Kim, Young-Sung;Lee, Choong-Sun;Kim, Ik-Joo;Ko, Hyung-Duk;Tai, Weon-Pil;Song, Yong-Jin;Suh, Su-Jeung
Journal of the Korean Crystal Growth and Crystal Technology
/
v.14
no.5
/
pp.187-192
/
2004
We try to use isopropanol which has low boiling point to prepare ZnO thin films at low temperature. ZnO thin films were prepared by sol-gel spin-coating method using zinc acetate dehydrate-isopropanol-monoethanolamine (MEA) solution. The c-axis preferred orientation and optical properties of ZnO films with preheating temperature have been investigated. ZnO thin films were preheated at 200 to $300^{\circ}C$ with an interval of $25^{\circ}C$ and post-heated at $650^{\circ}C$. The ZnO film preheated at $275^{\circ}C$ and post-heated at $650^{\circ}C$ was highly oriented along c-axis (002) plane, and the surface with homogeneous and dense microstructures was formed having nano-sized grains. The optical transmittance was above 90 % in the visible range and exhibited absorption edges at 368 nm wavelength.
Kim, Min-Ju;Kim, Jong-Yun;Jeong, Gi-Ho;Park, Chang-Sik
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.23
no.6
/
pp.458-463
/
2010
MLCC (multi-layer ceramic capacitor) is usually fabricated by lamination of predetermined number of single layers. Often, the state of MLCC before sintering is called the green state, whose strength comes from the adhesion between the dielectric material and the polymer binder. Therefore the lamination of a single layer before sintering can be easily deformed by environment due to the relatively lower strength. After the compression process, which helps single sheets cohereto with adjacent sheets, the MLCC green bar is preheated to resolve the probable internal stress. Unfortunately, unexpected deformation after preheating resulted in problems during cutting of the MLCC green bar. In this study, one of 2 primary hypotheses which were proposed to resolve the unexpected deformation after preheating was examined by quantitative experiment with GC/MS (gas chromatograpy/mass spectrometer). The proportion of deformation caused by DOP evaporation, which was primarily evaporated componet during preheating, to the total deformation of the MLCC green bar was found to be 53%.
The purpose of this study was to investigate the effects of preheating and salt concentration on the fermentation rate and firmness of cucumber kimchi, and the relationship between firmness and the contents of pectin fractions, hemicellulose and cellulose during fermentation. For this purpose, pH, acidity, firmness and the contents of pectic fractions, hemicellulose and cellulose were studied. 1. The changes of pH and titratable acidity indicated that preheating and high salt concentration delayed the fermentation rate in cucumber kimchi. 2. After 9 days, preheated cucumber kimchi was firmer than nonpreheated cucumber kimchi. 3. During fermentation, the cucumber kimchi fermented at 5% NaCl was firmer than that femented at 2% NaCl. 4. After 9 days, preheated cucumber kimchi was higher in insoluble pectin (HCISP)content and lower in soluble pectin (HWSP & HXSP) content than nonpreheated cucumberkimchi and hese results in accord with those of firmness measurements. 5. During fermentation, the cucumber kimchi fermented at 5% NaCl was higher in insoluble pectin content and lower in soluble pectin content than nonpreheated cucumber kimchi, and these results were in accord with those of firmness measurement. 6. During fermentation, cellulose content decreased.
Kim, Hyung-Seok;Han, Gi-Chun;Ahn, Ji-Whan;Park, Jae-Seok;Kim, Hwan;Kim, Kyung-Soo
Proceedings of the IEEK Conference
/
2001.10a
/
pp.571-575
/
2001
To examine the grinding effect through preheating of waste concrete as a way of retrieving coarse aggregates from waste concrete, the removal rates of cement mortar and paste of both recycled aggregates and heated and grinded ones were investigated. As the preheating temperature increased, the removal rate of cement mortar from waste concrete was raised, and this kind of removal hardly affected the abrasion rate and specific gravity of aggregates. On the other hand, when it was treated over 40$0^{\circ}C$ of preheating temperature, the absorptance was reduced to less than 2.17, and cement mortar was effectively separated from waste concrete. It could meet the Korean Standards on recycled aggregates for concrete, and it is expected to expand the scope of utilization by making it possible to retrieve the aggregates which have the properties close to natural aggregates.
In this study, an experimental apparatus has been designed and set-up to analyse the dissociating phenomena of hydrate in porous rock using electric heating method supplied at downhole. The electric heat injecting experiments have been performed to investigate the heat transfer within the core, the dissociating phenomena of hydrate, and the productivities of dissociated gas and water. These experiments were under constant heat injecting method as well as preheating methods. From the experimental results, it is seen that the hydrates is dissociated along the phase equilibrium curve and dissociation of hydrate is accelerated with heat. The injected heat is consumed for the dissociation and also it is lost together with outflow of the dissociated gas and water. From the investigation of gas producing behavior for various heat injecting methods, as the injected heat is greater, dissociation is accelerated faster at outlet and hence the initial gas production becomes higher. Also, it is shown that the initial gas productivity under the constant heating method is better, however, the energy efficiency is low because of smaller amount of the produced gas comparing to the amount of heat injected. In the experiments of preheating method, it was seen that gas production only initial stage is different with the preheating time, but the producing behaviors of gas production are similar.
