• Title/Summary/Keyword: Rubber strength

Search Result 660, Processing Time 0.024 seconds

Effects of thermal aging on mechanical properties of laminated lead and natural rubber bearing

  • Kim, Dookie;Oh, Ju;Do, Jeongyun;Park, Jinyoung
    • Earthquakes and Structures
    • /
    • v.6 no.2
    • /
    • pp.127-140
    • /
    • 2014
  • Laminated rubber bearing is very popular base isolation of earthquake engineering pertaining to the passive structural vibration control technologies. Rubber used in fabricating NRB and LRB can be easily attacked by various environmental factors such as oxygen, heat, light, dynamic strain, and organic liquids. Among these factors, this study carried out thermal aging test to investigate the effect of thermal aging on the mechanical properties of laminated rubber bearings in accelerated exposure condition of $70^{\circ}C$ temperature for 168 hours. The compressive-shear test was carried out to identify the variation of compressive and shear properties of the rubber bearings before and after thermal aging. In contrast to tensile strength and elongation tests, the hardness of rubber materials showed the increasing tendency dependent on exposure temperature and period. Based on the test results, the property changes of rubber bearing mainly aged by heat are quantitatively presented.

Study on the Change of Physical Properties with Silica Contents in Solution Styrene-Butadiene Rubber (SSBR)/Silica Composites

  • Kim, Tae Yeop;Won, Sung Yeon;Kang, Shin Hye;Cho, Ur Ryong
    • Elastomers and Composites
    • /
    • v.52 no.1
    • /
    • pp.17-21
    • /
    • 2017
  • The optimum mixing conditions of silica and silane containing rubber composites were evaluated by investigating the properties of rubber composites prepared with a silica composition of 10, 20, 40, 60, and 80 g, respectively. The crosslinking rate decreased with increasing silica content, with he promoters being adsorbed on the silica surface with in the rubber composite. As a result, the increase in crosslinking time resulted in the destruction of the silica structure. The increase of the bound rubber content due to the destruction of the silica structure inhibited the chain motion of the polymer molecules and reduced the cohesion of the silica itself. Finally, the increase of silica content showed the increase of hardness, tensile strength, and storage modulus of rubber composites.

Mechanical Properties and Morphology of the Recycled Thermoplastic Elastomer Molding (재생 엘라스토머 수지의 기계적 물성과 모폴로지)

  • No, B.S.;Lee, G.H.;Jeong, Y.D.
    • Transactions of Materials Processing
    • /
    • v.16 no.1 s.91
    • /
    • pp.31-35
    • /
    • 2007
  • Automotive weather strip should have good weather ability, sealability, durability, etc. to perform its duty as body sealing for vehicles under different harsh environments. Due to its comprehensive properties, thermoplastic vulcanizate(TPV) is widely employed in weather strip as alternative for ethylene propylene diene rubber(EPDM). In this study, the influences of the recycled TPV on the tensile strength and hardness were investigated. As results of the injection molding experiment, the recycled TPV's tensile strength and hardness were higher than the virgin TPV and recycled TPV's extension was improve. The morphology showed that recycled TPV's rubber particles became smaller than virgin TPV's rubber particles.

A study on deformation and strength of polymer composites using automobiles (자동차용 폴리머 복합재료의 변형과 강도에 관한 연구)

  • Shin, Je-Hoon;Lim, Jae-Kyoo;Park, Han-Ju
    • Proceedings of the KSME Conference
    • /
    • 2000.11a
    • /
    • pp.238-243
    • /
    • 2000
  • The effect of the temperature, the fatigue and the test speed on DEN(double edged notch) specimen which was made by the pp-rubber composites during fracture was stuied. DEN specimen was made on PP-rubber composites through the injection molding. With increasing temperature the fracture strength is linearly decrease and the fracture energy is first increase by $0^{\circ}C$ and after that decrease. In the same temperature the fracture strength during increasing the notch radius is hardly increase. The fracture behaviour at low and high test speed is different entirely. At high test speed plastic region is small and fracture behaviour was seen to brittle fracture tendency. The deformation mechanism of polypropylene-rubber composites during fracture was studied by SEM fractography. A strong plastic deformation of the matrix material ahead of the notch/crack occured. The deformation seem to be enhanced by a thermal blunting of the notch/crack.

