Evaluation of Fracture Behavior and Formation of Microcrack of Alumina Ceramics by Acoustic Emission (AE에 의한 알루미나 세라믹스의 Microcrack 생성과 파괴거동의 평가)

  • 장병국;우상국
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.6
    • /
    • pp.551-558
    • /
    • 1998
  • Detection of microcrack in {{{{ {Al }_{2 } {O }_{3 } }} ceramics were studided by AE(acoustic emission) technique with 4-point bending test in order to evaluate the fracture process and formation of microcrack. Fully-dense alu-mina ceramics having a different grain size were fabricated by varing the hot-pressing temperature. The grain size of alumina increased with increasing the hot-pressing temperature whereas the bending strength decreasd. The microcracks were observed by SEM and TEM. The generation of AE event increased with increasing the applied load and many AE event was generated at maximum applied load. Alumina with smaller grain size shows the generation of many AE event resulting in an increase of microcrack formation. An intergranular fracture is predominantly observed in fine-grained alumina whereas intragranular fracture occurs predominantly in coarse-grained alumina,. Analysis of micorstructure and AE prove that primary mi-crocracks occur within grain-boundaries of alumina. The larger microcracking were formed by the growth and/or coalesence of primary microcracks. Then the materials become to fracuture by main crack gen-eration at the maximum applied load.

  • PDF

One-Ampere Conductor Method for Tubular Linear Induction Motor for Size Reduction of Primary Iron Core

  • Lee, Byeong-Hwa;Kim, Kyu-Seob;Kwon, Soon-O;Sun, Tao;Hong, Jung-Pyo;Lee, Jung-Ho
    • Journal of Magnetics
    • /
    • v.16 no.1
    • /
    • pp.46-50
    • /
    • 2011
  • This paper presents size reduction of primary iron core for tubular linear induction motor by improved winding configuration. Using one-ampere conductor method, magnetic field analysis of tubular linear induction motor for size reduction is conducted. Size reduction and improvement of air gap flux distribution is achieved by improved winding configuration, and analysis results are verified by finite element analysis (FEA) and experiments.

Air concentration and particle size distribution of wood dust during wood-working processes (나무 종류에 따른 공기중 분진 농도와 입경 분포에 관한 연구)

  • Kim, Seung Ki;Roh, Jaehoon;Kim, Chi Nyon
    • Journal of Korean Society of Occupational and Environmental Hygiene
    • /
    • v.9 no.2
    • /
    • pp.145-157
    • /
    • 1999
  • Wood dust is created when machines are used to cut or shape wood materials. Industries of high risk of wood dust exposure are sawmills, dimension mills, furniture industries, and carpenters, etc. Health effects associated with wood dust exposure includes dermatitis, allergic respiratory effects and cancer. Health effects of wood dus t are mainly depend on the concentration, dust size and exposure time. This study were carried out to evaluate the concentration and particle size distribution of wood dust during working processes. The subjects of this study were 53 workers exposed to wood dust in 7 furniture factories and 5 musical instruments, and 5 sawmill factories. The average total wood dust concentrations measured by personal cascade impactor were $1.82{\pm}2.31mg/m^3$ in primary manufacture, $3.59{\pm}1.72mg/m^3$ in s econdary manufacture, $5.09{\pm}1.46mg/m^3$ in sanding operation. Mass median diameters of hardwoods dust were $3.36{\mu}m$ in primary manufacture, $4.25{\mu}m$ in secondary manufacture, $4.21{\mu}m$ in sanding operation. softwoods dust were $3.39{\mu}m$ in primary manufacture, $4.34{\mu}m$ in secondary manufacture. Particle size distributions showed a nearly the same pattern in each working processes. The sample concentration of all hardwood dust exceeded the Threshold Limit Value(TLV) and 20.8% of the softwood dust exceeded the Threshold Limit Value. The range of size distribution were $0.5-10{\mu}m$ in the soft and hardwood dust. The respirable dust of soft and hardwood took up 59% and above. Therefore new threshold limit value for wood dust should be needed in Korea. Also, it should be done for various studies on health effects related to occupational exposure of wood dust.

