• 제목/요약/키워드: Resin-bond Diamond Wheel

검색결과 28건 처리시간 0.021초

초경합금 연삭용 비트리파이드 다이아몬드숫돌의 개발 (Development of Vitrified Diamond Wheel for Grinding Tungsten Carbide)

  • 이재우
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 추계학술대회 논문집
    • /
    • pp.185-188
    • /
    • 2002
  • An abrasive vitreous bonded solid mass having a vitrified abrasive structure comprising diamond grains which are held by an in inorganic bonding agent, the vitrified diamond wheel is impregnated with a composition which comprises a thermosetting synthetic resin and a surfactant. The vitrified diamond wheel is manufactured by preparing the composition including the resin and the surfactant, impregnating the abrasive structure with the composition, and curing the composition. The diamond wheel newly developed showed excellent performance in grinding carbide.

  • PDF

Porous Ceramics의 연삭특성에 관한 연구 (A Study on the Grinding Characteristics of Porous Ceramics)

  • 박휘근;박세진;최윤서;황인환;이종찬
    • 한국기계가공학회지
    • /
    • 제11권2호
    • /
    • pp.165-170
    • /
    • 2012
  • The resin bonded diamond wheel is used to grind the difficult-to-cut materials. Traditionally, the resin bonded diamond wheel is manufactured without any pores due to the characteristics of resin bond. In this study, two porous resin bonded diamond wheel were made and the grinding characteristics were compared with traditional nonporous ones. The experimental results indicate that the porous resin bond diamond wheel require less grinding forces and powers.

아말감의 표면처리에 따른 복합레진과의 전단결합 강도에 관한 연구 (A STUDY ON THE SHEAR BOND STRENGTH OF THE COMPOSITE RESIN TO AMALGAM ACCORDING TO AMALGAM SURFACE TREATMENT METHODS)

  • 박문희;조영곤;황호길
    • Restorative Dentistry and Endodontics
    • /
    • 제18권1호
    • /
    • pp.114-121
    • /
    • 1993
  • The purpose of this study was to evaluate the effect on treatment methods to shear bond strength between composite resin and amalgam when the alloy surface was finished with a diamond wheel or an sandblaster. Forty round acrylic cylinders were fabricated with a diameter of 33mm and a height of 20mm to fit into the device used during shear bond strength testing. A round undercut cavity (diameter, 8mm: depth, 2.5mm) was prepared in the center of the acrylic surface and the cavity was restored using a amalgam. A total of 40 acrylic cylinders with amalgam were divided into 4 groups according to treatment method. The group treatment were as follows : Group 1 : acid etching after finishing the amalgam with diamond wheel Group 2 : no acid etching after finishing the amalgam with diamond wheel Group 3 : acid etching after sandblasting the amalgam Group 4 : no acid etching after sandblasting the amalgam The shear bond strength of composite resin bonded to amalgam of each specimen was tested with a universal testing machine at a crosshead speed of 0.5mm/min and 500kg in full scale. The results were as follow: 1. After diamond finishing, the non-acid etching group had highest shear bond strength with 7.29kg/$cm^2$ and after sandblasting, the acidetching group had lowest shear bond strength with 4.49kg/$cm^2$. 2. In both diamond finishing and sandblasting group, acid etching of the roughened amalgam surface decreased the shear bond strength. 3. The group treated with a diamond wheel had higher shear bond strength those treated with an sandblaster but there was not significanat.

  • PDF

다기공 다이아몬드 연삭숫돌의 개발에 관한 연구 (A Study on the Development of Diamond Grinding Wheel with Multi-Porous Structure)

    • 한국생산제조학회지
    • /
    • 제7권2호
    • /
    • pp.100-107
    • /
    • 1998
  • Diamond wheels with fine grains and multi-porous structures are newely trial developed for smoothing and mirror finishing materials. Grinding wheel must have performed both to remove tool marks efficienitly and to contact elastically with curved surfaces, that are employed for ultra precision and high performance grinding of difficult-to materials such as tungsten carbide alloy using tool and die materials, Diamond grains are bonded by a melamine resin to prevent the decrease of machining efficiency due to grain sinking within the bond materials. Also, highly foamed structures are developed to increase the flexibility of the grinding wheel, and to induce self-sharpening by increasing contact pressure between the grinding wheel and workpiece surfaces. In this paper, melamine-bonded diamond wheels try to manufacture, then the forming method of grinding wheel are suggested, and the grinding characteristics of melamine-bonded diamond grinding wheel are also illustrated.

