• 제목/요약/키워드: SAW/FCAW

검색결과 29건 처리시간 0.024초

800MPa급 무예열 용접 판재의 수중 폭파변형시험 (Explosion Bulge Test Underwater of 800MPa Grade Pre-heat Free Welding Plate)

  • 박태원;송영범;김진영;양성호;박철규;서준석;김희진
    • Journal of Welding and Joining
    • /
    • 제28권6호
    • /
    • pp.63-69
    • /
    • 2010
  • The pre-heat free consumables for GMAW, SAW and FCAW processes that matche with the Cu-bearing PFS-700 steel which has yield strength over 700MPa were developed and evaluated to see the suitability in military such as submarine and battle ship. Explosion Bulge Test underwater was developed and applied to see the reliability of welded structure. All welding was conducted without pre-heat before welding, the interpass temperature was below $150^{\circ}C$ for all welding conditions. Tensile strength for the weld metal in GMAW, SAW and FCAW process is 887MPa, 875MPa and 813MPa, respectively, these values are similar to the base metal of PFS-700 steel of 838MPa. EBT results in GMAW, SAW and FCAW show 14.0%, 14.02% and 15.9% reduction of thickness without generation of crack, respectively and stand-off distance was set up properly to have over 14.0% reduction of thickness. Through EBT results, the developed new consumables are applicable to the weapon systems such as submarine and battle ship.

800MPa급 무예열 용접 판재의 수중 폭파변형시험 (Explosion Bulge Test in Underwater of 800MPa Grade Pre-Heat Free Welding Plate)

  • 박태원;송영범;김진영;양성호;홍성석;심인옥;박철규;김희진
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2010년도 춘계학술발표대회 초록집
    • /
    • pp.63-63
    • /
    • 2010
  • The pre-heat free consumables for GMAW, SAW and FCAW processes that matches the Cu-bearing PFS-700 steel which has yield strength over 700MPa were developed and evaluated to see the suitability in military such as submarine and battle ship. Explosion bulge test in underwater was developed and applied to see the reliability of welded structure. All welding was conducted without pre-heat before welding, the interpass temperature was below $150^{\circ}C$ for all welding conditions. Tensile strength for the weld metal in GMAW, SAW and FCAW process is 887MPa, 875MPa and 813MPa, respectively, these values are similar to the base metal of PFS-700 steel of 838MPa. EBT results in GMAW, SAW and FCAW show 14.0%, 14.02% and 15.9% reduction of thickness without generation of crack, respectively and stand-off distance was set up properly to have over 14.0% reduction of thickness. Through EBT results, the developed new consumables are applicable to the weapon systems such as submarine and battle ship.

  • PDF

석유시추용 인코넬 625강의 FCAW용접에 의한 부식성에 관한 연구 (A Study on Corrosive Characteristics of Inconel 625 for Petroleum Application by FCAW Process)

  • 박경동;안도경;안재필
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2004년도 학술대회지
    • /
    • pp.365-369
    • /
    • 2004
  • Recently, Inconel 625 is used widely in offshore processing piping in order to extend the maintenance tenn and improve the quality of anti-corrosion. According to the resistance to attack in various corrosive media at temperatures from $200^{\circ}C$ to aver $1090^{\circ}C$, in combination with good low- and high-temperature mechanical strength. In general, High quality weldments for this material are readily produced by commonly used processes. in recent years, the flux cored arc welding(FCAW) process is becoming more popular due to higher deposition rate and a better weld quality as compared to the shielded metal arc welding (SMAW) process, at the same time, exhibiting equally good weld metal toughness similar to the SAW process. In this study, the weldability and weldment characteristics(mechanical properties and corrosive environment) of Inconel 625 are considered in FCAW weld associated with the several weld shielding gases($80\%Ar\;+\;20\%\;CO_2,\;50\%Ar\;+\;50\%\;CO_2,\;100\%\;CO_2$) in viewpoint of welding productivity.

