• Title/Summary/Keyword: Residual stress profile

Search Result 72, Processing Time 0.029 seconds

Residual Stress Prediction in Multi-layer Butt Weld Using Crack Compliance Method (컴플라이언스법에 의한 다층 맞대기 이음의 잔류응력 추정)

  • Kim, Yooil;Lee, Jang Hyun
    • Journal of Welding and Joining
    • /
    • v.30 no.6
    • /
    • pp.74-79
    • /
    • 2012
  • It depends on the joint configuration, dimensions and constraints of the joint whether the residual stress at the root of single-sided butt weld is tensile or not. Therefore, recommendation is generally made that high R ratio should be used in the fatigue test of welded joint in order to prevent excessively long life caused by compressive residual stress. In this research, the residual stress profile in butt weld joint was obtained through compliance method, using successive extension of a slot and measurement of the variation of strain during the slot extension. The residual stress profile was firstly assumed to be the linear summation of Legendre polynomials up to 9th order excluding 0th and 1st order. Strain variation on the surface was measured while the slot was being extended by cutting to find out the 8 unknown coefficients of each polynomial term. The cut was made by the electric discharge machine. It was concluded that the residual stress near the surface is positive valued, however, it turned into the negative value as soon as it passed through 2 or 3 mm of the depth.

Prediction of the Constitutive Properties of Metal from Laser Peening Simulation (레이저 피닝 시뮬레이션을 통한 금속재료의 물성치 예측)

  • Yeo, In Kyu;Lim, Hyun Taek;Lim, Jong Bin;Jeong, Sung Ho
    • Laser Solutions
    • /
    • v.16 no.1
    • /
    • pp.15-19
    • /
    • 2013
  • For numerical simulation of the deformation and residual stress development in metals during laser peening, the constitutive equations describing material behavior at various strain rates and plastic properties at high strain rate impact conditions are prerequisite. However, these parameters are often unknown for various engineering materials. In this study, the parameters of Johnson-Cook constitutive equation of duplex stainless steel were determined by comparing the residual stress profile predicted by numerical simulation using trial values and the measured residual stress profile with x-ray diffraction.

  • PDF

Approximate residual stress and plastic strain profiles for laser-peened alloy 600 surfaces

  • Eui-Kyun Park ;Hyun-Jae Lee ;Ju-Hee Kim ;Yun-Jae Kim
    • Nuclear Engineering and Technology
    • /
    • v.55 no.4
    • /
    • pp.1250-1264
    • /
    • 2023
  • This paper presents approximate in-depth residual stress and plastic strain profiles for laser-peened alloy 600 surface via FE analysis. In approximations, effects of the initial welding residual stress and the number of shots are quantified. Based on FE analysis results, residual stress profiles are quantified by two variables; the maximum difference in stress before and after LSP, and the depth up to which the compressive residual stress exists. Plastic strain profiles are quantified by one variable, the maximum equivalent plastic strain at the surface. The proposed profiles are validated by comparing with published LSP experimental results for welded plates. Effects of the initial welding residual stress and the number of shots on these variables are discussed. The proposed profile can be directly applied to predict the mitigation effect of LSP on PWSCC and to efficiently perform structural integrity assessment of laser peened nuclear components.

Analysis of the Residual Stress due to Cold Expansion and Stress Intensity Factor in CT specimen Using Finite Element Method (유한요소법을 이용한 CT 시편의 홀확장 잔류응력 및 응력확대계수 해석)

  • Jang, Jae-Soon;Yang, Won-Ho;Kim, Cheol;Ko, Myung-Hoon;Cho, Myoung-Rae
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.603-608
    • /
    • 2001
  • Recently, cold expansion of fastener holes is commonly used in the aerospace industry to increase the fatigue endurance of airframes. Cold expansion process is used as the retardation of crack initiation in the hole. This treatment leads to an improvement of fatigue behavior due to the compressive residual stresses developed on the hole surface. The residual stress profile depends on the cold expansion ratio. In the present paper, it is shown that residual stress is redistributed due to the application of cold expansion process for CT specimen. It is further shown that residual stress increases in proportion to cold expansion ratio. It is thought that crack growth rate increases as cold expansion ratio.

  • PDF

Welding Residual Stress Distributions for Dissimilar Metal Nozzle Butt Welds in Pressurized Water Reactors (가압경수로 노즐 맞대기 이종금속용접부의 용접잔류응력 예측)

  • Kim, Ji-Soo;Kim, Ju-Hee;Bae, Hong-Yeol;Oh, Chang-Young;Kim, Yun-Jae;Lee, Kyung-Soo;Song, Tae-Kwang
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.36 no.2
    • /
    • pp.137-148
    • /
    • 2012
  • In pressurized water nuclear reactors, dissimilar metal welds are susceptible to primary water stress corrosion cracking. To access this problem, accurate estimation of welding residual stresses is important. This paper provides general welding residual stress profiles in dissimilar metal nozzle butt welds using finite element analysis. By introducing a simplified shape for dissimilar metal nozzle butt welds, changes in the welding residual stress distribution can be seen using a geometry variable. Based on the results, a welding residual stress profile for dissimilar metal nozzle butt welds is proposed that modifies the existing welding residual stress profile for austenitic pipe butt welds.

