  • In domestic, various repair materials and method systems to keep up with these reinforced concrete deteriorated due to salt damage, carbonation, chemical decay et. developed and applied. However, on-site quality control of various repair materials and method systems isn't achieved desirably because it is depend completely on a men of experience' opinions above all else regardless of various on-site environments. In this background, mock up test with due regard to real on-site environments was performed to secure fundamental data for establishment of desirable on-site quality control. Mock up test using repair mortar analyzed from angles of construction methods, mechanical spraying pressures, W/M. Construction methods were designed manpower method and spraying method, spraying pressures were designed 32, 42, 52 psi, W/M were designed 14.4, 15.4, $16.4\%$. And compressive strength, Chloride ion diffusion coefficient, bond strength, SEM. of mock up test specimens were evaluated. In conclusion, we confirmed excellency of mechanical spraying pressures, fined extremely excellency of condition of spraying pressure 42 ps, W/M $14.4\%$ within this study. therefore the results of this study will be useful to provide fundamental data for establishment of desirable on-site quality control.

  • PDF

절임방법에 따른 깍두기의 관능적 및 미생물학적 특성 (Effects of Salting Methods on the Sensory and Microbiological Properties of Kakdugi)

  • 김나영;장명숙
    • 한국식품조리과학회지
    • /
    • 제16권1호
    • /
    • pp.75-83
    • /
    • 2000
  • The effects of salting methods on sensory and microbiological properties of Kakdugi were evaluated during fermentation at 10$\^{C}$ for up to 52 days. Kakdugi samples were prepared by 4 different salting methods at the final salt concentration about 1.5%, which was appropriate for organoleptic quality. The salting methods for radish cubes(2cm size) of Kakdugi included; 1) Treatment S-1: spraying dry salt uniformly onto the radish cubes, at the concentration of about 1.5%(w/w) and cured for 1 hr, 2) Treatment S-5: spraying dry salt uniformly onto the radish cubes, at the concentration of about 1.2%(w/w) and cured for 5 hr, 3) Treatment B-1: brining radish cubes in a 8.5%(w/v) salt solution and cured for 1 hr, 4) Treatment B-5: brining radish cubes in a 4.0%(w/v) salt solution and cured for 5 hr. During the early stage of fermentation, sensory test showed higher scores in the overall acceptability of Kakdugi prepared with salting methods S-1 and S-5 than those with B-1 and B-5. However, the trend of acceptability has been reversed by the treatments B-1 and, more notably, by B-5 at the later stage of fermentation. The counts of lactic acid bacteria increased remarkably and then decreased gradually after the optimum ripening period. The major lactic acid bacteria isolated and identified from Kakdugi were Pediococcus, Streptococcus, Leuconostoc, and Lactobacillus.

  • PDF

제설제 및 동결융해 환경하에서 콘크리트의 내구성 증진 방안에 관한 연구 (Improvement of Concrete Durability under Deicier and Freez-Thaw Environment)

  • 이병덕;윤병성
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 추계 학술발표회 제17권2호
    • /
    • pp.523-526
    • /
    • 2005
  • In order to traffic safety during winter season, snowfall and cold area has been spread the deicing chemicals, and the spraying amount is increasing every year. Use of deicing chemicals has been and will continue to be a major part of highway snow and ice control methods. Chloride-containing chemicals such as calcium chloride or rock salt are main deicers for the road. Extensive use of chloride deicers is, however, the source of substantial cost penalties due to their corrosive action and acceleration to deterioration concrete structures. Deterioration due to de-icer salt occurs in practice in concrete pavement, dike, barrier and similar structure. This paper reports the results of effect of de-icer salt on durability of concrete structure in winter. To protect concrete structure from damage by de-icer salt in winter, the exposure test was performed using three methods such as increase in design strength upto 32MPa application of granulated blast furnace slag powder, and concrete sealer. Of these, the method of increase in design strength upto 32MPa showed better durability for deterioration by de-icer salt.