  • PDF

Curing effect on mortar properties produced with styrene-butadiene rubber

  • Cemalgil, Selim;Etli, Serkan;Onat, Onur
    • Computers and Concrete
    • /
    • v.21 no.6
    • /
    • pp.705-715
    • /
    • 2018
  • This paper presents an experimentally investigation pertinent to the mechanical properties of rubberized mortar (RM) with styrene-butadiene rubber (SBR). The SBR were used with constant water-to-cement ratio of 0.485 and two different volume proportion of SBR particles were utilized as aggregates. One types of SBR particles with fineness modulus of 4.951 were utilized 0%, 10%, and 20% of aggregate volume. Effectiveness of SBR replacement ratio, curing and aging effect on the compressive strength, flexural strengths as well as load-displacement. Compressive and flexural strength of concrete were investigated at the end of 28-days and 56-days age. Obtained results demonstrated that utilization of SBR reduced the flexural strength of SBR mortar at the earlier curing age while SBR increased. Moreover, mechanical properties of mortar mentioned above were significantly affected by the water cure timing with an increasing proportion of the replacement level of SBR.

Effect of Changing of Filling Materials in NR-SBR Type Elastomer Based Rubber Materials on Mechanical Properties (필러재료의 변화에 따른 NR-SBR 타입 엘라스토머 기반 고무재료의 기계적물성)

  • Bulbul, Saban;Yasar, Mustafa;Akcakale, Nuretttin
    • Polymer(Korea)
    • /
    • v.38 no.5
    • /
    • pp.664-670
    • /
    • 2014
  • The effects of different filling materials and stabilizers in polymer based materials that are used as shoe soles in the shoemaking industry on the mechanical properties (strength, failure, tensile, tearing, bending etc.) of the final products have been examined in this study. Natural rubber (NR RSS3) and styrene-butadiene rubber (SBR 1502) were used as the main matrix material. New compounds were formed by replacing the fillings in the general compound of the existing factory ($SiO_2$, $CaCO_3$) with 40% (1200 g) blast furnace flue dust, rice husk, reclaimed rubber (recycled) and wood ash. Comparison of the new compounds with the existing compounds revealed a decrease in hardness, density, dimension stability, bending, tearing, % elongation and failure strength and an increase in wearing.

Adhesion properties and Breakdown behaviors of LSR Interface (LSR 계면의 접착특성 및 절연파괴거동)

  • Yoon, Seung-Hoon;Nam, Jin-Ho;Lee, Gun-Ju;Choi, Soo-Geol;Shin, Doo-Sung;Ji, Eung-Seo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.11a
    • /
    • pp.232-235
    • /
    • 2002
  • Recently developed liquid silicone rubber (LSR) can be cured by platinum catalyzed additional hydrosilylation mechanism and has the advantage of no byproduct compared to traditional millable peroxide curing silicone rubber. We investigated the characteristics of dielectric breakdown of silicone rubber and adhesion properties between semi-conductive LSR and insulating LSR for high voltage application of pre-molded joint (PMJ). In order to understand the dielectric breakdown characteristics, we used the sheet samples and the paired type rogowski insert electrode system. The breakdown strength and adhesion strength of LSR (E-3) were superior to those of several silicone rubbers. Adhesion strength could be improved by curing at high temperature without post-curing process or enhanced by post-curing process. When LSR (E-3) was cured at $(150^{\circ}C{\times}10min$ semi-conductive )${\times}$ ($175^{\circ}C{\times}10min$ insulation), it showed the high breakdown strength with low standard deviation, and good adhesion strength. In this results, we could apply this process to the fabrication of PMJ without post-curing.