A Study on Temperature Profile and Residual Stress in Pipeline Repair Welding Using Sleeve (슬리브덮개를 이용한 배관 보수용접시 온도분포와 잔류응력에 관한 연구)

  • 김영표;김형식;김우식;홍성호;방인완;오규환
    • Journal of Welding and Joining
    • /
    • v.14 no.5
    • /
    • pp.95-105
    • /
    • 1996
  • Korea Gas Corporation has operated high pressure gas transmission line of about 600 kilometers and, therefore, a series of repair welding processes are required in order to cope with external defects such as dent, gouge, cracking usually due to mechanical attacks. Most of gas pipelines repair processes are performed after completely venting remaining gas. However, in some case, though it is very unusual, repairs require without venting gas. For instance, this case is that damaged pipeline is remedied with split sleeve by welding. In this paper, in an effort to confirm a safe application of the split sleeve welding, residual stress, strain and temperature distributions are evaluated by computer simulation and experiments. The results obtained are as follows : 1) Computer modelling is supposed to be reasonable because microstructure changes due to welding is simulated coincidently as compare to that of real condition. 2) The maximal temperature on inside surface of pipeline is 50$0^{\circ}C$ for the repair welding process. 3) The amount of residual stress is estimated as the stress corresponding to 0.8% strain. 4) The repair process employed is determined to be technically preferable because of its avoiding cracks and fractures in the course of welding.

  • PDF

Nondestructive Evaluation of the Characteristics of Degraded Materials Using Backward Radiated Ultrasound

  • Sung D. Kwon;Sung J. Song;Dong H. Bae;Lee, Young Z.
    • Journal of Mechanical Science and Technology
    • /
    • v.16 no.9
    • /
    • pp.1084-1092
    • /
    • 2002
  • The frequency dependency of Rayleigh surface wave is investigated indirectly by measuring the angular dependency of the backward radiation of the incident ultrasonic wave in two kinds of degraded specimens by scuffing or corrosion. Then, the frequency dependency is compared with the residual stress distribution or the corrosion-fatigue characteristics for the scuffed or corroded specimens, respectively. The width of the backward radiation profile increases with the increase of the variation in residual stress distribution for the scuffed specimens. In the corroded specimens, the profile width decreases with the increase of the effective aging layer thickness and is inversely proportional to the exponent, m, in the Paris' law that can predict the crack size increase due to fatigue. The result observed in this study demonstrates high potential of backward radiated ultrasound as a tool for nondestructive evaluation of subsurface gradient of material degradation generated by scuffing or corrosion.

Discussion on Hardness Measuring of Bearing Steel by X-ray Diffraction (X선회절에 의한 베어링강의 경도측정에 대한 고찰)

  • 이한영
    • Tribology and Lubricants
    • /
    • v.18 no.3
    • /
    • pp.187-193
    • /
    • 2002
  • The half-value breadth off-ray diffraction profile line is generally used for a factor in nondestructive hardness measuring method of steel. In this paper, the problem in using the half-value breadth for the hardness measuring method is evaluated in strain hardened steel. And new hardness measuring method using residual stress is proposed X-ray diffraction test after rolling contact fatigue test of ball bearing with inner race of various hardness are carried out to measure the distribution of residual stress and half-value breadth from surface. The result of this study shows that there is little correlation between half-value breadth and hardness in the higher strength region and in the region increasing the hardness by strain hardening. But the magnitude of residual stress on/under race after rolling contact fatigue test becomes clearly to be correlative with hardness. Thus, it is concluded that the hardness of strain hardened steel can be estimated by this relationship between residual stress and hardness.

Estimation of Residual Stress Distribution for Pressurizer Nozzle of Kori Nuclear Power Plant Considering Safe End (고리 원전 가압기 노즐 용접부 잔류응력 예측 시 안전단 고려가 이종 금속 용접부 잔류응력 분포에 미치는 영향)

  • Song, Tae-Kwang;Bae, Hong-Yeol;Chun, Yun-Bae;Oh, Chang-Young;Kim, Yun-Jae;Lee, Kyoung-Soo;Park, Chi-Yong
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.32 no.8
    • /
    • pp.668-677
    • /
    • 2008
  • In nuclear power plants, ferritic low alloy steel nozzle was connected with austenitic stainless steel piping system through alloy 82/182 butt weld. Accurate estimation of residual stress for weldment is important in the sense that alloy 82/182 is susceptible to stress corrosion cracking. There are many results which predict residual stress distribution for alloy 82/182 weld between nozzle and pipe. However, nozzle and piping system usually connected through safe end which has short length. In this paper, residual stress distribution for pressurizer nozzle of Kori nuclear power plant was predicted using FE analysis, which consideded safe end. As a result, existing residual stress profile was redistributed and residual stress of inner surface was decreased specially. It means that safe end should be considered to reduce conservatism when estimating the piping system.

Measurement method for profiling residual stress of an optical fiber (광섬유의 잔류응력 측정 방법)

  • 박용우;백문철;진애경;백운출;김덕영
    • Korean Journal of Optics and Photonics
    • /
    • v.14 no.3
    • /
    • pp.219-223
    • /
    • 2003
  • A novel method was proposed for determining the residual stress profile of an optical fiber by using a modified polariscope. Measurement results of the axisymmetric residual stress for a conventional single-mode fiber were demonstrated by using this method. It was found that non-uniform stress is distributed in the cladding of the fiber. This means that large mechanical stress is induced as a function of temperature generated near the neck shape of the fiber preform.