• 제목/요약/키워드: Powder Forging Process

검색결과 38건 처리시간 0.038초

HIP(열간 등방압) 공정을 이용한 압연 롤 제조 공정의 해석 메커니즘 (Analysis Mechanism of Roll Forming Manufacturing Process using HIP (Hot Isostatic Press) Process)

  • 김웅
    • 소성∙가공
    • /
    • 제32권3호
    • /
    • pp.114-121
    • /
    • 2023
  • During rolling, rolling mill rolls endure wear when shaping metal billets into a desired form, such as bars, plates, and shapes. Such wear affects the lifespan of the rolls and product quality. Therefore, in addition to rigidity, wear performance is a key factor influencing the performance of rolling mill rolls. Conventional methods such as casting and forging have been used to manufacture rolling mill rolls. However, powder alloying methods are increasingly being adopted to enhance wear resistance. These powder manufacturing methods include atomization, canning to shape the powder, hot isostatic pressing to combine the powder alloy with conventional metals, and various wear performance tests on rolls prepared with powder alloys. In this study, numerical simulations and experimental tests were used to develop and elucidate the wear analysis mechanism of rolling mill rolls. The wear characteristics of the rolls under various rolling conditions were analyzed. In addition, experimental tests (wear and surface analysis tests) and wear theory (Archard wear model) were used to evaluate wear. These tests were performed on two different materials in various powder states to evaluate the different aspects of wear resistance. In particular, this study identifies the factors influencing the wear behavior of rolling mill rolls and proposes an analytical approach based on the actual production of products. The developed wear analysis mechanism can serve the future development of rolls with high wear resistance using new materials. Moreover, it can be applied in the mechanical and wear performance testing of new products.

클러치 디스크용 분말야금 스플라인 허브의 기계적성질에 관한 연구 (Study on the Mechanical Properties of Power Metallurgy Spline Hub for Clutch Disc)

  • 최문일;장진호;강성수
    • 한국자동차공학회논문집
    • /
    • 제6권5호
    • /
    • pp.104-110
    • /
    • 1998
  • In automotive industries, various processes for the cost reduction have been investigated lively. As one of them, powder metallurgy becomes influential. Compared to other methods used for he manufacture of steel components the Powder metallurgy process is competitive primarily due to the small number of production steps to reach the final geometry and thereby also the energy-efficiency. In this paper, to alter present forging process into powder metallurgy process by which the automotive clutch disc spline hub is manufactured machining process, the mechanical properties of sintered materials is investigated by specimen test. Selecting the 3 kinds of materials-SMF 4040, SMF 9060 and DHP-1, their properties according to heat treatment such as carburizing -tempering and plasma-nitrodizing are compared. By result of specimen test - tensile test, compression ring test, Impacting test, measurment of hardness, and microstructure analysis - we concluded that SMF 9060 and carburizing-tempering heat treatment is an optimal material and heat treatment method for the spline hub. It will be able to reduce manufacturing cost and weight.

  • PDF

Numerical simulation of dimensional changes during sintering of tungsten carbides compacts

  • Bouvard, D.;Gillia, O.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 1997년도 추계학술강연 및 발표대회 강연 및 발표논문 초록집
    • /
    • pp.7-7
    • /
    • 1997
  • During sintering of very porous green bodies, as obtained by compaction of hard powders - such as tungsten carbide or ceramics - or by injection moulding, important shrinkage occurs. Due to heterogeneous green density field, gravity effects, friction on the support, thermal gradients, etc., this shrinkage is often non-uniform, which' may induce significant shape changes. As the ratio of compact dimension to powder size is very high, the mechanics of continuum is relevant to model such phenomena. Thus numerical techniques, such as the finite element method can be used to simulate the sintering process and predict the final shape of the sintered part. Such type of simulation has much been developed in the last decade firstly for hot isostatic pressing and next for die compaction. Finite element modelling has been recently applied to free sintering. The simulation of sintering should be based on constitutive equations describing the thermo-mechanical behaviour of the material under any state of stress and any temperature which may arise within the sintering body. These equations can be drawn either from experimental data or from micromechanical models. The experiments usually consist in free sintering and sinter-forging tests. Indeed applying more complex loading conditions at high temperature under controlled atmosphere is delicate. Micromechanical models describe the constitutive behaviour of aggregates of spheres from the deformation of two-sphere contact either by viscous flow or grain boundary diffusion. Such models are not able to describe complex microstructure and mechanisms as observed in real materials but they can give some basic information on the formulation of constitutive equations. Practically both experimental and theoretical approaches can be coupled to identify the constitutive equations. Such procedure has been performed for modelling the sintering of compacts obtained by die pressing of a mixture of tungsten carbide and cobalt powders. The constitutive behaviour of this material during sintering has been described by a linear viscous constitutive model, whose functions have been fitted from results of free sintering and sinter-forging experiments. This model has next been introduced in ABAQUS finite element code to simulate the sintering of heterogeneous green compacts of various geometries at constant temperature. Examples of simulations are shown and compared with experiments.