Journal of the Korean Society of Manufacturing Technology Engineers
/
v.21
no.6
/
pp.988-997
/
2012
Laser surface hardening is one of core technologies to enhance various characteristics such as the strength, hardness, toughness, abrasion resistance, and fatigue resistance for the mold material. This paper focuses on testing characteristics of the laser heat treatment according to the preheating parameters in case of the SM45C medium carbon steel. In this paper, we assume that the power and travel speed of the laser are 1,800W and 0.5m/min, respectively, and the range of the preheating temperature is $50^{\circ}C{\sim}300^{\circ}C$. From the result of the test, we observed that the hardness width and depth are enhanced as the temperature is increased. Also, the best average hardness was 751.7Hv for the temperature of $100^{\circ}C$.
This study analyzed causes and status of cracks to suggest preventives for welding cracks generated on fillet welding zone of atmosphere corrosion resisting steel box girder. Penetrant testing, a sort of non-destructive testing, was conducted for inspection of crack status on welding zone. As a result of test, welding cracks were found on the point of start, center and end to fillet welding zone of 32 mm-thickness. The result of carbon equivalent composition of materials was 0.452%. According to welding specification, to preheat prevent welding crack, preheat temperature of $100{\sim}200^{\circ}C$ should be kept before welding execution. It was failed to keep preheat temperature because it had been executed on winter season and the structure of box girder had wide heat transfer area. As a result of examination of time varying preheating temperature of 32mm-thickness material, it was understood that preheat temperature of above $230^{\circ}C$ on both 130mm-long sides of welded joint can prevent welding crack.
The main objectives were to investigate the suitability of CaO crucible for melting TiAl alloys and to develop investment mold for investment casting of TiAl alloys. TiAl alloy specimen were prepared by plasma arc furnace under argon atmosphere. After melting of TiAl alloy using CaO crucible, the results showed that there is little contamination of oxygen in the TiAl bulk. Conventional vacuum induction furnaces can be readily adaptable to produce cast parts of TiAl without high skilled techniques. The determination of optical metallography and microhardness profiles in investment cast TiAl alloy rods has allowed the gradation of the relative thermal stability of the oxides examined. The molds used for the present study were $ZrO_2$, $Al_2O_3$, CaO stabilized $ZrO_2$ and $ZrSiO_4$. Even although high temperature of mold preheating, $Al_2O_3$ mold is a promising mold material for investment casting of TiAl alloys in terms of thermal stability, cost and handling strength. It is important to take thermal stability and preheating temperature of mold into consideration for investment casting of TiAl alloys.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2004.07a
/
pp.445-448
/
2004
Radio frequency and microwave dielectric heating are well-known electroheating methods, used in industrial applications where non electrically conducting materials are to be heated, dried or otherwise processed. The major reason for considering this technique for any process is based on its unique ability to transfer heat into the volume of an electrically non conducting material such as insulator directly, rather than, via a surface. Conventional heating must first bring heat to the product surface and there after it depends on the physical characteristics and condition of the material as to how effectively this heat is transmitted into the mass. The product would suffer surface damage before the main body is adequately processed. Dielectric heating is applied to enhance conventional heating methods and to drastically shorten the required processing duration. Although the use of dielectric heating has been a well proven technique for several years in some industries, its application in the preheating of FRP has been limited by the insufficient experience. In this paper a method is described for uniform radio frequency heating of preheating of FRP.
Journal of the Korean Society of Manufacturing Process Engineers
/
v.21
no.8
/
pp.99-109
/
2022
In this study, an electric resistance-heated surface friction spot-welding process was proposed and tested for the spot-welding ability of copper and aluminum dissimilar metal sheets using electric resistance heating and surface friction heating. This process has welding variables, such as the current value, energizing cycles, rotational speed, and friction time. The current value and energizing cycle can affect the resistance heat, and the rotational speed of the rotating pin and friction time influence frictional heat generation. Resistance heating before friction heating has a preheating effect on the Cu-Al contact interface and a positive effect on preventing friction heat loss during the friction stage. However, because resistance preheating can soften the copper sheet and affect the contact stress and friction coefficient, it has difficulties that may adversely affect frictional heat generation. Therefore, the optimal combination of welding variables should be determined through simulations and experiments of the spot-welding process to determine the effects of electric resistance preheating on the suggested process. Through this procedure, it is known that the proposed spot-welding process can improve the welding quality during the spot welding of Cu-Al sheets.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.