Semiconductor nanowires offer exciting possibilities as components of solar cells and have already found applications as active elements in organic, dye-sensitized, quantum-dot sensitized, liquid-junction, and inorganic solid-state devices. Among many semiconductors, silicon is by far the dominant material used for worldwide photovoltaic energy conversion and solar cell manufacture. For silicon wire to be used for solar device, well aligned wire arrays need to be fabricated vertically or horizontally. Macroscopic silicon wire arrays suitable for photovoltaic applications have been commonly grown by the vapor-liquid-solid (VLS) process using metal catalysts such as Au, Ni, Pt, Cu. In the case, the impurity issues inside wire originated from metal catalyst are inevitable, leading to lowering the efficiency of solar cell. To escape from the problem, the wires of purity of wafer are the best for high efficiency of photovoltaic device. The fabrication of wire arrays by the electrochemical etching of silicon wafer with photolithography can solve the contamination of metal catalyst. In this presentation, we introduce silicon wire arrays by electrochemical etching method and then fabrication methods of radial p-n junction wire array solar cell and the various merits compared with conventional silicon solar cells.
Solar cells have been more intensely studied as part of the effort to find alternatives to fossil fuels as power sources. The progression of the first two generations of solar cells has seen a sacrifice of higher efficiency for more economic use of materials. The use of a single junction makes both these types of cells lose power in two major ways: by the non-absorption of incident light of energy below the band gap; and by the dissipation by heat loss of light energy in excess of the band gap. Therefore, multi junction solar cells have been proposed as a solution to this problem. However, the $1^{st}$ and $2^{nd}$ generation solar cells have efficiency limits because a photon makes just one electron-hole pair. Fabrication of all-silicon tandem cells using an Si quantum dot superlattice structure (QD SLS) is one possible suggestion. In this study, an $SiO_x$ matrix system was investigated and analyzed for potential use as an all-silicon multi-junction solar cell. Si quantum dots with a super lattice structure (Si QD SLS) were prepared by alternating deposition of Si rich oxide (SRO; $SiO_x$ (x = 0.8, 1.12)) and $SiO_2$ layers using RF magnetron co-sputtering and subsequent annealing at temperatures between 800 and $1,100^{\circ}C$ under nitrogen ambient. Annealing temperatures and times affected the formation of Si QDs in the SRO film. Fourier transform infrared spectroscopy (FTIR) spectra and x-ray photoelectron spectroscopy (XPS) revealed that nanocrystalline Si QDs started to precipitate after annealing at $1,100^{\circ}C$ for one hour. Transmission electron microscopy (TEM) images clearly showed SRO/$SiO_2$ SLS and Si QDs formation in each 4, 6, and 8 nm SRO layer after annealing at $1,100^{\circ}C$ for two hours. The systematic investigation of precipitation behavior of Si QDs in $SiO_2$ matrices is presented.
It has been known that quantum confinement effect of CdSe nanocrystal was observed by increasing the number of deposition cycle using successive ionic layer adsorption and reaction (SILAR) method. Here, we report on thermally-induced quantum confinement effect of CdSe at the given cycle number using spin-coating technology. A cation precursor solution containing $0.3\;M\;Cd(NO_3)_2{\cdot}4H_2O$ is spun onto a $TiO_2$ nanoparticulate film, which is followed by spinning an anion precursor solution containing $0.3\;M\;Na_2\;SeSO_3$ to complete one cycle. The cycle is repeated up to 10 cycles, where the spin-coated $TiO_2$ film at each cycle is heated at temperature ranging from $100^{\circ}C$ to $250^{\circ}C$. The CdSe-sensitized $TiO_2$ nanostructured film is contacted with polysulfide redox electrolyte to construct photoelectrochemical solar cell. Photovoltaic performance is significantly dependent on the heat-treatment temperature. Incident photon-to-current conversion efficiency (IPCE) increases with increasing temperature, where the onset of the absorption increases from 600 nm for the $100^{\circ}C$- to 700 nm for the $150^{\circ}C$- and to 800 nm for the $200^{\circ}C$- and the $250^{\circ}C$-heat treatment. This is an indicative of quantum size effect. According to Tauc plot, the band gap energy decreases from 2.09 eV to 1.93 eV and to 1.76 eV as the temperature increases from $100^{\circ}C$ to $150^{\circ}C$ and to $200^{\circ}C$ (also $250^{\circ}C$), respectively. In addition, the size of CdSe increases gradually from 4.4 nm to 12.8 nm as the temperature increases from $100^{\circ}C$ to $250^{\circ}C$. From the differential thermogravimetric analysis, the increased size in CdSe by increasing the temperature at the same deposition condition is found to be attributed to the increase in energy for crystallization with $dH=240cal/^{\circ}C$. Due to the thermally induced quantum confinement effect, the conversion efficiency is substantially improved from 0.48% to 1.8% with increasing the heat-treatment temperature from $100^{\circ}C$ to $200^{\circ}C$.