  • PDF

금속 적층제조기술의 국내외 개발동향과 기술적 이슈 (International Development Trend and Technical Issues of Metal Additive Manufacturing)

  • 강민철;예대희;고근호
    • Journal of Welding and Joining
    • /
    • 제34권4호
    • /
    • pp.9-16
    • /
    • 2016
  • Metal parts are produced by conventional methods such as casting, forging and cutting, extrusion, etc. However, nowadays, with additive manufacturing (AM), it is possible to directly commercialize by means of stacking of equipment to the 3D drawing and use of high precision tools such as laser source. Thus, drawing of materials is an important aspect in delivering good products. AM deals with production of lighter aircraft parts and few more three-dimensional molds, it wish to manufacture special medical parts and want to steadily expand the new market area. The cost of related equipment and materials are still expensive and difficult to obtain on a mass production. However, the ability to make changes and lead the innovation in the paradigm of traditional manufacturing process is still effective. In this paper, we introduce metal AM and the principles of the related devices, metal powder production process, and their application.

산화물환원과 압축성형 공정에 의한 Bi2Te2.5Se0.5 화합물의 제조와 열전특성 (Fabrication of Bi2Te2.5Se0.5 by Combining Oxide-reduction and Compressive-forming Process and Its Thermoelectric Properties)

  • 임영수;이길근
    • 한국분말재료학회지
    • /
    • 제31권1호
    • /
    • pp.50-56
    • /
    • 2024
  • We report the effect of plastic deformation on the thermoelectric properties of n-type Bi2Te2.5Se0.5 compounds. N-type Bi2Te2.5Se0.5 powders are synthesized by an oxide-reduction process and consolidated via spark-plasma sintering. To explore the effect of plastic deformation on the thermoelectric properties, the sintered bodies are subjected to uniaxial pressure to induce a controlled amount of compressive strains (-0.2, -0.3, and -0.4). The shaping temperature is set using a thermochemical analyzer, and the plastic deformation effect is assessed without altering the material composition through differential scanning calorimetry. This strategy is crucial because the conventional hot-forging process can often lead to alterations in material composition due to the high volatility of chalcogen elements. With increasing compressive strain, the (00l) planes become aligned in the direction perpendicular to the pressure axis. Furthermore, an increase in the carrier concentration is observed upon compressive plastic deformation, i.e., the donor-like effect of the plastic deformation in n-type Bi2Te2.5Se0.5 compounds. Owing to the increased electrical conductivity through the preferred orientation and the donor-like effect, an improved ZT is achieved in n-type Bi2Te2.5Se0.5 through the compressive-forming process.

Spray conversion 법으로 제조된 W/Cu 나노복합분말의 소결특성 및 단조특성 평가 (Estimaion of the sintering and forging characteristics of the W/Cu nanocomposite powders produced by the spray conversion process)