  • PDF

난삭재의 초정밀.고능률 연삭가공을 위한 다이아몬드숫돌의 개발 (Development of diamond wheel for ultra precision and high performance grinding of difficult-to-materials)

  • 허성중
    • 대한기계학회논문집A
    • /
    • 제21권12호
    • /
    • pp.2172-2178
    • /
    • 1997
  • Development of diamond wheel with fine grains and multi-pore structures were newely attempted. Wheels, that are employed for ultra precision and high performance grinding of difficult-to materials such as tungsten carbide alloy using tool and die materials, must have both performances to remove tool marks efficiently and to contact elastically with curved surfaces. Diamond grains were bonded firmly by a melamine resin to prevent the decrease of machining efficiency due to grain sinking within the bond materials. Also, highly foamed structures were developed to increase the flexibility of the wheel, and to induce active self-sharpening by increasing contact pressure between the wheel and work surfaces. In this paper, melamine-bonded diamond wheels are trial manufactured, then the forming method of wheels are suggested, and the grinding characteristics of wheels are also illustrated.

마이크로 V홈 연삭가공을 위한 다이아몬드숫돌의 V형상 트루잉에 관한 연구 (A Study on the Truing of Diamond Wheel for Micro V-shaped Groove Grinding)

  • 이주상
    • 한국정밀공학회지
    • /
    • 제22권9호
    • /
    • pp.27-33
    • /
    • 2005
  • This study deals with the truing of diamond wheel fur the manufacture of micro v-shaped grooves with fine sharp edges in the grinding. Fine micro v-shaped grooves are key components to fabricate LGP(light guide plate), optical fiber connector and so on. Conventional v-shaped groove methods such as etching and lithography are difficult to make grooves with accuracy and cutting by lathe is difficult to select target materials. Therefore, as a preliminary stage to developing the grinding technology that will be expected fabrications for micro 3-dimensional structure of high effectivity and accuracy and freed up the restrictions of machinability to the materials for micro v-shaped grooves, truing is carried out with resin bond diamond wheel and electroforming diamond wheel using a cup-type truer. From the experimental results, it is found that the effects according to working direction of the cup-type truer and the restrainable methods of plastic deformation that is generated at wheel edge are examined. As a result, fine micro v-shaped diamond wheel was obtained, which are applicable to micro grinding for optical devices.

엔지니어링 세라믹스의 평면 연삭 가공 특성에 관한 연구 (A Study on the Surface Grinding Characteristic of Engineering Cramics)

  • 강재훈;허성중;김원일
    • 한국자동차공학회논문집
    • /
    • 제2권6호
    • /
    • pp.38-49
    • /
    • 1994
  • In this study, grindability of some representative engineering ceramics are experimentally investigated using resin bond diamond wheel with conventional surface grinding machine, and proper grinding conditions which can be obtained from various experimental results are established also for mechanical components which are proper to domestic circumstances with high reliability. And through the results of experiment, it is confirmed that grinding energies of the ceramics, especially in the case of $Al_2O_3$, are lower than steel with same machining condition in the conventional grinding because of their fine-brittle fracture mode type removal process, though the ceramics are well-known to unmachinable materials. And moreover, the total pass numbers needed for spark-out process to be completed are depend on their mechanical properties because that grinding stiffness is different from each other. The grinding force, ginding power and ground surface roughness are also measured and compared. Furthermore, the experiments carried out in this study, some useful results are obtained with can guide to grind engineering ceramics with conventional surface grinding machine.

