• 제목/요약/키워드: RF magnetron Sputtering system

검색결과 266건 처리시간 0.041초

UV 처리된 유리기판위에 RF-스퍼터된 PTFE 박막들의 발수 특성 (Hydrophobic Properties on RF-sputtered PTFE Films coated on UV-treated Glass Substrates)

  • 손진운;윤현오;배강;손선영;김화민
    • 한국전기전자재료학회논문지
    • /
    • 제23권1호
    • /
    • pp.6-9
    • /
    • 2010
  • Surface properties of polytetrafluoroethylene(PTFE) films fabricated by rf-magnetron sputtering system with UV surface treatment were investigated to increase water contact angle for their hydrophobic property. We found that the surface morphology and water contact angles of PTFE film modified as a function of the UV treatment times using UV-irradiation were influenced. The water contact angle of PTFE film with optimized UV treatment time for 15 minute showed a high hydrophobicity compared with the film without any surface treatment. We thought that it was due to the energy change of PTFE surface with an adhesion improvement to the glass surface as a smoothing a rough surface with needle-shape and/or the enhancement of an interface property as a removing some defects on the surface like a cleaning effect.

Effect of Annealing Time on Electrical Performance of SiZnSnO Thin Film Transistor Fabricated by RF Magnetron Sputtering

  • Ko, Kyung Min;Lee, Sang Yeol
    • Transactions on Electrical and Electronic Materials
    • /
    • 제16권2호
    • /
    • pp.99-102
    • /
    • 2015
  • Thin film transistors (TFTs) with amorphous 2 wt% silicon-doped zinc tin oxide (a-2SZTO) channel layer were fabricated using an RF magnetron sputtering system, and the effect of post-annealing treatment time on the structural and electrical properties of a-2SZTO systems was investigated. It is well known that Si can effectively reduce the generation of oxygen vacancies. However, it is interesting to note that prolonged annealing could have a bad effect on the roughness of a-2SZTO systems, since the roughness of a-2SZTO thin films increases in proportion to the thermal annealing treatment time. Thermal annealing can control the electrical characteristics of amorphous oxide semiconductor (AOS) TFTs. It was observed herein that prolonged annealing treatment can cause bumpy roughness, which led to increase of the contact resistance between the electrode and channel. Thus, it was confirmed that deterioration of the electrical characteristics could occur due to prolonged annealing. The longer annealing time also decreased the field effect mobility. The a-2SZTO TFTs annealed at 500℃ for 2 hours displayed the mobility of 2.17 cm2/Vs. As the electrical characteristics of a-2SZTO annealed at a fixed temperature for long periods were deteriorated, careful optimization of the annealing conditions for a-2SZTO, in terms of time, should be carried out to achieve better performance.

전자빔 조사에 따른 IZO 박막의 물성 변화

  • 이학민;남상훈;김용환
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2013년도 제44회 동계 정기학술대회 초록집
    • /
    • pp.575-575
    • /
    • 2013
  • Indium Zinc Oxide (IZO)는 가시광 영역(380~780 nm)에서 높은 투과율과 적외선영역에서 높은 반사율을 보이는 투명산화막으로서 Flexible display 적용으로 주목 받는 재료이다. 특히 비 화학적 양론비(non-stoichiometric)로 성장된 박막은 N형 반도체 특성을 갖기 때문에 광전자 소자, 액정표시소자와 태양전지의 투명전극 재료로 이용되고 있으며, 향 후에도 수요는 계속 증가될 전망이다. 일반적으로 IZO 박막은 높은 열처리 온도에 의한 기판재료의 선택이 한정적인 단점이 있다. 따라서 최근에는 정밀하게 제어된 에너지를 가진 전자를 표면에 조사(E-beam irradiation)하여 박막의 물성을 개선하고 기판재료의 선택성을 넓히는 연구가 활발히 진행되고 있다 [1]. 본 연구에서는 RF Magnetron Sputtering 법을 이용하여 Glass 위에 IZO를 증착하였다. 스퍼터링타겟은 고순도 IZO 타겟을 이용하여 100 nm의 두께를 가지는 박막을 증착하였다. 증착된 IZO 박막에 E-beam Source ((주)인포비온)를 이용하여 E-beam irradiation energy 조건에 변화를 주어 박막의 물성 변화를 관찰하였다. IZO 박막의 두께를 측정하기 위해 SEM (Cross section)을 이용하였다. E-beam irradiation energy에 따른 가시광 영역(380~780 nm)에서의 광투 과도는 UV-Vis spectrometer를 사용하여 측정하였고, 전기적인 특성은 Hall measurement system 을 이용하여 측정하였다. 또한 박막의 결정성과 거칠기의 변화는 XRD (X-ray Diffraction)와 원자 간력현미경(Atomic Force Microscope; AFM)을 이용하여 측정하였다. Rf magnetron Sputtering 법을 이용하여 증착한 IZO 박막에 Post E-beam irradiation이 전기전도 및 광 투과특성과 결정성과 표면 조도를 향상시키는데 크게 기여함을 확인할 수 있었다.

