• Title/Summary/Keyword: Rock Strength

Search Result 1,152, Processing Time 0.041 seconds

Ring Shear Characteristics of Waste Rock Materials in Terms of Water Leakage (누수유무에 따른 광산폐석의 링전단특성)

  • Jeong, Sueng Won
    • The Journal of Engineering Geology
    • /
    • v.26 no.3
    • /
    • pp.307-314
    • /
    • 2016
  • Shear characteristics of soils can be investigated using various types of shear stress measuring apparatus. Ring shear tests are often applied for examining the residual shear strength under the unlimited deformation. This paper presents drainage-consolidation-shear velocity dependent undrained shear strengths measured in terms of water leakage. A series of ring shear tests were performed under the constant normal stress (50 kPa) and controled shear velocity ranging from 0.01~1 mm/sec under the undrained condition. As a result, undrained shear strengths are dependent on shear velocity. It exhibits that straining hardening behavior is observed for the shear velocity lower than 0.1 mm/sec; however, the strain softening behavior is observed for the shear velocity higher than 0.1 mm/sec. Water leakage can cause the increase in shear stress irrespective of shear velocity. Shear stress increases with increasing amount of water leakage. It is due to the fact that the small grains and water flow out through the rubble edge in the ring shear box. Repetitive saturation and consolidation processes may minimize the error.

Engineering Properties of Uncemented Mudrock from Yeoju Area, Gyeonggi-Do (경기도 여주지역 미고결 이암의 공학적 특성)

  • Ban, Hoki;Lee, Huiyoun;Bae, Kyujin;Cho, Wanjei
    • Journal of the Korean GEO-environmental Society
    • /
    • v.16 no.12
    • /
    • pp.53-58
    • /
    • 2015
  • Engineers should take great care of characterizing the engineering properties of mudrock, because the uncemented mudrock can be considered as a hard rock in appearance. Therefore, the mudrock samples obtained from the cut slope in Gyeongki-do were tested to evaluate the strength characteristics of uncemented mudrock in this study. The performed tests are index properties, slake durability, and swelling tests for the classification of the mudrock for engineering practice. To evaluate the effect of water on the engineering properties of the uncemented mudrock, resonant column, triaxial compression and direct shear tests with various water contents were performed. With the increasing water contents, stiffness at very small to small strain region and the cohesion value of the strength parameters decrease. Based on the test results, engineers should take great care of evaluating the engineering properties of uncemented mudrock.

Influence of Low-Quality Aggregate on Engineering Properties of Concrete (동일배합 조건에서 저품질 골재가 콘크리트의 공학적 특성에 미치는 영향)

  • Min, Kyeong-Chul;Han, Cheon-Goo
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.2
    • /
    • pp.187-194
    • /
    • 2016
  • In this research, the influence of low-quality aggregate on engineering properties of concrete was experimentally evaluated. From a series of experiment, the results can be summarized as follow: first, the low-quality aggregate in concrete mixture caused up to 83% of decreased slump. For air content, low-quality aggregate increased air content of concrete mixture. Especially, when sea sand was used, because of the narrow gradation with small size, the air content was significantly increased. The compressive strength of concrete mixtures with low-quality aggregates were decreased up to 29% while some cases showed slightly increased compressive strength at early age. Additionally, the concrete mixture mixed with the exploded debris as a coarse aggregate showed approximately 5 to 20% of decreased compressive strength comparing with high-quality of manufacturing rock. In summary, because of the decreased workability of concrete mixture mixed with low-quality aggregates such as exploded debris, clay, and sea sand, it is concerned that worse quality of the ready mixed concrete, produced with the extra water to compensate the decreased workability.

A preliminary study of watertightness and salt water resistance of spray-applied membrane (뿜어붙임멤브레인의 방수성능 및 염수저항성의 기초평가)

  • Choi, Soon-Wook;Kang, Tae-Ho;Chang, Soo-Ho;Lee, Cheol-Ho;Kim, Jintae;Choi, Myung-Sik
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.19 no.2
    • /
    • pp.283-299
    • /
    • 2017
  • The leakage of tunnel causes the long-term durability of the structures such as concrete lining to deteriorate. The cause of durability degradation can be various substances contained in groundwater such as chloride, sulphate, water, and gas. In this study, a series of test were carried out to determine the watertightness performance and the resistance to salt water of the spray-applied membrane used as non-structural rock support or as a waterproof material for tunnels. As a result, it was found that the penetration of water could occur in a specimen, and the reason was that the internal pores generated by the mixing of the liquid polymer and the powder material and the internal pores were connected by the water pressure. The tensile strength of the test specimens immersed in distilled water and saline water was found to be reduced to less than half of the tensile strength in normal condition. In addition, The elongation was measured to be higher in distilled water than in salt water. However, this result will require further investigation.