  • PDF

선체 탑재 이음부의 고능률 SAW 적용 (Application of high efficiency SAW process in erection joint of ship)

  • 윤광희;김진용;허만주
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2010년도 춘계학술발표대회 초록집
    • /
    • pp.52-52
    • /
    • 2010
  • 선박건조에 있어서 대형 블록의 조립이 이루어지는 선행 탑재 및 탑재 단계에서 Tank Top과 Upper Deck의 V 개선 용접은 FCAW+SAW의 복합용접이 실시되고 있다. 그러나 가장 범용적 모재 두께인 18~20t의 경우 SAW 시공에만 약 5~6Pass가 소요됨으로써 다급한 진수 일정에 많은 지장을 초래하고 있다. 또한 능률 향상을 목적으로 용착량 증가효과를 얻기 위해 철분말이나 절선와이어를 개선면내에 충진하고 용접을 수행하나 획기적인 용접능률을 기대하기 어렵고 용접사 기량에 따라 용접 결함이 발생될 수 있다. 이에 따라 용접패스 수를 줄이고 결함 발생이 없는 용접기법 개발이 절실히 필요하였다. 이를 위해 매우 간단하고 효율적인 위빙장치를 제작하여 선탑/탑재 아래보기 용접이음에 1~2패스의 SAW 용접법을 개발하여 용접생산성은 물론 용접품질까지 획기적으로 향상시키는 기술 개발을 완료하였다.

  • PDF

용접 공정 디자인에 따른 클래드강의 기계적 성질 변화 (Change of Mechanical Properties of Clad Steel According to the Welding Process Design)

  • 이정현;박재원
    • 한국생산제조학회지
    • /
    • 제22권3호
    • /
    • pp.372-379
    • /
    • 2013
  • In this study, we investigated the traits of the clad metals used in hot-rolled clad steel plates. We examined the sensitization and mechanical properties of STS 316 steel plate and carbon steel (A516) under the specific circumstances of post heat treatment and whether a weld was multilayered and thick or repeated because of repairs. The test conditions were as follows. The clad steel plates were butt-welded using FCAW/SAW, and the heat treatment was conducted at $625^{\circ}C$, for 80, 160, 320, 640, or 1280 min. The change in the corrosion resistance was evaluated in these specimens. In the case of the carbon steel (A516), as the heat treatment time increased, the annealing effect caused the tensile strength to decrease. The micro- hardness gradually increased and then decreased after 640 min. The elongation and contraction of the area increased gradually. An oxalic acid etch test and EPR test on STS316, a clad metal, showed a STEP structure and no sensitization. From the test results for the multi-layered and repair welds, it could be concluded that there is no effect on the corrosion resistance of clad metals. In summary, the purpose of this study was to suggest some considerations when developing on-site techniques and evaluate the sensitization of stainless steels.

컨테이너선의 후 물재 용접부 취성 균열 전파에 대한 FCAW와 SAW의 비교 특성에 관한 연구 (Comparison of the Characteristics of FCAW and SAW for the Brittle Crack Propagation of Welded Parts of BCA Steel in Container Ships)

  • 최경신;이상훈;최정주
    • 한국기계가공학회지
    • /
    • 제20권3호
    • /
    • pp.24-32
    • /
    • 2021
  • The size of container ships is increasing to increase the cargo loading capacity. However, container ships are limited in terms of the hull longitudinal strength. To overcome this limitation, brittle crack arrest steel can be used. This study was aimed at examining the influence of the heat input on the welding procedures of flux cored arc welding and submerged arc welding. In the experiment, the crack tip opening displacement test, which pertains to a parameter of fracture mechanics, was performed, and a 3-point bending tester was adopted. Based on the results, the crack measurement method was presented, and the stress expansion coefficient value for the pre-fatigue crack length was derived according to the heat input after the pre-cracking length was measured. It was noted that the heat input affected the crack tip opening displacement of brittle crack arrest steel.

