Polyvinyl Alcohol 폴리머 용액법으로 합성한 스포듀민 분말의 특성연구 (Characteristics of Spodumene Powders Synthesized by Polyvinyl Alcohol Solution Technique)

  • 이상진;박지은
    • 한국분말재료학회지
    • /
    • 제18권1호
    • /
    • pp.35-40
    • /
    • 2011
  • LAS-system ceramic powder, spodumene ($Li_2O{\cdot}Al_2O_3{\cdot}4SiO_2$), was successfully synthesized by a chemical solution technique employing PVA(polyvinyl alcohol) as an organic carrier. The PVA content affected the microstructure of porous precursor gels and the crystalline development. The optimum PVA content contributed to homogeneous distribution of metal ions in the precursor gel and it resulted in the synthesis of glass free $\beta$-spodumene powder having a specific surface area of $7.57\;m^2/g$. The agglomerated $\beta$-spodumene powders were also enough soft to grind to fine powders by a simple ball milling process. The microstructures of the densified powder compacts were strongly dependant on the minor phases of spodumene solid solution and amount of liquid phase, which were formed from the inhomogeneous precursors.

동테이프 위의 Bi-계 초전도 후막에서 전구체분말 조성의 영향 (The Effect of the precursor powder composition for Bi-system superconducting thick films on Cu tapes)

  • 한상철;성태현;한영희;이준성;김상준
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 춘계학술대회 논문집
    • /
    • pp.65-68
    • /
    • 1999
  • A well oriented Bi2212 superconductor thick films were fabricated by screen printing with a Cu-free Bi-Sr-Ca-O mixture powder on a copper plate and heat-treating at 820-88$0^{\circ}C$ for several minute in air. During the heat-treatment, the printing layer partially melted by reaction between the Cu-free precursor and CuO of the oxidizing copper plate. In the partial melting state, it is believed that the solid phase is Bi-free phase and Cu-rich phase and the composition of the liquid is around Bi : Sr : Ca : Cu = 2 : 2 : 0 : 1. Following the partial melting, the Bi2212 superconducting phase is formed at Bi-free phase/liquid interface by nucleation and grows. With decreasing the Bi composition in the precursor powder, the critical temperature(T$_{c}$) of the fabricated Bi2212 thick film increased to about 79 K.K.

  • PDF

Characteristics of Porous YAG Powders Fabricated by PVA Polymer Solution Technique

  • Lee, S.J.;Shin, P.W.;Kim, J.W.;Chun, S.Y.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.438-439
    • /
    • 2006
  • Pure and stable YAG $(Y_3Al_5O_{12})$ powders were synthesized by a PVA (polyvinyl alcohol) polymer solution technique. PVA was used as an organic carrier for the precursor ceramic gel. The precursor gels were crystallized to YAG at relatively a low temperature of $900\;^{\circ}C$. The synthesized powders, which have nano-sized primary particles, were soft and porous, and the porous powders were ground to sub-micron size by a simple ball milling process. The ball-milled powders were densified to 94% relative density at $1500\;^{\circ}C$ for 1h. In this study, the characteristics of the synthesized YAG powders were examined.

  • PDF

Bi-2223/Ag 선재의 전구 분말에서 수분함량에 따른 효과 (The effects of moisture content in precursor powder for Bi-2223/Ag tape)

  • 김성환;유재무;고재웅;김영국;김철진
    • Progress in Superconductivity
    • /
    • 제4권2호
    • /
    • pp.162-167
    • /
    • 2003
  • The critical current value of Bi-2223/Ag tape can be influenced by various factors. In particular, it was known that properties of precursor powders could affect the formation of Bi -2223 and grain growth rate of the same. Since, moistures and organic matters can easily contaminate the precursor powders of Bi-2223 tapes and degrade properties of superconductors, the precursor powders should be kept in optimal conditions to minimize contamination. In this study, the effect of moisture and organic matters has been investigated. A Bi-2223/Ag tape contaminated with a large amount of moisture and organic matter has been characterized by low critical current values and bubbling. It has been found that as the quantity of moisture increases, the Bi-2223 phases are formed at lower temperature and the amount of non-superconducting phase increases.