  • PDF

Is "Initial Size of the Graft the Real Culprit behind Primary Contraction of Full-Thickness Skin Graft"?-A Cross-Sectional Study

  • Madhubari Vathulya;Shalinee Rao;Akanksha Malik;Smita Sinha;Nikhilesh Kumar;Akshay Kapoor;Yogesh Bahurupi
    • Archives of Plastic Surgery
    • /
    • v.50 no.1
    • /
    • pp.106-115
    • /
    • 2023
  • Background Primary contraction of full-thickness graft has been traditionally quoted to be 40%. There are lacunae in literature to elaborate on the factors influencing it ever since. Methods About 75 subjects who underwent full-thickness grafting procedures to resurface small defects were included in the study. The initial and final graft dimensions after primary contraction were traced on X-ray templates and the percentage of contraction was evaluated using the graphical method. This was further correlated with age, collagen, elastic matrix metalloproteinases-1 (MMP-1) and -2 content along with dermal thickness of the skin specimen sent from the graft. Results The primary contraction of the graft had a very significant correlation only with the initial size of graft harvested with a linear regression of 33.3% and a Spearman's correlation of 0.587 significant at a p-value of 0.001. Conclusion This study though preliminary tries to highlight an important factor that primary contraction of grafts is a physical phenomenon independent of its contents like collagen, elastin, or MMP-1 and -2 or age and dependent on its initial size of harvest instead.

Microstructure of Semi-solid A356 Alloys made Using Cooling Plate (냉각판을 이용한 반응고 A356합금의 미세조직)

  • 엄정필;김득규;윤병은;임수근
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1997.06a
    • /
    • pp.148-159
    • /
    • 1997
  • In this study, microstructure, size of primary $\alpha$, solid fraction and hardness of A356 Al alloy, were investigated. Semi-solid A356 allos were obtained by semi-solid continuous casting apparatus consists of melting furnace, formation apparatus of granular primary $\alpha$ and continuous casting apparatus. Size of promary $\alpha$ and fraction solid were decreased with decreasing temperature, and with increasing volume of cooling water. At the cooling water temperature of 15$^{\circ}C$ and cooling water volume of 18.2$\ell$/min, the sizes of primary $\alpha$ phases were decreased up to 40${\mu}{\textrm}{m}$, and fraction solid was 0.68.

  • PDF

Preliminary Structural Sizing of the Co-axial Double-tube Type Primary Hot Gas Duct for the Nuclear Hydrogen Reactor (수소생산용 원자로에서 동심축 이중관형 1차 고온가스덕트의 예비 구조정산)

  • Song, Kee-nam;Kim, Y-W
    • Transactions of the Korean Society of Pressure Vessels and Piping
    • /
    • v.4 no.2
    • /
    • pp.1-6
    • /
    • 2008
  • Very High Temperature Gas Cooled Reactor (VHTR) has been selected as a high energy heat source for nuclear hydrogen generation. The VHTR can produce hydrogen from heat and water by using a thermo-chemical process or from heat, water, and natural gas by steam reformer technology. A co-axial double-tube primary hot gas duct (HGD) is a key component connecting the reactor pressure vessel and the intermediate heat exchanger (IHX) for the VHTR. In this study, a preliminary design analysis for the primary HGD of the nuclear hydrogen system was carried out. These preliminary design activities include a determination of the size, a strength evaluation and an appropriate material selection. The determination of the size was undertaken based on various engineering concepts, such as a constant flow velocity model, a constant flow rate model, a constant hydraulic head model, and finally a heat balanced model.

  • PDF

Comparison of Magnesium Hydroxide Particles by Precipitation and Hydrothermal Treatment for Flame Retardant Application to Low Density Polyethylene and Ethylene-Co-Vinyl Acetate Resin (침전법과 수열처리로 제조된 수산화마그네슘 비교와 이의 저밀도 폴리에틸렌-에틸렌 비닐 아세테이트 수지 난연제 적용)

  • Hyun, Mi Kyung;Lim, Hyung Mi;Yoon, Joonho;Lee, Dong Jin;Lee, Seung-Ho;Whang, Chin Myung;Jeong, Sang Ok
    • Applied Chemistry for Engineering
    • /
    • v.20 no.2
    • /
    • pp.234-240
    • /
    • 2009
  • $Mg(OH)_2$ particles were prepared by precipitation and a hydrothermal treatment to examine the effect of $MgCl_2$ concentration, alkali type and concentration, temperature, hydrothermal treatment on the formation of $Mg(OH)_2$ particles using full factorial design, as one of DOE (Design of experiment) methods. The primary particle size is similar to the secondary particle size for the samples after the hydrothermal treatment, where the average particle size of $Mg(OH)_2$ increased with increasing the concentration of $MgCl_2$ and hydrothermal temperature and decreasing alkali/Mg molar ratio. On the other hand, for the samples prepared from precipitation, the secondary particle size is larger than the primary particles due to aggregation. The difference in alkaline source is that the particles prepared from $NH_4OH$ exhibit the larger size with better dispersion than those from NaOH. Low density polyethylene and ethylene-co-vinyl acetate (LDPE-EVA) resin composed of the smaller secondary particle size of $Mg(OH)_2$ shows a higher limited oxygen index (LOI) at 50 and 55% loading, but the smaller primary particle size may result in a better grade in UL-94 tests. At the high loading of 60%, all samples with any preparation methods exhibit V-0 grade but the LOI value depends on not only primary particle size but also dispersion state.