  • PDF

적설한랭지역에서 콘크리트의 내구성 (Durable of Concrete in Snowfall and Cold Regions)

  • 이병덕;정해문;윤병성
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.221-224
    • /
    • 2005
  • In order to traffic safety during winter season, snowfall and cold area has been spread the deicing chemicals, and the spraying amount is increasing every year. Use of deicing chemicals has been and will continue to be a major part of highway snow and ice control methods. Chloride-containing chemicals such as calcium chloride or rock salt are main deicers for the road. Extensive use of chloride deicers is, however, the source of substantial cost penalties due to their corrosive action and acceleration to deterioration concrete structures. Deterioration due to de-icer salt occurs in practice in concrete pavement, dike, barrier and similar structure. This paper reports the results of effect of de-icer salt on durability of concrete structure in winter. To protect concrete structure from damage by de-icer salt in winter, the exposure test was performed using three methods such as increase in design strength upto 35MPa application of granulated blast furnace slag powder, and concrete sealer. Of these, the method of increase in design strength upto 35MPa showed better durability for deterioration by de-icer salt.

  • PDF

Dust & Fog법을 이용한 트래킹가속열화 (Accelated Aging Test of Tracking Using the Dust & Fog Method)

  • 임장섭;이진;이정식;정우성;김태성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1996년도 추계학술대회 논문집
    • /
    • pp.117-120
    • /
    • 1996
  • In this paper, It is tested by spraying the spoiled liquids on the materials to prove the process of tracking under the various environments. Our experiments ware examined by setting the materials in the spray chamber, and by spraying the distilled water(DW), the city water(CW), the underground water(UW), the artificial acid rain(AR) and the salt water(SW) in applied voltage 3-6[KV]. As the result, the time of tracking breakdown became shorter in the order of DW < CW < UW < AR < SW. XLPE was eroded and its anti-bracking property was very strong, but that of PVC sheath was week. Especially it was confirmed that spraying by AR and SW on the PVC sheath had a serious effect on the lifetime of cable by the tracking breakdown.

  • PDF

도로 제설제 권장 살포량 산정식의 적정성 평가 (Evaluation of Reasonableness of the Recommended Spraying Amount Equation for De-icing Chemicals)

  • 김진국;양충헌
    • 한국도로학회논문집
    • /
    • 제19권4호
    • /
    • pp.9-18
    • /
    • 2017
  • PURPOSES : This study evaluates the reasonableness of the recommended amount of deicing chemicals based on historical data for snow removal. The result can be used to aid decision-making for the reservation of cost-effective de-icing chemicals. METHODS : First, the recommended amount of de-icing chemical to use and historical usage data were evaluated to identify specific usage characteristics for each region. Road maintenance length and snow-removal working days were analyzed over the past five winter seasons. Next, differences in the recommended amount of chemical to use and actual use were compared using the Kolmogorov-Smirnov test. Last, the two types of data were analyzed using a chi-square test to verify if the two distributions of variation pattern are statistically significant. We found that there are significant differences between the data from each region during the past five winter seasons. RESULTS : The results showed that the equation for calculating the amount of de-icing chemical to use appears to be revised. CONCLUSIONS : The results imply that the equation for calculating the amount of de-icing chemical to apply as a national standard is very important when the public agency makes decisions related to snow-removal.

CORROSION BEHAVIOR OF Al-Zn ALLOY AS A SACRIFICIAL ANODE OF ORV TUBES

  • Jin, Huh;Lee, Ho-Kyun;Lee, Jae-Ho
    • 한국표면공학회지
    • /
    • 제32권3호
    • /
    • pp.452-455
    • /
    • 1999
  • ORV which vaporizes LNG to NG is consisted of tube and header whose substrate is aluminum alloy. The corrosion of the tube is very severe because of sea water being used as the heating source. In this research to protect ORV substrate material, the corrosion behavior of aluminum alloys was investigated for the sacrificial role of Al-Zn alloy for ORV tubes. The electrochemical behavior of aluminum alloys in sea water was investigated. The corrosion behavior of thermally-sprayed and cladded samples were compared through salt spray tests. Al-Zn alloy can act as a sacrificial anode and cladded Al-Zn alloy has a better corrosion resistance than that of thermally sprayed one. The galvanic effect of Al-Zn to substrate material was conformed from scratched sample tests.

