Bioleaching Behavior of Cu and Co by Aspergillus Niger Strains from Molasses Culture (당밀배지에서 Aspergillus niger 균주에 의한 구리 및 코발트의 미생물 침출 거동)

  • Ahn, Hyo-Jin;Ahn, Jae-Woo;Ryu, Seong-Hyung
    • Resources Recycling
    • /
    • v.23 no.1
    • /
    • pp.64-69
    • /
    • 2014
  • For the recovery of Co and Cu, bioleaching behavior of Co, Cu, Fe, Mg, Al by Aspergillus niger culture from the molasses growth medium was investigated. Series of leaching tests have been conducted by varying Aspergillus niger's type, molasses concentration in the growth medium, pulp density and reaction time. The results showed that increase of the molasses concentration in the growth medium from 1% to 4% increased the leaching percentage of Co and Cu and the optimal molesses concentration was found to be 4% in the growth medium. Maxinum 90% of Co and 70% of Cu were dissolved from the leaching test at the 10 g/L pulp density, 4 % of molasses concentration in the growth medium after 21 days by Aspergillus niger KCTC 6985. But in case of using Aspergillus niger KCTC 6144, the maxium leaching percentage of Co and Cu was reached 90% respectively at a pulp density 5 g/L and 4% of molasses concentration.

Behavior of the High Temperature Oxygen Pressure Leaching of Chalcopyrite in Sulfuric Acid Solution (고온.산소가압하(高溫.酸素加壓下)에서의 황동광(黃銅鑛)의 황산침출 거동 고찰)

  • Eom, Hyoung-Choon;Yoon, Ho-Sung;Yoo, Kyoung-Keun;Sohn, Jeong-Soo
    • Resources Recycling
    • /
    • v.16 no.3 s.77
    • /
    • pp.44-49
    • /
    • 2007
  • In the present work, the high temperature oxygen pressure leaching behavior of chalcopyrite was studied in sulfuric acid solution. The influence of leaching time, temperature and oxygen partial pressure on leaching process were examined. Leaching rate of copper increased significantly with increasing leaching temperature. Copper recovery reached 87.1% within 2 hours at $200^{\circ}C$ and 10 atm oxygen pressure, while most of the solubilized iron readily re-precipitates as hematite($Fe_2O_3$). It was confirmed that e main leach reaction of chalcopyrite occurred through oxidation with oxygen under oxygen pressure and high temperature(above $150^{\circ}C$). Because sulfur was oxidized entirely to sulfate, passivating elemental sulfur layer was not formed.

Release of Organic Matter and Behavior of Nitrogen in the Degradation of Sewage Sludge Using Ultrasound (초음파를 이용한 하수 슬러지 분해에서 유기물 방출과 질소 거동)

  • Yoon, Yong-Soo;Kang, Gwang-Nam;Choi, Suk-Soon
    • Journal of the Korea Organic Resources Recycling Association
    • /
    • v.10 no.4
    • /
    • pp.75-80
    • /
    • 2002
  • The sewage sludge with concentrated MLSS, ranging from 5967 to 8400mg/L was degraded by ultrasound. In this study, ultrasound treatment was used to investigate the behavior characterization of SBOD, sludge biodegradation, C/N ratio, TN, turbidity and sludge morphology. From the experimental results of C/N ratio change and TN removal, the optimal irradiation time was found to be 10 minutes. The results showed the relative index of sludge biodegradation(SBOD/TCOD) was enhanced to 0.76 from the initial value of 0.013 at the 5967mg/L MLSS, during the 60minutes treatment. Throughout this research, the results provide useful engineering reference data for reuse of sewage sludge using ultrasound.

