Pb($Zn_{1/3}Nb_{2/3})O_3-Ba(Zn_{1/3}Nb_{2/3})O_3-PbTiO_3$ 세라믹의 압전특성에 관한 연구 (A Study on the Piezoelectric Properties of the Pb($Zn_{1/3}Nb_{2/3})O_3-Ba(Zn_{1/3}Nb_{2/3})O_3-PbTiO_3$)

  • 박혜옥;박인길;이성갑;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1989년도 춘계학술대회 논문집
    • /
    • pp.70-73
    • /
    • 1989
  • (1-x-y)Pb($Zn_{1/3}Nb_{2/3})O_3-Ba(Zn_{1/3}Nb_{2/3})O_3-PbTiO_3(0.12{\leq}x{\leq}0.21, 0.24{\leq}y{\leq}0.33$) ternary compound ceramics were fabricated by the mixed oxide method. The sintering temperature and time were 1050 [$^{\circ}C$], 2[hr]. Morphotropic phase boundary region was chosen for the composition. 0.55 PZN-0.21 BZN-0.24 PT specimen had the highest value of relative dielectric constants, 5353. The curie temperature of specimens were increased linearly with PT content. Near the morphotropic phase boundary, electro-mechanical coupoling factor and mechanical quality factor of the specimens had the highest values.

  • PDF

Pb($Sb_{1/2}Sn_{1/2}O_3-PbTiO_3-PbZrO_3$ 세라믹의 초전특성에 관한 연구 (A Study on the Pyroelectric Properties of the Pb($Sb_{1/2}Sn_{1/2}O_3-PbTiO_3-PbZrO_3$ Ceramics)

  • 윤종원;이성갑;배선기;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1989년도 춘계학술대회 논문집
    • /
    • pp.74-76
    • /
    • 1989
  • x Pb($Sb_{1/2}Sn_{1/2}O_3-PbTiO_3-PbZrO_30.05{\leq}x{\leq}0.25$) ternary compound ceramics were fabricated by the mixed oxide method. The sintering temperature and time were 1200-1270[$^{\circ}C$], 2 hour, respectively. Increasing the PSS contents, the transition temperatures were decreased. The relative dielectric constant and Curie temperature of the 0.25 PSS-0.25 PT-0.5 PZ specimens were 450, 220[$^{\circ}C$]. The Pyroelectric coefficient of the 0.25PSS-0.25PT-0.50 PZ specimen was $5.20{\times}10^4$[C$\textrm{cm}^2$K].

  • PDF

전왜 액츄에이터용 PZMN-BT-PT계 세라믹스에 관한 연구 (The PZMN-BT-PT ceramics for Electrostrictive Actuator)

  • 윤현상;윤광희;박용욱;최형욱;백동수;박창엽
    • 대한전기학회논문지
    • /
    • 제43권4호
    • /
    • pp.620-626
    • /
    • 1994
  • As the electrostrictive actuator for optic control, PZN-BT-PT ceramics were investigated for the influences of sintering conditions on the structural, electrostrictive properties and the optical properties of Fabry-perot Interferometer using eletrostrictive ceramics. The specimen SS15T, sintered 1hr at 1150$^{\circ}C$, is sutible for eletrostrictive actuator because its piezoelectric constants(dS131T) and strain(XS131T) at dc 10kV/cm had the higest value of 175${\times}$10S0-12TC/N, -255${\times}$10S0-6TΔl/l respectively. As the dc electric field increased, the interference effect of Fabry-Perot Interferometer was increased. The most intense interference fringe and the maximum power of 160${\mu}$W were observed at dc 6kV/cm. Thus it was considered that specimen SS15T could be used as the electrostrictive actuator for optic control.

분위기 소결한 PZT 후막의 구조적 특성 (Structural Properties of PZT Thick Films Fabricated by the Atmospheric Sintering)

  • 이성갑;심영재;이영희;배선기
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 하계학술대회 논문집 Vol.6
    • /
    • pp.313-314
    • /
    • 2005
  • $PbTiO_3$ and PZT(52/48) powders, prepared by the sol-gel method, were mixed with an organic vehicle and the PT/PZT(52/40) heterolayered thick films were fabricated by the screen-printing method on Pt/$Al_2O_3$ substrates. The structural properties such as DTA, X-ray diffraction and microstructure, were examined as a amount of the PbO-$PbF_2$ flux. In the X-ray diffraction analysis, PZT(52/48) thick films showed a perovskite polycrystalline structure without a pyrochlore phase.

