• Title/Summary/Keyword: Recycled Coarse Aggregate

Search Result 274, Processing Time 0.029 seconds

Strength Properties of Recycled Concrete Containing Water-redispersible Copolymer Powder (재유화형분말수지를 혼입한 재생콘크리트의 강도 특성)

  • Kim, In-Su;Sung, Chan-Yong
    • Proceedings of the Korean Society of Agricultural Engineers Conference
    • /
    • 2005.10a
    • /
    • pp.128-134
    • /
    • 2005
  • This study was performed to evaluate the strength and durability properties of recycled concrete containing water - redispersible copolymer powder(WRP) and blast furnace slag powder(BSP) [RCWS]. Material used were cemente, recycled coarse aggregare, natural fine aggregate, water-redispersible copolymer powder, blast-furnace slag powder. Especially, Water-redispersible powder was used for blending with Inorganic binders such as cemente, gypsum and hydrated lime etc. First of all, Mixed ratio method of RCWS made Two Type. One was called type-1 which used to BSP content 5% and WRP(Water-redispersible powder) content 0%, 1%, 2%, 3%, 4%, 5%, 6%. respectively. Another was called Type-2 which used to BSP(blast furnace slag powder)content 10% and WRP(Water-redispersible powder) content 0%, 1%, 2%, 3%, 4%, 5%, 6%. respectively. According to the experimental results of (RCWS), Incase Type-2 at curing age 28days, Compressive strength, pulse velocity and dynamic modulous of elasticity were shown higher than Type-1 and The more WRP content increasing($0%{\sim}6%$) was the lower Compressive strength, Pulse velocity and Dynamic modulous of elasticity. Water absorption ratio was in the range of $3.85%\;{\sim}\;3.23%$, it was almost equal to Type-1, 2 but Increasing the WRP content($0%{\sim}6%$), The water absorption ratio is decreased.

  • PDF

Damping Characteristics of Polyurethane Composites Incorporating Recycled Rubber Particles and Aggregates (폐타이어 고무분말과 골재를 혼입한 폴리우레탄 복합재료의 감쇠 특성)

  • Park, Se Eon;Choi, Jeong-Il;Hwang, Jae-Seung;Lee, Bang Yeon
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.8 no.3
    • /
    • pp.263-268
    • /
    • 2020
  • The purpose of this study is to investigate the damping properties of polyurethane composites incorporating waste tire rubber powder and preplaced coarse aggregates. Four types of polyurethane-based composites were manufactured, and longitudinal impact tests were performed. And vibration signals in the time domain and frequency domain were measured and values of damping ratio for each specimen were calculated. Test results showed that the damping ratios of polyurethane composites, in which the amount of polyurethane was reduced by 10.6% and 21.2% through incorporation of rubber particles, were 8.4% and 4.6% lower than that of pure polyurethane. The damping ratio of the polyurethane composite produced in a similar manner to the prepact concrete production method was found to be 22% lower than that of pure polyurethane, however, the amount of polyurethane was reduced by 50% and the stiffness was 25.7 times higher than that of pure polyurethane.

The Fractural-Mechanical Properties and Durability of Lightweight Concrete Using the Synthetic Lightweight Aggregate (합성경량골재(SLA)를 사용한 경량콘크리트의 파괴, 역학적 특성 및 내구성)

  • Jo Byung-Wan;Park Seung-Kook;Park Jong-Bin;Daniel C. Jansen
    • Journal of the Korea Concrete Institute
    • /
    • v.17 no.1 s.85
    • /
    • pp.19-25
    • /
    • 2005
  • Recycling of waste materials in the construction Industry is a useful method that can cope with an environment restriction of every country. In this study, synthetic lightweight aggregates are manufactured with recycled plastic and fly ash with 12 percent carbon. Nominal maximum-size aggregates of 9.5 mm were produced with fly ash contents of 0, 35, and $80\%$ by the total mass of the aggregate. An expanded clay lightweight aggregate and a normal-weight aggregate were used as comparison. Gradation, density, and absorption capacity are reported for the aggregates. Five batches of concrete were made with the different coarse aggregate types. Mechanical properties of the concrete were determined including density, compressive strength, elastic modulus, splitting tensile strength, fracture toughness, and fracture energy. Salt-scaling resistance, a concrete durability property, was also examined. Compressive and tensile strengths were lower for the synthetic aggregates; however, comparable fracture properties were obtained. Relatively low compressive modulus of elasticity was found for concretes with the synthetic lightweight aggregate, although high ductility was also obtained. As nv ash content of the synthetic lightweight aggregate increased, all properties of the concrete were improved. Excellent salt-scaling resistance was obtained with the synthetic lightweight aggregate containing 80 percent fly ash.