Evaluation on the Basic Properties of Phosphate Modified Portland Cement Paste for Potential Application of Geologic CO2 Sequestration (이산화탄소 지중 격리용 인산염 혼입 시멘트 페이스트에 관한 기초물성 평가)

  • Yoon, Ju-Han;Kim, Seong-Geun;Kim, Ji-Hyun;Lee, Jae-Yong;Chung, Chul-Woo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.17 no.3
    • /
    • pp.253-260
    • /
    • 2017
  • As global warming became a worldwide issue, a significant effort has been made on the development of technology related to $CO_2$ capture and storage. Geologic sequestration of $CO_2$ is one of those technologies for safe disposal of $CO_2$. Geologic sequestration stores $CO_2$ in the form of supercritical fluid into the underground site surrounded by solid rock, and concrete is used for prevention of $CO_2$ leakage into the atmosphere. In such case, concrete may experience severe damage by attack of supercritical $CO_2$, and especially in contact with underground water, very aggressive form of carbonation can occur. In this work, to prevent such deterioration in concrete, calcium phosphates were added to the portland cement to produce hydroxyapatite, one of the most stable mineral in the world. Temperature rise, viscosity, set and stiffening, and strength development of cement paste incorporating three different types of calcium phosphates were investigated. According to the results, it was found that the addition of calcium phosphate increased apparent viscosity, but decreased maximum temperature rise and 28 day compressive strength. It was found that monocalcium phosphate was found to be inappropriate for portland cement based material. Applicability of dicalcium and tricalcium phosphates for portland cement needs to be evaluated with further investigation, including the long term compressive strength development.

A Study on Physicochemical Properties of Epoxy Coatings for Liner Plate in Nuclear Power Plant (원자력발전소 격납건물 철재면 에폭시 도장시편의 물리화학적 특성 평가)

  • Lee, Jae-Rock;Seo, Min-Kang;Lee, Sang-Kook;Lee, Chul-Woo;Park, Soo-Jin
    • Applied Chemistry for Engineering
    • /
    • v.16 no.6
    • /
    • pp.809-814
    • /
    • 2005
  • In this work, the thermal properties of epoxy coating system on the liner plate in the containment structure of nuclear power plants had been examined by irradiation and design basis accident (DBA) conditions. The effect of immersion in hot water on adhesion strength of the coating system had been also studied. The glass transition temperature ($T_g$) and thermal stability of ET-5290/carbon steel A 32 epoxy coating systems were measured by DSC and TGA analyses, respectively. Contact angle measurements were used to determine the effect of immersion on the surface energetics of epoxy coating system, with a viewpoint of surface free energy. Adhesion tests were also executed to evaluate the adhesion strength at interfaces between carbon steel plate and epoxy resins. As a result, it was found that the irradiation led to an improvement of internal crosslinked structure in cured epoxy systems, resulting in significantly increasing the thermal stability, as well as the $T_g$. Also, the immersion in hot water made a role in the post-curing of epoxy resins and increased the mechanical interlocking of the network system, resulting in increasing the adhesion strength of the epoxy coating system.

Development of Reinforcement Grout Materials Using Blast Furnace Slag Powder and Aramid Fiber (고로슬래그 미분말과 아라미드 섬유를 이용한 보강그라우트재 개발)

  • Seo, Hyeok;Park, Kyung-Ho;Kim, Chan-Jung;Kim, Ho-Chul;Kim, Daehyeon
    • Journal of the Korean Geosynthetics Society
    • /
    • v.18 no.1
    • /
    • pp.67-77
    • /
    • 2019
  • The grouting method is utilized to reinforce and waterproof poor grounds, enhance the bearing capacity of structures damaged resulting from settlement due to elevation and vibration or differential settlement, and for cutoff. The purpose of this research is to enhance the compressive strength of grout materials by using aramid fiber and develop a high-strength ground improvement method by using blast furnace slag powder. In this regard, this study has conducted a uniaxial compression test after checking the high charge (higher than 50%) of the ratio of blast furnace slag powder and cement at 100:0, 70:30 and 40:60%, adding the aramid mixture based on 0, 0.5 and 1.0% of the cement and furnace slag powder weight and creating sand gels based on surface oiling rate of 0.7 and 1.2%. For the environmental review evaluation, a heavy metal exudation test and a pH test measurement have been conducted. The experiment results showed that 1% increase of aramid fiber led to 1.3 times greater uniaxial compression intensity. As for the hexavalent chrome, a 30% increase in blast furnace slag powder led to approximately 50% decrease in heavy metal exudation. However, the pH test revealed that a 30% increase in blast furnace slag powder resulted in approximately 0.5 increase in pH. Further research on the pH part is needed in the future.