  • PDF

Comparative Evaluation of Manufacturing Properties of Carbon Fiber Reinforced Thermoplastic Polymer (CFRTP) according to Nanofiller Type (나노필러 종류에 따른 열가소성 탄소 섬유강화 복합재료의 제작 물성 비교 평가)

  • Jun Ha Park;Soon Ho Yoon;Minkook Kim
    • Composites Research
    • /
    • v.37 no.3
    • /
    • pp.186-189
    • /
    • 2024
  • This study compared and evaluated the mechanical properties of carbon fiber reinforced thermoplastic polymer (CFRTP) mixed with nanofillers. After mixing various nanofillers such as Multi-wall carbon nanotube (MWCNT), Silicon oxide, Core shell rubber, and Aramid nanofiber with Polyamide 6 (PA6) resin, this is used as a matrix to create a carbon fiber reinforced composite material (CFRP) was manufactured and its physical properties were measured. Depending on the type and mixing ratio of nanofiller, tensile strength, inter-laminar shear strength (ILSS), and Izod impact strength were measured. In terms of tensile strength and impact strength, the highest values were obtained when mixing core shell rubber, however the ILSS was optimal when mixing less than 1 wt.% of silicon oxide.

Effect of Silica Nanoparticles on Tear Strength of CR Compounds: A Comparison Study between the ASTM D470 and DIN VDE 0472-613

  • Changsin Park;Byeong-Rea Son;Gi-Bbeum Lee;Changwoon Nah
    • Elastomers and Composites
    • /
    • v.59 no.1
    • /
    • pp.34-41
    • /
    • 2024
  • In this study, the effects of the type and content of silica on the mechanical and tear properties of chloroprene rubber (CR), which is mainly used as a jacket material for mining cables, were studied. The crosslinking density (ΔM) and reinforcing factor (αf) defined using cure characteristics increased with increasing silica content, whereas the cure rate decreased. The hardness, tensile strength, and modulus of the CR compounds increased depending on the silica content and structural development. The reinforcing behavior of the silica-filled CR compounds according to the silica type and content showed the best fit with the Thomas equation of the predictive model. Tear strength was evaluated using two standard test methods, ASTM D470 and DIN VDE 0472-613, and the results were compared. The tear strength increased as the silica content increased, regardless of the test method, and the different tear strengths obtained by the two standard test methods showed a linear relationship with each other, indicating a high correlation.

A Study on Deformation and Strength of High-Strength Polymer Composites Using Automobiles (자동차용 고강도 폴리머 복합재료의 변형과 강도에 관한 연구)

  • Im, Jae-Gyu;Sin, Jae-Hun;Park, Han-Ju;Shoji, T.;Takeda, H.
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.25 no.7
    • /
    • pp.1082-1088
    • /
    • 2001
  • Nowadays study on recycling disused plastics for automobiles was lively progressed. Rubber and talcum powder was added to retrieve degradation of physical properties caused by recycling disused polypropylene. The effect of the temperature, the fatigue load and the loading speed on DEN(double edged notch) specimen which was made by the pp-rubber composites during fracture was studied by. DEN specimen was made on PP-rubber composites through the injection molding. With increasing temperature the fracture strength was linearly decreased and the fracture energy was increased by $0^{\circ}C$ and after that decreased. In the same temperature the fracture strength during increasing the notch radius was hardly increased. The fracture behaviour at low and high loading speed was different entirely. At high loading speed plastic region was small and fracture behaviour was seen to brittle fracture tendency. With increasing fatigue load fracture energy was first rapidly decreased and subsequently steady when radius of notch tip was 2mm, but Maximum load during fracture scarcely varied. The deformation mechanism of polypropylene-rubber composites during fracture was studied by SEM fractography. A strong plastic deformation of the matrix ahead of the notch/crack occurred. The deformation seem to be enhanced by a thermal blunting of the notch/crack.