Fundamental Properties of Lightweight Concrete with Dry Bottom Ash as Fine Aggregate and Burned Artificial Lightweight Aggregate as Coarse Aggregate (건식 바텀애시 경량 잔골재와 소성 인공경량 굵은골재를 사용한 콘크리트의 기초 특성)

  • Choi, Hong-Beom;Kim, Jin-Man
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.4
    • /
    • pp.267-274
    • /
    • 2018
  • Though the wet bottom ash has been used as a type of lightweight aggregate, dry bottom ash, new type bottom ash from coal combustion power plant, has scarcely researched. It is excellent lightweight aggregate in the view point of construction material. This study is performed to check the applicability of dry bottom ash as a fine aggregate in lightweight aggregate concrete, by analyzing various properties of fresh and hardened concrete. We get results that the slump of concrete is within the target range at less than 75% replacement rate of dry bottom ash, the air content is not affected by the replacement rate of dry bottom ash, the bleeding capacity is less than $0.025cm^3/cm^2$ at 75% under of the replacement rate of dry bottom ash, and the compressive strength of concrete show 90% or more comparing the base mix while initial strength development is a little low. Oven dry unit weight of concrete is reduced by 8.9% when replaced 100% dry bottom ash, and dry shrinkage tends to decrease depending on increase of replacement rate of dry bottom ash. Modulus of elasticity of concrete shows no decease at 50% over of the replacement rate of dry bottom ash, while modulus of elasticity of concrete decreases when the replacement rate increases further. The dry bottom ash, when used as a fine aggregate in lightweight concrete, can be used effectively without any deterioration in quality.

Shear behavior of composite frame inner joints of SRRC column-steel beam subjected to cyclic loading

  • Ma, Hui;Li, Sanzhi;Li, Zhe;Liu, Yunhe;Dong, Jing;Zhang, Peng
    • Steel and Composite Structures
    • /
    • v.27 no.4
    • /
    • pp.495-508
    • /
    • 2018
  • In this paper, cyclic loading tests on composite frame inner joints of steel-reinforced recycled concrete (SRRC) column-steel beam were conducted. The main objective of the test was to obtain the shear behavior and analyze the shear strength of the joints. The main design parameters in the test were recycled coarse aggregate (RCA) replacement percentage and axial compression ratio. The failure process, failure modes, hysteresis curves and strain characteristics of the joints were obtained, and the influences of design parameters on the shear strength of the joints have been also analysed in detail. Results show that the failure modes of the joints area are typical shear failure. The shear bearing capacity of the joints maximally decreased by 10.07% with the increase in the RCA replacement percentage, whereas the shear bearing capacity of the joints maximally increased by 16.6% with the increase in the axial compression ratio. A specific strain analysis suggests that the shear bearing capacity of the joints was mainly provided by the three shear elements of the recycled aggregate concrete (RAC) diagonal compression strut, steel webs and stirrups of the joint area. According to the shear mechanism and test results, the calculation formulas of the shear bearing capacity of the three main shear elements were deduced separately. Thus, the calculation model of the shear bearing capacity of the composite joints considering the adverse effects of the RCA replacement percentage was established through a superposition method. The calculated values of shear strength based on the calculation model were in good agreement with the test values. It indicates that the calculation method in this study can reasonably predict the shear bearing capacity of the composite frame inner joints of SRRC column-steel beam.

Application of Waste Concrete Powder as Silica Powder of Cement Extruding Panel (시멘트 압출패널의 규사분말 대체재로서 폐콘크리트 미립분의 활용)

  • Kim, Jin-Man;Kim, Kee-Seok;La, Jung-Min;Choi, Duck-Jin
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.1
    • /
    • pp.88-94
    • /
    • 2011
  • To make recycling aggregate, quantity of fine particles increase due to multi-crushing. Though this particles were mixed with recycling aggregate, those have to be disparted from aggregate in the high quality recycling aggregate, because of the cause of low quality. Considering reactivity, fine particles is better than coarse one. Therefore, it needs to develop suitable usage. We try to make cement extruding material by using the fine particles from concrete recycling, as a silicious replacement. Test results are as follows ; 1) Waste concrete powder has major ingredients such as $SiO_2$ and CaO, its density is $2.45g/cm^3$ being similar to silica powder, its diameter is range 13 to $141{\mu}m$. 2) Considering to strength properties according to particle size, specimen was made using small particles is higher strength than large one. 3) Despite of exception in the autoclaved curing, when the replacement of waste fine particle increase, strength of extruding panel shows almost same level.

  • PDF

Effects of Low-quality Aggregates in the Same Workability Conditions on the Engineering Properties of Concrete (저품질 골재가 동일 작업성 조건에서 콘크리트 공학적 특성에 미치는 영향)

  • Min, Kyeong-Chul;Han, Cheon-Goo
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.3
    • /
    • pp.299-306
    • /
    • 2016
  • In this research, influence of low quality aggregate on engineering properties of concrete was evaluated experimentally. From the experiment, the fresh properties of slump and air content were controlled with unit water and AE dosage and all mixture were designed to have similar fresh properties of slump and air content with various quality of aggregate. Under this conditions, comparing with the mixture with high quality aggregate, the mixture with low quality aggregate showed the unit water and AE dosage were increased about 18 and 98%, respectively, because of poor grading and quantity of fines. For compressive strength, the low quality aggregate, specifically, exploded debris, clay sand, and sea sand contributed on decreasing compressive strength about 20~35%. Additionally, the concrete mixture including low quality fine and coarse aggregate showed adverse quality in not only compressive strength but also durability of freeze-thawing resistance, drying shrinkage, carbonation, and chloride ingression. Therefore, it is considered that for low quality aggregate, extra treatment processes such as washing or controlling gradation, and regulation to limit the use of low quality aggregate are needed.