  • PDF

Leaching behavior of rhenium and molybdenum from molybdenite roasting dust in NaOH solutions (휘수연석(輝水鉛石)의 배소(焙燒) 중 발생한 분경(粉慶)으로부터 NaOH에 의한 Rhenium과 Molybdenum의 침출(浸出))

  • Kim, Young-Uk;Kang, Jin-Gu;Sohn, Jeong-Soo;Cho, Bong-Gyu;Shin, Shun-Myung
    • Resources Recycling
    • /
    • v.18 no.5
    • /
    • pp.37-43
    • /
    • 2009
  • The demand for rhenium has considerably increased recently owing to the large-scale consumption in industries and the price of rhenium has increased owing to the lack of supply and its availability. The dust from the roasting of molybdenite was employed to investigate the leaching behavior of rhenium and molybdenum. Leaching experiments were done by varying optimum parameters, such as reaction time, NaOH concentration and leaching temperature. The optimum leaching condition was found to be $4\;mol{\cdot}L^{-1}$ NaOH, 2 hours leaching time, $100\;g{\cdot}L^{-1}$ solid/liquid ratio, $80^{\circ}C$ temperature, and 250 rpm. At this condition, leaching percentage of rhenium and molybdenum was 86.1% and 88.6%, respectively.

Preparation of Platinum Amine Complex Solution from Pt Scrap and its Catalytic Activity of Soot Oxidation (백금 스크랩으로부터 아민산백금용액 제조 및 Soot Oxidation 특성)

  • Choi, Seung Hoon
    • Resources Recycling
    • /
    • v.27 no.3
    • /
    • pp.93-99
    • /
    • 2018
  • Effective extraction of platinum group elements by dissolving waste platinum scrap from the display industry and solvent extraction, was studied. The extracted platinum solution was prepared as a precursor solution for diesel automotive exhaust gas purification catalyst and its catalytic activity was tested. The behavior of aqueous species of platinum was investigated through solution chemistry and based on the existence and behavior of these chemical species, the possibility of extraction and separation was established. By dissolving waste scrap by electrochemical method, the dissolution time of scrap was shortened and the extraction efficiency was increased. Through separation and removal of rhodium component, solvent extraction by TBP, and stripping by hydrochloric acid, Pt-Chloride-$H_2O$ solution was prepared. And then, an platinum amine complex solution through amination reaction with this solution as a raw material was prepared. The possibility of producing high-value platinum compounds from platinum group waste scrap was investigated by preparing platinum amine complex solution and then examining the catalytic activity with this amine precursor on the combustion reaction of carbon black.

A Study on the Behavior of Boron Extraction from Brine by Diol-type Extractant (Diol계(系) 추출제(抽出劑)에 의한 염수(鹽水) 중(中) 보론의 추출거동(抽出擧動) 연구(硏究))

  • Yoon, Mi-Hee;Kang, Dong-Jun;An, Jeon-Woong;Min, Dong-Joon
    • Resources Recycling
    • /
    • v.21 no.1
    • /
    • pp.41-48
    • /
    • 2012
  • A study on the behavior of boron extraction by TMPD(2,2,4-trimethyl-1,3-pentanediol) was carried out to find the optimum conditions for the boron extraction from brine. In case of boron extraction from 0.736 g/L boron-containing brine, typical optimum extractive conditions would be confirmed to be 0.75 mol/L of extractant concentration at 3.0 pH of brine with 1 of phase ratio and 20 min. of shaking time at 298 K respectively. And 1 mol/L sodium hydroxide of stripping agent was shown above 99 % of boron extraction and stripping efficiencies. Also, extraction equilibrium equation were obtained through experiments as follows : log D = 1.7 log $[TMPD]_O$ + constant at pH < 6.

Influence of pH on Leaching Behavior of Phosphorous from Steelmaking Slag (제강슬래그에서 인의 침출 거동에 대한 pH의 영향)

  • Kim, Jeong-In;Kim, Sun-Joong
    • Resources Recycling
    • /
    • v.25 no.6
    • /
    • pp.23-28
    • /
    • 2016
  • In this study, leaching process to extract phosphorus from the steelmaking slag was investigated for using the fertilizer resources of agriculture. In general, the phosphorus of steelmaking slag is formed as $C_2S-C_3P$ solid solution, and also, this solid solution is soluble in water more than the other phase in slag, and less than free CaO phase. In the present experiment, the influence of pH on the leaching behavior of various elements from the steelmaking slag was investigated by using multi-component steelmaking slag. When the pH was decreased, the concentration of Ca, Si, P and Fe in solution from the steelmaking slag was increased. Furthermore, at a pH of 3, the concentration of P ion in solution was decreased as leaching time increased. It is considered that the decrement of P was caused from the precipitation reaction between P ion and Fe ion in solution.

