공기와 증류수에서 노화시킨 천연고무 복합체의 원형 변형으로부터의 회복 거동의 차이를 연구하였다. 공기에서 노화시킨 시험편의 회복률이 증류수에서 노화시킨 것보다 더 컸다. 충진제로 보강한 시험편의 회복속도가 비충진 시험편보다 더 빨랐다. 카본블랙으로 보강한 시험편의 회복속도가 실리카로 보강한 시험편보다 더 빨랐다. 노화 매질에 따른 회복 거동의 차이는 가교밀도 변화와 아닐링 효과로 설명하였다.
The breaking capacity of circuit breakers could be no more increased in the electric power system. This is because the fault current increases due to continuous increases in electric power demand and facilities. To solve the problem, it is necessary to come up with an alternative. The superconducting fault current limiter (SFCL) has received an attention among various alternatives. The SFCL effectively reduce a fault current in cooperation with a power circuit breaker. A various types of the SFCL are suggested and a study on them have been progressed. As a result of it, the SFCL can be applyed to the electric power system in the near future. But, a study on recovery behaviors of the SFCL is not enough for applying to the electric power system. If the superconducting elements do not completely recover to the superconducting state after fault operation, it might be a breakdown of the superconducting elements due to heavy power burden and it gives an bad influence on the working of other electric devices. Additionally, the distribution power system has reclosing operation such as open-0.3sec-closed/open-3min-closed/open procedure. So we need to study more about improvement of the recovery behaviors of the SFCL. In this paper, we analyzed the recovery behaviors of a flux-coupling type SFCL according to reclosing operation when a single line-to-ground fault occurred and we compared recovery behaviors of the SFCL with and without a neutral line between secondary reactors and superconducting elements. Also, the flux-coupling type SFCL has advantageous for increases of capacity by controlling the variation in turn ratios between two reactors. Consequently, when the number of turns of the secondary reactors increased, the power burden of the superconducting elements was bigger due to the increase of impedances of the secondary reactors. To distribute the power burden, two superconducting elements connected in series and the balanced quenching of the superconducting elements was induced by connecting a neutral line.
충전제의 영향을 막기 위해 비보강 NR, BR, SBR 고무 가황물을 원형 변형시켜 노화시킨 후 회복 거동을 비교하였다. 시료는 상온, 50, 70, $90^{\circ}C$에서 10일간 노화시켰다. 측정 시간이 증가함에 따라 회복률은 증가하였다. 노화 후 측정 시간에 따른 회복률의 변화로부터 1.0 초 미만의 순간회복률을 구하였다. 상온 노화에서는 노화 기간이 짧아 고무 간의 회복률 차이가 거의 나타나지 않았다. 하지만 50, 70, $90^{\circ}C$에서의 가속 노화 실험 결과에서는 각 고무 간의 회복률 차이가 뚜렷하게 나타났다. BR의 회복률이 가장 우수하였고, SBR의 회복률이 가장 적었다. 그러나 $90^{\circ}C$ 가속 노화 에서는 NR의 회복률이 BR보다 높게 나타났다. 노화 온도가 높아 질수록 초기 회복률이 감소하였으며, 그 감소 폭은 SBR이 가장 크게 나타났다. 실험 결과는 고무의 반발 특성과 노화에 의한 가교밀도 변화로 설명하였다.
중성자에 조사 $(fluence: 2.3\times10^{19}ncm^{-2}, 553 K, E\geq1.0 MeV)$된 Mn-Mo-Ni 저 합금강 모재의 열처리 회복 거동을 조사하기 위하여 등시소둔과 등온소둔을 수행하여 회복 활성화에너지, 회복 반응차수 그리고 회복 반응률상수를 결정하였다. 열처리 후 회복은 비커스 미세 고온경도기로 측정하였고 실험결과를 이용, 열처리 회복단계, 회복결함들의 거동 및 회복 kinetics을 분석하였다. 실험결과 2단계의 회복구간(stage I : 703-753K, stage II : 813K-873K)이 나타났으며 각 단계의 회복활성화 에너지는 2.50 eV(1단계) 및 2.93 eV(2단계)이었다. 조사재와 비조사재의 등시소둔 곡선의 비교를 통하여 813K에서 RAH(radiation anneal hardening) 피크를 확인할 수 있었다. 743K 및 833K에서 수행한 등온소둔 결과, 회복의 60%가 모두 120분 이내에 일어나는 것으로 관찰되었다. 회복 반응차수는 두 회복구간에서 모두 2로 나타났으며 회복 반응율상수는 $3.4\times10^{-4}min^{-1}$(1단계)과 $7.1\times10^{-4}min^{-1}$(2단계) 이었다. 이상의 결과와 기 발표된 자료들을 함께 분석한 결과, 본 재료의 회복은 오랜 중성자조사로 형성된 점결함 집합체들이 열처리에 의한 분해와 Fe 기지에 격자간 원자로 존재하던 self-interstitial들과 vacancy들의 재결합에 의해 일어나는 것으로 해석된다.
