Porous ceramics are widely used for applications such as catalysis supports, gas distributors and filters such as DPF. For these purpose, it is important to have proper porosity controlling pore structure while maintaining mechanical and thermal properties. In this work, we have prepared the porous ceramic structures made of reaction bonded silicon nitride with hierarchical pore structures. Uni-directionally aligned pore channels, which are mostly filled with ${\beta}$-Si3N4 whiskers, were achieved by an ice-templating method. The structures of the pore channels and the walls are controllable by the processing conditions, such as solid concentration, freezing rate of the slurry, and additives. We have investigated and characterized the influences of the conditions on the microstructures and the properties, such as porosity, pore size distribution, lamellar thickness, wavelength, and orientations. The compressive strength test and flow test was performed to determine the structural integrity and air permeability.
Kim, Sung-Han;Lee, Sang-Min;Choi, Duk-Hyun;Lee, Kun-Hong;Park, Hyun-Chul;Hwang, Woon-Bong
Advanced Composite Materials
/
제17권2호
/
pp.101-110
/
2008
Metal nanohoneycomb structures were fabricated by E-beam evaporation and a two-step anodization process in phosphoric acid. Their tribological properties of adhesion and friction were investigated by AFM in relation to the pore size of the nanohoneycomb structures. Variations of the adhesive force are not found with pore size, but formation of the pore greatly reduces the adhesive force compared to the absence of pore structure. The coefficient of friction increased nonlinearly with pore size, due to surface undulation around the pore. Tribological properties do not differ greatly between the original nanohoneycomb structure and the metal nanohoneycomb structure.
The transport characteristics of deleterious ions such as chlorides depend on the pore structures of concrete and are the major factors in the durability of concrete structures in subjected to chloride attack such as in marine environments. In this paper, the effect of the pore structure on compressive strength and chloride diffusivity of concrete was investigated. Six types of concretes were tested. The pore volume of concrete containing mineral admixtures increased in the range of 3∼30nm due to micro filling effect of hydrates of the mineral admixtures. There was a good correlation between the median pore diameter, the pore volume above 50nm and compressive strength of concrete, but there was not a significant correlation between the total pore volume and compressive strength. The relationship between compressive strength and chloride diffusivity were not well correlated, however, pore volume above 50nm were closely related to the chloride diffusion coefficient.
This study analyzes the behavior of adhesion and friction according to the pore size of nanohoneycomb structures in atomic force microscope (AFM). Anodic aluminum oxide (AAO) films are fabricated as nanohoneycomb structures. According to the pore diameters of the nanohoneycomb structures, the adhesive forces and the frictional coefficients arc obtained in AFM, and the behaviors are analyzed in the view of the contact area between the sphere particle and nanohoneycomb substrate. The effective Young's moduli of the nanohoneycomb structures are measured from the nanoindentation tests, and the contact areas at zero applied load are calculated by combining the porosity of the nanohoneycomb structures and the contact radius determined from JKR and DMT theory.
다공질 암석의 공극구조는 그 암석의 수리-역학적 거동에 매우 큰 영향을 미친다. 다공질 암석의 공극구조 특성을 표현하는 대표적인 방법은 공극률, 공극크기분포, 방향성 등이 있다. 암석의 유효공극률은 실험적으로 비교적 쉽게 구할 수 있지만, 공극의 크기분포 특성을 파악하는 것은 매우 어려운 실정이다. 본 연구에서는 X-ray CT를 이용하여 대표적 다공질 암석인 베레아 사암의 공극구조 중 공극크기분포를 이미지 기반으로 평가하였다. 공극크기분포 평가를 위해 본 연구에서는 이미지 필터링, 이진화, 골격화 등의 이미지 기반 처리 작업을 수행하였으며, 국부 두께평가 및 star chord를 이용하여 베레아 사암의 공극크기분포를 구하였다. 본 연구에서 제시된 X-ray CT 기반의 공극크기분포 평가방법을 이용하여 향후 다공질 재료의 공극구조 평가에 새롭고 효율적인 방안을 제시하고자 하였다.
In this study, mercury vapor adsorption behaviors for some kinds of porous materials having various pore structures were investigated. The specific surface area and pore structures were studied by BET and D-R plot methods from $N_2$/77 K adsorption isotherms. It was found that the micropore materials (activated carbons, ACs) showed the highest mercury adsorption capacity. In a comparative study of mesoporous materials (SBA-15 and MCM-41), the adsorption capacity of the SBA-15 was higher than that of MCM-41. From the pore structure analysis, it was found that SBA-15 has a higher micropore fraction compared to MCM-41. This result indicates that the mercury vapor adsorptions can be determined by two factors. The first factor is the specific surface area of the adsorbent, and the second is the micropore fraction when the specific surface areas of the adsorbent are similar.