  • 김태형;노준웅;김은표
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2002년도 추계학술강연 및 발표대회
    • /
    • pp.36-36
    • /
    • 2002
  • 최근 한국기계연구원에서 개발된 Mechanochemical process (MCP)는 Spray conversion 법에 의하여 나노크기의 W/Cu 복합 분말을 제조하는 방법으로서, 현재 (주)나노테크에서 산업화를 위한 시험/개발이 진행 중이다. 이 방법에 의하여 W /1 0 ~ 40wt. %Cu 조성의 초미렵 W/Cu 복합 분말의 양산화가 가능하게 됨으로써, 나노복합분말을 사용한 초미립 W/Cu 합금의 소결 제조 연구 역시 나 노태크에서 분말사업화와 동시에 수행되고 있다. 현재 Spray conversion 법으로 제조되고 있는 W/Cu 나노복합분말 및 그 소결체는 Cu의 조성범 위에 따라 민수용 및 군수용 제품으로의 적용이 시도되고 있으며, 각기 특성향상을 목표로 각 적용 분야에서 요구되는 제반 성능에 대한 검토가 이루어지고 있다. 특히 군수용의 목적으로 사용될 경우, 정적 및 동적부하상태에서 재료의 균일한 변형이 가장 중요한 특성이다. 현 개발품의 경우, 일반 W 빛 Cu 원료에 비하여 상대적으로 높은 순도의 원료를 사용하였기 때문에 분말 및 소재상태 에서의 순도가 높아서, 연성을 저하시키는 것으로 알려진 기지상내 합금원소 또는 interface 게재물 이 존재할 가능성이 매우 낮다. 또한 초미립 W 입자들과 Cu 상의 혼합도가 극대화된 상태이기 때문에 상대적으로 저옹에서도 완전치밀화된 미세조직을 얻을 수 있는데, 이는 분말상태의 균일한 미세구조를 유지할 수 있으며, 동시에 W 업자간의 과도한 neck 형성을 방지함으로써 기계적 변형시 재료의 연성 향상이 기대된다. 이러한 W/Cu 나노복합분말 소결체의 특성은 균일한 밀도분포와 동시에 과도한 동적 부하상태에서 균일한 변형이 보장되어야만 하는 특정 군수용 목적에 잘 부합하는 것으로 판단된다. 본 고에서는 상기한 W/Cu 나노복함분말을 사용하여 균일한 미세구조를 가지는 완전치밀화된 소결재를 제조하는 과정과 제조된 소결재를 향후 군수용 제품에 척용시키기 위하여 진행된 단조특성에 대한 연구결과틀을 재료의 미세구조척 관점에서 논의하였다.

  • PDF

Effect of Microstructure on the Environmentally Induced Cracking Behavior of Al-Zn-Mg-Cu-Zr Aluminum Alloy

  • Ghosh, Rahul;Venugopal, A.;Pradeep, PI;krishna, L. Rama;Narayanan, P. Ramesh;Pant, Bhanu;Cherian, Roy M
    • Corrosion Science and Technology
    • /
    • 제17권3호
    • /
    • pp.101-108
    • /
    • 2018
  • AA7010 is an Al-Zn-Mg-Cu alloy containing Zr, developed as an alternate to traditional AA7075 alloy owing to their high strength combined with better fracture toughness. It is necessary to improve the corrosion resistance and surface properties of the alloy by incorporating plasma electrolytic oxidation (PEO) method. AA7010-T7452 aluminum alloy has been processed through the forging route with multi-stage working operations, and was coated with $10{\mu}m$ thick $Al_2O_3$ ceramic aluminina coating using the plasma electrolytic oxidation (PEO) method. The corrosion, stress corrosion cracking (SCC) and nano-mechanical behaviours were examined by means of potentiodynamic polarization, slow strain rate test (SSRT) and nano-indentation tests. The results indicated that the additional thermomechanical treatment during the forging process caused a fully recrystallized microstructure, which lead to the poor environmental cracking resistance of the alloy in 3.5% NaCl solution, despite the overaging treatment. Although the fabricated PEO coating improved general corrosion resistance, the brittle nature of the coating did not provide any improvement in SCC resistance of the alloy. However, the hardness and elastic modulus of the coating were significantly higher than the base alloy.

SLM 기술을 이용한 Ti-6Al-4V 합금의 고속 적층 공정 최적화 연구 (Optimization for high speed manufacturing of Ti-6Al-4V alloy by a selective laser melting technique)

  • 이강표;김강민;강석현;한준현;정경환
    • 한국결정성장학회지
    • /
    • 제28권5호
    • /
    • pp.217-221
    • /
    • 2018
  • Selective laser melting(SLM)은 적층 제조 방법 중 하나로서, 분말을 선택적으로 용융하여 기능적이고, 복잡한 형상을 즉각적으로 제작 가능하다는 장점이 있다. Ti-6Al-4V 합금의 경우 높은 융점과 산화문제로 인하여 SLM 공정도입에 어려움을 겪고 있다. 본 연구에서는 SLM 장비를 사용하여 Ti-6Al-4V 파트를 성공적으로 적층하였으며 스캔속도, 레이저 파워의 변수를 조절하여 적층 가능 조건을 도출하였다. 또한 적층 된 Ti-6Al-4V 파트의 형상 정밀도, 면밀도 및 기계적특성 평가를 통하여 일반적으로 사용되는 공정조건(스캔 속도 200~700 mm/s)으로 제작된 제작품 물성치와 비교를 통해 Ti-6Al-4V 합금의 고속 적층 영역에서의 최적 공정을 확립하였다.