본 연구에서는 황화납(PbS)을 감응 물질로 하는 양자점 감응형 태양전지를 제작하고 효율을 측정해보았다. 기판에 진공증착을 통해 seed layer를 형성하고 수열합성법으로 산화아연(ZnO) 나노선 어레이를 기른 후 SILAR(Successive ionic layer adsorption and reaction)법으로 PbS 양자점을 합성하였고, 농도와 cycle에 따른 특성의 변화를 주사전자현미경(SEM), X-선 회절, UV-visible spectrometer를 통해 확인하였다. SILAR법을 통해 PbS가 ZnO 나노선 위에 film 형태로 균일하게 성장한 것을 확인할 수 있었고, 이렇게 합성한 물질을 직접 태양전지로 제작하여 그 효율을 측정하였다. 또한 co-sensitizer 물질로 CdS를 합성하여 두 물질의 감응 물질로서의 성능을 확인하였다. PbS는 비교적 작은 밴드갭을 가지며 양자 제한 효과가 커 밴드갭 조절이 용이하며 여러 종류의 태양전지에서 이용되고 있다. 이러한 PbS를 감응 물질로 하는 양자점 감응형 태양전지 제작을 통해 태양전지에의 적용 가능성을 살펴보고 그러기 위해 필요한 부분들을 모색해보았다.
Serious environmental problems have been caused by the greenhouse effect due to carbon dioxide($CO_2$) or nitrogen oxides($NO_x$) generated by the use of fossil fuels, including oil and liquefied natural gas. Many countries, including our own, the United States, those of the European Union and other developed countries around the world; have shown growing interest in clean energy, and have been concentrating on the development of new energy-saving materials and devices. Typical non-fossil-fuel sources include solar cells, wind power, tidal power, nuclear power, and fuel cells. In particular, organic solar cells(OSCs) have relatively low power-conversion efficiency(PCE) in comparison with inorganic(silicon) based solar cells, compound semiconductor solar cells and the CIGS [$Cu(In_{1-x}Ga_x)Se_2$] thin film solar cells. Recently, organic cell efficiencies greater than 10 % have been obtained by means of the development of new organic semiconducting materials, which feature improvements in crystalline properties, as well as in the quantum-dot nano-structure of the active layers. In this paper, a brief overview of solar cells in general is presented. In particular, the current development status of the next-generation OSCs including their operation principle, device-manufacturing processes, and improvements in the PCE are described.