  • PDF

페라이트의 연삭성에 관한 연구 (Study on grindability of ferrite)

  • 김성청;이재우
    • 대한기계학회논문집A
    • /
    • 제21권9호
    • /
    • pp.1507-1519
    • /
    • 1997
  • This paper aims to clarify the effects of grinding conditions on bending strength in surface grinding of various ferrites with the resin bond diamond wheel. The main conclusions obtained were as follows. At a constant material removal rate, the strength improves with increased wheel depth of cut and decreased workpiece speed. It is desirable to grind at higher peripheral wheel speed and under the critical workpiece speed presented in this paper. Grinding the ferrite of higher brittleness, the wheel depth of cut limited to hold 50% of their inherent strength becomes lower. The effect of various grinding conditions on bending strength becomes more larger in the order of Sr, Mn-Zn and Cu-Ni-Zn. When using the diamond grain of the lower toughness, the bending strength becomes higher, and the wheel wear occurs faster. Considering both bending strength and wheel wear rate, the best concentration of wheel is 100. The ground surfaces exhibit that the fracture process during grinding becomes more brittle in the order of Sr, Mn-Zn and Cu-Ni-Zn.

페라이트의 연삭저항 및 연삭면 특성 (Study on Grinding Force and Ground Surface of Ferrite)

  • 김성청
    • 한국생산제조학회지
    • /
    • 제6권3호
    • /
    • pp.17-25
    • /
    • 1997
  • This paper aims to clarify the effects of grinding conditions on the grinding force, ground surface and chipping size of workpiece in surface grinding of various ferrites with the resin bond diamond wheel. The main conclusions obtained were as follows: In a constant peripheral wheel speed, the specific grinding energy is fitted by straight lines with grinding depth coefficient($\delta$) in a logarithmic graph. The effect of both depth of cut and workpiece speed on grinding energy becomes larger in the order of Mn-Zn, Cu-Ni-Zn and Sr. When using the diamond grain of the lower toughness, the roughness of the ground surface becomes lower. The ground surfaces show that the fracture process during grinding becomes more brittle in the order of Sr, Mn-Zn and Cu-Ni-Zn. The chipping size at the corner of workpiece in grinding increases with the the increases of the depth of cut and workpiece speed, and the decrease of peripheral wheel speed. The effect of both depth of cut and workpiece speed on chipping size becomes more larger in the order of Sr, Mn-Zn and Cu-Ni-Zn.

  • PDF

표면처리에 따른 상아질과 콤포짓드 레진간의 전단결합강도에 관한 연구 (A STUDY ON SHEAR BOND STRENGTH OF COMPOSITE RESIN TO DENTIN FOLLOWING SURFACE TREATMENTS)

  • 노은희;박상진
    • Restorative Dentistry and Endodontics
    • /
    • 제16권1호
    • /
    • pp.200-208
    • /
    • 1991
  • The purpose of this study was to observe shear bond strength of composite resin to dentin following surface treatment. Freshly extracted forty-eight sound human molars were used in this study. They were stored at $4^{\circ}C$ physiologic saline solution before experiment. The teeth was then mounted with self curing acrylic resin in brass mold. The buccal surfaces of the teeth were grinding approximately 1.5mm by means of water-irrigated grinding wheel to expose the flattened fresh dentin surfaces. The specimens were divided into 6 groups according to preparation and treatment procedures on dentin surfaces; Group 1: Untreated after preparation with No.301 diamond point Group 2: Treated with primer for 60 seconds after preparation with No.301 diamond point Group 3: Untreated after preparation with No.700 fissure carbide bur Group 4: Treated with primer for 60 seconds after preparation with No.700 fissure carbide bur Group 5: Untreated after grinding with 600 grit silicon carbide paper Group 6: Treated with primer for 60 seconds after grinding with 600 grit silicon carbide paper Light cure dental adhesive was applicated to each specimen. Silux plus(3M) was inserted then into polyethylene tube of 3mm diameter and 3mm height, and polymerized to dentin surface. All of the specimens were stored in distilled water at $35.6^{\circ}C$ for 24 hours prior to testing. The shear bond strength was measured using an Instron Universal Testing Machine. The results obtained from this study were as follows: 1. The shear bond strength to dentin was the highest in group II. 2. The shear bond strength to dentin was the lowest in group III. 3. There was no significant difference in shear bond strength to dentin according to preparation instrument. 4. The primer treatment group showed significantly greater shear bond strength than untreated group.

  • PDF