• 제목/요약/키워드: Replacement Ratio of Aggregate

검색결과 306건 처리시간 0.03초

The effects of different cement dosages, slumps and pumice aggregate ratios on the freezing and thawing of concrete

  • Turkmen, Ibrahim;Demirboga, Ramazan;Gul, Rustem
    • Computers and Concrete
    • /
    • 제3권2_3호
    • /
    • pp.163-175
    • /
    • 2006
  • This research was conducted to determine effect of pumice aggregate ratio, cement dosage and slumps on freeze-thaw resistance, density, water absorption and elasticity of concrete. In the first batch, $300kg/m^3$ cement dosage were kept constant and pumice ratios were changed as 25%, 50%, 75% and 100% of replacement for normal aggregate by volume for $3{\pm}1cm$, $5{\pm}1cm$ and $7{\pm}1cm$ slumps. Other batches were prepared with $200kg/m^3$, $250kg/m^3$, $350kg/m^3$, $400kg/m^3$ and $500kg/m^3$ cement dosages and 25% pumice aggregate +75% normal aggregate at a constant slump. Test results showed that when pumice-aggregate ratio decreased the density and freeze-thaw resistance of concretes increased. With increasing of cement dosage in the mixtures, density of the concretes increased, however, freeze-thaw resistance of concretes decreased. Water absorption of the concrete decreased with increasing cement dosage but increased with the pumice ratio. Water absorption of the concrete also decreased after freeze-thaw cycles. Freeze-thaw resistance of concretes was decreased with increasing the slumps.

내구성증진용 혼화제(DIA) 및 부순 잔골재의 복합 치환이 순환잔골재를 사용한 고로슬래그 벽돌의 특성에 미치는 영향 (Effects of Crushed Fine Aggregate and Durability Improvement Agent (DIA) on Blast Furnace Slag-Based Brick)

  • 박경택;손호정;김대건;김복규;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2011년도 추계 학술논문 발표대회
    • /
    • pp.225-227
    • /
    • 2011
  • This study investigates the effect of crushed fine aggregate and chemical admixture (durability improvement agent, named DIA) on blast furnace slag-based brick. The control brick was made with recycled fine aggregate of 100% and, no cement was used. Test results showed that all specimens developed similar strength, except for the specimen without partial replacement of crushed fine aggregate at 3 days. However, it is interesting to note that this specimen without crushed fine aggregate resulted in the highest strength at 7 days. In addition, the DIA had a major effect on the absorption ratio of brick specimens. For the brick specimens with partial replacement of crushed fine aggregate with 10%, the addition of DIA with only 1% was enough to satisfy the code regulated by KS F 4004.

  • PDF

순환골재콘크리트의 탄성계수 추정에 관한 연구 (The prediction of Elastic Modulus of Recycled Aggregate Concrete)

  • 심종성;박철우;박성재;김용재;김현중
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.105-108
    • /
    • 2005
  • This study investigated fundamental properties of the recycled aggregate which was produced through recent hi-techniques of recycling. In addition, the mechanical properties of the concrete that used the recycled aggregate were compared to the concrete used the natural aggregate. From the results of the mechanical property tests, as the recycled aggregate replacement ratio increased, the compressive strength and elastic modulus decreased. When the recycled aggregate completely replaced the natural aggregate, the compressive strength and elastic modulus was about 15$\%$ and 35$\%$ lower than the natural aggregate concrete, respectively. Based on the test results, equations for prediction of compressive strength and elastic modulus were suggested in the consideration of the amount of the replaced recycled aggregate. Based on the test results and study, the equation predicting the required development length of the recycled aggregate concrete is proposed.

  • PDF

잔골재를 패각으로 치환한 모르터의 강도, 흡수율 및 계면 결합형태 (Strength, Absorption and Interfacial Properties of Mortar Using Waste Shells as Fine Aggregates)

  • 문훈;김지현;이재용;정철우
    • 한국건축시공학회지
    • /
    • 제14권6호
    • /
    • pp.523-529
    • /
    • 2014
  • 국내에서는 많은 양의 패류가 생산되고 있으나, 이로 인해 발생하는 대량의 패각을 처리하는데 많은 어려움을 겪고 있다. 따라서 본 연구에서는 이러한 패각을 대량으로 처리하기 위하여 건설재료로서의 가능성을 평가하고자 한다. 모르터의 잔골재를 패각으로 치환하여 흡수율, 압축강도를 측정하고 계면결합 형태를 관찰하였다. 대체적으로 패각의 치환율이 증가함에 따라 흡수율은 증가하였으며, 압축강도는 감소하였다. 예외적으로 꼬막 패각을 치환한 모르터는 치환율이 증가함에 따라 압축강도가 증가하였다. 패각 치환율의 증가에 따른 흡수율의 증가 및 압축강도의 감소는 패각 주위에 발생한 다공성 때문인 것으로 파악되었으며, 꼬막 패각을 치환한 모르터는 패각과 시멘트 입자간의 계면결합 형태가 양호하였기 때문에, 오히려 강도가 상승한 것으로 판단된다.

무수석고와 소각장애시의 치환율 변화에 따른 고로슬래그 미분말 활용 무 시멘트 모르타르의 기초적특성 (Fundamental Properties of Zero-Cement Mortar with Variation Replacement Ratio of Incineration Waste Ash and Gypsum)

  • 여량량;김준호;백병훈;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.242-243
    • /
    • 2014
  • In this study, industrial by-products including blast furnace slag, incineration ash and waste gypsum were used with recycled fine aggregates to manufacture the zero-cement mortar. The replacement ratio of anhydrite gypsum was fixed as 0, 10%, 20% the replacement ratio fo WA1 was fixed as 0.5% and 1.0%, respectively. It could be identified that when the replacement of gypsum was 20% and WA1 of 1.0%, the strength could be in the range of normal strength.