  • PDF

SD460 철근의 세라믹 코팅에 의한 내식성 향상연구 (Corrosion Resistance of SD460 Reinforcing Rod by Ceramic Coating)

  • 박기용;이종권;홍석우
    • Corrosion Science and Technology
    • /
    • 제8권4호
    • /
    • pp.157-161
    • /
    • 2009
  • The corrosion resistance of reinforcing bar was studied to endure the marine environment during shipment. The red rust on the surface did not damage the adherence in the concrete structures, especially in highly alkaline environment, but made the consumer doubt of the quality. The passivation process by alkalization of the quenching water in the tempcore process failed to endure the long shipping period. The ceramic coating by sol-gel process improved the corrosion resistance without damaging the mechanical properties and adherence between concrete and reinfiorcing bar. Optimal concentration of the coating solution and coating temperature were tested. No additional energy was necessary for the coating process by spraying during cooling process, resulting simplified process and low cost. Salt spray test, cyclic corrosion test and atmospheric test were employed to confirm the resistance. The corrosion rates were presented by rating number and polarization resistance. The coating layer was examined by FIB, XRD and SEM etc.

Zn-Al의 구성비율에 따른 금속용사 공법의 방식성능에 대한 실험적 연구 (Experimental Study of The Corrosion Protection Performance of The Metal Spraying Process in accordance with ratio of Zn-Al)

  • 김해;엄성현;정현규;이정배;김성수;안재우
    • 자원리싸이클링
    • /
    • 제26권2호
    • /
    • pp.56-65
    • /
    • 2017
  • 본 연구는 금속용사 공법의 희생양극재료인 Zn, Al의 구성비율에 따른 방식성능에 관한 실험적 연구이다. 금속용사의 분사 방법으로는 Arc 금속용사 공법을 사용하였으며, Zn, Al의 구성비율 및 코팅 두께를 달리하여 시편을 제작하였다. 실험방법으로는 CASS 염수분무 실험에 준하여 실시하였으며 CASS 염수분무 시작일로부터 1, 3, 7, 15일 동안 실험체의 부식상태를 육안으로 관찰하였다. 본 연구결과 Al의 함량이 증가함에 따라 부식에 대한 방식성능이 증가함을 확인하였으며, 코팅두께 $80{\mu}m$ 이상을 확보하여야만 우수한 방식성능이 발현되는 것을 확인하였다. 또한 CASS 실험 후 금속용사 실험체의 단면 형상 관찰하기 위해 SEM 분석을 실시하였으며, 분석결과 Al의 함량이 증가할수록 금속용사 코팅층의 열화가 감소하는 것을 확인하였다.

304L 스테인리스강 분말의 내식성 개선을 위한 무전해 구리 도금과 분말 소결체의 내식성 조사 연구 (Electroless Copper Plating on 304L Stainless Steel Powders and Corrosion Resistance of the Sintered Compacts of Composite Powders)

  • 안재우;이재훈
    • 대한금속재료학회지
    • /
    • 제47권2호
    • /
    • pp.79-90
    • /
    • 2009
  • A study has been made about the effects of powder content, reaction temperature, reaction time, and stirring speed on the preparation of the stainless steel(STS) 304L powders plating with copper by an electroless plating method. The behavior of corrosion resistance of the sintered STS-Cu composite powders was also investigated by the salt spraying test The electroless plating technique was an effective method to manufactur the copper-uniform plating composite powders, the corrosion resistance of this sintered specimen was improved bysuppressing Cr precipitates on grain boundaries in the sintered compacts of composite powders.