RCF 시험을 통한 KTX 윤축베어링의 분해 정비 주기 평가 (Estimation of the Overhaul Cycle Time for KTX Wheelset Bearing by RCF Test)

  • 심대섭;허태현;박영일;김홍석;신기훈;정성균
    • 한국안전학회지
    • /
    • 제31권1호
    • /
    • pp.13-18
    • /
    • 2016
  • KTX wheelset bearings have thus far been maintained in accordance with the maintenance system of French national railway company, SNCF. The overhaul cycle time (OCT) of KTX wheelset bearings is now 1.4 million km in mileage. This value, however, has not been validated in Korea that has much different railway environments with France. In fact, it is impossible to validate OCT of wheelset bearings directly because they are disassembled and cleaned only when some faults are detected. In this paper, the accuracy of the current OCT value was evaluated indirectly by investigating the effect of grease lubricants on the bearing life. Five grease samples (one new and four aged greases) were used in this study. Four aged greases of different conditions were obtained from four wheelset bearings whose mileages were about 0.3, 1.2, 1.3, and 1.8 million km, respectively. Each grease sample was then injected into the RCF (Rolling Contact Fatigue) tester and fatigue lifetime was experimentally estimated. In addition, the wt% of Fe in each grease sample was analysed. The experiment results reveal that the bearing lifetime is inversely proportional to the mileage of grease sample while the wt% of Fe increases with the mileage of grease sample. Based on the experimental results, it can be concluded that the current OCT value is appropriate for the first overhaul of wheelset bearings. However, further validation is required to determine the second and third OCT values.

구름접촉피로시험을 통한 고속철도 레일연마량 분석 (Analysis for Optimal Rail Grinding Amount by Rolling Contact Fatigue Test in High Speed Railway)

  • 성덕룡;장기성;박용걸
    • 한국철도학회논문집
    • /
    • 제15권2호
    • /
    • pp.141-146
    • /
    • 2012
  • 차륜과 레일의 반복적인 구름접촉은 레일 표면결함을 유발하고, 레일 표면결함은 충격하중을 유발하여 소음 진동, 레일파단, 궤도파괴로 이어지고 심할 경우 열차사고(탈선)를 발생할 수 있다. 이러한 레일 표면결함을 제어하기 위한 방법으로 레일연마가 시행되고 있다. 본 연구는 KTX차륜과 UIC레일에서 발생하는 최대 접촉압력을 유한요소해석을 통해 산정하였고, 일반레일 및 열처리레일에 대한 구름접촉피로시험을 수행하여 접촉압력 및 반복횟수에 따른 레일표면 경화층 형성 경향을 분석하였으며, 누적통과톤수에 따라 고속철도 레일에서 발생하는 표면 경화층을 제거하여 건전한 레일표면을 유지하기 위해 0.2mm/2천만톤의 적정 레일연마량을 제안하였다.

니들 롤러 베어링의 피로 수명 향상에 대한 연구 (Improvement in Fatigue Life of Needle Roller Bearing)

  • 다리스렝 스르멩닥와;아마노프 아웨즈한;편영식
    • Tribology and Lubricants
    • /
    • 제35권4호
    • /
    • pp.237-243
    • /
    • 2019
  • Through this study, we investigate the effects of ultrasonic nanocrystal surface modification (UNSM) technology on the fatigue life of needle roller bearings. The fatigue life of untreated and UNSM-treated needle roller bearings is evaluated using a roller fatigue tester at various contact stress levels under oil-lubricated conditions. We can ascertain that the fatigue life of an UNSM-treated needle roller bearing was extended by approximately 34.3% in comparison with an untreated one, where the effectiveness of UNSM technology diminishes with increasing contact stress. The surface roughness and surface hardness of needle roller bearings before and after being treated by UNSM technology are compared and discussed to understand the role of UNSM technology in improving the fatigue life of needle roller bearings. In addition, a fractograph of the damaged bearings is observed using a scanning electron microscopy to shed light on the fracture mechanisms of bearings under different contact stress levels. We can therefore conclude that the application of UNSM technology to the needle roller bearings improves the fatigue life by reducing the friction coefficient and increasing the wear resistance; this may be attributed to a reduction in surface roughness from 0.5 to $0.149{\mu}m$ and an increase in surface hardness from 58 to 62 HRc.