  • PDF

석고종류 및 소각장애시 치환율 변화에 따른 고로슬래그 미분말 활용 무시멘트 모르타르의 공학적 특성 (Engineering Properties of Zero-Cement Mortar with Variation Replacement Ratio of Incineration Waste Ash and Gypsum)

  • 박준희;황금광;김준호;조만기;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.222-223
    • /
    • 2014
  • In this study, industrial by-products including blast furnace slag, incineration ash and waste gypsum were used with recycled fine aggregates to manufacture the zero-cement mortar.The replacement ratio of dihydrate gypsum and anhydrite gypsum was fixed as 0 and 10%, the replacement ratio fo WA1 was fixed as 0.5% and 1.0%, respectively. It could be identified that when the replacement of gypsum was 10% and WA1 of 1.0%, the strength could be in the range of normal strength.

  • PDF

순환골재와 폐주물사를 활용한 철근콘크리트보의 휨거동에 관한 실험연구 (Experimental Study of Flexural Behavior of Reinforced Concrete Beam Using WFS and Recycled Aggregate)

  • 김성수;이대교
    • KIEAE Journal
    • /
    • 제8권5호
    • /
    • pp.61-68
    • /
    • 2008
  • For the recycling of the resources and the preservation of the environment, this study's purpose is to measure flexural behavior of the reinforced concrete beams with the major variables like concrete strength, replacement ratio of the recycled aggregate and the waste foundry sand and the tension reinforcement ratio and to present the data of the recycled aggregate used for the structure design. The experiment on the flexural behavior resulted in the followings. The ultimate strength of recycled R/C beam was manipulated proportionate to the tension reinforcement ratio, however the strength instantly decreased after passing the ultimate load due to the destroyed concrete of the compression side. The deflection at the maximum load varied from the tension reinforcement ratio by 5.5 times. The test specimen with the tension reinforcement ratio less than $0.5{\rho}b$ showed constant curve without change in the load from the yield to the ultimate load in contrast to the distinctive plastic region where the displacement was rising. Although the strain of main tension steel with the reinforcement ratio indicate different, the design of recycled concrete member can be applied for current design code for reinforced concrete structure as the ratio of tension reinforcement district the under the reinforcement ration in a balanced strain condition.

순환(循環)굵은/잔골재(骨材)를 사용한 굳지 않은 콘크리트의 특성(特性) (Properties of Fresh Concrete with Recycled Coarse and Fine Aggregates)

  • 최기선;유영찬;김긍환;이도헌
    • 자원리싸이클링
    • /
    • 제18권3호
    • /
    • pp.20-26
    • /
    • 2009
  • 본 연구는 순환잔골재를 사용한 콘크리트의 굳지 않은 콘크리트 특성을 파악하고 순환골재 콘크리트의 품질관리 방안을 제시하고자 하였다. 이를 위하여 순환굵은골재 및 순환잔골재의 치환율을 조합하여 설계압축강도 30MPa의 콘크리트를 제작하였으며, 공기량 및 슬럼프를 측정하였다. 측정된 공기량 및 슬럼프 경시변화를 통하여 순환잔골재의 재료적 특성이 콘크리트의 물성에 미치는 영향을 파악하였으며, 골재의 흡수율 차에 따른 품질성능 저하를 고려할 수 있도록 현장 도착 슬럼프를 기준으로 전체 배합수를 일정하게 유지하는 품질관리 방안을 제시하도록 하였다. 본 실험에서는 골재 종류(천연, 순환)에 따른 표면수 보정을 통해 1시간 후 현장도착 슬럼프가 일정하게 유지될 수 있도록 콘크리트를 배합하였다. 순환골재의 사용에 따른 압축강도의 저하는 나타나지 않았다. 또한 표면수 보정을 통한 전체 배합수의 관리를 통하여 순환골재 콘크리트의 품질관리가 가능할 것으로 판단된다.

Successive recycled coarse aggregate effect on mechanical behavior and microstructural characteristics of concrete

  • Ashish, Deepankar K.;Saini, Preeti
    • Computers and Concrete
    • /
    • 제21권1호
    • /
    • pp.39-46
    • /
    • 2018
  • With the increase in industrialization and urbanization, growing demand has enhanced rate of new constructions and old demolitions. To avoid serious environmental impacts and hazards recycled concrete aggregates (RCA) is being adopted in all over the world. This paper investigates successive recycled coarse aggregates (SRCA) in which old concrete made with RCA in form of concrete cubes was used. The cubes were crushed to prepare new concrete using aggregates from crushing of old concrete, used as SRCA. The mechanical behavior of concrete was determined containing SRCA; the properties of SRCA were evaluated and then compared with natural aggregates (NA). Replacement of NA with SRCA in ratio upto 100% by weight was studied for workability, mechanical properties and microstructural analysis. It was observed that with the increase in replacement ratio workability and compressive strength decreased but in acceptable limits so SRCA can be used in low strength concretes rather than high strength concrete structures.

진동대 시험을 이용한 쇄석다짐말뚝의 액상화 저감효과에 관한 연구 (Evaluation of Liquefaction Mitigation of RAP (Rammed Aggregate Piers) using Shaking Table Test)

  • 김현정;배경태;김지환;조국환
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2008년도 추계 학술발표회
    • /
    • pp.1193-1198
    • /
    • 2008
  • Shaking table tests were performed to investigate the response of liquefaction mitigation of rammed aggregate piers(RAP) on soft ground. The displacements of the soft ground reinforced by RAP under area replacement ratio 7, 14, 28% during seismic loading were measured. The result of tests showed that effects of liquefaction mitigation were affected various area replacement ratios and ground acceleration on RAP systems.

  • PDF