• Title/Summary/Keyword: Precursor Powder

Search Result 344, Processing Time 0.023 seconds

Fruits Extracts Mediated Synthesis of Zinc Oxide Nanoparticles Using Rubus coreanus and its Catalytic Activity for Degradation of Industrial Dye

  • Rupa, Esrat Jahan;Gokulanathan, Anandapadmanaban;Ahn, Jong-Chan;Mathiyalagan, Ramya;Markus, Josua;Elizabeth, Jimenez Perez Zuly;Soshnikova, Veronika;Kim, Yeon-Ju;Yang, Deok-Chun
    • Proceedings of the Plant Resources Society of Korea Conference
    • /
    • 2018.04a
    • /
    • pp.93-93
    • /
    • 2018
  • This study disclosed the aqueous fruits extract of Rubus coreanus as a sustainable agent for the synthesis of Rubus coreanus zinc oxide nanoparticle (Rc-ZnO Nps) using as a reducing and capping precursor for co-precipitation method. The development of Rc-ZnO was assured by white precipitated powder and analyzed by spectroscopic and analytical instruments. The UV-visible (UV-Vis) studies indicate the maximum absorbance at 357nm which confirmed the formation of ZnO Nps and the purity, functional group and monodispersity were assured by field emission transmission electron microscopy (FE-TEM), Fourier Transform Infrared (FTIR) Spectroscopy and dynamic light scattering (DLS). The X-ray powder diffraction (XRD) data revealed the Nps is 23.16 nm in size, crystalline in nature and possess hexagonal wurtzite structure. The Rc-ZnO Nps were subjected for catalytic studies. The Malachite Green dye was degraded by Rc- ZnO NPs in both dark and light (100 W tungsten) conditions and it degraded about 90% at 4 hours observation in both cases. The biodegradable, low cost Rc-ZnO NPs can be a better weapon for waste water treatment.

  • PDF

Fabrication of Cu2SnS3 (CTS) thin Film Solar Cells by Sulfurization of Sputtered Metallic Precursors (스퍼터법을 이용한 메탈 전구체기반의 Cu2SnS3 (CTS) 박막 태양전지 제조 및 특성 평가)

  • Lee, Ju Yeon;Kim, In Young;Minhao, Wu;Moon, Jong Ha;Kim, Jin Hyeok
    • Current Photovoltaic Research
    • /
    • v.3 no.4
    • /
    • pp.135-139
    • /
    • 2015
  • $Cu_2SnS_3$ (CTS) based thin film solar cells (TFSCs) are of great interest because of its earth abundant, low-toxic and eco-friendly material with high optical absorption coefficient of $10^4cm^{-1}$. In this study, the DC sputtered precursor thin films have been sulfurized using rapid thermal annealing (RTA) system in the graphite box under Ar gas atmosphere for 10 minute. The systematic variation of sulfur powder during annealing process has been carried out and their effects on the structural, morphological and optical properties of CTS thin films have been investigated. The preliminary power conversion efficiency of 1.47% with a short circuit current density of $33.9mA/cm^2$, an open circuit voltage of 159.7 mV, and a fill factor of 27% were obtained for CTS thin film annealed with 0.05g of S powder, although the processing parameter s have not yet been optimized.

Thermal Stability of Furfuryl Alcohol/Graphite Powder Mixtures for Impregnation of Carbonaceous Composite (탄화복합재료 함침을 위한 퍼퓨릴알콜/흑연분말 혼합물의 열안정성)

  • An, Yeong-Seok;Jo, Dong-Hwan
    • Korean Journal of Materials Research
    • /
    • v.8 no.4
    • /
    • pp.299-303
    • /
    • 1998
  • We examined, using thermoanalytical methods, the effects of $2000^{\circ}C$ heat-treated graphite powders and heating rate of cure after impregnation on the thermal stability and carbon yield of furfuryl alcohol, which is frequently used not only as an impregnant but also as a matrix precursor for carbon fiber-reinforced carbon composites. It was founded that the addition of 30wt% graphite powders to furfuryl alcohol and the heating rate of $35^{\circ}C$/min showed the highest thermal stability of furfuryl alcohol/graphite powder mixture. The carbon yield above $1000^{\circ}C$ was enhanced more than 10% in comparison with the absence of graphite powders. It would be expected that this result can contribute to some extent to reduce the repeating number of processing cycle (carbonization-impregnation-cure-re-carbonization) required to densify a carbonaceous composite.