곡선부 차륜/레일 접촉압력에 따른 레일마모진전 경향 분석 (Analysis of Rail Wear Rate according to Wheel/Rail Contact Pressure on Curved Track)

  • 성덕룡
    • 한국철도학회논문집
    • /
    • 제20권4호
    • /
    • pp.512-520
    • /
    • 2017
  • 일반적인 철도에서는 차륜과 레일의 마찰력을 이용하여 열차가 주행하게 된다. 차륜과 레일 사이에는 접촉압력이 발생하게 되고, 차량의 중량, 속도, 사행동, 접촉점 등에 따라 접촉압력의 크기가 변화하게 된다. 본 연구에서는 곡선부 차륜/레일에 대한 유한요소해석을 통해 접촉특성을 분석하였으며, 구름접촉피로시험을 통해 접촉압력에 따른 차륜/레일의 피로손상 및 마모율을 분석하였다. 구름접촉피로시험결과, 일반 및 열처리레일은 차륜에 비해 마모율이 높았으며, 일반 및 열처리레일마모율은 일정한 반복횟수 이상에서 급격히 증가하는 것으로 분석되었다. 또한, 일반레일이 열처리레일 보다 약 7~15% 마모율이 높았으며, 접촉압력 900~1,500MPa 범위에서 접촉압력에 따른 레일마모율에 대한 회귀분석식을 제시하였다.

Optimisation of Rolling Stock Wheelset Life through Better Understanding of Wheel Tyre Degradation

  • Vermeij, I.;Bontekoe, T.;Liefting, G.;Peen, J.
    • International Journal of Railway
    • /
    • 제1권3호
    • /
    • pp.83-88
    • /
    • 2008
  • Since the 1990's the fleet of the Dutch Railways showed a dramatic decrease in wheel tyre life. This lifetime reduction led to an unacceptable increase in life cycle costs. Therefore Lloyd's Register Rail has proposed to NedTrain to investigate the possibilities of improving the wheel tyre life. Three improvements were determined as most promising and relatively easy to achieve: - Profile optimisation for Rolling Contact Fatigue (RCF) reduction - a new wheel profile has been developed with a better resistance against rolling contact fatigue of the wheel tread. The profile has been implemented on single deck intercity trains and shows an increase in wheel tyre life of 30%. - Selection of improved wheel tyre materials - combining information from literature and experiences of manufacturers five alternative wheel tyre materials have been selected and are now being tested in practice. - Optimisation of the maintenance strategy - an alternative, preventative maintenance regime has been developed. With this Scraping regime, during short term maintenance every wheel is reprofiled. Higher mileages are reached and savings on life cycle costs up to 50% and more have been achieved. Unplanned maintenance goes down with $30{\sim}60%$. The results from field tests, using a reference group for comparison, and preliminary results after implementation show that the increase in wheel tyre life that is achieved with this project is significant. The results will continue to be monitored using the asset management tool 'Wheel Watch', that was specially developed for this project and is also described in this paper.

  • PDF

자동조심 롤러 베어링의 재제조 공정 및 피로수명 향상 (Remanufacturing Process and Improvement in Fatigue Life of Spherical Roller Bearings)

  • 다리스렝 스르멩닥와;아마노프 아웨즈한;김준형;이승철;최갑수;편영식
    • Tribology and Lubricants
    • /
    • 제30권6호
    • /
    • pp.350-355
    • /
    • 2014
  • This study proposes a sustainable bearing remanufacturing process using the ultrasonic nanocrystal surface modification (UNSM) technique. The UNSM technique is a newly developed and sophisticated surface modification technique that can increase the mechanical properties and improve the friction and wear performance of materials. Taking advantage of the bearing manufacturing process is the most significant way of optimizing the life of a bearing. The proper maintenance and usage of repaired bearings can increase their life to be equal to or greater than that of new bearings. This paper discusses the restoration of certain mechanical properties of worn, damaged, and discarded bearings, and suggests a remanufacturing process for used bearings, which can impart them with a lifespan equivalent to that of new bearings. The most damaged part of the discarded bearings is the raceway, which is the site of accumulated fatigue. The existing polishing or barrel finishing processes can recover the accumulated fatigue only partially. Rolling contact fatigue tests performed on UNSM-treated new and used specimens polished after $4{\times}10^6$ cycles reveal that UNSM-treated new specimens exhibit the longest fatigue life compared to other specimens. This study verifies the proposed complete fatigue recovery process, which can increase the fatigue life of used bearings to a level greater than that of new bearings.