This paper deals with the accumulated damage in concrete structures due to the cyclic freeze-thaw as an environmental load. The cyclic ice body nucleation and growth processes in porous systems are affected by the thermo-physical and mass transport properties, and gradients of temperature and chemical potentials. Furthermore, the diffusivity of deicing chemicals shows significantly higher value under cyclic freeze-thaw conditions. Consequently, the disintegration of concrete structures is aggravated at marine environments, higher altitudes, and northern areas. However, the properties of cyclic freeze-thaw with crack growth and diffusion of chloride ion effects are hard to be identified in tests, and there has been no analytic model for the combined degradations. The main objective is to determine the driving force and evaluate the reduced strength and stiffness by freeze-thaw. For the development of computational model of those coupled deterioration, micro-pore structure characterization, pore pressure based on the thermodynamic equilibrium, time and temperature dependent super-cooling with or without deicing salts, nonlinear-fracture constitutive relation for the evaluation of internal damage, and the effect of entrained air pores (EA) has been modeled numerically. As a result, the amount of ice volume with temperature dependent surface tensions, freezing pressure and resulting deformations, and cycle and temperature dependent pore volume has been calculated and compared with available test results. The developed computational program can be combined with DuCOM, which can calculate the early aged strength, heat of hydration, micro-pore volume, shrinkage, transportation of free water in concrete. Therefore, the developed model can be applied to evaluate those various practical degradation cases as well.
Adsorption process is largely influenced by pore structures of adsorbents and physical properties of adsorbates and adsorbents. The previous studies of this laboratory was focused on the role of pore structures of adsorbents. And we found some pores of adsorbates which have larger pore diameters than the diameter of adsorbate are filled with easily. In this study the effects of physical and chemical properties of adsorbates and adsorbents, such as pore size distribution, vapor pressure on adsorption were investigated more thoroughly at the concentration of adsorbate of 1000 ppm. The adsorption in the pore ranges of $2{\sim}4$ times of adsorbates's diameter could be explained by space filling concept. But there was some condensation phenomena at larger pore ranges. The errors between the adsorbed amount of non-polar adsorbates and the calculated amounts by considering factors were found to be 44.46%, positively, and -142%, negatively. When vapor pressure is considered, the errors between the adsorbed amount of non-polar adsorbates and the calculated amounts were in the range of $1.69%{\sim}32.25%$ positively, and negatively $-1.08%{\sim}-63.10%$.
강한 지진 발생 시 뒤채움내의 과잉간극수압의 증가에 의해 지반이 액상화 되었을 때, 주변의 액상화 지반보다 작은 단위중량을 가진 지중 매설구조물은 부상하는 현상이 발생한다. 뒤채움에서의 과잉간극수압의 증가와 지중 매설 구조물 부상량의 관계를 설명하기 위해 동적 원심모형 실험을 수행되었다. 본 연구에서는, 매설구조물의 부상현상에 영향을 미치는 요인으로써 직접요인과 간접요인이 실험에 고려되었다. 이러한 요인들 중에, 과잉간극수압비의 증가에 영향을 주는 중요한 요인은 직접요인으로써의 지하수위, 뒤채움의 상대밀도, 그리고 입력 지진가속도의 크기이다. 그리고 이 요인들은 지중 매설구조물의 부상량에도 크게 영향을 주는 것으로 나타났다.
암석의 물성을 정확히 예측하기 위해서는 물성에 일차적인 효과를 미치는 공극구조에 대한 이해가 매우 중요하며, 정확한 공극구조와 물성시뮬레이션을 이용한 다양한 물성예측 및 변화양상의 정량적 상관관계는 많은 지구물리분야에 응용할 수 있다. 최근 비파괴 구조해석방법, 특히 X선 토모그래피를 이용한 고분해능 스캔 등이 상용화되고 컴퓨터의 성능이 향상됨에 따라 실제의 공극구조를 이용하여 투수율을 예측하는 연구가 시도되고 있다. 본 연구에서는 이러한 연구를 투수율뿐만 아니라 속도와 전기전도도의 영역으로 확장하려는 시도를 하였다. 하지만 토모그래피 방법에서 발생하는 smoothing 효과에 의해 공극구조가 왜곡되고 계산된 물성에 오차가 발생하여, 영상처리기법(sharpening filtering 및 인공신경망 분류법)을 사용하여 smoothing 효과를 제거하는 방법을 시도하였다. 그 결과 가시적으로 향상된 공극구조를 얻을 수 있었고, 투수율 및 전기전도도의 계산값도 이론적 모델링과 유사한 정도의 정확도를 얻을 수 있었다. 하지만 속도의 경우에는 smoothing 효과의 제거에도 불구하고 오차도 상대적으로 크고 향상정도도 매우 미미하였다. 박편과 토모그래피에서 얻어진 공극구조의 비교 연구를 통하여 본 연구에서 사용된 사암의 경우에는 토모그래피에서 얻어진 해상도가 너무 낮은 것을 확인할 수 있었으며, 이러한 이유로 smoothing 효과가 제거되어도 속도예측의 향상은 그리 크지 않은 것으로 나타났다. 결론적으로 본 연구에서 제시된 방법은 토모그램의 smoothing 효과를 효율적으로 제거하였으며 이는 토모그래피방법으로 공극구조를 획득할 때 유용하게 사용될 것으로 기대된다. 또한 속도예측의 경우 토모그램의 해상도가 매우 중요한 인자로 판명되었으며 투수율 예측에 일반적으로 사용되는 해상도보다 최소 세 배 이상의 높은 해상도가 요구되는 것으로 파악되었다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.