Investigation of Mix Design Method in Concrete Mixed with SSPCM Based on Mechanical Behaviors (SSPCM 혼입 콘크리트의 역학적 성능 기반 배합설계기법 연구)

  • Min, Hae-Won;Kim, Hee-Sun
    • Journal of the Korean Society for Advanced Composite Structures
    • /
    • v.6 no.2
    • /
    • pp.1-7
    • /
    • 2015
  • As energy consumption of building and the reduction of carbon dioxide emissions have been emphasized, phase change materials(PCM) have been introduced as building materials due to its high heat storage performance. Using shape-stabilizing technique, octadecane/xGnP shape-stabilized PCM(SSPCM) can prevent leakage and improve heat storage performance. The objectives of this study are to propose mix design method of concrete mixed with SSPCM and to evaluate mechanical behaviors of the concrete mixed with SSPCM manufactured according to the proposed mix design. Based on the previously reported material test result, the existing mix design of plain concrete(Concrete standard specification, 2009) is modified to consider reduction of strength in concrete due to the addition of SSPCM. To verify the proposed mix design, specimens are fabricated according to the proposed mix design and axial strength tests and three-point loading tests are performed. Test results show that compressive strengths of the tested specimens reach the designed strength even when two different mix ratios of SSPCM are used. From three-point loading tests, flexural stresses decrease as mix ratio of SSPCM increases.

Preparation and Properties of Shape-Stabilized Phase Change Materials from UHMWPE and Paraffin Wax for Latent Heat Storage (파라핀과 초고분자량 폴리에틸렌으로 구성된 형태안정성 상 전이 물질의 제조 및 특성)

  • Lee, Hyun-Seok;Park, Jae-Hoon;Yim, Jong-Ha;Seo, Hye-Jin;Son, Tae-Won
    • Polymer(Korea)
    • /
    • v.39 no.1
    • /
    • pp.23-32
    • /
    • 2015
  • Phase change materials based on ultra high molecular weight of polyethylene (UHMWPE) blended with paraffin wax (mp $65^{\circ}C$) were studied in this paper. In addition, this paper reviews recent studies on the preparation of shape stabilized phase change materials (SSPCM), such as SSPCM from UHMWPE and paraffin wax (mp $65^{\circ}C$), their basic properties and possible applications to latent heat storage. The preparation method was an absorption method. Also, SSPCM composites were prepared by using a hot press at $200^{\circ}C$ for 10 min. The analysis for the shape ability of SSPCM to improve heat efficiency was measured by FTIR, SEM, DSC, XRD, and ARES. UHMWPE composites with 30 wt% paraffin wax (mp $65^{\circ}C$) demonstrated less deterioration of physical property and effective thermal property compared with other conditions. As a result, these SSPCMs could be used for the heat storage and release materials for various products.

Preparation and Thermal Characteristics of Hexadecane/xGnP Shape-stabilized Phase Change Material for Thermal Storage Building Materials (축열건축자재 적용을 위한 Hexadecane/xGnP SSPCM 제조 및 열적특성)

  • Kim, Sug-Hwan;Jeong, Su-Gwang;Lim, Jae-Han;Kim, Su-Min
    • Journal of the Korean Solar Energy Society
    • /
    • v.33 no.1
    • /
    • pp.73-78
    • /
    • 2013
  • Hexadecane and exfoliated graphite nanoplate (xGnP)composite was prepared as a shape-stabilized phase change material (SSPCM) in a vacuum to develope thermal energy storage. The Hexadecane as an organic phase change material (PCM) is very stable against phase separation of PCM and has a melting point at $18^{\circ}C$ that is under the thermally comfortable temperature range in buildings. The xGnP is a porous carbon nanotube material with high thermal conductivity. Scanning electron microscope (SEM) and Fourier transformation infrared spectrophotometer (FT-IR)were used to confirm the chemical and physical stability of Hexadecane/xGnP SSPCM. In addition, thermal properties were determined by Deferential scanning calorimeter(DSC) and Thermogravimetric analysis (TGA). The specific heat of Hexadecane/xGnPSSPCM was $10.0J/g{\cdot}K$ at $21.8^{\circ}C$. The melting temperature range of melting and freezing were found to be $16-25^{\circ}C$ and $17-12^{\circ}C$. At this time, the laten heats of melting and freezing were 96.4J/g and 94.8J/g. The Hexadecane was impregnated into xGnP as much about 48.8% of Hexadecane/xGnP SSPCM's mass fraction.