Solvent Extraction of Mo(VI) and W(VI) from Dilute Chloride Solution by Amine and Neutral Extractants (묽은 염산용액에서 아민과 중성추출제에 의한 몰리브덴(VI)과 텅스텐(VI)의 용매추출)

  • Le, Minh Nhan;Son, Seong Ho;Lee, Man Seung
    • Resources Recycling
    • /
    • v.28 no.1
    • /
    • pp.55-61
    • /
    • 2019
  • The extraction behavior of Mo(VI) and W(VI) from dilute chloride solution was investigated by employing amine (Alamine308 and TEHA) and neutral extractants (TOP) in the solution pH range from 2 to 9. W (VI) was selectively extracted over Mo(VI) by these three extractants and TEHA led to the highest separation factor. Without the pretreatment protonation of the tertiary amines, the extraction percentage of the two metal ions decreased steadily to zero as solution pH increased to 9. The extraction behavior of the metals was discussed on the basis of the distribution diagram of each metal. Alamine 308 and TEHA were much better than TOP in extracting and separating the two metal ions.

Interpretation of Ammonia Absorption Behavior in Water Turbulent Flow (물 난류에서의 암모니아 흡수 거동 해석)

  • Lee, Sang-Ryong;Park, Jin-Won
    • Journal of the Korea Organic Resources Recycling Association
    • /
    • v.27 no.3
    • /
    • pp.75-80
    • /
    • 2019
  • The article is devoted to the interpretation of ammonia, one of the fine dust precursors, absorption behavior in water turbulent flow. The water flow was considered as a turbulent flow with Reynolds number more than $10^4$, because ammonia gas penetration depth was deeper at turbulent flow compared to laminar flow. For the interpretation, the dimensionless mass transfer governing-equation and the constant physical-properties at room temperature were used. The diffusivity of ammonia in water and the kinematic viscosity of water were $2{\times}10^{-9}m^2/s$ and $1{\times}10^{-6}m^2/s$, respectively. The concentration distribution of ammonia in water was estimated with respect to the position from the point where the water started to be exposed to ammonia. The quantitative distribution as a function of the mixing length was also acquired. The quantitative interpretation may provide the insight how much the turbulent flow was more efficient to remove ammonia rather than the laminar flow.

Adsorption Behaviors of Nickel ton on the Waste Pulp Produced in the Paper Recycling Process (고지(古紙) 재생(再生) 과정(過程)에서 발생(發生)하는 폐(廢)펄프를 흡착제(吸着劑)로 이용(利用)한 니켈 폐수(廢水) 처리(處理) 특성(特性))

  • Baek, Mi-Hwa;Shin, Hyun-Young;Kim, Dong-Su
    • Resources Recycling
    • /
    • v.15 no.3 s.71
    • /
    • pp.58-65
    • /
    • 2006
  • The applicability of the waste pulp which produced in the paper recycling process as an adsorbent for the treatment of $Ni^{2+}$ ion in wastewater has been investigated taking the initial concentration of adsorbate, temperature, the amount of adsorbent, and solution pH as the experimental variables. In addition, the effect of the concentration of coexisting solute and pre-treatment of adsorbent on the adsorbability of $Ni^{2+}$ ion were also examined. The electrokinetic potential of waste pulp was observed to be positive below pH 7.8 and negative above this pH. The adsorption reaction of $Ni^{2+}$ ion reached its equilibrium within 4 hours after the reaction was initiated and the adsorbed amount of adsorbate was found to increase with its initial concentration. The adsorbability of $Ni^{2+}$ was raised with temperature so that its adsorption reaction was considered to be exothermic, which was substantiated by thermodynamic calculation. Also, the adsorbed amount of $Ni^{2+}$ was raised with the amount of waste pulp and with pH in the range of pH $3{\sim}6$. This behavior of the adsorption of $Ni^{2+}$ according to the solution pH was well agreed with the electrokinetic characteristics of waste pulp in solution. The amount of coexisting solute was observed to reversely affect on the $Ni^{2+}$ adsorption onto waste pulp under the experimental conditions. With regard to the pre-treatment of adsorbent with NaOH, the adsorbability of $Ni^{2+}$ was increased with the concentration of NaOH to a certain extent. However, it was found to decrease contrarily when the concentration of NaOH became too high.