강관철근을 보강한 합성기둥의 3시간 가열 후 잔존 압축력 실험평가 (Evaluation of Residual Strength and Behavior of Reinforced STG 800 Welded Square Composite Column after Fire 3 Hour)

  • 김선희;염경수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2021년도 가을 학술논문 발표대회
    • /
    • pp.242-243
    • /
    • 2021
  • The concrete inside the steel tube of CFT columns enables them to have great strength and ductility. CFT columns are also excellent in fire-resistance because explosive heat upon a fire can be contained in the tube by the concrete debris. However, the studies to evaluate the residual strength of CFT columns after a fire have not been conducted enough. The studies to evaluate the residual strength of CFT columns after a fire are indispensable because it is the barometer of the damage of composite columns caused by a fire and the degree of repair and reinforcement work for the columns after a fire. Accordingly, the purpose of this study is to evaluate the deterioration of load capacity and structural behavior of square CFT columns with the same shapes and boundary conditions before and after a fire. The study also evaluates the influential factors of the CFT columns reinforced to secure the residual strength after a fire.

  • PDF