  • PDF

Effect of Li2O-Bi2O3 Addition on the Piezoelectric Properties of Pb(Mg1/3Nb2/3)0.65Ti0.35O3 Ceramics (Li2O-Bi2O3 첨가가 Pb(Mg1/3Nb2/3)0.65Ti0.35O3 세라믹의 압전 특성에 미치는 영향)

  • Kim, Jae Hyuk;Kim, Shi Yeon;Choi, Jeoung Sik;Yeo, Dong-Hun;Shin, Hyo-Soon;Nahm, Sahn
    • Journal of Powder Materials
    • /
    • v.26 no.5
    • /
    • pp.405-409
    • /
    • 2019
  • Piezoelectric ceramic specimens with the $Pb(Mg_{1/3}Nb_{2/3})_{0.65}Ti_{0.35}O_3$ (PMN-PT) composition are prepared by the solid state reaction method known as the "columbite precursor" method. Moreover, the effects of the $Li_2O-Bi_2O_3$ additive on the microstructure, crystal structure, and piezoelectric properties of sintered PMN-PT ceramic samples are investigated. The addition of $Li_2O-Bi_2O_3$ lowers the sintering temperature from $1,200^{\circ}C$ to $950^{\circ}C$. Moreover, with the addition of >5 wt.% additive, the crystal structure changes from tetragonal to rhombohedral. Notably, the sample with 3 wt.% additive exhibits excellent piezoelectric properties ($d_{33}=596pC/N$ and Kp = 57%) and a sintered density of $7.92g/cm^3$ after sintering at $950^{\circ}C$. In addition, the sample exhibits a curie temperature of $138.6^{\circ}C$ at 1 kHz. Finally, the compatibility of the sample with a Cu electrode is examined, because the energy-dispersive X-ray spectroscopy data indicate the absence of interdiffusion between Cu and the ceramic material.

Effect of Pyrolysis temperature on TiO2 Nanoparticles Synthesized by a Salt-assisted Ultrasonic Spray Pyrolysis Process (염 보조 초음파 분무 열분해 공정으로 합성된 TiO2 나노입자의 특성에 열분해 온도가 미치는 영향)

  • Yoo, Jae-Hyun;Ji, Myeong-Jun;Park, Woo-Young;Lee, Young-In
    • Journal of Powder Materials
    • /
    • v.26 no.3
    • /
    • pp.237-242
    • /
    • 2019
  • In this study, ultrasonic spray pyrolysis combined with salt-assisted decomposition, a process that adds sodium nitrate ($NaNO_3$) into a titanium precursor solution, is used to synthesize nanosized titanium dioxide ($TiO_2$) particles. The added $NaNO_3$ prevents the agglomeration of the primary nanoparticles in the pyrolysis process. The nanoparticles are obtained after a washing process, removing $NaNO_3$ and NaF from the secondary particles, which consist of the salts and $TiO_2$ nanoparticles. The effects of pyrolysis temperature on the size, crystallographic characteristics, and bandgap energy of the synthesized nanoparticles are systematically investigated. The synthesized $TiO_2$ nanoparticles have a size of approximately 2-10 nm a bandgap energy of 3.1-3.25 eV, depending on the synthetic temperature. These differences in properties affect the photocatalytic activities of the synthesized $TiO_2$ nanoparticles.