  • PDF

Phase identification of $C_3N_4$ in CN films prepared by rf plasma chemical vapor deposition and dc magnetron sputtering

  • Fu, Dejun;Wu, Dawei;Zhang, Zhihong;Meng, Xianquan;He, Mengbing;Guo, Huaixi;Peng, Yougui;Fan, Xiangjun
    • 한국진공학회지
    • /
    • 제7권s1호
    • /
    • pp.140-148
    • /
    • 1998
  • We prepared $C_3N_4$ films by rf plasma enhanced chemical vapor deposition(PCVD) and alternating $C_3N_4$/TiN composite films by dc magnetron sputtering. X-ray diffraction (XRD) and transmission electron diffraction (TED) revealed that the structure of the films is amorphous or polycrystalline, depending on deposition conditions and heat treatment. X-ray photoelectron spectroscopy (XPS) and Fourier transform infrared (FTIR) spectroscopy confirmed the presence of $sp_3\; and sp _2$ hybridized C atoms bonded with N atoms in the tetrahedral and hexagonal configurations, respectively. Graphite-free $C_3N_4$ films were obtained by PCVD under optimal conditions. To prepare well crystallized $C_3N_4$ films by magnetron sputtering, we introduced negatively biased gratings in the sputtering system. CN films deposited at grating voltages (Vg) lower than 400V are amorphous. Crystallites of cubic and $\beta$-$C_3N_4$ were formed at increased voltages.

  • PDF

Conductive Characterization of DLC Thin Films Fabricated by Radio-Frequency Magnetron Sputtering

  • ;김태규
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제41회 하계 정기 학술대회 초록집
    • /
    • pp.290-290
    • /
    • 2011
  • In this study Diamond-like carbon (DLC) films were deposited on p-type Si substrates using a Radio-Frequency magnetron Sputtering system. The DLC film was deposited by bombarding graphite target with a N2/Ar plasma mixture with various conditions: substrate, pressure, deposition time, temperature of substrate, power and ratio of gas mixture. The effect on the conduction and hardness of DLC thin films were investigated. The conduction of DLC films were measured by I-V measurement. In addition, Raman analysis was performed to study the chemical bonding structure. The hardness was measured by Nano indentation. Atomic Force Microscopy was used for determined surface morphology of DLC film.

  • PDF

스퍼터링을 이용한 $YMnO_3$/Si(100) 구조의 제작 (Fabrication of $YMnO_3$/Si(100) Structures by RF Magnetron Sputtering)

  • 김진규;김채규;정순원;김용성;이남열;김광호;유병곤;이원재;유인규
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 추계학술대회 논문집
    • /
    • pp.429-432
    • /
    • 1999
  • The growth of $\textrm{YMnO}_3$ films directly on Si(100) substrates by RF magnetron sputtering system has been performed. The structural properties of $\textrm{YMnO}_3$ films on Si(100) by rapid thermal annealing(RTA) analysed by XRD(X-ray diffraction). The c-axis oriented $\textrm{YMnO}_3$ peaks were observed deposited in $\textrm{YMnO}_3$/Si(100) structure at RF power of 100W and at a temperature range of $840^{\circ}C$~$870^{\circ}C$ in oxygen ambient.

