coating methods and annealing treatment conditions. It was confirmed that as the number of annealing treatment increases, the anti-pollution property of the film synthesized on glass substrate becomes better.
화석연료의 고갈과 온실가스 배출의 증가로 지속 가능한 친환경 에너지 생산이 요구되는 가운데, 태양광 발전은 이러한 조건을 만족시키는 에너지 생산 방안으로 주목받고 있다. 태양광 발전은 태양 직사광을 이용한 발전 방법 때문에 실외에 설치되어야 하며 이에 따라 외부의 충격이나 오염물질로부터 태양전지 패널을 보호하기 위한 보호층이 필수적이다. 그러나 보호층에 의한 입사광의 반사 및 먼지나 황사에 의한 보호층의 오염 등은 태양전지의 발전 효율을 감소시키는 요인으로 작용하여 이에 대한 대응이 필요하다. 본 연구에서는 PET 필름에 나노 임프린트 리소그래피 및 핫 엠보싱 공정을 이용하여 moth-eye 반사방지 패턴을 형성함으로써 보호층에서의 입사광 반사를 억제하였다. 또한, 이러한 반사방지 패턴에 초소수성 자기조립단분자막을 코팅하여 표면 에너지를 낮춤으로써 먼지 및 황사에 의해 오염되었을 경우에도 빗물에 의해 오염 물질이 쉽게 씻겨 내릴 수 있는 자정기능을 부여하였다. 이러한 반사방지를 통한 입사광 투과량의 향상 및 초소수성 표면에 의한 자정작용에 의하여 태양전지의 발전 효율이 증가되었다.
Proceedings of the Korean Vacuum Society Conference
/
2013.02a
/
pp.293-293
/
2013
최근 디스플레이산업이 발달하면서 투명전도성 물질에 대한 산업의 요구도가 높아지고 있다. ITO투명전도성 박막은 낮은 비저항과 우수한 식각특성을 가지고 있어 평면표시소자, 광소자, 터치패널 그리고 가스 센서 등 다양한 분야에 응용되고 있으며 디스플레이 소자가 소형화 되어감에 따라 박막의 다기능화가 요구되고 있다. 본 실험에서는 전기적 특성과 친, 발수특성을 동시에 가지는 다기능성 ITO 박막을 연구하였다. RIE방식으로 식각을 통하여 Poly Si-wafer 표면에 미세구조를 만든 기판과 Slide Glass기판에 RF-magnetron sputtering 방법을 이용해 ITO박막을 증착하여 비교분석 하였다. ITO박막 증착시 $100{\sim}400^{\circ}C$ 열처리와 산소를 사용하지 않고 Ar 가스만을 사용하여 실험한 후 열처리온도에 따른 전기적 특성 및 접촉각에 대하여 조사하였다. 3 uL의 Di-water를 사용하여 접촉각을 측정한 결과 $400^{\circ}C$ 열처리가 된 Poly si-wafer 위에 증착된 ITO 박막에서 초-친수 특성을 나타냈으며, 그 위에 PTFE을 증착하였을 경우 12 uL의 Di-water를 사용하여 약 $150^{\circ}$ 이상의 초-발수 특성을 나타내었다. 전기적 특성은 $5.8{\times}10^{-4}$의 비 저항을 나타내었다. 이러한 전기적 특성과 친 발수 특성을 동시에 가지는 ITO 박막은 Anti-Fogging, self-Cleaning, Solar cell 및 디스플레이소자 등 다양한 산업에 이용 가능할 것으로 생각된다.
Journal of the Korea Organic Resources Recycling Association
/
v.24
no.4
/
pp.5-9
/
2016
In the modern industrial society, huge amount of organic wastes have exceeded the society's self-cleaning capability, caused pollution of the whole environment, including water quality, soil, and the air, and become a big burden of waste treatment. Moreover, the emission of green house gases brought by the continual combustion of fossil fuels has facilitated the global warming. The simultaneous effect of initial and operational pH on $H_2$ yield was expressed using mathematical equation and optimized. The optimal initial and cultivation pH was 7.50 and 6.01, respectively. Addition of livestock wastewater to food waste substantially decreased the amount of alkali requirement and also improved the $H_2$ fermentation performance.