금속계 플럭스들이 용접이음부의 피로강도 특성에 관한 연구 (A Study on Fatigue Strength Characteristics of Weld Joint using Metal Type Flux Cored Wire)

  • 강성원;신동진;김환식
    • Journal of Welding and Joining
    • /
    • 제12권4호
    • /
    • pp.151-161
    • /
    • 1994
  • FCAW has wide application in ship fabrication, maintenance and field erection. It has many advantages over SMAW.SAW and GMAW process. In many applications, the FCAW provides highquality weld metal. This method can reduce weld defects especially porosity and spatter. But the fatigue characteristics of those deposited metal have been rarely investigated. The purpose of this study is to investigate the cyclic stress-strain behavior and fatigue tests by the constant strain control were carried out on the rounded smooth specimen with deposited metal using the metal type flux cored wire. As the results of this study for the deposited metal welded by the metal type flux cored wire, the hardening or softening characteristics under cyclic load were investigated and cyclic stress-strain curve, strain-fatigue life curve, stress-strain function and fatigue life relation which are useful to estimate the fatigue life under the stress concentration condition were obtained.

  • PDF

AUTOMATIC MULTITORCH WELDING SYSTEM WITH HIGH SPEED

  • Moon, H.S;Kim, J.S.;Jung, M.Y.;Kweon, H.J.;Kim, H.S.;Youn, J.G.
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.320-323
    • /
    • 2002
  • This paper presents a new generation of system for pressure vessel and shipbuilding. Typical pressure vessel and ship building weld joint preparations are either traditional V, butt, fillet grooves or have narrow or semi narrow gap profiles. The fillet and U groove are prevalently used in heavy industries and shipbuilding to melt and join the parts. Since the wall thickness can be up to 6" or greater, welds must be made in many layers, each layer containing several passes. However, the welding time for the conventional processes such as SAW(Submerged Arc Welding) and FCAW(Flux Cored Arc Welding) can be many hours. Although SAW and FCAW are normally a mechanized process, pressure vessel and ship structures welding up to now have usually been controlled by a full time operator. The operator has typically been responsible for positioning each individual weld run, for setting weld process parameters, for maintaining flux and wire levels, for removing slag and so on. The aim of the system is to develop a high speed welding system with multitorch for increasing the production speed on the line and to remove the need for the operator so that the system can run automatically for the complete multi-torch multi-layer weld. To achieve this, a laser vision sensor, a rotating torch and an image processing algorithm have been made. Also, the multitorch welding system can be applicable for the fine grained steel because of the high welding speed and lower heat input compare to a conventional welding process.

  • PDF

열간압연 클래드강의 맞대기용접부 내식성 및 용접성 평가 (Evaluation of Corrosion Resistance and Weldability for the Butt Welding Zone of Hot Rolled Clad Steel Plates)

  • 박재원;이철구
    • Journal of Welding and Joining
    • /
    • 제31권5호
    • /
    • pp.47-53
    • /
    • 2013
  • We have investigated the traits of clad metals in hot-rolled clad steel plates, including the sensitization and mechanical properties of STS 316 steel plate and carbon steel (A516), under various specific circumstances regarding post heat treatment, multilayered welds, and thick or repeated welds for repair. For evaluations, sectioned weldments and external surfaces were investigated to reveal the degree of sensitization by micro vickers hardness, tensile, and etching tests the results were compared with those of EPR tests. The clad steel plates were butt-welded using FCAW and SAW with the time of heat treatment as the variable, a that was conducted at $625^{\circ}C$, for 80, 160, 320, 640, and 1280 min. Then, the change in corrosion resistance was evaluated in these specimens. With carbon steel (A516), as the heat treatment time increased, the annealing effect caused the tensile strength to decrease. The micro-hardness gradually increased and decreased after 640 min. The elongation and contraction of the area also increased gradually. The oxalic acid etch test and EPR test on STS316 and the clad metal showed STEP structure and no sensitization. From the test results on multi-layered and repair welds, it could be concluded that there is no effect on the corrosion resistance of clad metals. The purpose of this study was to suggest some considerations for developing on-site techniques to evaluate the sensitization of stainless steels.