Synthesis and Optical Property of TiO2 Nanoparticles Using a Salt-assisted Ultrasonic Spray Pyrolysis Process (염 보조 초음파 분무 열분해법을 이용한 TiO2 나노입자의 합성 및 광학적 성질)

  • Ji, Myeong-Jun;Park, Woo-Young;Yoo, Jae-Hyun;Lee, Young-In
    • Journal of Powder Materials
    • /
    • v.26 no.1
    • /
    • pp.34-39
    • /
    • 2019
  • Current synthesis processes for titanium dioxide ($TiO_2$) nanoparticles require expensive precursors or templates as well as complex steps and long reaction times. In addition, these processes produce highly agglomerated nanoparticles. In this study, we demonstrate a simple and continuous approach to synthesize $TiO_2$ nanoparticles by a salt-assisted ultrasonic spray pyrolysis method. We also investigate the effect of salt content in a precursor solution on the morphology and size of synthesized products. The synthesized $TiO_2$ nanoparticles are systematically characterized by X-ray diffraction, transmission electron micrograph, and UV-Vis spectroscopy. These nanoparticles appear to have a single anatase phase and a uniform particle-size distribution with an average particle size of approximately 10 nm. By extrapolating the plots of the transformed Kubelka-Munk function versus the absorbed light energy, we determine that the energy band gap of the synthesized $TiO_2$ nanoparticles is 3.25 eV.

Fabrication of Molybdenum Alloys with Improved Fracture Toughness through the Dispersion of Lanthanum Oxide (란타넘 산화물의 분산을 통해 향상된 파괴인성을 갖는 몰리브데넘 합금의 제조)

  • Choi, Won June;Park, Chun Woong;Park, Jung Hyo;Kim, Young Do;Byun, Jongmin
    • Journal of Powder Materials
    • /
    • v.26 no.3
    • /
    • pp.208-213
    • /
    • 2019
  • In this study, lanthanum oxide ($La_2O_3$) dispersed molybdenum ($Mo-La_2O_3$) alloys are fabricated using lanthanum nitrate solution and nanosized Mo particles produced by hydrogen reduction of molybdenum oxide. The effect of $La_2O_3$ dispersion in a Mo matrix on the fracture toughness at room temperature is demonstrated through the formation behavior of $La_2O_3$ from the precursor and three-point bending test using a single-edge notched bend specimen. The relative density of the $Mo-0.3La_2O_3$ specimen sintered by pressureless sintering is approximately 99%, and $La_2O_3$ with a size of hundreds of nanometers is uniformly distributed in the Mo matrix. It is also confirmed that the fracture toughness is $19.46MPa{\cdot}m^{1/2}$, an improvement of approximately 40% over the fracture toughness of $13.50MPa{\cdot}m^{1/2}$ on a pure-Mo specimen without $La_2O_3$, and this difference in the fracture toughness occurs because of the changes in fracture mode of the Mo matrix caused by the dispersion of $La_2O_3$.

A Study on the Microstructure and Physical Properties of Cold Sprayed Cu/CNT Composite Coating (저온 분사 코팅법으로 제조된 Cu/CNT 복합 코팅층의 미세조직 및 물성 연구)

  • Kwon, Seong-Hee;Park, Dong-Yong;Lee, Dae-Yeol;Euh, Kwang-Jun;Lee, Kee-Ahn
    • Korean Journal of Metals and Materials
    • /
    • v.46 no.3
    • /
    • pp.182-188
    • /
    • 2008
  • Carbon nanotubes(CNTs) have outstanding mechanical, thermal, and electrical properties. Thus, by placing nanotubes into appropriate matrix, it is postulated that the resulting composites will have enhanced properties. Cold spray can produce thick metal-based composite coatings with very high density, low oxygen content, and phase purity, which leads to excellent physical properties. In this study, we applied cold spray coating process for the consolidation of Cu/CNT composite powder. The precursor powder mixture, in which CNTs were filled into copper particles, was prepared to improve the distribution of the CNT in copper matrix. Pure copper coating was also conducted by cold spraying as a reference. Annealing heat treatment was applied to the coating to examine its effect on the properties of the composite coating. The hardness of Cu/CNT composite coating represented similar value to that of pure copper coating. It was importantly found that the electrical conductivity of the Cu/CNT composite coating significantly increased from 53% for the standard condition to almost 55% in the optimized condition, taking annealed ($500^{\circ}C/1hr$.) copper coating as a reference (100%). The thermal conductivity of Cu/CNT composite coating layer was higher than that of pure Cu coating. It was also found that the electrical and thermal conductivities of Cu/CNT composite could be improved through annealing heat treatment. The microstructural evolution of Cu/CNT coating was also investigated and related to the macroscopic properties.