  • PDF

KLN 스퍼터링용 타겟의 제조 및 코닝 1737 유리 기판위에 성장시킨 박막의 광학적 성질 (Target Preparation for KLN sputtering and optical properties of thin films deposited on Corning 1737 glass)

  • 박성근;서정훈;김성연;전병억;김진수;김지현;최시영;김기완
    • 한국재료학회지
    • /
    • 제11권3호
    • /
    • pp.178-184
    • /
    • 2001
  • rf-마그네트론 스퍼터링 방법을 이용하여 높은 광투과성을 지니며 c-축 배향된 KLN 박막을 제작하였다. 하소 및 소결 과정을 거쳐서 균일하고 안정한 상태의 KLN 타겟을 제조하였다. KLN 타겟은 화학량론적인 조성 및 K가 30%, 60%, 그리고 Li가 각각 15%, 30% 과량된 조성을 사용하였으며 K와 Li의 휘발을 방지하기 위하여 낮은 온도에서 소결시켰다. 제조된 타겟을 사용하여 rf-magnetron sputtering 방법으로 박막을 제조하였으며, 이때 K가 60% Li가 30% 과량된 타겟으로 제조할 때 단일상의 KLN 박막을 얻을 수 있었다. KLN 박막은 코닝 1737 기판 위에서 우수한 결정성과 높은 c-축 배향성을 나타내었으며, 이때 박막의 성장조건은 고주파 전력 100 W, 공정 압력 150 mTorr, 기판 온도 58$0^{\circ}C$였다. 가시광 영역에서 박막의 투과율은 약 90% 이고, 흡수는 333 nm에서 발생하였으며 632.8 nm에서 박막의 굴절율은 1.93이었다.

  • PDF

Ampoule-tube 법을 이용한 P와 As 도핑 p형 ZnO 박막의 광학적 특성 (Optical properties of Phosphorus- and Arsenic-doped p-type ZnO Thin Films with Ampoule-tube Method)

  • 소순진;이은철;유인성;박춘배
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 추계학술대회 논문집 Vol.18
    • /
    • pp.97-98
    • /
    • 2005
  • To investigate the ZnO thin films which is interested in the next generation of short wavelength LEDs and Lasers, our ZnO thin films were deposited by RF sputtering system. Phosphorus (P) and arsenic (As) were diffused into about 2.1${\mu}m$ ZnO thin films sputtered by RF magnetron sputtering system mn ampoule tube which was below $5\times10^{-7}$ Torr. The dopant sources of phosphorus and arsenic were $Zn_3P_2$ and $ZnAs_2$. Those diffusion was perform at 500, 600, and 700$^{\circ}C$ during 3hr. We find the condition of p-type ZnO whose diffusion condition is 700$^{\circ}C$, 3hr Our p-type ZnO thin film has not only very high carrier concentration of above $10^{19}/cm^3$ but also low resistivity of $5\times10^{-3}{\Omega}cm$.

  • PDF

AZO/p-Si 자외선 수광소자의 전기적.광학적 특성 (Realization and Electrical-Optical Properties of AZO/p-Si UV Photodetector)

  • 오상현;정윤환;진호;박춘배
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.323-324
    • /
    • 2007
  • Investigation of improving the properties of UV photodetector which uses the wide bandgap of ZnO are under active progress. In this paper, transparent conducting aluminum-doped Zinc oxide films(AZO) were prepared by rf magnetron sputtering on glass(corning 1737) and p-Si substrate, were then annealed at temperature $400^{\circ}C$ for 2hr. The AZO thin films were deposited by RF sputtering system. HF power and work pressure is 120 W and 15 mTorr, respectively, and the purity of AZO target is 5N. The AZO thin films were deposited at 300, 400, $500^{\circ}C$, and $600^{\circ}C$. For sample deposited at $400^{\circ}C$, we observed best $V_r-I_{ph}$ of 0.94 mA and good transmittance.

  • PDF