  • PDF

Sol-Gel법에 의한 Pb(Zr,Ti)$O_3$ 박막의 제조 및 유전 특성 (Preparation and Dielectric properties of the Pb(Zr,Ti)$O_3$ Thin Film by Sol-Gel Method)

  • 정장호;박인길;류기원;이성갑;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1995년도 하계학술대회 논문집 C
    • /
    • pp.1022-1024
    • /
    • 1995
  • In this study, $Pb(Zr_xTi_{1-x})O_3$(x=0.65, 0.52, 0.35) thin films were fabricated by Sol-Gel method. A stock solution with excess Pb 10[mol.%] of $Pb(Zr_xTi_{1-x})O_3$ was made and spin-coated on the Pt/$SiO_2$/Si substrate at 4000[rpm] for 30[sec.]. Coated specimens were dried on the hot-plate at $400[^{\circ}C]$ for 10[min.]. Sintering temperature and time were $500{\sim}800[^{\circ}C]$ and $1{\sim}60$[min.]. To investigate crystallization condition, PZT thin films were analyzed with sintering temperature, time and composition by the XRD. The microstructure of thin films were investigated by SEM. The ferroelectric perovskite phases precipitated under the sintering of $700[^{\circ}C]$ for 1 hour. In the PZT(52/48) composition, dielectric constant and dielectric loss were 2133, 2.2[%] at room temperature, respectively.

  • PDF

Sol-Gel 법에 의한 Pb(Zr, Ti)${O}_{3}$ 박막의 제조 및 구조적 특성 (Preparation and structural properties of the Pb(Zr, Ti)${O}_{3}$ thin film by Sol-Gel method)

  • 이영준;정장호;이성갑;이영희
    • 대한전기학회논문지
    • /
    • 제44권7호
    • /
    • pp.914-918
    • /
    • 1995
  • In this study, Pb(Zr$_{x}$ Ti$_{1-x}$ )O$_{3}$ (x=0.65, 0.52, 0.35) thin films were fabricated by Sol-Gel method. A stock solution with excess Pb 10[mol%] of Pb(Zr$_{x}$ Ti$_{1-x}$ )O$_{3}$ was made and spin-coated on the Pt/SiO$_{2}$/Si substrate at 4000[rpm] for 30[sec.]. Coated specimens were dried on the hot-plate at 400[.deg. C] for 10[min.]. Sintering temperature and time were 500~800[.deg. C] and 1~60[min.]. The coating process was repeated 6 times and the final thickness of the thin films were about 4800[A]. To investigate crystallization condition, PZT thin films were analyzed with sintering temperature, time and composition by the XRD. The microstructure of thin fulms were investigated by SEM. The ferroelectric perovskite phases precipitated under the sintering of 700[.deg. C] for 1 hours. In the PZT(52/48) composition, dielectric constant and dielectric loss were 2133, 2.2[%] at room temperature, respectively.ively.

  • PDF

Mn Oxide의 첨가에 따른 PSS-PT-PZ 세라믹의 초전특성 (Pyroelectric Properties of Modified PZT Ceramics with $MnO_2$ Addition)

  • 신상현;김영훈;박기운;강동헌;김영호;길상근
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집 Vol.3 No.2
    • /
    • pp.746-748
    • /
    • 2002
  • The effect of $MnO_2$ addition in $0.05Pb(Sn_{0.5}Sb_{0.5})O_3-0.8PbZrO_3-0.15PbTiO_3$(0.05PSS-0.8PZ-0.15PT) ceramics on crystal structure and electrical properties were studied. The sintering temperature and time were $1230^{\circ}C{\sim}1270^{\circ}C$ and 2hr, respectively. Then crystal structure, dielectric and pyroelectric properties were investigated. All the poled specimens showed the lower dielectric constant and $tan{\delta}$ than the unpoled specimens. Dielectric constant at 1kHz of the 0.05PSS-0.8PZ-0.15PT(MnO2 0.3wt%) system specimen sintered at $1250^{\circ}C$ for 2hr were 270 and showed the lowest $tan{\delta}$ of 0.2% after poling of $2kV_{DC}/mm$ at $150^{\circ}C$ for 30 minutes. Pyroelectric coefficient was maximum value of $50nC/cm^2K$ and Curie temperature was $224^{\circ}C$.