Size Control of Iron Oxide (Fe3O4) Nanoclusters according to Reaction Factors and Consequent Change in Their Magnetic Attraction (반응 인자 제어에 의한 산화철(Fe3O4) 나노클러스터의 크기와 자기 특성 조절)

  • Sanghoon Lee;Arim Byun;Jin-sil Choi
    • Journal of Powder Materials
    • /
    • v.30 no.4
    • /
    • pp.297-304
    • /
    • 2023
  • Iron oxide (Fe2O3) nanoclusters exhibit significant potential in the biomedical and pharmaceutical fields due to their strong magnetic properties, stability in solutions, and compatibility with living systems. They excel in magnetic separation processes, displaying high responsiveness to external magnetic fields. In contrast to conventional Fe2O3 nanoparticles that can aggregate in aqueous solutions due to their ferrimagnetic properties, these nanoclusters, composed of multiple nanoparticles, maintain their magnetic traits even when scaled to hundreds of nanometers. In this study, we develop a simple method using solvothermal synthesis to precisely control the size of nanoclusters. By adjusting precursor materials and reducing agents, we successfully control the particle sizes within the range of 90 to 420 nm. Our study not only enhances the understanding of nanocluster creation but also offers ways to improve their properties for applications such as magnetic separation. This is supported by our experimental results highlighting their size-dependent magnetic response in water. This study has the potential to advance both the knowledge and practical utilization of Fe2O3 nanoclusters in various applications.

Microstructure of ZnO Thin Film on Nano-Scale Diamond Powder Using ALD (나노급 다이아몬드 파우더에 ALD로 제조된 ZnO 박막 연구)

  • Park, S.J.;Song, S.O.
    • Journal of the Korean Vacuum Society
    • /
    • v.17 no.6
    • /
    • pp.538-543
    • /
    • 2008
  • Recently a nano-scale diamond is possible to manufacture forms of powder(below 100 nm) by new processing of explosion or deposition method. Using a sintering of nano-scale diamond is possible to manufacture of grinding tools. We have need of a processing development of coated uniformly inorganic to prevent an abnormal grain growth of nano-crystal and bonding obstacle caused by sintering process. This paper, in order to improve the sintering property of nano-scale diamond, we coated ZnO thin films(thickness: $20{\sim}30\;nm$) in a vacuum by ALD(atomic layer deposition) Economically, in order to deposit ZnO all over the surface of nano-scale diamond powder, we used a new modified fluidized bed processing replaced mechanical vibration effect or fluidized bed reactor which utilized diamond floating owing to pressure of pulse(or purge) processing after inserted diamond powders in quartz tube(L: 20 mm) then closed quartz tube by porosity glass filter. We deposited ZnO thin films by ALD in closed both sides of quartz tube by porosity glass filter by ALD(precursor: DEZn($C_4H_{10}Zn$), reaction gas: $H_2O$) at $10^{\circ}C$(in canister). Processing procedure and injection time of reaction materials set up DEZn pulse-0.1 sec, DEZn purge-20 sec, $H_2O$ pulse-0.1 sec, $H_2O$ purge-40 sec and we put in operation repetitive 100 cycles(1 cycle is 4 steps) We confirmed microstructure of diamond powder and diamond powder doped ZnO thin film by TEM(transmission electron microscope) Through TEM analysis, we confirmed that diamond powder diameter was some $70{\sim}120\;nm$ and shape was tetragonal, hexagonal, etc before ALD. We confirmed that diameter of diamond powders doped ZnO thin film was some $70{\sim}120\;nm$ and uniform ZnO(thickness: $20{\sim}30\;nm$) thin film was successfully deposited on diamond powder surface according to brightness difference between diamond powder and ZnO.