최근 태양전지의 Donor/Acceptor 계면에 그래핀 양자점을 완충 층으로 삽입하여 광 전환 효율을 향상시킨 많은 연구 결과들이 보고되었다. 그래핀 양자점은 그래핀 단일 층이 여러 겹 쌓여서 구성된 수 나노미터 크기의 물질로, 양자 제한 효과에 의한 밴드갭 조절이 가능하다는 장점을 가지고 있다. 하지만 대부분의 그래핀 양자점을 활용한 연구에서 레이저 분쇄나 수열 처리 등과 같은 복잡하고 접근성이 떨어지는 용액 공정들이 박막 형성에 사용되고 있다. 본 연구에서는 Indium tin oxide(ITO)/$TiO_2$/Poly(3-hexylthiophene)(P3HT)/Al 구조로 구성된 태양전지의 Donor/Acceptor 계면에 그래핀 양자점을 단순한 초음파 처리를 통해 용매에 분산시켜 박막 공정에 사용하였음에도 불구하고, 단락 전류를 $1.26{\times}10^{-5}A/cm^2$에서 $7.46{\times}10^{-5}A/cm^2$으로, 곡선인자(Fill factor)를 0.27에서 0.42로 향상된 결과를 확인하였다. 이러한 결과를 트랜지스터 구조의 소자를 활용한 전기적 성질 확인과 순환 전압-전류법을 통한 에너지 레벨 분석 및 가시광 흡수 스펙트럼 분석 등을 통하여 고찰하였다. 본 연구 결과를 통해 그래핀 양자점 용액 공정이 복잡한 처리 공정 없이도, 보다 폭넓게 활용 가능할 것으로 예상된다.
It is known that semiconductor quantum-dot (QD) heterostructures have superior zero-dimensional quantum confinement, and they have been successfully applied to semiconductor laser diodes (QDLDs) for optical communication and infrared photodetectors (QDIPs) for thermal images [1]. The self-assembled QDs are normally formed at Stranski-Krastanov (S-K) growth mode utilizing the accumulated strain due to lattice-mismatch existing at heterointerfaces between QDs and cap layers. In order to increase the areal density and the number of stacks of QDs, recently, sub-monolayer (SML)-thick QDs (SQDs) with reduced strain were tried by equivalent thicknesses thinner than a wetting layer (WL) existing in conventional QDs (CQDs) by S-K mode. Despite that it is very different from CQDs with a well-defined WL, the SQD structure has been successfully applied to QDIP[2]. In this study, optical characteristics are investigated by using photoluminescence (PL) spectra taken from self-assembled InAs/GaAs QDs whose coverage are changing from submonolayer to a few monolayers. The QD structures were grown by using molecular beam epitaxy (MBE) on semi-insulating GaAs (100) substrates, and formed at a substrate temperature of 480$^{\circ}C$ followed by covering GaAs cap layer at 590$^{\circ}C$. We prepared six 10-period-stacked QD samples with different InAs coverages and thicknesses of GaAs spacer layers. In the QD coverage below WL thickness (~1.7 ML), the majority of SQDs with no WL coexisted with a small amount of CQDs with a WL, and multi-peak spectra changed to a single peak profile. A transition from SQDs to CQDs was found before and after a WL formation, and the sublevel of SQDs peaking at (1.32${\pm}$0.1) eV was much closer to the GaAs bandedge than that of CQDs (~1.2 eV). These revealed that QDs with no WL could be formed by near-ML coverage in InAs/GaAs system, and single-mode SQDs could be achieved by 1.5 ML just below WL that a strain field was entirely uniform.
Franz Keldysh Oscillation (FKO)은 p-n 접합 구조의 공핍층(depletion zone)에서 전기장(electric field)에 의해 발생되며, Photoreflectance (PR) spectroscopy를 통하여 관측된다. InAs/GaAs 양자점 태양전지(Quantum Dot Solar Cells, QDSCs)에서 PR 신호에 대한 Fast Fourier Transform (FFT)을 통하여 FKO 주파수들을 관측할 수 있고, 각각의 FKO 주파수들은 태양전지 구조에 대응하는 표면 및 내부전기장(internal electric field) 들로 분류할 수 있다. InAs/GaAs 양자점 태양전지에서 AlGaAs potential barrier의 두께에 따른 내부전기장의 변화를 조사하기 위해, GaAs-matrix에 8주기의 InAs 양자점 층이 삽입된 태양전지를 molecular beam epitaxy (MBE) 방법으로 성장하였다. 양자점의 크기는 2.0 monolayer (ML)이며, 각 양자점 층은 1.6 nm에서 6.0 nm의 AlGaAs potential barrier들로 분리되어 있다. 또한 양자점 층의 위치에 따라 내부전기장 변화를 조사하기 위해, p-i-n 구조에서 양자점 층이 공핍층 내에 위치한 경우와 p+-n-n+ 구조에서 양자점 층이 공핍 층으로부터 멀리 떨어진 n-base 영역에 삽입하여 실험결과를 비교분석하였다. PR 실험결과로부터, p-i-n 구조에서 InAs 양자점 태양전지의 내부전기장 변화는 potential barrier 두께에 따라 다소 복잡한 변화를 보였으며, 이는 양자점 층이 공핍층 내에 위치함으로써 격자 불일치(lattice mismatch)로 발생된 응력(strain)의 영향으로 설명할 수 있다. 이러한 결과들을 각각의 태양전지 구조에서 표면 및 내부전기장에 대해 계산된 값들에 근거하여, p+-n-n+ 구조에서 양자점 층이 공핍 층으로부터 멀리 떨어진 영역에 삽입된 경우의 결과와 비교해 보면 내부전기장의 변화는 더욱 분명해진다. 즉, 양자점 층의 potential barrier의 두께를 조절하거나, 양자점 층의 위치를 변화시킴으로써 양자점 태양전지의 내부전기장을 조작할 수 있으며, 이는 PR 실험을 통해 FKO를 관측함으로써 확인할 수 있다.