Proceedings of the Materials Research Society of Korea Conference
/
2011.05a
/
pp.33.1-33.1
/
2011
최근 산업에서는 산업의 고도화로 인한 환경오염이 큰 문제로 대두되고 있다. 이러한 문제점을 해결하기 위한 방안 중, 친환경소재에 대해 연구가 활발히 진행하고 있다. 연잎의 자기세정효과(self-cleaning effect)에 관한 연구는 이러한 친환경소재에 대한 연구 중 하나이다. 연잎의 표면은 마이크로 크기의 돌기와 나노 크기의 왁스의 dual-scale의 구조로 이루어져 있으며, 왁스의 경우 소수성을 가진다. 이러한 dual-scale 구조와 소수성의 왁스에 의해 초소수성이 발현되고, 결과적으로 연잎의 자기세정효과가 발현된다. 본 연구에서는 나노임프린트 리소그래피와 수열합성법을 이용한 나노로드 성장을 이용하여, 연잎의 dual-scale의 표면구조를 형성하는 실험을 진행하였다. 나노임프린트 리소그래피와 수열합성법은 다른 공정에 비하여 상대적으로 적은 비용을 필요로 하고, 대면적에 적용이 가능한 기술이다. 실험 진행은 먼저 silicon 마스터 스탬프를 역상으로 복제한 PDMS (Polydimethylsiloxane) 스탬프와 $TiO_2$ sol을 이용하여 기판 위에 $TiO_2$ gel 패턴을 형성한 후, 열처리 과정을 통해 $TiO_2$ gel 패턴을 결정화한다. 다음으로 결정화된 $TiO_2$ 패턴 기판을 수열합성 방법을 이용하여 $TiO_2$ 나노로드를 무작위적으로 형성하였다. 마지막으로 소수성을 갖는 자기 조립 단분자막 용액을 이용하여 소수성 표면처리를 한 후 접촉각을 측정하였다. 본 연구에서 개발한 기술을 이용하여 다양한 형태의 기판에 초소수성 표면을 형성할 수 있고, 자기세정효과를 갖는 표면을 구현할 수 있다.
Kim, Eun-Gyeong;Lee, Cheol-Seong;Choe, Seon-U;Hwang, Tae-Jin;Kim, Sang-Seop
Proceedings of the Materials Research Society of Korea Conference
/
2011.05a
/
pp.41.1-41.1
/
2011
초소수성 표면은 $150^{\circ}$ 이상의 높은 접촉각을 가지며 표면에 오염물질이 묻지 않게 하는 anti-contamination, anti-fingerprint, self-cleaning 기능을 갖고 있는 것이 특징이다. 재료표면의 친/소수성을 제어하기 위해서는 고체 표면의 화학적인 요인과 물리적인 요인 두 가지를 조절함으로써 이루어지는데 즉 물질의 표면에너지와 표면 거칠기를 변화시켜 친/소수성을 부여할 수 있다. 초소수성 표면을 구현하기 위해서는 고체 표면의 에너지를 낮춰야 하며 이는 일반적으로 불소화합물을 사용한다. 불소는 지구상의 원소 중 가장 낮은 표면에너지를 가지고 있어 주로 후라이팬이나 치아 표면에 코팅되며 오염을 방지하는 특성을 지닌다. 실리카는 박막소재로 이용하기 위한 우수한 특성을 가진 물질로서 자연계에서 매우 풍부하게 존재하고 있으며, 생체무해하며 내구성과 내마모성, 화학적 안정성, 고온 안정성 등을 지니고 있어 여러 가지 종류의 전자기기 및 부품의 내외장 코팅에 적용이 적극 검토되고 있다. 이러한 실리카 코팅소재를 바탕으로 초소수성 코팅층을 구현하는 하나의 방법으로서 본 연구에서는 전기분무법을 사용하여 실리카 코팅층을 형성하였으며, 표면에너지를 제어하기 위해 플루오린 처리를 하여 초소수성 실리카 코팅층을 제조하였다. 합성된 실리카 코팅층은 물 뿐만이 아니라 표면장력이 낮은 다른 용액에서도 초소유성을 나타내었다. 이러한 코팅층에 대한 고온 안정성과 UV 저항성, 내구성(durability) 등을 조사하여 실제 응용 가능성을 타진하였다.