  • PDF

요소를 이용한 활성 이트리아 분말의 합성 (Synthesis of Sinter-active $Y_2O_3$ Powders Using Urea)

  • 한주환
    • 한국세라믹학회지
    • /
    • 제34권12호
    • /
    • pp.1247-1253
    • /
    • 1997
  • Sinter-active yttria powders were prepared by a solution precipitation with using a self-decomposing precipitation agent NH2CONH2(urea). The cold-pressed powders can be sintered to full density and the microstructure of grains less than 200 nm at a temperature as low as 120$0^{\circ}C$. The activity of the yttria powder has been controlled by varying nucleation conditions during precipitation and by minimizing formation of aggregates. The type of precursor is decisive in preparation of a sinter-active oxide powder, and urea is desirable as a precipitation agent for an active yttrium oxide powder.

  • PDF

분무건조된 Nd-Fe-B 전구체 입자의 크기조절 및 환원-확산 후 자기 특성에 미치는 영향 (Size Control of Nd-Fe-B Precursor Particles Prepared by Spray Drying and Its Effect on the Magnetic Properties of Nd-Fe-B Alloy Powders after Reduction-Diffusion)

  • 백연경;서영택;이정구;김동수;배동식;최철진
    • 한국분말재료학회지
    • /
    • 제20권5호
    • /
    • pp.359-365
    • /
    • 2013
  • In this study, we fabricated $Nd_2Fe_{14}B$ hard magnetic powders with various sizes via spray drying combined with reduction-diffusion process. Spray drying is widely used to produce nearly spherical particles that are relatively homogeneous. Thus, the precursor particles were prepared by spray drying using the aqueous solution containing Nd salts, Fe salts and boric acid with the target stoichiometric composition of $Nd_2Fe_{14}B$. The mean particle sizes of the spray-dried powders are in the range from one to seven micrometer, which are adjusted by controlling the concentrations of precursor solutions. After debinding the as-prepared precursor particles, ball milling was also conducted to control the particle sizes of Nd-Fe-B oxide powders. The resulting particles with different sizes were subjected to subsequent treatments including hydrogen reduction, Ca reduction and washing for CaO removal. The size effect of Nd-Fe-B oxide particles on the formation of $Nd_2Fe_{14}B$ phase and magnetic properties was investigated.

RF 유도 열플라즈마를 이용한 유기 용매로 부터의 탄화규소 나노 분말 합성 (Synthesis of Silicon Carbide Nano-Powder from a Silicon-Organic Precursor by RF Inductive Thermal Plasma)

  • 고상민;구상만;김진호;조우석;황광택
    • 한국세라믹학회지
    • /
    • 제49권6호
    • /
    • pp.523-527
    • /
    • 2012
  • Silicon carbide (SiC) has recently drawn an enormous amount of industrial interest due to its useful mechanical properties, such as its thermal resistance, abrasion resistance and thermal conductivity at high temperatures. In this study, RF thermal plasma (PL-35 Induction Plasma, Tekna CO., Canada) was utilized for the synthesis of high-purity SiC powder from an organic precursor (hexamethyldisilazane, vinyltrimethoxysilane). It was found that the SiC powders obtained by the RF thermal plasma treatment included free carbon and amorphous silica ($SiO_2$). The SiC powders were further purified by a thermal treatment and a HF treatment, resulting in high-purity SiC nano-powder. The particle diameter of the synthesized SiC powder was less than 30 nm. Detailed properties of the microstructure, phase composition, and free carbon content were characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), a thermogravimetric (TG) analysis, according to the and Brunauer-Emmett-Teller (BET) specific surface area from N2 isotherms at 77 K.