전도성 혹은 비전도성 지지체에서 전기변색이 가능한 수 nm에서 수액 nm 두께의 금속 니켈 박막 형성에 대한 연구를 수행하였다. 광학렌즈나 혹은 LCD에 사용되는 ITO, 실리콘 웨이퍼에 박막 형성에 대한 연구는 다양한 두께의 니켈 박막은 자체로서의 응용 가능성 뿐 아니라, 광전기화학 소자, 특히 선글라스로 대변되는 변색 소자에의 응용 가능성이 아주 크다. 이러한 소자들은 나노 기술 응용과 양자점의 응용 등으로 경박단소형의 렌즈나 전지, 유리 그리고 태양 선지 등에 응용이 가능하다. 전기화학적으로 니켈 금속을 ITO 유리위에 코팅한 후, AFM, XRD을 이용하여 미세구조를 확인하고, 순환전압전류법, 시간대전류법, 임피던스를 이용하여 이들의 전기화학적 박막 특성을 조사하였다.
염료감응 태양전지는 실리콘 태양전지에 비해 단가가 낮고 반투명하며 친환경적 특성으로 차세대 태양전지로 주목을 받았으나 염료의 안정성의 문제와 특정 파장대의 빛만 흡수하는 단점을 가지고 있다. 이러한 문제점을 해결하기 위하여 양자구속 효과에 의해 크기에 따라 밴드갭 조절이 용이하여 다양한 파장대의 빛을 흡수 할 수 있는 양자점 감응태양전지가 많은 관심을 받고 있다. 하지만 양자점 감응 태양 전지의 활성층으로 사용되는 반도체 산화물인 이산화티타늄의 두께는 $13{\sim}18{\mu}m$로 짧은 확산거리로 인해 전하수집의 한계를 가지고 있다. 이를 극복하기 위해 인듐 주석 산화물 나노선을 합성하여 전자가 광전극에 직접유입이 가능하도록 해 빠른 전하이동 및 전하수집을 가능하게 한다. 인듐 주석 산화물 나노선은 증기수송 방법(VTM)을 이용하여 인듐 주석 산화물 유리 기판 위에 $5{\sim}30{\mu}m$ 길이로 합성하였다. 전해질과 전자가 손실되는 것을 방지하기 위해 원자층 증착법(ALD)을 이용하여 이산화 티타늄 차단층을 20 nm 두께로 코팅한 후 화학증착방법(CBD)을 이용하여 인듐 주석 산화물 나노선-이산화 티타늄 코어-쉘 구조를 만든다. 마지막으로 황화카드뮴, 카드늄셀레나이드, 황화아연을 증착시킨 후 다황화물 전해질을 이용하여 양자점 감응 태양전지를 제작하였다. 특성 평가를 위해 전계방사 주사전자현미경, X-선 회절, 고분해능 투과 전자 현미경을 이용하며 intensity modulated photocurrent spectroscopy (IMPS), intensity modulated voltage spectroscopy (IMVS)를 이용하여 전하수집 특성평가를 하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.