  • PDF

다결정 및 박막형 $Sr_2Nb_2O_7$의 입자배향과 전기적특성 (Grain Orientation and Electrical Properties of $Sr_2Nb_2O_7$ Ceramics and Thin Films)

  • 손창헌;전상재;남효덕;이희영
    • 한국전기전자재료학회논문지
    • /
    • 제11권4호
    • /
    • pp.274-280
    • /
    • 1998
  • Polycrystalline $Sr_2Nb_2O_7$ ceramics with very high Curie temperature were sintered using the powder derived by the chemical coprecipitation method (CCP). The phase evolution and grain-orientation of sintered samples were examined by XRD, while sintering behavior, dielectric properties and polarization were studied by SEM and ferroelectric tester. Extremely high degree of grain-orientation was observed along the (0k0) direction, which resulted in anisotropic dielectric properties of the sintered samples, with the dielectric constant values approaching those for single crystal. Thin film fabrication of $Sr_2Nb_2O_7$ in the pyroniobate family was also attempted on $SiO_2$/Si(100), Pt/$SiO_2$/Si(100), Pt/Ti/$SiO_2$/Si(100) and Pt/$ZrO_2/SiO_2/Si_2(100)$ substrates, using metalorganic decomposition (MOD) process. Neodecanoate precursor solution was prepared by mixing strontium neodecanoate with niobium neodecanoate synthesized from niobium ethoxide. It was found that $Sr_2Nb_2O_7$ single phase appeared in XRD patterns the samples annealed above $950^{\circ}C$. The effect of substrate type on film microstructure and dielectric properties was observed.

  • PDF

불순물 첨가에 따른 PSS-PT-PZ 세라믹의 유전 및 압전특성 (Dielectric and Piezoelectric Properties of PSS-PT-PZ Ceramics with the Addition of Dopant)

  • 강정민;이성갑;이상헌;배선기;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 추계학술대회 논문집 Vol.16
    • /
    • pp.296-299
    • /
    • 2003
  • In this paper, $0.10Pb(Sb_{1/2}Sn_{1/2})O_3-0.25PbTiO_3-0.65PbZrO_3$ ceramics were fabricated by the mixed-oxide method. The sintering temperature and time were $1230^{\circ}C$ and 2[hr], respectively. The structural, dielectric and piezoelectric properties with addition of NiO were studied. The crystal structure of a specimen was rhombohedral. As a result of SEM, the average grain size were decreased with increasing the contents of NiO. But the grains of the specimens doped with 0.4wt% NiO were increased, due to deposits of excess NiO at grain boundaries in the liquid phase. Relative dielectric constant and dielectric loss of the specimen doped with 0.1wt% NiO were 701 and 0.026, respectively.

  • PDF

PNN-PZT 세라믹스의 저온 소결 및 전기적 특성 평가 (Low Temperature Sintering of PNN-PZT Ceramics and Its Electrical Properties)

  • 이명우;김성진;윤만순;류성림;권순용
    • 한국전기전자재료학회논문지
    • /
    • 제21권12호
    • /
    • pp.1077-1082
    • /
    • 2008
  • To fabricate a multi-layered piezoelectrics/electrodes structure, the piezoelectrics should be sintered at the temperature lower than $950^{\circ}C$ to use the silver electrode, which is cheaper than the electrodes containing noble metals such as Pd and Pt. Therefore, in this study, we modified the composition of $Pb(Zr,Ti)O_3$-based material as $(Pb_{0.98}Cd_{0.02})(Ni_{1/3}Nb_{2/3})_{0.25}Zr_{0.35}Ti_{0.4}O_3$ to lower the sintering temperature and to improve the piezoelectric properties. Small amount of $MnCO_3$, $SiO_2$, and $Pb_3O_4$ were also added to lower the sintering temperature of the ceramic. The prepared raw powders were mixed by using a ball mill for 24 hours. And then the mixed powders were calcinated for 2 hours at $800^{\circ}C$. The calcinated powders were again crushed with the ball mill for 72 hours. The final powders were pressed for making the shape of ${\emptyset}15\;mm$ disk. The disk-type samples were sintered at temperature range of $850{\sim}950^{\circ}C$. The crystal phases of the sintered specimens were perovskite structure without secondary phases. All of the measured electrical properties such as electromechanical coupling coefficients ($k_p$), mechanical quality factors ($Q_m$), and piezoelectric charge constants ($d_{33}$) were decreased with decreasing the sintering temperatures. The electrical properties measured at the sample sintered at $950^{\circ}C$ were 54% of $k_p$, 503 of $Q_m$, and 390 pC/N of $d_{33}$, respectively. These properties were considered to be fairly good for the application of multi-layered piezoelectric generators or actuators.