레일코팅재를 이용한 곡선부 레일마모저감에 관한 실험적 연구 (An Experimental Study on the Rail Wear Reduction Using Coating Material in Curved Track)

  • 하범용;박용걸;이동욱;최정열;강윤석
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2011년도 정기총회 및 추계학술대회 논문집
    • /
    • pp.2153-2162
    • /
    • 2011
  • The goal of this Paper is to reduce rail's wear in curved track by applying an additional surface layer material(High hardness and High resistance capacity of wear) on the top of the railhead. In order to evaluate appropriation of a coating material, experimental tests such as the varieties of fundamental properties tests (hardening, wear, tensile, and bending) and RCF(rolling contact fatigue)test were performed to establish fatigue wear and damage mechanism. As a result, wear performance of coating rail is better than heated rail about 6times and normal rail about 8~9times.

  • PDF

도시철도에서 열차제동하중이 레일표면 열화에 미치는 영향 (An Effect on Braking Force for Degradation of Rail Surface in the Urban Railway)

  • 양태경;오희완;성덕룡;최진유;박용걸
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2011년도 정기총회 및 추계학술대회 논문집
    • /
    • pp.2135-2146
    • /
    • 2011
  • The rail surface irregularity is generated severely by train braking effect in the section of station. The braking force increases slip rate and friction factors caused by wheel-rail contact points. It brings rail surface irregularity as well. In this study, interactions between wheel and rail were investigated using rolling contact fatigue theory and mechanism of rail degradation through fracture mechanics. For the more, the Von-Mises stress occurred on the rail due to the interaction between wheel and rail was analyzed using 3-D finite element method. The amounts of surface irregularity of rail were measured according to accumulated passing tonnage in urban railway in fields. Therefore, the maintenance of rail should be separated by running and braking sections to prevent RCF defects.

  • PDF

고주파 유도경화처리한 중탄소강의 회전접촉 피로거동에 미치는 탄소함량의 영향 (Influence of Carbon Content on Rolling Contact Fatigue of High Frequency Induction-Hardened Medium Carbon Steels)

  • 최병영;이동민
    • 한국재료학회지
    • /
    • 제7권9호
    • /
    • pp.744-749
    • /
    • 1997
  • 본 연구에서는 고주파 유도경화처리한 중탄소강의 회전접촉 피로거동을 0.44wt.%C강과 0.55wt.%C강을 사용하여 조사하였다. 회전접촉 피로시험은 Polymet RCF-1 시험기에서 탄성유체 윤활 조건으로 회전속도 8,000rpm, 최대 Hertz응력 492kg/m$m^2$을 가하면서 실시하였다. 미세한 lath마르텐사이트가 고주파 유도경화한 0.44wt.%C강과 0.55wt.%C강의 표면경화층에 형성되었고 소량의 페라이트가 일부 형성되었으며 0.44wt.%C강과 0.55wt.%C에 비해 비교적 큰 페라이트가 나타났다. 회전접촉 피로시험 후 표면경도가 거의 유지되는 표면경화층에서 회전접촉 피로시험전에 비해 경도가 상승하였다. 이 경도증가량의 최대치($\Delta$ Hv$_{max}$)와 피로수명과의 관계를 조사한 결과 0.55wt.%C강이 0.44wt.%C강에 비해 회전접촉 피로중에 일어나는 소변형에 대한 높은 저항성에 주로 기인하여 $\Delta$ Hv$_{max}$값은 낮게 나타나고 피로수명은 높게 나타났다.

  • PDF

도시철도 레일연마주기 산정을 위한 시험적 연구 (Experimental Study for Establishing Rail Grinding Period in the Urban Railway)

  • 성덕룡;고동춘;박용걸;공선용
    • 한국철도학회논문집
    • /
    • 제13권4호
    • /
    • pp.447-454
    • /
    • 2010
  • 레일 피로 열화손상유형들은 크게 레일표면에서 발생하는 결함들과 레일내부에서 진전되어 발생하는 결함들로 구분되어질 수 있다. 본 연구에서는 국내에서 연간 누적통과톤수가 가장 많은 도시철도의 운행조건을 고려하여 현장측정을 통해 레일표면 요철성장률을 분석하였으며, 연마 후 누적통과톤수에 따른 시험편을 현장에서 발췌하여 현미경을 이용한 조직검사, 화학성분검사, 마이크로 비커스 경도시험을 수행하였다. 시험결과 신품레일의 경우 유효탈탄층 제거를 위해 약 0.3mm의 초기연마를 시행해야하며, 예방연마의 경우 전구간을 일괄적으로 연마할 경우와 특정 구간별로 구분하여 연마할 경우에 대하여 2가지 방안을 제시하여 레일표면에서 발생하는 RCF결함을 예방하거나 제거할 수 있도록 제시하였다.