The fabrication of a controlled surface is of great interest because it can be applied to various engineering facilities due to the various properties of the surface, such as self-cleaning, anti-bio-fouling, anti-icing, anti-corrosion, and anti-sticking. Controlled surfaces with micro/nano structures were fabricated using an ion beam focused onto a polypropylene (PP) surface with a fluoridation process. We developed a facile method of fabricating hydrophobic surfaces through ion beam treatment with argon and oxygen ions. The fabrication of low surface energy materials can replace the current expensive and complex manufacturing process. The contact angles (CAs) of the sample surface were $106^{\circ}$ and $108^{\circ}$ degrees using argon and oxygen ions, respectively. X-ray photoelectron spectroscopy (XPS) and Fourier transform infrared (FT-IR) spectroscopy were used to determine the chemical composition of the surface. The morphology change of the surfaces was observed by scanning electron microscopy (SEM). The change of the surface morphology using the ion beam was shown to be very effective and provide enhanced optical properties. It is therefore expected that the prepared surface with wear and corrosion resistance might have a considerable potential in large scale industrial applications.
Proceedings of the Korea Concrete Institute Conference
/
2006.05b
/
pp.585-588
/
2006
The environment-friendly building material, photocatalyst/scoria/loess concrete, was prepared using scoria and loess (which have merits as building materials) and photocatalyst (which has the functions to compose the environmental contaminants and of self cleaning). In order to apply this material as a building material, the compressive and flexible strengths, and water absorptivity (which have been set by Korea Industrial Standard) were measured. The optimum mixing ratio of photocatalyst/scoria/loess concrete was obtained at the condition of $393kg/m^3$ of coarse aggregate, $802kg/m^3$ of fine aggregate in case of scoria, $80kg/m^3$ of loess, $12kg/m^3$ of photocatalyst, $400kg/m^3$ of cement, and $2kg/m^3$ of AE water reducing agent. The photocatalyst/scoria/loess concrete prepared by above mixing ratio of raw materials showed 25 MPa of compressive strength, $3.8{\sim}4.6$ MPa of flexible strength and $11.4{\sim}12.0%$ of water absorptivity, indicating that the quality of this material was suitable for Korea Industrial Standard (more than 21 MPa for compressive strength, more than 2.0 MPa for flexible strength in case of lightweight aggregate, and less than 15 % for water absorptivity in case of clay brick) for using as a building material.
Proceedings of the Korea Concrete Institute Conference
/
2006.05b
/
pp.593-596
/
2006
The environment-friendly building material, photocatalyst/scoria/loess concrete, was prepared using scoria and loess (which have merits as building materials) and photocatalyst (which has the functions to compose the environmental contaminants and of self cleaning). In order to apply this material as a building material, the compressive and flexible strengths, and water absorptivity (which have been set by Korea Industrial Standard) were measured. In order to know the environment-friendly characteristics of this material, several tests, such as, the tests of emissivity and emission power of far infrared ray and acoustic absorptivity, antibacterial test for Escherichia coli and Pseudomonas aeruginosa, antifungal test for mixed fungal strains, and deodorization test of ammonia were carried out. Moreover, the removal characteristics of NOx, and formaldehyde (HCHO) by photocatalyst/scoria/loess concrete were examined as the following different parameters: the removal characteristics of these contaminants with the substitution ratio and the kind of photocatalyst, light source, UV intensity of sunlight, relative humidity, intial NOx concentration.
Shan, Bowen;Kang, Hyunil;Choi, Won Seok;Lee, Kyoung-Bok;Ma, Sanggyeon
The Transactions of the Korean Institute of Electrical Engineers P
/
v.65
no.1
/
pp.53-56
/
2016
Because of the low pollution resistance of the porcelain electrical insulator itself, in this work the anti-pollution performance of insulator was improved by using the functional coating. The ceramic substrates that components were same as the porcelain electrical insulator were used in this experiment. The functional films were coated on the ceramic substrate by using a spray coating method, and then the coated substrate were annealed under different coating condition such as natural curing and annealing temperature of $200^{\circ}C$, $300^{\circ}C$ and $400^{\circ}C$. Then, the contact angles of the coated surfaces were measured and the minimum angle ($8.3^{\circ}$) was obtained at $400^{\circ}C$. The anti-contamination properties were measured, revealing that as the contact angle decreased, the anti-contamination properties improved. The hardness and adhesion were small at the natural curing condition however the excellent mechanical properties were obtained under higher temperature annealing.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.