Undrained Shear Behavior of Sand with Dispersed Gravels (자갈이 포함된 모래의 비배수 전단거동)

  • Park, Sung-Sik;Kim, Young-Su;Sung, Hee-Young
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.30 no.5C
    • /
    • pp.209-218
    • /
    • 2010
  • In residual soils, large particles such as rock fragments or gravel are surrounded by sand or clay. The strength of such granular mixtures can be controlled by the concentration of fine or coarse grains. The percentage by weight, size or shape of gravel in the mixture that can control the strength of the mixture has not been clearly determined for various granular mixtures. In this study, the effect of dispersed gravels on the shear characteristics of sand was evaluated. Large and small gravels were inserted in the middle of each layer with moist Nakdong River sand and compacted into a cylindrical sample with five equal layers. Embedded gravel ratios by weight were 0, 3, 9, and 14%. After consolidation, a series of undrained triaxial compression tests was performed on Nakdong River sand with dispersed gravels. Maximum deviator stresses of the Nakdong River sand with large gravels decrease up to 38% as a percentage of embedded gravels increases. Such strength degradation decreases as a confining pressure increases. The maximum deviator stress increases as the percentage by weight of small gravel increases; at 3 or 9% of gravel weight it slightly increases but at 14% of gravel weight it increases up to 34%.

Applied Petrologic Study of the Daebo Biotite Granites in the mid Gyeonggi Massif (경기육괴 중부에 분포하는 대보 흑운모화강암류의 응용암석학적 연구)

  • Yun, Hyun-Soo;Hong, Sei-Sun;Park, Deok-Won;Lee, Jin-Young
    • The Journal of the Petrological Society of Korea
    • /
    • v.21 no.2
    • /
    • pp.263-275
    • /
    • 2012
  • Jurassic Daebo biotite granites, known as one of the main stone resources in the country, are widely and away distributed in the Pocheon and Yangju areas of the mid Gyeonggi massif. The objects of the study are mainly to reveal the unique characteristics of grain size, rock color, mineral composition, physical property and fracture system from the above biotite granites. Biotite granites from the Pocheon area (PG) and Yangju area (YG) are represented by coarse-grained and light gray, and medium to coarse-grained and grayish to light gray, respectively. In modes, main minerals of Qz+Af+Pl (quartz+alkali feldspar+plagioclase) are more increased in the PG, and accessories of biotite are more increased in the YG, which differences can cause the PG more bright light gray than the YG. Specific gravity (SG) shows somewhat more increasing in the YG than the PG. These differences can be caused by more increasing in biotite contents of higher specific gravity compared to the major minerals in the former than the latter. Absorption ratio (AR) and porosity (PR) of the PG and YG show the same values of 0.33 % and 0.86 %, respectively. In the correlations, PR vs SG and AR vs PR show gradually negative and distinctly positive trends, respectively. Compressive strength (CS) and tensile strength (TS) show increasing in the PG (CS: 1,775 $kg/cm^2$, TS: 87 $kg/cm^2$) than the YG (CS: 1,647 $kg/cm^2$, TS: 79 $kg/cm^2$). These strength characteristics could be attributed to the inherent rock textures of them. Abrasive hardness (AH) also shows a little increasing in PG, which can be caused by increase in quartz contents having higher hardness than the other major minerals. Orientations of fracture sets from the PG and YG were compared with those of vertical rift and grain planes in Mesozoic granites of the country. From the overlapped diagram, the distribution pattern between fracture sets and above vertical planes suggests that microcrack systems developed in Mesozoic granites in Korea occur also in the Daebo biotite granite bodies of the mid Gyeonggi massif. From the relation diagram showing the characteristics of fracture patterns for the above two area, PG and YG may have more potentiality for dimension and non-dimension stone resources, respectively.

Slope Stability Analysis by Slice Method and Finite Difference Method- A Comparative Study - (절편법과 유한차분법에 의한 사면안정해석 비교연구)

  • 박연준;채영수;유광호;백영식
    • Journal of the Korean Geotechnical Society
    • /
    • v.15 no.6
    • /
    • pp.263-272
    • /
    • 1999
  • Slice method is commonly used in solving slope stability problems since it is easy to use and its computation time is rather short. But depending upon the assumptions on the inter-slice forces, different methods are available. Quite often the difference between methods are so big that it is very difficult to make engineering decisions. This paper describes a method to calculate the factor of safety of a slope using FLAC, a finite difference based program. A FISH routine is developed to calculate the factor of safety, and verified by comparing with Chen's limit equilibrium solution. An example problem was selected from Fredlund and Krhan's paper, and results were compared for different soil and water conditions. The difference was less than 0.01 when the soil is homogeneous, and less than 5 % when a weak layer is embedded. Since most geotechnical application programs are capable of considering complicated ground conditions as well as the effect of ground supports, numerical methods are believed to be very useful in making engineering decisions. The developed routine can be applied to the calculation of the factor of safety of jointed rock slopes or weathered rock slopes where the use of slice method is limited.

  • PDF