Analysis the Use of Concrete Fine Aggregates of Coal Gasification Slag (콘크리트용 잔골재로서 석탄가스화 용융슬래그(CGS)의 활용성 분석)

  • Park, Kyung-Taek;Han, Min-Cheol;Hyun, Seung-Yong
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.7 no.2
    • /
    • pp.101-108
    • /
    • 2019
  • This study is analysis of the utilization as a concrete fine aggregate on CGS, a by-product of Integrated coal gasification combined cycle(IGCC). That is, in KS F 2527 "Concrete aggregate," properties of 1~12times to CGS were evaluated, focusing on quality items corresponding to natural aggregate sand(NS) and melted slag aggregate sand(MS). As a result, the distribution of grain shape, safety and expansion were all satisfied with KS standards by physical properties, but the quality was unstable at 7~12times of water absorption ratio and absolute dry density. The particle size distribution was unstable due to asymmetry distribution of coarse particles, and particles were too thick for 7~12times. The passing ratio of 0.08mm sieve was also out of the KS standard at part factor of 7~12times, but chloride content, clay contents, coal and lignite were all satisfactory. Meanwhile, chemical composition was satisfactory except for $SO_3$ in 1~6times, and content and amount of harmful substances were all within the specified value except for F in 7~12times. As a result of SEM analysis, the surface quality and porosity were 7~12times more than 1~6times, and it was the quality was degraded. Therefore, it is necessary to reduce the quality deviation by using separate measures in order to utilize it as concrete aggregate in the future, and if it is premixed with fine quality aggregate, it will contribute positively to solve aggregate supply shortage and utilize circulation resources.

Characterization of Concrete Composites with Mixed Plastic Waste Aggregates (복합 폐플라스틱 골재 치환 콘크리트의 기초 물성 평가)

  • Lee, Jun;Kim, Kyung-Min;Cho, Young-Keun;Kim, Ho-Kyu;Kim, Young-Uk
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.8 no.3
    • /
    • pp.317-324
    • /
    • 2020
  • Plastic wastes generated from domestic waste are separated by mixed discharge with foreign substances, and the cost of the separation and screening process increases, so recycling is relatively low. In this study, as a fundamental study for recycling mixed plastic wastes generated from domestic waste into concrete aggregates, changes in concrete properties according to the plastic waste types and the substitution rate were evaluated experimentally. The mixed plastic waste aggregate(MPWA) was found to have a lower density and a higher absorption rate compared to the coarse aggregate with good particle size distribution. On the other hand, the single plastic waste aggregate(SPWA) was composed of particles of uniform size, and both the density and the absorption rate were lower than that of the fin e aggregate. It was found that the MPWA substitution concrete did not cause a material separation phenomenon due to a relatively good particle size distribution even with the largest amount of plastic waste substitution, and the amount of air flow increased little. The compressive strength and flexural strength of the PWA substitution concrete decreased as the amount of substitution of the PWA increased due to the low strength of the PWA, the suppression of the cement hydration reaction due to hydrophobicity, and the low adhesion between the PWA and the cement paste. It was found that the degree of deterioration in compressive strength and flexural strength of concrete substituted with MPWA having good particle size distribution was relatively small.

Experimental Study on the Development of EMP Shielded Concrete Using Industrial By-products (산업부산물을 사용한 EMP차폐 콘크리트 개발에 관한 실험적 연구)

  • Min, Tae-Beom;Kim, Hyeong-Cheol;Choi, Hyun-Kuk;Roh, Jeong-Heon;Kim, Kuk-Joo;Park, Young-Jun
    • Journal of the Korea Institute of Building Construction
    • /
    • v.19 no.6
    • /
    • pp.477-484
    • /
    • 2019
  • The purpose of this study is to present basic data for developing concrete with EMP shielding as the structure materials when constructing an EMP shielded building structure. In order to use metal-based recycled aggregates with excellent conductivity and easy procurement for EMP shielding concrete, an evaluation of the stability evaluation and EMP shielding performance was performed. Through the stability evaluation, it was found that the coarse aggregate stability criterion was satisfied, but the oxidized slag did not satisfy the fine aggregate stability criterion, the oxidized slag is not satisfied. In addition, as a result of fresh concrete, the workability is increased and the air volume is decreased. The compressive strength is increased due to the high density and coarse granularity of the recycled aggregates, which increased the cement paste and adhesion, thereby increasing the compressive strength. The results of an EMP shielding test show that aggregates with high shielding performance are electronic arc furnace(EAF) Oxidizing Slag and Cooper Slag. The shielding performance is expected to increase if the average particle size of aggregate is small or uniformly distributed.