비충전, 카본블랙 충전, 그리고 실리카 충전 천연고무(NR) 복합체를 원형 변형 상태로 $60-90^{\circ}C$에서 노화시켜 회복 거동을 조사하였다. 시험편은 공기와 물을 매일 교대로 교체하는 교매질 시스템 하에서 노화시켰다. 충전시스템에 따른 회복률의 순서는 비보강 > 실리카 보강 > 카본블랙 보강 순이었다. 공기에서 물로 교체하는 교매질 시스템에서 노화된 시험편의 회복률이 물에서 공기로 교체하는 교매질 시스템에서 노화된 시험편의 회복률보다 더 컸다. 최초 노화 매질은 변형 정도에 지배적으로 영향을 끼쳤다.
스티렌 함량이 SBR 가황물의 회복 거동에 미치는 영향에 대해 연구하였다. 스티렌 함량이 15와 21 wt%인 SBR을 사용하였다. 스티렌 함량이 적은 가황물이 스티렌 함량이 많은 가황물에 비해 더 낮은 온도에서 회복하기 시작하였으며, 스티렌 함량이 적은 가황물의 회복 속도가 스티렌 함량이 많은 가황물보다 느렸다. 두 가황물 간의 회복 차이는 카본블랙으로 보강된 가황물이 실리카로 보강된 것보다 컸다. 실험 결과는 유리전이온도와 모듈러스로 설명하였다.
There have been a lot of approaches to evaluate and predict transmission control protocol (TCP) performance in a numerical way. Especially, under the recent advance in wireless transmission technology, the issue of TCP performance over wireless links has come to surface. It is because TCP responds to all packet losses by invoking congestion control and avoidance algorithms, resulting in degraded end-to-end performance in wireless and lossy systems. By several previous works, although it has been already proved that overall TCP performance is largely dependent on its loss recovery performance, there have been few works to try to analyze TCP loss recovery performance with thoroughness. In this paper, therefore, we focus on analyzing TCP's loss recovery performance and have developed a simple model that facilitates to capture the TCP sender's behaviors during loss recovery period. Based on the developed model, we can derive the conditions that packet losses may be recovered without retransmission timeout (RTO). Especially, we have found that TCP Reno can retransmit three packet losses by fast retransmits in a specific situation. In addition, we have proved that successive three packet losses and more than four packet losses in a window always invoke RTO easily, which is not considered or approximated in the previous works. Through probabilistic works with the conditions derived, the loss recovery performance of TCP Reno can be quantified in terms of the number of packet losses in a window.
Deposition behaviors of Sr and Cs in various liquid cathodes, such as Zn, Bi, Cd, and Pb, were examined to evaluate their recovery from LiCl-KCl eutectic salt. Cations in the salt were deposited on the liquid cathode, exhibiting potential of -1.8 to -2.1 V (vs. Ag/AgCl). Zn cathode had successful deposition of Sr and exhibited the highest recovery efficiency, up to 55%. Meanwhile, the other liquid cathodes showed low current efficiencies, below 18%, indicating LiCl-KCl salt decomposition. Sr was recovered from the Zn cathode as irregular rectangular SrZn13 particles. A negligible amount of Cs was deposited on the entire liquid cathode, indicating that Cs was hardly deposited on liquid cathodes. Based on these results, we propose that liquid Zn cathode can be used for cleaning Sr in LiCl-KCl salt.
한국고분자학회 2006년도 IUPAC International Symposium on Advanced Polymers for Emerging Technologies
/
pp.205-205
/
2006
Adsorption behaviors of positively charged matrix (PAH) onto negatively charged probe (sulfate PS particle) were investigated using DLS (dynamic light scattering) and FPR (fluorescence photobleaching recovery) as view points of matrix and salt concentration. The system experienced sharp decrease of diffusion (flocculation) at dilute condition while the system underwent gradual decrease of diffusion above semi-dilute concentration. With FPR and viscometry experiments, we revealed the probe behaviors in polyelectrolyte solution were strongly affected by the coil overlap concentration (0.5 g/L PAH concentration).
The bending properties, wrinkle resistance, and fabric retention behaviors of cotton knitted fabrics in the wale and course directions were studied for their dependence upon resin finishing, knit structure, and washing cycles. Stiffness, wrinkle recovery angles, and dimensional stability were investigated before and after resin finishing and laundering. It has been found that any change in the physical properties of the knitted fabrics with respect to knit structure and fabric directions are related to accompanying modifications to the state of the fiber properties. The decrease of fabric shrinkage rates and wrinkle recovery properties from increasing laundering cycles is related with resin incorporated on the fiber surface. This study shows that resin finishing on knitted fabrics can be performed only to improve fabric retention properties with reduced wrinkle recovery properties.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.