The Effect of Electromagnetic Stirring on the Semi-Solid Microstructure of Cu-0.15wt%Zr Alloy (전자교반에 의한 Cu-0.5wt%Zr 합금의 반응고 조직제어에 관한 연구)

  • Lim, Sung-Chul;Lee, Heung-Bok;Kim, Kyung-Hoon;Kwon, Hyuk-Chon;Yoon, Eui-Pak
    • Journal of Korea Foundry Society
    • /
    • v.26 no.1
    • /
    • pp.40-45
    • /
    • 2006
  • Most of the work reported concerned the semi-solid processing of low melting point alloys, and in particular light alloys of aluminum and magnesium. The purpose of this paper is to develop a semi-solid microstructure of Cu alloys using electromagnetic stirring applicable for squirrel cage rotor of induction motor. The size of primary solid particle and the degree of sphericity as a function of the variation in cooling rate, stirring speed, and holding time were observed. By applying electromagnetic stirring, primary solid particles became finer and rounder relative to as-cast sample. As the input frequency increased from 30 to 40 Hz, particle size decreased. The size of primary solid particle was found to be decreased with increasing cooling rate. Also, it decreased with stirring up to 3 minutes but increased above that point. The degree of sphericity became closer to be 1 with hold time. Semi-solid microstructure of Cu alloys, one of the high melting point alloys, could be controlled by electromagnetic stirring.

Synthesis and Characterization of TiO2, Cu2O and Al2O3 Aerosol Nanoparticles Produced by the Multi-Spark Discharge Generator

  • Efimov, Alexey;Lizunova, Anna;Sukharev, Valentin;Ivanov, Victor
    • Korean Journal of Materials Research
    • /
    • v.26 no.3
    • /
    • pp.123-129
    • /
    • 2016
  • The morphology, crystal structure and size of aerosol nanoparticles generated by erosion of electrodes made of different materials (titanium, copper and aluminum) in a multi-spark discharge generator were investigated. The aerosol nanoparticle synthesis was carried out in air atmosphere at a capacitor stored energy of 6 J, a repetition rate of discharge of 0.5 Hz and a gas flow velocity of 5.4 m/s. The aerosol nanoparticles were generated in the form of oxides and had various morphologies: agglomerates of primary particles of $TiO_2$ and $Al_2O_3$ or aggregates of primary particles of $Cu_2O$. The average size of the primary nanoparticles ranged between 6.3 and 7.4 nm for the three substances studied. The average size of the agglomerates and aggregates varied in a wide interval from 24.6 nm for $Cu_2O$ to 46.1 nm for $Al_2O_3$.

Comparison of Crown Shape and Amount of Tooth Reduction for Primary Anterior Prefabricated Crowns (유전치 기성 크라운의 형태 및 치질 삭제량 비교)

  • Kim, Soyoung;Lim, Youjin;Lee, Sangho;Lee, Nanyoung;Jih, Myeongkwan
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.46 no.1
    • /
    • pp.64-75
    • /
    • 2019
  • The purpose of this study was to obtain instructions for size selection of prefabricated crown and tooth reduction by 3-dimensional analysis of the size and shape of the maxillary primary central and lateral incisors and prefabricated crowns (celluloid strip, resin veneered stainless steel, and zirconia crowns). The maxillary primary central and lateral incisors of 300 Korean children was scanned with three types of prefabricated crown to create standard three-dimensional tooth models and prefabricated crowns. The shapes of the prefabricated crowns and natural teeth were compared according to four parameters (mesio-distal width, height, labio-palatal width, and labial surface curvature coefficient) and calculated the amount of tooth reduction required for each prefabricated crown. The size 2 resin veneered stainless steel crown, size 1 zirconia crown, and size 2 celluloid strip crown were most similar in shape to the primary central incisor. The size 3 rein veneered stainless steel crown, size 2 zirconia crown, and size 3 celluloid strip crown were most similar to the primary lateral incisor. The amount of tooth reduction was similar in both maxillary primary central and lateral incisors. The incisal reduction was greatest for the zirconia crown. At the proximal surface, the zirconia and celluloid strip crowns required a similar amount of tooth reduction, but more than the resin veneered stainless steel crown. The labial surface reduction was greatest for the zirconia crown. The degree of lingual surface reduction was not significant among the three prefabricated crowns. Among the assessment parameters, mesio-distal crown width was the most important for choosing a prefabricated crown closest to the actual size of the natural crown.